Stabilization of poly(l-lactide) in the melt
The DOI matches its Crossref record; 11 of the 11 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Thermal characterization of polylactides
Jamshidi, K., Hyon, S.-H., & Ikada, Y. (1988) · Polymer · doi:10.1016/0032-3861(88)90116-4 · Cited by 692
McNeill, I. C., & Leiper, H. A. (1985) · Polymer Degradation and Stability · doi:10.1016/0141-3910(85)90035-7 · Cited by 404
Crystal structure of stereocomplex of poly(L-lactide) and poly(D-lactide)
Okihara, T., Tsuji, M., Kawaguchi, A., Katayama, K.-I., Tsuji, H., Hyon, S.-H., & Ikada, Y. (1991) · Journal of Macromolecular Science, Part B · doi:10.1080/00222349108245788 · Cited by 382
Gogolewski, S., Jovanovic, M., Perren, S. M., Dillon, J. G., & Hughes, M. K. (1993) · Polymer Degradation and Stability · doi:10.1016/0141-3910(93)90137-8 · Cited by 160
Kleine, V. J., & Kleine, H. (1959) · Die Makromolekulare Chemie · doi:10.1002/macp.1959.020300102 · Cited by 151
Gupta, M. C., & Deshmukh, V. G. (1982) · Colloid & Polymer Science · doi:10.1007/bf01452999 · Cited by 139
An investigation of the synthesis and thermal stability of poly(dl-lactide)
Zhang, X., WYSS, U. P., Pichora, D. R., & Goosen, M. F. A. (1992) · Polymer Bulletin · doi:10.1007/bf00297431 · Cited by 130
Gupta, M. C., & Deshmukh, V. G. (1982) · Colloid & Polymer Science · doi:10.1007/bf01447969 · Cited by 110
Injection moulding of biodegradable implants
von Oepen, R., & Michaeli, W. (1992) · Clinical Materials · doi:10.1016/0267-6605(92)90080-d · Cited by 77
Stress relaxation and chemical kinetics in pairwise associating polymers
Cates, M. E. (1988) · Macromolecules · doi:10.1021/ma00179a049 · Cited by 20
Cited by
Farah, S., Anderson, D. G., & Langer, R. (2016) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2016.06.012 · Cited by 3,443
Poly(lactic acid) crystallization
Saeidlou, S., Huneault, M. A., Li, H., & Park, C. B. (2012) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2012.07.005 · Cited by 1,606
Properties of lactic acid based polymers and their correlation with composition
Södergård, A., & Stolt, M. (2002) · Progress in Polymer Science · doi:10.1016/s0079-6700(02)00012-6 · Cited by 1,461
Self-citationPoly(lactic acid)—Mass production, processing, industrial applications, and end of life
Castro-Aguirre, E., Iñiguez-Franco, F., Samsudin, H., Fang, X., & Auras, R. (2016) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2016.03.010 · Cited by 1,329
Al-Itry, R., Lamnawar, K., & Maazouz, A. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.06.028 · Cited by 906
Naser, A. Z., Deiab, I., & Darras, B. M. (2021) · RSC Advances · doi:10.1039/d1ra02390j · Cited by 836
Carrasco, F., Pagès, P., Gámez-Pérez, J., Santana, O. O., & Maspoch, M. L. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.11.045 · Cited by 738
Thermal degradation of poly[(R)-3-hydroxybutyrate], poly[ε-caprolactone], and poly[(S)-lactide]
Aoyagi, Y., Yamashita, K., & Doi, Y. (2002) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(01)00265-8 · Cited by 456
Fukushima, K., & Kimura, Y. (2006) · Polymer International · doi:10.1002/pi.2010 · Cited by 432
The thermal effects on electrospinning of polylactic acid melts
Zhou, H., Green, T. B., & Joo, Y. L. (2006) · Polymer · doi:10.1016/j.polymer.2006.08.042 · Cited by 399
Melt–solid polycondensation of lactic acid and its biodegradability
Maharana, T., Mohanty, B., & Negi, Y. S. (2009) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2008.10.001 · Cited by 368
Biodegradation of poly(lactic acid) and its nanocomposites
Fukushima, K., Abbate, C., Tabuani, D., Gennari, M., & Camino, G. (2009) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.07.001 · Cited by 368
High Molecular Weight Polylactic Acid Polymers
Hartmann, M. H. (1998) · Biopolymers from Renewable Resources · doi:10.1007/978-3-662-03680-8_15 · Cited by 307
Enhanced thermal stability of poly(lactide)s in the melt by enantiomeric polymer blending
Tsuji, H., & Fukui, I. (2003) · Polymer · doi:10.1016/s0032-3861(03)00175-7 · Cited by 275
Recent Advances in Reactive Extrusion Processing of Biodegradable Polymer‐Based Compositions
Raquez, J., Narayan, R., & Dubois, P. (2008) · Macromolecular Materials and Engineering · doi:10.1002/mame.200700395 · Cited by 251
Thermal degradation behaviour of poly(lactic acid) stereocomplex
Fan, Y., Nishida, H., Shirai, Y., Tokiwa, Y., & Endo, T. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2004.03.001 · Cited by 199
Hydrolysis and Biodegradation of Poly(lactic acid)
Gorrasi, G., & Pantani, R. (2017) · Advances in Polymer Science · doi:10.1007/12_2016_12 · Cited by 181
“Benzoyl peroxide was found to stabilize the polymer against thermal degradation by deactivating the catalyst residues for PLLA prepared by ring-opening polymerization in the melt using stannous octoate as catalyst [33].”
MethodOjijo, V., & Ray, S. S. (2015) · Polymer · doi:10.1016/j.polymer.2015.10.038 · Cited by 179
Effect of tin on poly(l-lactic acid) pyrolysis
Nishida, H., Mori, T., Hoshihara, S., Fan, Y., Shirai, Y., & Endo, T. (2003) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(03)00152-6 · Cited by 176
Filling of poly(lactic acid) with native starch
Jacobsen, S., & Fritz, H. G. (1996) · Polymer Engineering & Science · doi:10.1002/pen.10680 · Cited by 162
Mechanical recycling of polylactide, upgrading trends and combination of valorization techniques
Badia, J. D., & Ribes-Greus, A. (2016) · European Polymer Journal · doi:10.1016/j.eurpolymj.2016.09.005 · Cited by 161
“For example, the intermolecular transesterification occurring during the melt [84], [85] of PLA could be minimized by stabilizers such as 1-4 dianthraquinone [80] or benzoyl peroxide [86].”
BackgroundThermal degradation of poly-l-lactide—studies on kinetics, modelling and melt stabilisation
Wachsen, O., Platkowski, K., & Reichert, K.-H. (1997) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(96)00226-1 · Cited by 158
Davachi, S. M., & Kaffashi, B. (2015) · Polymer-Plastics Technology and Engineering · doi:10.1080/03602559.2014.979507 · Cited by 156
“The melt enthalpy (▵Hm) for PLA with 100% crystallinity has been reported 93–148 J/g([49]).”
BackgroundWang, Y., Steinhoff, B., Brinkmann, C., & Alig, I. (2008) · Polymer · doi:10.1016/j.polymer.2008.01.010 · Cited by 154
Free radical branching of polylactide by reactive extrusion
Carlson, D., Dúbois, P., Nie, L., & Narayan, R. (1998) · Polymer Engineering and Science · doi:10.1002/pen.10192 · Cited by 141
Kinetics of Ring-Opening Polymerization of l,l-Lactide
Yu, Y.-S., Storti, G., & Morbidelli, M. (2011) · Industrial & Engineering Chemistry Research · doi:10.1021/ie200117n · Cited by 106
Reactive Compatibilization of Poly(l-lactide) and Conjugated Soybean Oil
Gramlich, W. M., Robertson, M. L., & Hillmyer, M. A. (2010) · Macromolecules · doi:10.1021/ma902449x · Cited by 116
The influence of the functional end groups on the properties of polylactide-based materials
Kost, B., Basko, M., Bednarek, M., Socka, M., Kopka, B., Łapienis, G., Biela, T., Kubisa, P., & Brzeziński, M. (2022) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2022.101556 · Cited by 114
Influence of melting conditions on the thermal behaviour of poly(l-lactic acid)
Wang, Y., & Mano, J. F. (2005) · European Polymer Journal · doi:10.1016/j.eurpolymj.2005.04.030 · Cited by 113
In vitro cell response to differences in poly-L-lactide crystallinity
Park, A., & Griffith, L. G. (1996) · Journal of Biomedical Materials Research · doi:10.1002/jbm.1996.820310102 · Cited by 123
New developments on the ring opening polymerisation of polylactide
Jacobsen, S., Fritz, H. ‐., Degée, P., Dúbois, P., & Jérôme, R. (2000) · Industrial Crops and Products · doi:10.1016/s0926-6690(99)00053-9 · Cited by 112
Thermal stability of poly (l-lactide): influence of end protection by acetyl group
Fan, Y., Nishida, H., Shirai, Y., & Endo, T. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2003.10.004 · Cited by 104
“The residual metals, such as Sn and Al, which come from the polymerization catalysts, are understood to greatly decrease the thermal stability of PLLA [11,14-19].”
BackgroundIn vitro cell response to differences in poly-L-lactide crystallinity
Park, A., & Griffith, L. G. (2007) · Journal of Biomedical Materials Research · doi:10.1002/jbm.1996.820310103 · Cited by 104
Khankrua, R., Pivsa‐Art, S., Hamada, H., & Suttiruengwong, S. (2014) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2014.04.019 · Cited by 110
Kanemura, C., Nakashima, S., & Hotta, A. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.03.015 · Cited by 116
Degée, P., Dubois, P., Jacobsen, S., Fritz, H. ‐., & Jérôme, R. (1999) · Journal of Polymer Science Part A: Polymer Chemistry · doi:10.1002/(sici)1099-0518(19990715)37:14<2413::aid-pola15>3.0.co;2-# · Cited by 92
Effect of type of peroxide on cross-linking of poly(l-lactide)
Takamura, M., Nakamura, T., Takahashi, T., & Koyama, K. (2008) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2008.07.001 · Cited by 104
New catalysis for fast bulk ring‐opening polymerization of lactide monomers
Degée, P., Dubois, P., Jérǒme, R., Jacobsen, S., & Fritz, H. (1999) · Macromolecular Symposia · doi:10.1002/masy.19991440126 · Cited by 90
Crystallinity Determination of Polylactide by FT-Raman Spectrometry
Qin, D., & Kean, R. T. (1998) · Applied Spectroscopy · doi:10.1366/0003702981943950 · Cited by 82
Lactic acid based polymers as hot melt adhesives for packaging applications
Viljanmaa, M., Södergård, A., & Törmälä, P. O. (2002) · International Journal of Adhesion and Adhesives · doi:10.1016/s0143-7496(01)00057-4 · Cited by 76
Self-citationPolylactides ‐ degradable polymers for fibres and films
Meinander, K., Niemi, M., Hakola, J. S., & Selin, J. (1997) · Macromolecular Symposia · doi:10.1002/masy.19971230115 · Cited by 63
Melt Stability Study of Various Types of Poly( l -lactide)
Södergård, A., & Näsman, J. H. (1996) · Industrial & Engineering Chemistry Research · doi:10.1021/ie950338f · Cited by 62
Self-citationBiodegradable Polyesters from Renewable Resources
Tsui, A., Wright, Z. C., & Frank, C. W. (2013) · Annual Review of Chemical and Biomolecular Engineering · doi:10.1146/annurev-chembioeng-061312-103323 · Cited by 68
Hydrolytic degradation of peroxide modified poly(L-lactide)
Södergård, A., Selin, J., & Näsman, J. H. (1996) · Polymer Degradation and Stability · doi:10.1016/0141-3910(95)00271-5 · Cited by 59
Self-citationThermal properties of poly(l-lactide)/olive stone flour composites
Perinović, S., Andričić, B., & Erceg, M. (2010) · Thermochimica Acta · doi:10.1016/j.tca.2010.07.002 · Cited by 63
Tsuji, H., Fukui, I., Daimon, H., & Fujie, K. (2003) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(03)00150-2 · Cited by 64
Rosli, N. A., Ahmad, I. B., Anuar, F. H., & Abdullah, I. (2018) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2018.07.119 · Cited by 55
New Polylactide-Based Materials by Chemical Crosslinking of PLA
Bednarek, M., Borská, K., & Kubisa, P. (2020) · Journal of macromolecular science. Part C, Reviews in macromolecular chemistry and physics/Journal of macromolecular science. Reviews in macromolecular chemistry and physics · doi:10.1080/15583724.2020.1855194 · Cited by 53
“Sodergard([14]) studied the thermal degradation of PLLA (at 180–220 C) during mixing in the rheometer in order to develop the stabilizer.”
BackgroundMethodDegée, P., Dubois, P., & Jérôme, R. (1997) · Macromolecular Chemistry and Physics · doi:10.1002/macp.1997.021980624 · Cited by 47
Chang, B. P., Mohanty, A. K., & Misra, M. (2018) · RSC Advances · doi:10.1039/c8ra05161e · Cited by 45
Heterogeneous ring‐opening polymerization of lactones for biomedical applications
Khan, J. H., Schué, F., & George, G. A. (2009) · Polymer International · doi:10.1002/pi.2531 · Cited by 41
D’Antone, S., Bignotti, F., Sartore, L., D’Amore, A., Spagnoli, G., & Penco, M. (2001) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(01)00110-0 · Cited by 42
Polymers from Renewable Resources
Chiellini, E., Chiellini, E., & Cinelli, P. (2002) · Springer eBooks · doi:10.1007/978-94-017-1217-0_7 · Cited by 46
Rheological Behavior and Modeling of Thermal Degradation of Poly(∊-Caprolactone) and Poly(L-Lactide)
Arraiza, A. L., Sarasua, J.-R., Verdu, J., & Colin, X. (2007) · International Polymer Processing · doi:10.3139/217.2067 · Cited by 50
Sustainable Raw Materials in Hot Melt Adhesives: A Review
Vineeth, S. K., & Gadhave, R. V. I. (2020) · Open Journal of Polymer Chemistry · doi:10.4236/ojpchem.2020.103003 · Cited by 59
Niaounakis, M. (2013) · Elsevier eBooks · doi:10.1016/b978-1-4557-3145-9.00003-8 · Cited by 39
稲葉, 千., Maekawa, K., Morisaka, H., Kuroda, K., & Ueda, M. (2009) · Applied Microbiology and Biotechnology · doi:10.1007/s00253-009-1931-x · Cited by 38
“Some researchers studied the thermal stability of polylactic acid (McNeill and Leiper 1984; Jamshidi et al. 1988; Södergård and Näsman 1994; Wachsen et al. 1996).”
BackgroundWang, S., Pang, S., Xu, N., Pan, L., & Lin, Q. (2016) · Journal of Applied Polymer Science · doi:10.1002/app.43424 · Cited by 36
Medical grade polylactide, copolyesters and polydioxanone: Rheological properties and melt stability
Ahlinder, A., Fuoco, T., & Finne‐Wistrand, A. (2018) · Polymer Testing · doi:10.1016/j.polymertesting.2018.10.007 · Cited by 35
Characteristics and Applications of PLA
Domenek, S., & Ducruet, V. (2016) · Wiley eBooks · doi:10.1002/9781119117360.ch6 · Cited by 40
Biobased myo-inositol as nucleator and stabilizer for poly(lactic acid)
Tachibana, Y., Maeda, T., Ito, O., Maeda, Y., & Kunioka, M. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.02.007 · Cited by 36
Takamura, M., Nakamura, T., Kawaguchi, S., Takahashi, T., & Koyama, K. (2010) · Polymer Journal · doi:10.1038/pj.2010.42 · Cited by 30
Characteristics and Applications of Poly(lactide)
Domenek, S., Courgneau, C., & Ducruet, V. (2011) · Wiley eBooks · doi:10.1002/9781118164792.ch8 · Cited by 41
Poh, P. S. P., Hege, C. S., Chhaya, M. P., Balmayor, E. R., Foehr, P., Burgkart, R., Schantz, J., Schiller, S., Schilling, A. F., & Hutmacher, D. W. (2016) · Polymer International · doi:10.1002/pi.5181 · Cited by 31
Wojtczak, E., Kubisa, P., & Bednarek, M. (2018) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2018.03.003 · Cited by 28
Nishida, H. (2010) · Wiley eBooks · doi:10.1002/9780470649848.ch23 · Cited by 27
Gorrasi, G., Meduri, A., Rizzarelli, P., Carroccio, S. C., Curcuruto, G., Pellecchia, C., & Pappalardo, D. (2016) · Reactive and Functional Polymers · doi:10.1016/j.reactfunctpolym.2016.10.002 · Cited by 26
Tiwary, P., & Kontopoulou, M. (2018) · Journal of Rheology · doi:10.1122/1.5025817 · Cited by 29
Effect of structure modification on rheological properties of biodegradable poly(ester‐urethane)
Helminen, A. O., Kylmä, J., Tuominen, J. U., & Seppälä, J. V. (2000) · Polymer Engineering and Science · doi:10.1002/pen.11297 · Cited by 25
Bayart, M., Foruzanmehr, M. R., Vuillaume, P. Y., Ovlaque, P., Robert, M., & Elkoun, S. (2021) · Composite Interfaces · doi:10.1080/09276440.2021.1884470 · Cited by 25
“PLA mostly crystallizes into two crystalline forms, named α and α̍, from melt state or solution [15].”
BackgroundTakamura, M., Sugimoto, M., Kawaguchi, S., Takahashi, T., & Koyama, K. (2011) · Journal of Applied Polymer Science · doi:10.1002/app.34618 · Cited by 25
Influence of catalysts used in synthesis of poly(p-dioxanone) on its thermal degradation behaviors
Li, X., Zhou, Q., Wen, Z., Yan, H., Yang, K., & Wang, Y. (2015) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2015.09.016 · Cited by 25
Yang, J., Nie, S., & Zhu, J. (2016) · Journal of Applied Polymer Science · doi:10.1002/app.43340 · Cited by 21
Recycling and revalorization of PLA and PHA-based food packaging waste: A review
Jannatiha, N., & Gutiérrez, T. J. (2025) · Sustainable materials and technologies · doi:10.1016/j.susmat.2025.e01364 · Cited by 33
Polylactide: from Synthesis and Modification to Final Properties
Aniśko, J., & Barczewski, M. (2021) · Advances in Science and Technology – Research Journal · doi:10.12913/22998624/137960 · Cited by 19
“One of the mechanisms of thermal degradation, i.e., intermolecular transesterification, can be minimized by adding benzoyl peroxide [19], 1,4-dianthraqui-none [20], and other stabilizers [9, 14, 17, 18].”
Rheological and Thermal Properties of Peroxide-Modified Poly(l-lactide)s for Blending Purposes
Khajeheian, M., & Rosling, A. (2014) · Journal of Polymers and the Environment · doi:10.1007/s10924-014-0693-4 · Cited by 19
Hydrolytic and environmental degradation of lactic acid based hot melt adhesives
Viljanmaa, M., Södergård, A., Mattila, R., & Törmälä, P. O. (2002) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(02)00171-4 · Cited by 20
Self-citationEnhanced thermal stability of poly(1,4-dioxan-2-one) in melt by adding a chelator
Ding, S., & Wang, Y. (2006) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2006.03.007 · Cited by 19
Arrieta, M. P., Peltzer, M. A., López, J., & Peponi, L. (2017) · Springer eBooks · doi:10.1007/978-3-319-61288-1_11 · Cited by 23
Poly(vinyl alcohol)‐g‐lactic acid copolymers and films with silver nanoparticles
Tudorachi, N., & Lipşa, R. (2011) · Journal of Applied Polymer Science · doi:10.1002/app.34241 · Cited by 19
Reactive extrusion of poly( L ‐lactic acid) with glycidol
Deenadayalan, E., Lele, A. K., & Balasubramanian, M. (2009) · Journal of Applied Polymer Science · doi:10.1002/app.29581 · Cited by 18
Wang, Y., Liu, X., Zhu, C., Parsons, A. J., Liu, J., Huang, S., Ahmed, I., Rudd, C. D., & Sharmin, N. (2019) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2019.07.017 · Cited by 18
“This rapid loss of molecular weight was responsible for the reduction of the polymer properties (Taubner and Shishoo, 2001; Yu et al., 2010; Södergård and Näsman, 1994).”
BackgroundHierarchical structures in poly(lactic acid)/poly(ethylene glycol) blends
Tien, N.-D., & Sakurai, S. (2017) · European Polymer Journal · doi:10.1016/j.eurpolymj.2017.02.012 · Cited by 16
Perspectives on Modification of Aliphatic Polyesters by Radiation Processing
Södergård, A. (2004) · Journal of Bioactive and Compatible Polymers · doi:10.1177/0883911504048376 · Cited by 19
Self-citationThe effects on thermal stability of polyglycolic acid by adding dihydrazide metal chelators
Cui, A., Xue, S., He, M., Xin, J., & Chen, Q. (2017) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2017.01.016 · Cited by 14
Mamiński, M., Novák, I., Mičušík, M., Małolepszy, A., & Toczyłowska‐Mamińska, R. (2021) · Materials · doi:10.3390/ma14133672 · Cited by 14
Enhancing the thermo‐oxidative stability of PLA through the use of hybrid organic–inorganic coatings
Toselli, M., & Saccani, A. (2016) · Journal of Applied Polymer Science · doi:10.1002/app.43897 · Cited by 13
Crystallization kinetics of chain extended poly(L-lactide)s having different molecular structures
Yousefzade, O., Jeddi, J., Franco, L., Puiggalí, J., & Garmabi, H. (2019) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2019.122217 · Cited by 17
Hydrogen Peroxide-Induced Controlled Degradation of Poly(lactic acid) for Melt-Blown Nonwovens
Binley, G., Jubinville, D., Prince, E., & Mekonnen, T. H. (2024) · ACS Applied Polymer Materials · doi:10.1021/acsapm.4c02897 · Cited by 12
Palm oil deodorizer distillate as toughening agent in polylactide packaging films
Ruellan, A., Ducruet, V., Gratia, A., Jimenez, L. S., Guinault, A., Sollogoub, C., Chollet, G., & Domenek, S. (2016) · Polymer International · doi:10.1002/pi.5114 · Cited by 13
Hwang, S. W., Jung, W. S., Kim, D. Y., & Seo, K. H. (2021) · Journal of Polymers and the Environment · doi:10.1007/s10924-021-02174-7 · Cited by 12
“Another limitation of the PLA is its low melt viscosity, which limits its blow molding or foaming processability [9].”
BackgroundDegradation and Stability of Poly(lactic Acid)
Sin, L. T., Rahmat, A. R., & Rahman, W. A. W. A. (2012) · Elsevier eBooks · doi:10.1016/b978-1-4377-4459-0.00007-x · Cited by 15
Chain linked lactic acid polymers : polymerization and biodegradation studies
Tuominen, J. U. (2003) · Aaltodoc (Aalto University) · Cited by 16
Polylactide-Based Biocomposites
Plackett, D., & Södergård, A. (2005) · CRC Press eBooks · doi:10.1201/9780203508206.ch17 · Cited by 14
Self-citationEffects of side chains in compatibilizers on interfacial adhesion of immiscible PLLA/ABS blends
He, M., Wang, J., Wang, Z., Mo, J., Zhang, J., Xiao-zhen, F., Dong, W., & Li, Y. (2021) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2021.124219 · Cited by 9
Development of Polylactide-Clay Nanocomposites for Food Packaging Applications
Chaloupi, N. N. (2011) · Cited by 9
Degradation and Stability of Poly(Lactic Acid)
Sin, L. T., & Tueen, B. S. (2019) · Elsevier eBooks · doi:10.1016/b978-0-12-814472-5.00007-8 · Cited by 8
Environmental degradation of peroxide modified poly(L-lactide)
Södergård, A., Selin, J., & Pantke, M. (1996) · International Biodeterioration & Biodegradation · doi:10.1016/s0964-8305(96)00031-5 · Cited by 7
Self-citationGeneral Methodology for Chemical Synthesis of Polyesters
Seppälä, J. V., Korhonen, H., Kylmä, J., & Tuominen, J. U. (2002) · Wiley eBooks · doi:10.1002/3527600035.bpol3b11 · Cited by 10
Darie-Niță, R. N., Munteanu, B. S., Tudorachi, N., Lipşa, R., Stoleru, E., Spiridon, I., & Vasile, C. (2016) · Bioinspired Biomimetic and Nanobiomaterials · doi:10.1680/jbibn.15.00011 · Cited by 6
Metadata
- Authors
- Södergård, A., & Näsman, J. H.
- Affiliations
- Åbo Akademi University (FI)
- Corresponding author
- Näsman, J.H.
- Venue
- Polymer Degradation and Stability
- Publisher
- Elsevier BV
- Published
- 1994-01
- Volume
- 46
- Issue
- 1
- Pages
- 25-30
- ISSN
- 0141-3910 (ISSN-L)
- OpenAlex
- W2088197369
- Semantic Scholar
- 541bbac9f1227952af3d86ba62bb2d66a9ad3a3f
- Cited by
- 122
- References
- 11
- Citations by year
- 2026: 1 · 2025: 1 · 2024: 2 · 2023: 1 · 2022: 4 · 2021: 6 · 2020: 2 · 2019: 3 · 2018: 6 · 2017: 5 · 2016: 15 · 2015: 5 · 2014: 3 · 2013: 2 · 2012: 4
- FWCI
- 2.66
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- Polymer Degradation and Stability (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer Science and PVC
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer crystallization and properties
- Keywords
- poly(L-lactic acid), thermal degradation, polymer stabilization, benzoyl peroxide, depolymerization, oxidative degradation, main chain scission, melt viscosity, catalyst residues, melting point depression
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.