Sn Alloying to Inhibit Hydrogen Evolution of Zn Metal Anode in Rechargeable Aqueous Batteries
Abstract
The detrimental hydrogen evolution side reaction is one of the major issues hindering the commercialization of Zn metal anode in high‐safety and low‐cost rechargeable aqueous batteries. Herein, the authors present a Sn alloying approach to effectively inhibit the hydrogen evolution and dendrite growth of the Zn metal anode. Through in situ monitoring of the hydrogen production during repeated plating/stripping tests, it is quantitatively demonstrated that the hydrogen evolution of alloy electrode with appropriate Sn amount is only half of that of pure Zn electrode. Furthermore, the Sn alloying allows for favorable Zn nucleation sites, lowering the Zn nucleation energy barrier and promoting more uniform Zn deposition. The Zn‐Sn alloy electrode offers much‐improved plating/stripping cycling, that is, over 240 h at 5 mA cm−2 and 35.2% depth of discharge. This work provides a practically viable strategy to stabilize Zn metal electrode in rechargeable aqueous batteries.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
Advancing Lithium Metal Batteries
Liu, B., Zhang, J.-G., & Xu, W. (2018) · Joule · doi:10.1016/j.joule.2018.03.008 · Cited by 1,647
Kang, L., Cui, M., Jiang, F., Gao, Y., Luo, H., Liu, J., Liang, W., & Zhi, C. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201801090 · Cited by 1,245
Fluorinated interphase enables reversible aqueous zinc battery chemistries
Cao, L., Li, D., Pollard, T., Deng, T., Zhang, B., Yang, C., Chen, L., Vatamanu, J., Hu, E., Hourwitz, M. J., et al. (2021) · Nature Nanotechnology · doi:10.1038/s41565-021-00905-4 · Cited by 1,188
Dendrites in Zn‐Based Batteries
Yang, Q., Li, Q., Liu, Z., Wang, D., Guo, Y., Li, X., Tang, Y., Li, H., Dong, B., & Zhi, C. (2020) · Advanced Materials · doi:10.1002/adma.202001854 · Cited by 1,181
Defect Graphene as a Trifunctional Catalyst for Electrochemical Reactions
Jia, Y., Zhang, L., Du, A., Gao, G., Chen, J., Yan, X., Brown, C. L., & Yao, X. (2016) · Advanced Materials · doi:10.1002/adma.201602912 · Cited by 1,169
Zeng, Y., Zhang, X., Qin, R., Liu, X., Fang, P., Zheng, D., Tong, Y., & Lu, X. (2019) · Advanced Materials · doi:10.1002/adma.201903675 · Cited by 1,117
Strategies for the Stabilization of Zn Metal Anodes for Zn‐Ion Batteries
Yi, Z., Chen, G., Hou, F., Wang, L., & Liang, J. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202003065 · Cited by 942
Self-citationHao, J., Li, X., Zeng, X., Li, D., Mao, J., & Guo, Z. (2020) · Energy & Environmental Science · doi:10.1039/d0ee02162h · Cited by 840
Self-citationZeng, X., Mao, J., Hao, J., Liu, J., Liu, S., Wang, Z., Wang, Y., Zhang, S., Zheng, T., Liu, J., et al. (2021) · Advanced Materials · doi:10.1002/adma.202007416 · Cited by 796
Self-citationMa, L., Li, Q., Ying, Y., Ma, F., Chen, S., Li, Y., Huang, H., & Zhi, C. (2021) · Advanced Materials · doi:10.1002/adma.202007406 · Cited by 739
Zhao, J., Zhang, J., Yang, W., Chen, B., Zhao, Z., Qiu, H., Dong, S., Zhou, X., Cui, G., & Chen, L. (2019) · Nano Energy · doi:10.1016/j.nanoen.2018.12.086 · Cited by 665
Alleviation of Dendrite Formation on Zinc Anodes via Electrolyte Additives
Guo, X., Zhang, Z., Li, J., Luo, N., Chai, G.-L., Miller, T. S., Lai, F., Shearing, P., Brett, D. J. L., Han, D., et al. (2021) · ACS Energy Letters · doi:10.1021/acsenergylett.0c02371 · Cited by 594
A critical review of cathodes for rechargeable Mg batteries
Mao, M., Gao, T., Hou, S., & Wang, C. (2018) · Chemical Society Reviews · doi:10.1039/c8cs00319j · Cited by 591
Yang, Q., Guo, Y., Yan, B., Wang, C., Liu, Z., Huang, Z., Wang, Y., Li, Y., Li, H., Song, L., et al. (2020) · Advanced Materials · doi:10.1002/adma.202001755 · Cited by 436
Zhang, X., Li, J., Liu, D., Liu, M., Zhou, T., Qi, K., Shi, L., Zhu, Y., & Qian, Y. (2021) · Energy & Environmental Science · doi:10.1039/d0ee03898a · Cited by 400
Hao, J., Long, J., Li, B., Li, X., Zhang, S., Yang, F., Zeng, X., Yang, Z., Pang, W. K., & Guo, Z. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201903605 · Cited by 362
Self-citationDendrite-free Zn anode with dual channel 3D porous frameworks for rechargeable Zn batteries
Guo, W., Cong, Z., Guo, Z., Chang, C., Liang, X., Liu, Y., Hu, W., & Pu, X. (2020) · Energy Storage Materials · doi:10.1016/j.ensm.2020.04.038 · Cited by 357
Self-citationGraphene-Boosted, High-Performance Aqueous Zn-Ion Battery
Shen, C., Li, X., Li, N., Xie, K., Wang, J.-G., Liu, X., & Wei, B. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b07781 · Cited by 352
Stable, high-performance, dendrite-free, seawater-based aqueous batteries
Tian, H., Li, Z., Feng, G., Yang, Z., Fox, D., Wang, M., Zhou, H., Zhai, L., Kushima, A., Du, Y., et al. (2021) · Nature Communications · doi:10.1038/s41467-020-20334-6 · Cited by 316
Li, W., Wang, K., Zhou, M., Zhan, H., Cheng, S., & Jiang, K. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b04085 · Cited by 306
Calendar Life of Zn Batteries Based on Zn Anode with Zn Powder/Current Collector Structure
Li, Q., Wang, Y., Mo, F., Wang, D., Liang, G., Zhao, Y., Yang, Q., Huang, Z., & Zhi, C. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202003931 · Cited by 265
Alloy Anode Materials for Rechargeable Mg Ion Batteries
Niu, J., Zhang, Z., & Aurbach, D. (2020) · Advanced Energy Materials · doi:10.1002/aenm.202000697 · Cited by 254
Dendrites issues and advances in Zn anode for aqueous rechargeable Zn‐based batteries
Li, Q., Zhao, Y., Mo, F., Wang, D., Yang, Q., Huang, Z., Liang, G., Chen, A., & Zhi, C. (2020) · EcoMat · doi:10.1002/eom2.12035 · Cited by 226
Liu, B., Zhang, Y., Wang, Z., Ai, C., Liu, S., Liu, P., Zhong, Y., Lin, S., Deng, S., Liu, Q., et al. (2020) · Advanced Materials · doi:10.1002/adma.202003657 · Cited by 142
Lv, H., Yang, S., Li, C., Han, C., Tang, Y., Li, X., Wang, W., Li, H., & Zhi, C. (2021) · Energy storage materials · doi:10.1016/j.ensm.2021.04.044 · Cited by 123
Gong, D., Wei, C., Liang, Z., & Tang, Y. (2021) · Small Science · doi:10.1002/smsc.202100014 · Cited by 117
High‐Voltage Rechargeable Aqueous Zinc‐Based Batteries: Latest Progress and Future Perspectives
Yu, Y., Xie, J., Zhang, H., Qin, R., Liu, X., & Lu, X. (2021) · Small Science · doi:10.1002/smsc.202000066 · Cited by 91
High capacity Mg batteries based on surface-controlled electrochemical reactions
Wang, L., Vullum, P. E., Asheim, K., Wang, X., Svensson, A. M., & Vullum‐Bruer, F. (2018) · Nano Energy · doi:10.1016/j.nanoen.2018.03.061 · Cited by 47
Self-citation
Cited by
Recent Progress on Zn Anodes for Advanced Aqueous Zinc‐Ion Batteries
Nie, C., Wang, G., Wang, D., Wang, M., Gao, X., Bai, Z., Wang, N., Yang, J., Xing, Z., & Dou, S. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202300606 · Cited by 561
Metadata
- Authors
- Wang, L., Huang, W., Guo, W., Guo, Z. H., Chang, C., Gao, L., & Pu, X.
- Venue
- Advanced Functional Materials
- Publisher
- Wiley
- Published
- 2021-10
- Volume
- 32
- Issue
- 1
- ISSN
- 1616-301X (ISSN-L)
- 1616-3028
- OpenAlex
- W3203284335
- Cited by
- 312
- References
- 29
- FWCI
- 15.84
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.