High temperature annealing of ion irradiated tungsten
Open accessThe DOI matches its Crossref record; 20 of the 20 references it cites were found in a registry or an index.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Hirth, J. P., & Lothe, J. (1968) · Medical Entomology and Zoology · Cited by 9,770
Electron Microscopy of Thin Crystals
(1963) · Nature · doi:10.1038/197438d0 · Cited by 3,989 · cited 1×
“2nm for a g=(200) condition at 200kV [43]).”
BackgroundElectron microscopy of thin crystals
Cahn, B. W. (1967) · Journal of Nuclear Materials · doi:10.1016/0022-3115(67)90194-8 · Cited by 947
Recent progress in research on tungsten materials for nuclear fusion applications in Europe
Rieth, M., Dudarev, S. L., Gonzalez de Vicente, S. M., Aktaa, J., Ahlgren, T., Antusch, S., Armstrong, D. E. J., Balden, M., Baluc, N., Barthe, M.-F., et al. (2013) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2012.08.018 · Cited by 808 · cited 1×
“Pure tungsten has been chosen as ITER’s PFC material [1], and substantial research is being undertaken internationally to improve its performance (through alloying, tailoring microstructure [2], and compositing), and to understand its fundamental mechanical behaviour [3].”
MethodSelf-citationPlasma facing and high heat flux materials – needs for ITER and beyond
Bolt, H., Barabash, V., Federici, G., Linke, J., Loarte, A., Roth, J., & Kohnosuke, S. A. T. O. (2002) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(02)01175-3 · Cited by 549 · cited 1×
“For fusion-relevant temperatures (from 500-1000◦C [28]), the recovery of defects created by fast neutrons in tungsten has been observed to occur in three major stages (III-V),”
BackgroundMultiscale modeling of crowdion and vacancy defects in body-centered-cubic transition metals
Derlet, P. M., Nguyen-Manh, D., & Dudarev, S. L. (2007) · Physical Review B · doi:10.1103/physrevb.76.054107 · Cited by 505 · cited 1×
“56eV respectively [59], and the vacancy diffusion prefactor is ∼1.”
BackgroundObservation of the One-Dimensional Diffusion of Nanometer-Sized Dislocation Loops
Arakawa, K., Ono, K., Isshiki, M., Mimura, K., Uchikoshi, M., & Mori, H. (2007) · Science · doi:10.1126/science.1145386 · Cited by 360
Self-citationMeechan, C. J., & Brinkman, J. A. (1956) · Physical Review · doi:10.1103/physrev.103.1193 · Cited by 302
Characterisation of Radiation Damage by Transmission Electron Microscopy
Jenkins, M. L., & Kirk, M. A. (2000) · CRC Press eBooks · doi:10.1201/9781420034646 · Cited by 280
Brown, W. K., & Wohletz, K. H. (1995) · Journal of Applied Physics · doi:10.1063/1.360073 · Cited by 266
High-energy collision cascades in tungsten: Dislocation loops structure and clustering scaling laws
Sand, A. E., Dudarev, S. L., & Nordlund, K. (2013) · EPL (Europhysics Letters) · doi:10.1209/0295-5075/103/46003 · Cited by 240
Characterization of Radiation Damage by Transmission Electron Microscopy
Jenkins, M. L., & Kirk, M. A. (2001) · Institute of Physics eBooks · doi:10.1887/075030748x · Cited by 237
Atwani, O. E., Hinks, J. A., Greaves, G., Gonderman, S., Qiu, T., Efe, M., & Allain, J. P. (2014) · Scientific Reports · doi:10.1038/srep04716 · Cited by 224
Quenching and recovery investigations of vacancies in tungsten
Rasch, K.-D., Siegel, R. W., & Schultz, H. (1980) · Philosophical Magazine A · doi:10.1080/01418618008241833 · Cited by 183 · cited 1×
“This explanation was later revised to being due to monovacancy mobility activation [29, 30, 31, 27]; this interpretation is also supported by DFT calculations [32].”
ResultTransmission electron microscope studies of point defect clusters in fcc and bcc metals
Eyre, B. L. (1973) · Journal of Physics F Metal Physics · doi:10.1088/0305-4608/3/2/009 · Cited by 177 · cited 2×
“Such a study has found to be lacking in the literature, with systematic experiments being limited to loops and stacking fault tetrahedra formed during quenching processes of fcc metals [8].”
BackgroundMethodBrittle–ductile transitions in polycrystalline tungsten
Giannattasio, A., Yao, Z., Tarleton, E., & Roberts, S. G. (2010) · The Philosophical Magazine A Journal of Theoretical Experimental and Applied Physics · doi:10.1080/14786435.2010.502145 · Cited by 169 · cited 1×
“A major issue with tungsten is its acute brittleness and high brittle-to-ductile transition temperature (BDTT) of ∼400−500◦C [4, 5, 6], rendered more severe by radiation damage, which immediately creates dislocation loops and other defect structures (SIAs, voids), and in the longer term can produce brittle phases as a…”
BackgroundSelf-citationDensity Functional Theory Models for Radiation Damage
Dudarev, S. L. (2013) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-071312-121626 · Cited by 129
Hardening of self ion implanted tungsten and tungsten 5-wt% rhenium
Armstrong, D. E. J., Yi, X., Marquis, E. A., & Roberts, S. G. (2012) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2012.07.044 · Cited by 128
Self-citationEffects of sequential tungsten and helium ion implantation on nano-indentation hardness of tungsten
Armstrong, D. E. J., Edmondson, P. D., & Roberts, S. G. (2013) · Applied Physics Letters · doi:10.1063/1.4811825 · Cited by 110 · cited 1×
“A major issue with tungsten is its acute brittleness and high brittle-to-ductile transition temperature (BDTT) of ∼400−500◦C [4, 5, 6], rendered more severe by radiation damage, which immediately creates dislocation loops and other defect structures (SIAs, voids), and in the longer term can produce brittle phases as a…”
BackgroundSelf-citationDirect simulation of resistivity recovery experiments in carbon-doped α-iron
Jourdan, T., Fu, C., Joly, L., Bocquet, J. L., Caturla, M. J., & Willaime, F. (2011) · Physica Scripta · doi:10.1088/0031-8949/2011/t145/014049 · Cited by 30
Cited by
Wylie, A. P. C., Woller, K. B., Al Dajani, S. A. A., Dacus, B. R., Pickering, E. J., Preuss, M., & Short, M. P. (2022) · Journal of Applied Physics · doi:10.1063/5.0089048 · Cited by 22
Metadata
- Authors
- Ferroni, F., Yi, X., Arakawa, K., Fitzgerald, S. P., Edmondson, P. D., & Roberts, S. G.
- Venue
- Acta Materialia
- Publisher
- Elsevier BV
- Published
- 2015-05
- Volume
- 90
- Pages
- 380-393
- ISSN
- 1359-6454 (ISSN-L)
- OpenAlex
- W2024723884
- Cited by
- 221
- References
- 20
- FWCI
- 7.33
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.