Degradation studies of some polyesters and polycarbonates—2. Polylactide: Degradation under isothermal conditions, thermal degradation mechanism and photolysis of the polymer
The DOI matches its Crossref record; 6 of the 6 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“For example, pyrolysis of PLLA at ambient pressure leads to uncontrolled degradation through various non-radical and radical pathways that yield a mixture of products consisted of L-LA, meso-LA, cyclic oligomers, acetaldehyde, acrylic acid, CO, CO2.444- 446”
From Catalysis as an Enabling Science for Sustainable Polymers (2018) · cites this paper as [445]
In the citing paper
“For polyesters and polycarbonates with large polymerization enthalpies, a simple pyrolysis process leads to undesired products.”
From Catalysis as an Enabling Science for Sustainable Polymers (2018) · cites this paper as [445]
In the citing paper
“McNeill and Leiper also proposed that the formation of butane-2,3-dione, another detected byproduct, is likely caused by the radical combination of acetyl radicals from the chain reaction (Fig. 5) [152].”
From Physical and mechanical properties of PLA, and their functions in widespread applications — A comprehensive review (2016) · cites this paper as [152]
In the citing paper
“In contrast, McNeill and Leiper proposed that thermal degradation of PLA is a non-radical, “backbiting” ester interchange reaction involving the -OH chain ends [152].”
From Physical and mechanical properties of PLA, and their functions in widespread applications — A comprehensive review (2016) · cites this paper as [152]
In the citing paper
“Depending on the point in the backbone at which the reaction occurs, the product can be a lactide molecule, an oligomeric ring, or acetaldehyde plus CO (Fig. 5).”
From Physical and mechanical properties of PLA, and their functions in widespread applications — A comprehensive review (2016) · cites this paper as [152]
1 more claim about this paper
Create a free account to see every claim other papers make about this one.
Citations
Cites
The thermal degradation of poly(methyl acrylate). Part II. The mechanism of chain breaking
Cameron, G. G., & Kane, D. R. (1967) · Die Makromolekulare Chemie · doi:10.1002/macp.1967.021090117 · Cited by 59
The thermal degradation of poly(methyl acrylate). III. The mechanism of volatile formation
Cameron, G. G., & Kane, D. R. (1968) · Die Makromolekulare Chemie · doi:10.1002/macp.1968.021130105 · Cited by 44
An improved method for the preparation of monoalkylketens
McCarney, C. C., & Ward, R. S. (1975) · Journal of the Chemical Society Perkin Transactions 1 · doi:10.1039/p19750001600 · Cited by 36
Poly α‐ester degradation studies. V. Thermal degradation of polyglycollide
Cooper, D. R., Sutton, G. J., & Tighe, B. J. (1973) · Journal of Polymer Science Polymer Chemistry Edition · doi:10.1002/pol.1973.170110823 · Cited by 27
Poly‐α‐ester degradation studies. II. Thermal degradation of poly(isopropylidene carboxylate)
Sutton, G. J., Tighe, B. J., & Roberts, M. (1973) · Journal of Polymer Science Polymer Chemistry Edition · doi:10.1002/pol.1973.170110514 · Cited by 12
McNeill, I. C., & Zulfiqar, S. (1985) · Polymer Degradation and Stability · doi:10.1016/0141-3910(85)90027-8 · Cited by 7
Self-citation
Research works printed but not linked: 2
- I. C. McNeill and H. A. Leiper, Polym. Defrad. Stab., in press.
- Lüderwald, 1979, Vol. 2, 77
Cited by
A Literature Review of Poly(Lactic Acid)
Garlotta, D. (2001) · Journal of Polymers and the Environment · doi:10.1023/a:1020200822435 · Cited by 3,707
Farah, S., Anderson, D. G., & Langer, R. (2016) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2016.06.012 · Cited by 3,443
Processing technologies for poly(lactic acid)
Lim, L.-T., Auras, R., & Rubino, M. (2008) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2008.05.004 · Cited by 2,766
An overview of the recent developments in polylactide (PLA) research
Madhavan Nampoothiri, K., Nair, N. R., & John, R. P. (2010) · Bioresource Technology · doi:10.1016/j.biortech.2010.05.092 · Cited by 2,448
“Interestingly, McNeill and Leiper (1985) on the other hand proposed that thermal degradation of PLA is a non-radical, ‘‘backbiting” ester interchange reaction involving the -”
BackgroundProperties of lactic acid based polymers and their correlation with composition
Södergård, A., & Stolt, M. (2002) · Progress in Polymer Science · doi:10.1016/s0079-6700(02)00012-6 · Cited by 1,461
Poly(lactic acid)—Mass production, processing, industrial applications, and end of life
Castro-Aguirre, E., Iñiguez-Franco, F., Samsudin, H., Fang, X., & Auras, R. (2016) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2016.03.010 · Cited by 1,329
Catalysis as an Enabling Science for Sustainable Polymers
Zhang, X., Fevre, M., Jones, G. O., & Waymouth, R. M. (2018) · Chemical Reviews · doi:10.1021/acs.chemrev.7b00329 · Cited by 936
Carrasco, F., Pagès, P., Gámez-Pérez, J., Santana, O. O., & Maspoch, M. L. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.11.045 · Cited by 738
From Lactic Acid to Poly(lactic acid) (PLA): Characterization and Analysis of PLA and Its Precursors
Inkinen, S., Hakkarainen, M., Albertsson, A.-C., & Södergård, A. (2011) · Biomacromolecules · doi:10.1021/bm101302t · Cited by 710
Hong, M., & Chen, E. Y.-X. (2016) · Nature Chemistry · doi:10.1038/nchem.2391 · Cited by 677
Thermal decomposition of biodegradable polyesters—II. Poly(lactic acid)
Kopinke, F.-D., Remmler, M., Mackenzie, K., Möder, M., & Wachsen, O. (1996) · Polymer Degradation and Stability · doi:10.1016/0141-3910(96)00102-4 · Cited by 614
Thermal degradation of poly[(R)-3-hydroxybutyrate], poly[ε-caprolactone], and poly[(S)-lactide]
Aoyagi, Y., Yamashita, K., & Doi, Y. (2002) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(01)00265-8 · Cited by 456
Payne, J., & Jones, M. D. (2021) · ChemSusChem · doi:10.1002/cssc.202100400 · Cited by 426
Analysis, Occurrence, and Degradation of Microplastics in the Aqueous Environment
Klein, S., Dimzon, I. K., Eubeler, J., & Knepper, T. P. (2018) · The Handbook of Environmental Chemistry · doi:10.1007/978-3-319-61615-5_3 · Cited by 308
“Under normal environmental conditions in aquatic systems, the temperature is not high enough to start chemical changes of synthetic polymers; thus, thermal degradation is not significant for freshwaters [58, 59].”
BackgroundHigh Molecular Weight Polylactic Acid Polymers
Hartmann, M. H. (1998) · Biopolymers from Renewable Resources · doi:10.1007/978-3-662-03680-8_15 · Cited by 307
Nanocomposites of PLA and PCL based on montmorillonite and sepiolite
Fukushima, K., Tabuani, D., & Camino, G. (2009) · Materials Science and Engineering: C · doi:10.1016/j.msec.2008.11.005 · Cited by 303
The Chemical Recycling of PLA: A Review
McKeown, P., & Jones, M. D. (2020) · Sustainable Chemistry · doi:10.3390/suschem1010001 · Cited by 294
Enhanced thermal stability of poly(lactide)s in the melt by enantiomeric polymer blending
Tsuji, H., & Fukui, I. (2003) · Polymer · doi:10.1016/s0032-3861(03)00175-7 · Cited by 275
Thermal degradation kinetics of plastics and model selection
Das, P., & Tiwari, P. (2017) · Thermochimica Acta · doi:10.1016/j.tca.2017.06.001 · Cited by 265
Polymer nanocomposites based on silylated-montmorillonite: A review
Bee, S.-L., Abdullah, M. A. A., Bee, S.-T., Sin, L. T., & Rahmat, A. R. (2018) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2018.07.003 · Cited by 263
Witzke, D. R., Narayan, R., & Kolstad, J. J. (1997) · Macromolecules · doi:10.1021/ma970631m · Cited by 263
Polylactic Acid: Synthesis, Properties and Applications
Avérous, L. (2008) · Monomers, Polymers and Composites from Renewable Resources · doi:10.1016/b978-0-08-045316-3.00021-1 · Cited by 258
Zou, H., Yi, C., Wang, L., Liu, H., & Xu, W. (2009) · Journal of Thermal Analysis and Calorimetry · doi:10.1007/s10973-009-0121-5 · Cited by 255
“Therefore, CO2 is one of the main decomposition products, which is attributed to the thermal degradation based upon chain homolysis of PLA [6].”
BackgroundMethodInfluentialThermal degradation of polylactic acid (PLA)/polyhydroxybutyrate (PHB) blends: A systematic review
Kervran, M., Vagner, C., Cochez, M., Ponçot, M., Saeb, M. R., & Vahabi, H. (2022) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2022.109995 · Cited by 239
Towards Controlled Degradation of Poly(lactic) Acid in Technical Applications
Teixeira, S., Eblagon, K. M., Miranda, F., R. Pereira, M. F., & Figueiredo, J. L. (2021) · C · doi:10.3390/c7020042 · Cited by 237
“Due to acrylic acid found in the reaction products, cis-elimination (shown in Figure 6) was also suggested as another reaction pathway [103].”
BackgroundInfluentialZhang, Y., Jing, J., Liu, T., Xi, L., Sai, T., Ran, S., Fang, Z., Huo, S., & Song, P. (2021) · Chemical Engineering Journal · doi:10.1016/j.cej.2021.128493 · Cited by 218
Crystallinity and mechanical properties of optically pure polylactides and their blends
Sarasua, J. R., Arraiza, A. L., Balerdi, P., & Maiza, I. (2005) · Polymer Engineering & Science · doi:10.1002/pen.20331 · Cited by 214
Progress in upcycling polylactic acid waste as an alternative carbon source: A review
Sun, C., Wei, S., Tan, H., Huang, Y., & Zhang, Y. (2022) · Chemical Engineering Journal · doi:10.1016/j.cej.2022.136881 · Cited by 206
Thermal degradation behaviour of poly(lactic acid) stereocomplex
Fan, Y., Nishida, H., Shirai, Y., Tokiwa, Y., & Endo, T. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2004.03.001 · Cited by 199
Oxidative degradation of polylactide (PLA) and its effects on physical and mechanical properties
Rasselet, D., Ruellan, A., Guinault, A., Miquelard-Garnier, G., Sollogoub, C., & Fayolle, B. (2014) · European Polymer Journal · doi:10.1016/j.eurpolymj.2013.10.011 · Cited by 196
TG–FTIR characterization of volatile compounds from flame retardant polyurethane foams materials
Chen, X., Huo, L., Jiao, C., & Li, S. (2013) · Journal of Analytical and Applied Pyrolysis · doi:10.1016/j.jaap.2012.12.017 · Cited by 189
Mofokeng, J. P., & Luyt, A. S. (2015) · Polymer Testing · doi:10.1016/j.polymertesting.2015.05.007 · Cited by 186
Tang, X., Hong, M., Falivene, L., Caporaso, L., Cavallo, L., & Chen, E. Y.-X. (2016) · Journal of the American Chemical Society · doi:10.1021/jacs.6b07974 · Cited by 179
Cuadri, A. A., & Martín-Alfonso, J. E. (2018) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2018.02.011 · Cited by 175
Mechanistic aspects of the thermal degradation of poly(lactic acid) and poly(β-hydroxybutyric acid)
Kopinke, F.-D., & Mackenzie, K. (1997) · Journal of Analytical and Applied Pyrolysis · doi:10.1016/s0165-2370(97)00022-3 · Cited by 176
Effect of tin on poly(l-lactic acid) pyrolysis
Nishida, H., Mori, T., Hoshihara, S., Fan, Y., Shirai, Y., & Endo, T. (2003) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(03)00152-6 · Cited by 176
Zhu, J.-B., & Chen, E. Y.-X. (2015) · Journal of the American Chemical Society · doi:10.1021/jacs.5b08658 · Cited by 173
Thermal decomposition of biodegradable polyesters—I: Poly(β-hydroxybutyric acid)
Kopinke, F.-D., Remmler, M., & Mackenzie, K. (1996) · Polymer Degradation and Stability · doi:10.1016/0141-3910(95)00221-9 · Cited by 170
Fan, Y., Nishida, H., Mori, T., Shirai, Y., & Endo, T. (2004) · Polymer · doi:10.1016/j.polymer.2003.12.058 · Cited by 171
Ceretti, D. V. A., Edeleva, M., Cardon, L., & D’hooge, D. R. (2023) · Molecules · doi:10.3390/molecules28052344 · Cited by 164
Mechanical recycling of polylactide, upgrading trends and combination of valorization techniques
Badia, J. D., & Ribes-Greus, A. (2016) · European Polymer Journal · doi:10.1016/j.eurpolymj.2016.09.005 · Cited by 161
“For example, the intermolecular transesterification occurring during the melt [84], [85] of PLA could be minimized by stabilizers such as 1-4 dianthraquinone [80] or benzoyl peroxide [86].”
BackgroundGogolewski, S., Jovanovic, M., Perren, S. M., Dillon, J. G., & Hughes, M. K. (1993) · Polymer Degradation and Stability · doi:10.1016/0141-3910(93)90137-8 · Cited by 160
Synthesis of polylactides in the presence of co-initiators with different numbers of hydroxyl groups
Korhonen, H., Helminen, A., & Seppälä, J. V. (2001) · Polymer · doi:10.1016/s0032-3861(01)00150-1 · Cited by 160
Thermal degradation of poly-l-lactide—studies on kinetics, modelling and melt stabilisation
Wachsen, O., Platkowski, K., & Reichert, K.-H. (1997) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(96)00226-1 · Cited by 158
Ran, G., Liu, X., Guo, J., Sun, J. C., Li, H., Gu, X., & Zhang, S. (2019) · Composites Part B Engineering · doi:10.1016/j.compositesb.2019.04.033 · Cited by 153
Bio-Based Sustainable Polymers and Materials: From Processing to Biodegradation
Okolie, O., Kumar, A., Edwards, C., Lawton, L., Oke, A., McDonald, S., Thakur, V., & Njuguna, J. (2023) · Journal of Composites Science · doi:10.3390/jcs7060213 · Cited by 129
“Jamshidi et al. [177] and McNeill and Leiper [176] described the necessity of a non-radical destructive ester exchange, which involves terminal hydroxyl groups.”
BackgroundResultInfluentialCornelissen, T., Yperman, J., Reggers, G., Schreurs, S., & Carleer, R. (2007) · Fuel · doi:10.1016/j.fuel.2007.07.019 · Cited by 167
“PLA has already been studied in detail [19-22].”
BackgroundThe Effects of Process Engineering on the Performance of PLA and PHBV Blends
Nanda, M. R., Misra, M., & Mohanty, A. K. (2011) · Macromolecular Materials and Engineering · doi:10.1002/mame.201000417 · Cited by 145
Tsuji, H. (2013) · Bio‐Based Plastics · doi:10.1002/9781118676646.ch8 · Cited by 142
Free radical branching of polylactide by reactive extrusion
Carlson, D., Dúbois, P., Nie, L., & Narayan, R. (1998) · Polymer Engineering and Science · doi:10.1002/pen.10192 · Cited by 141
PLA with Intumescent System Containing Lignin and Ammonium Polyphosphate for Flame Retardant Textile
Cayla, A., Rault, F., Giraud, S., Salaün, F., Fierro, V., & Celzard, A. (2016) · Polymers · doi:10.3390/polym8090331 · Cited by 149
“On the other hand, PLA degradation completely decomposes with no residue in one quick step which starts at 309 °C (5% weight loss) to finish up at 390 °C [40,41].”
BackgroundNanosize and microsize clay effects on the kinetics of the thermal degradation of polylactides
Zhou, Q., & Xanthos, M. (2008) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2008.12.009 · Cited by 151
Biodegradable biopolymers: Real impact to environment pollution
Pinaeva, L. G., & Носков, А. С. (2024) · The Science of The Total Environment · doi:10.1016/j.scitotenv.2024.174445 · Cited by 157
McGuire, T. M., Buchard, A., & Williams, C. (2023) · Journal of the American Chemical Society · doi:10.1021/jacs.3c05863 · Cited by 126
The role of shear and stabilizer on PLA degradation
Oliveira, M., Santos, E., Araújo, A., Fechine, G. J. M., Machado, A. V., & Botelho, G. (2016) · Polymer Testing · doi:10.1016/j.polymertesting.2016.03.005 · Cited by 140
Long-term properties and end-of-life of polymers from renewable resources
Badia-Valiente, J. D., Gil-Castell, O., & Ribes-Greus, A. (2017) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2017.01.002 · Cited by 143
“Transesterification reactions of thermal decomposition of PLA, as adapted from [356].”
MethodPyrolysis kinetics of poly(l-lactide) with carboxyl and calcium salt end structures
Fan, Y., Nishida, H., Hoshihara, S., Shirai, Y., Tokiwa, Y., & Endo, T. (2003) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(02)00374-9 · Cited by 124
“Other reactions, such as cis-elimination and non-selective radical reactions, can also occur competitively [12-14].”
BackgroundStabilization of poly(l-lactide) in the melt
Södergård, A., & Näsman, J. H. (1994) · Polymer Degradation and Stability · doi:10.1016/0141-3910(94)90104-x · Cited by 122
Thermal Degradation of Environmentally Degradable Poly(hydroxyalkanoic acid)s
Abe, H. (2006) · Macromolecular Bioscience · doi:10.1002/mabi.200600070 · Cited by 121
Kinetics of Ring-Opening Polymerization of l,l-Lactide
Yu, Y.-S., Storti, G., & Morbidelli, M. (2011) · Industrial & Engineering Chemistry Research · doi:10.1021/ie200117n · Cited by 106
Li, S., Yuan, H., Yu, T., Yuan, W., & Ren, J. (2009) · Polymers for Advanced Technologies · doi:10.1002/pat.1372 · Cited by 119
The influence of the functional end groups on the properties of polylactide-based materials
Kost, B., Basko, M., Bednarek, M., Socka, M., Kopka, B., Łapienis, G., Biela, T., Kubisa, P., & Brzeziński, M. (2022) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2022.101556 · Cited by 114
Yuzay, I. E., Auras, R., Soto-Valdez, H., & Selke, S. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.05.011 · Cited by 111
An investigation of the synthesis and thermal stability of poly(dl-lactide)
Zhang, X., WYSS, U. P., Pichora, D. R., & Goosen, M. F. A. (1992) · Polymer Bulletin · doi:10.1007/bf00297431 · Cited by 130
Thermal degradation studies of terephthalate polyesters: 1. Poly(alkylene terephthalates)
McNeill, I. C., & Bounekhel, M. (1991) · Polymer Degradation and Stability · doi:10.1016/0141-3910(91)90119-c · Cited by 131
Self-citationSun, C., Li, C., Tan, H., & Zhang, Y. (2019) · Energy Conversion and Management · doi:10.1016/j.enconman.2019.112212 · Cited by 116
Jain, S., Reddy, M. M., Mohanty, A. K., Misra, M., & Ghosh, A. K. (2010) · Macromolecular Materials and Engineering · doi:10.1002/mame.201000063 · Cited by 110
Analysis of the Degradation During Melt Processing of PLA/Biosilicate® Composites
Backes, E. H., Pires, L., Costa, L., Passador, F. R., & Pessan, L. A. (2019) · Journal of Composites Science · doi:10.3390/jcs3020052 · Cited by 121
“The reactions involved during 152 the thermal degradation of PLA are non-radical, backbiting ester interchange, cis-elimination and 153 they are dependent of the hydroxyl groups at end of PLA chain [14].”
BackgroundThermal decomposition of poly(1,4-dioxan-2-one)
Nishida, H., Yamashita, M., Hattori, N., Endo, T., & Tokiwa, Y. (2000) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(00)00145-2 · Cited by 111
Abe, H., Takahashi, N., Kim, K. J., Mochizuki, M., & Doi, Y. (2004) · Biomacromolecules · doi:10.1021/bm0497872 · Cited by 106
Vogel, C., & Siesler, H. W. (2008) · Macromolecular Symposia · doi:10.1002/masy.200850520 · Cited by 123
Thermal stability of poly (l-lactide): influence of end protection by acetyl group
Fan, Y., Nishida, H., Shirai, Y., & Endo, T. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2003.10.004 · Cited by 104
“Many factors have been reported as affecting the thermal stability of PLLA, including moisture, molecular weight, residual monomers, and metal catalysts [8-14].”
BackgroundPreparation, characterization and biodegradation of biopolymer nanocomposites based on fumed silica
Fukushima, K., Tabuani, D., Abbate, C., Arena, M., & Rizzarelli, P. (2010) · European Polymer Journal · doi:10.1016/j.eurpolymj.2010.10.027 · Cited by 114
Wachsen, O., Reichert, K. H., Krüger, R., Much, H., & Schulz, G. (1997) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(96)00127-9 · Cited by 122
Kontou, E., Niaounakis, M., & Georgiopoulos, P. (2011) · Journal of Applied Polymer Science · doi:10.1002/app.34234 · Cited by 105
Poly(Ethylene Glycol) as a Compatibilizer for Poly(Lactic Acid)/Thermoplastic Starch Blends
Ferrarezi, M. M. F., Taipina, M. D. O., da Silva, L. C. E., & Gonçalves, M. (2013) · Journal of Polymers and the Environment · doi:10.1007/s10924-012-0480-z · Cited by 92
Effects of MgO catalyst on depolymerization of poly-l-lactic acid to l,l-lactide
Motoyama, T., Tsukegi, T., Shirai, Y., Nishida, H., & Endo, T. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.03.014 · Cited by 96
“many kinds of degradation products have been detected during the pyrolysis of PLLA [16,19],”
BackgroundThermal stability of poly(lactic acid) before and after γ-radiolysis
Babanalbandi, A., Hill, D. J. T., Hunter, D. S., & Kettle, L. (1999) · Polymer International · doi:10.1002/(sici)1097-0126(199910)48:10<980::aid-pi257>3.0.co;2-b · Cited by 90
Graphite Modified Polylactide (PLA) for 3D Printed (FDM/FFF) Sliding Elements
Przekop, R., Kujawa, M., Pawlak, W., Dobrosielska, M., Sztorch, B., & Wieleba, W. (2020) · Polymers · doi:10.3390/polym12061250 · Cited by 83
“The first follows the McNeill and Leiper mechanism [38].”
BackgroundBiodegradable Polymers for Orthopedic Applications
Zhang, X., Mattheus, Goosen, F. A., Wyss, S. P., & Pichora, D. (1993) · Journal of Macromolecular Science, Part C: Polymer Reviews · doi:10.1080/15321799308021434 · Cited by 88
Racemization behavior of l,l-lactide during heating
Tsukegi, T., Motoyama, T., Shirai, Y., Nishida, H., & Endo, T. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.01.009 · Cited by 85
“The activation energy, Ea, of degradation has also been reported to change irregularly in a range of 70-270 kJ·mol as degradation progresses [16-18], and many kinds of degradation products have been detected during the pyrolysis of PLLA [16,19], especially cyclic oligomers and their diastereoisomers.”
BackgroundMarec, P. E. L., Ferry, L., Quantin, J.-C., Bénézet, J., Bonfils, F., Guilbert, S., & Bergeret, A. (2014) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2014.10.003 · Cited by 93
Gorrasi, G., Milone, C., Piperopoulos, E., Lanza, M., & Sorrentino, A. (2012) · Applied Clay Science · doi:10.1016/j.clay.2012.11.004 · Cited by 86
Thermal degradation characteristics of flame retardant polylactide using TG-IR
Chen, X., Zhuo, J., & Jiao, C. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.08.016 · Cited by 84
Song, L., Xuan, S., Wang, X., & Hu, Y. Z. (2011) · Thermochimica Acta · doi:10.1016/j.tca.2011.07.012 · Cited by 86
Badia-Valiente, J. D., Strömberg, E., Ribes-Greus, A., & Karlsson, S. (2011) · European Polymer Journal · doi:10.1016/j.eurpolymj.2011.05.001 · Cited by 90
Effects of processing conditions on mechanical properties of PLA printed parts
Behzadnasab, M., Yousefi, A. A., Ebrahimibagha, D., & Nasiri, F. (2019) · Rapid Prototyping Journal · doi:10.1108/rpj-02-2019-0048 · Cited by 90
Evaluation of hot‐pressed hydroxyapatite/poly‐ L ‐lactide composite biomaterial characteristics
Ignjatović, N. L., Suljovrujić, E. H., Budìnski‐Simendìć, J., Krakovský, I., & Uskokovic, D. P. (2004) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.30093 · Cited by 93
Mofokeng, J. P., & Luyt, A. S. (2015) · Journal of Applied Polymer Science · doi:10.1002/app.42138 · Cited by 87
Study of the thermal stabilization mechanism of biodegradable poly(L‐lactide)/silica nanocomposites
Wen, X., Zhang, K.-Y., Wang, Y., Han, L.-J., Han, C.-Y., Zhang, H.-L., Chen, S., & Dong, L.-S. (2011) · Polymer International · doi:10.1002/pi.2927 · Cited by 72
Poly(lactic acid) stereocomplexes based molecular architectures: Synthesis and crystallization
Michell, R. M., Ladelta, V., Da Silva, E., Müller, A. J., & Hadjichristidis, N. (2023) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2023.101742 · Cited by 77
Enzymatic and Thermal Degradation of Poly(ε-caprolactone), Poly(d,l-lactide), and Their Blends
Sivalingam, G., Vijayalakshmi, S. P., & Madras, G. (2004) · Industrial & Engineering Chemistry Research · doi:10.1021/ie049589r · Cited by 76
Badia-Valiente, J. D., Santonja‐Blasco, L., Moriana, R., & Ribes-Greus, A. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.06.002 · Cited by 80
“Evolved gases in inert atmosphere also contain acetaldehyde, carbon monoxide, carbon dioxide and methylketene, among others [18].”
BackgroundSamsudin, H., Soto‐Valdez, H., & Auras, R. A. (2014) · Food Control · doi:10.1016/j.foodcont.2014.04.045 · Cited by 83
“Even though the occurrence of this phenomenon was reported at an excessive temperature (>270 C) (McNeill & Leiper, 1985), and the maximum processing temperature used in this study was only at 155 C, the presence of additional eOH groups from astaxanthin could be conjectured to cause the chain…”
BackgroundAmorin, N. S. Q. S., da Rosa, G. S., Alves, J. F., Gonçalves, S. P. C., Franchetti, S. M. M., & Fechine, G. J. M. (2013) · Journal of Applied Polymer Science · doi:10.1002/app.40023 · Cited by 81
Biodegradable hollow fibres for the controlled release of hormones
Eenink, M. J. D., Feijén, J., Olijslager, J., Albers, J. H. M., Rieke, J., & Greidanus, P. J. (1987) · Journal of Controlled Release · doi:10.1016/0168-3659(87)90079-4 · Cited by 87
Depolymerization of End‐of‐Life Poly(lactide) to Lactide via Zinc‐Catalysis
Alberti, C., & Enthaler, S. (2020) · ChemistrySelect · doi:10.1002/slct.202003979 · Cited by 86
Racemization on thermal degradation of poly(l-lactide) with calcium salt end structure
Fan, Y., Nishida, H., Shirai, Y., & Endo, T. (2003) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(03)00033-8 · Cited by 86
“Several groups [10-19] have studied the thermal degradation of PLLA using thermogravimetric analysis-differential thermal analysis (TG/DTA), pyrolysis-mass spectrometry (Py-MS), pyrolysis-gas chromatography-mass spectrometry (Py-GC/MS), and isothermal methods.”
MethodControl of racemization for feedstock recycling of PLLA
Fan, Y., Nishida, H., Shirai, Y., & Endo, T. (2003) · Green Chem. · doi:10.1039/b304792j · Cited by 71
Zembouai, I., Bruzaud, S., Kaci, M., Benhamida, A., Corre, Y., Grohens, Y., Taguet, A., & Lopez‐Cuesta, J. (2013) · Journal of Polymers and the Environment · doi:10.1007/s10924-013-0626-7 · Cited by 82
Metadata
- Authors
- McNeill, I. C., & Leiper, H. A.
- Affiliations
- University of Glasgow (GB)
- Venue
- Polymer Degradation and Stability
- Publisher
- Elsevier BV
- Published
- 1985-01
- Volume
- 11
- Issue
- 4
- Pages
- 309-326
- ISSN
- 0141-3910 (ISSN-L)
- OpenAlex
- W2068442209
- Cited by
- 404
- References
- 6
- Citations by year
- 2026: 14 · 2025: 16 · 2024: 20 · 2023: 17 · 2022: 26 · 2021: 13 · 2020: 15 · 2019: 11 · 2018: 18 · 2017: 15 · 2016: 27 · 2015: 18 · 2014: 25 · 2013: 19 · 2012: 19
- FWCI
- 2.32
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- Polymer Degradation and Stability (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer Science and PVC
- Physical Sciences › Materials Science › Materials Chemistry › Thermal and Kinetic Analysis
- Keywords
- polylactic acid, thermal degradation, isothermal degradation, degradation mechanism, activation energy, lactide, cyclic oligomers, ester interchange, photolysis, polycarbonate, polyesters
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).