We have produced three kinds of apatite‐containing glass ceramics of the same chemical composition: MgO (4.6), CaO (44.9), SiO 2 (34.2), P 2 O 5 (16.3), CaF 2 (0.5) (in weight ratio). They contain different crystal combinations and have different mechanical properties. The first glass ceramic (A–;GC) was prepared by heating a glass plate to 870°C. It contains only oxy‐ and fluoroapatite (35 wt%). The second glass ceramic (A–W–GC), and the third (A–W–CP–GC), were prepared by heating glass powder compacts to 1050°C and 1200°C, respectively. A–W–GC contains oxyapatite and fluoroapatite (Ca 10(PO 4)6(O,F 2)) (35 wt%) and β‐wollastonite (40 wt%). A–W–CP–GC contains oxyapatite and fluoroapatite (20 wt%), β‐wollastonite (CaO·SiO 2) (55 wt%), and β‐whitlockite (3CaO·P 2 O 5) (15 wt%). The bending strengths of A–;GC, A–W–GC, and A–W–CP–GC were 88MPa, 178MPa, and 213MPa, respectively, in air. Rectangular ceramic plates (15mm × 10mm × 2mm) were implanted into a rabbit tibia. Ten and 25 weeks after implantation, the segment of tibia with implant was excised for examination. The segment was held by a special jig and the traction breaking load (failure load) was measured by an autograph. A–;GC showed a lower load than A–W–GC and A–W–CP–GC. The loads for A–W–GC and A–W–CP–GC were almost equal. The failure loads did not change significantly between 10 and 25 weeks for any of the materials. The interface was examined by Giemsa surface staining, contact micro‐radiography, and SEM‐EPMA. Giemsa surface staining and CMR revealed direct bonding between the materials and the bone for all the three materials. SEM‐EPMA showed that Si and Mg content decreased, Ca content did not change, and P content increased at the reaction zone between all three glass ceramics and bone. This was observed at 10 weeks, as well as at 25 weeks, after implantation. The reaction zone was narrowest with A–;GC, wider with A–W–GC, and widest with A–W–CP–GC.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cited by
Solutions able to reproduce in vivo surface‐structure changes in bioactive glass‐ceramic A‐W3
Kokubo, T., Kushitani, H., Sakka, S., Kitsugi, T., & Yamamuro, T. (1990) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820240607 · Cited by 3,836
Self-citationBiomaterial-Centered Infection: Microbial Adhesion Versus Tissue Integration
Gristina, A. G. (1987) · Science · doi:10.1126/science.3629258 · Cited by 2,156
Suchanek, W., & Yoshimura, M. (1998) · Journal of Materials Research · doi:10.1557/jmr.1998.0015 · Cited by 2,028
Bioactive glass ceramics: properties and applications
Kokubo, T. (1991) · Biomaterials · doi:10.1016/0142-9612(91)90194-f · Cited by 1,202
Self-citationMechanism of apatite formation on CaO SiO2P2O5 glasses in a simulated body fluid
Ohtsuki, C., Kokubo, T., & Yamamuro, T. (1992) · Journal of Non-Crystalline Solids · doi:10.1016/s0022-3093(05)80556-3 · Cited by 879
Self-citationCa, P‐rich layer formed on high‐strength bioactive glass‐ceramic A‐W
Kokubo, T., Ito, S., Huang, Z. T., Hayashi, T., Sakka, S., Kitsugi, T., & Yamamuro, T. (1990) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820240306 · Cited by 859
Self-citationThe role of hydrated silica, titania, and alumina in inducing apatite on implants
Li, P., Ohtsuki, C., Kokubo, T., Nakanishi, K., Soga, N., & de Groot, K. (1994) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820280103 · Cited by 735
Self-citationBiodegradation and bioresorption of calcium phosphate ceramics
LeGeros, R. Z. (1993) · Clinical Materials · doi:10.1016/0267-6605(93)90049-d · Cited by 647
Apatite Formation Induced by Silica Gel in a Simulated Body Fluid
Li, P., Ohtsuki, C., Kokubo, T., Nakanishi, K., Soga, N., Nakamura, T., & Yamamuro, T. (1992) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1992.tb04470.x · Cited by 517
Self-citationDependence of Apatite Formation on Silica Gel on Its Structure: Effect of Heat Treatment
Cho, S., Nakanishi, K., Kokubo, T., Soga, N., Ohtsuki, C., Nakamura, T., Kitsugi, T., & Yamamuro, T. (1995) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1995.tb08887.x · Cited by 489
Self-citationCalcium orthophosphate-based biocomposites and hybrid biomaterials
Dorozhkin, S. V. (2009) · Journal of Materials Science · doi:10.1007/s10853-008-3124-x · Cited by 300
Growth of continuous bonelike mineral within porous poly(lactide-co-glycolide) scaffoldsin vitro
Murphy, W. L., Kohn, D. H., & Mooney, D. J. (2000) · Journal of Biomedical Materials Research · doi:10.1002/(sici)1097-4636(200004)50:1<50::aid-jbm8>3.0.co;2-f · Cited by 296
Chemical reaction of bioactive glass and glass-ceramics with a simulated body fluid
Kokubo, T., Kushitani, H., Ohtsuki, C., Sakka, S., & Yamamuro, T. (1992) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00705272 · Cited by 269
Self-citationApatite formation on the surface of ceravital‐type glass‐ceramic in the body
Ohtsuki, C., Kushitani, H., Kokubo, T., Kotani, S., & Yamamuro, T. (1991) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820251105 · Cited by 259
Self-citation
Metadata
- Authors
- Kitsugi, T., Yamamuro, T., Nakamura, T., Higashi, S., Kakutani, Y., Hyakuna, K., Ito, S., Kokubo, T., Takagi, M., & Shibuya, T.
- Venue
- Journal of Biomedical Materials Research
- Publisher
- Wiley
- Published
- 1986-11
- Volume
- 20
- Issue
- 9
- Pages
- 1295-1307
- ISSN
- 0021-9304 (ISSN-L)
- 1097-4636
- OpenAlex
- W2047722298
- Cited by
- 178
- References
- 0
- FWCI
- 5.51
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.