Trade-off between fracture resistance and translucency of zirconia and lithium-disilicate glass ceramics for monolithic restorations
Open accessThe DOI matches its Crossref record; 32 of the 32 references it cites were found in a registry or an index.
Abstract
High strength and translucency are generally not coincident in one restorative material and there is still a continuous development for a better balance between these two properties. Zirconia and lithium-disilicate glass-ceramics are currently the most popular alternatives for monolithic restorations. In this work, the mechanical properties and more important, the slow crack growth (SCG) resistance, which rules long-term durability, were thoroughly studied for three zirconia ceramics stabilized by 3, 4 and 5 mol% yttria in comparison to lithium-disilicate glass-ceramic. Translucency versus strength maps revealed that the more translucent zirconia compositions (i.e. with higher yttria contents) fill the gap between the standard 3 mol% yttria stabilized zirconia (3Y-TZP) and lithium-disilicate. Moreover, increasing yttria content did not always result in lower strength, as values for 3 mol% and 4 mol% yttria were the same. Independent on the yttria contents, all zirconia showed similar relative susceptibility to SCG under static and cyclic conditions and were significantly more SCG-resistant than lithium-disilicate glass ceramic. A concern with higher yttria contents (5 and 4 mol%) however could lie in the higher sensitivity to defects, resulting in a larger scatter in strength. STATEMENT OF SIGNIFICANCE: In addition to the common investigations on the generally reported strength, toughness and translucency, V-KI diagrams (crack velocity versus stress-intensity factor) from fast fracture to threshold for three newly developed zirconia were directly measured by double torsion methods under static and cyclic loading conditions. The crack-growth mechanisms were analyzed in depth. Results were compared with another popular dental ceramic, namely lithium-disilicate glass-ceramic, revealing the pros and cons of polycrystalline and glass-ceramics in terms of long-term durability. This is the first time that V-KI curves are compared for the major ceramic and glass-ceramic used for dental restorations. Strength versus translucency maps for different CAD/CAM dental restorative materials were described, showing the current indication range for zirconia ceramics.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
VI. The phenomena of rupture and flow in solids
Griffith, A. A. (1921) · Philosophical Transactions of the Royal Society of London. Series A, Containing Papers of a Mathematical or Physical Character · doi:10.1098/rsta.1921.0006 · Cited by 11,052
Lawn, B. (1993) · Cambridge University Press eBooks · doi:10.1017/cbo9780511623127 · Cited by 4,759
Zirconia as a ceramic biomaterial
Piconi, C., & Maccauro, G. (1999) · Biomaterials · doi:10.1016/s0142-9612(98)00010-6 · Cited by 2,806
Transformation Toughening in Zirconia‐Containing Ceramics
Hannink, R. H. J., Kelly, P., & Muddle, B. C. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01221.x · Cited by 2,268
State of the art of zirconia for dental applications
Denry, I., & Kelly, J. R. (2008) · Dental Materials · doi:10.1016/j.dental.2007.05.007 · Cited by 2,133
The Tetragonal‐Monoclinic Transformation in Zirconia: Lessons Learned and Future Trends
Chevalier, J., Gremillard, L., Virkar, A. V., & Clarke, D. R. (2009) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2009.03278.x · Cited by 1,609
Self-citationInfluence of Water Vapor on Crack Propagation in Soda‐Lime Glass
WIEDERHORN, S. M. (1967) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1967.tb15145.x · Cited by 1,123
Novel Zirconia Materials in Dentistry
Zhang, Y., & Lawn, B. R. (2018) · Journal of Dental Research · doi:10.1177/0022034517737483 · Cited by 998
On the Fracture Toughness of Advanced Materials
Launey, M. E., & Ritchie, R. O. (2009) · Advanced Materials · doi:10.1002/adma.200803322 · Cited by 967
Mechanisms of fatigue-crack propagation in ductile and brittle solids
Ritchie, R. O. (1999) · International Journal of Fracture · doi:10.1023/a:1018655917051 · Cited by 962
Current status of zirconia restoration
Miyazaki, T., Nakamura, T., Matsumura, H., Ban, S., & Kobayashi, T. (2013) · Journal of Prosthodontic Research · doi:10.1016/j.jpor.2013.09.001 · Cited by 894
Kosmač, T., Oblak, C., Jevnikar, P., Funduk, N., & Marion, L. (1999) · Dental Materials · doi:10.1016/s0109-5641(99)00070-6 · Cited by 818
Making yttria-stabilized tetragonal zirconia translucent
Zhang, Y. (2014) · Dental Materials · doi:10.1016/j.dental.2014.08.375 · Cited by 627
De Aza, A. H., Chevalier, J., Fantozzi, G., Schehl, M., & Torrecillas, R. (2002) · Biomaterials · doi:10.1016/s0142-9612(01)00206-x · Cited by 625
Self-citationCeramics: Mechanical properties, failure behaviour, materials selection
(2000) · Annales de Chimie Science des Mat�riaux · doi:10.1016/s0151-9107(00)88627-4 · Cited by 595
Mechanical properties of zirconia reinforced lithium silicate glass-ceramic
Elsaka, S. E., & Elnaghy, A. M. (2016) · Dental Materials · doi:10.1016/j.dental.2016.03.013 · Cited by 483
Strength, toughness and aging stability of highly-translucent Y-TZP ceramics for dental restorations
Zhang, F., Inokoshi, M., Batuk, M., Hadermann, J., Naert, I., Van Meerbeek, B., & Vleugels, J. (2016) · Dental Materials · doi:10.1016/j.dental.2016.09.025 · Cited by 418
Self-citationDanzer, R., Lube, T., Supancic, P., & Damani, R. (2008) · Advanced Engineering Materials · doi:10.1002/adem.200700347 · Cited by 361
Chairside CAD/CAM materials. Part 2: Flexural strength testing
Wendler, M., Belli, R., Petschelt, A., Mevec, D., Harrer, W., Lube, T., Danzer, R., & Lohbauer, U. (2017) · Dental Materials · doi:10.1016/j.dental.2016.10.008 · Cited by 345
A Simple Method for Studying Slow Crack Growth
Williams, D., & Evans, A. (1973) · Journal of Testing and Evaluation · doi:10.1520/jte10015j · Cited by 324
Stawarczyk, B., Liebermann, A., Eichberger, M., & Güth, J.-F. (2016) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2015.10.004 · Cited by 279
In vitro lifetime of dental ceramics under cyclic loading in water
Studart, A. R., Filser, F., Kocher, P., & Gauckler, L. J. (2007) · Biomaterials · doi:10.1016/j.biomaterials.2006.12.033 · Cited by 228
Crystallization toughening of a model glass-ceramic
Serbena, F. C., Mathias, I., Foerster, C. E., & Zanotto, E. D. (2015) · Acta Materialia · doi:10.1016/j.actamat.2014.12.007 · Cited by 222
Recent advances in understanding the fatigue and wear behavior of dental composites and ceramics
Kruzic, J. J., Arsecularatne, J. A., Tanaka, C. B., Hoffman, M., & Cesar, P. F. (2018) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2018.08.008 · Cited by 183
ADM guidance-ceramics: Fatigue principles and testing
Kelly, J. R., Cesar, P. F., Scherrer, S. S., Della Bona, A., van Noort, R., Tholey, M., Vichi, A., & Lohbauer, U. (2017) · Dental Materials · doi:10.1016/j.dental.2017.09.006 · Cited by 175
Makhija, S. K., Lawson, N. C., Gilbert, G. H., Litaker, M. S., McClelland, J. A., Louis, D. R., Gordan, V. V., Pihlstrom, D. J., Meyerowitz, C., Mungia, R., et al. (2016) · Journal of Dentistry · doi:10.1016/j.jdent.2016.09.010 · Cited by 175
Cyclic fatigue in water of veneer–framework composites for all-ceramic dental bridges
Studart, A. R., Filser, F., Kocher, P., Lüthy, H., & Gauckler, L. J. (2006) · Dental Materials · doi:10.1016/j.dental.2006.01.011 · Cited by 127
Zhang, F., Vanmeensel, K., Inokoshi, M., Batuk, M., Hadermann, J., MEERBEEK, B. V., Naert, I. E., & Vleugels, J. (2014) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2014.09.018 · Cited by 120
Self-citationLoad-bearing capacity of lithium disilicate and ultra-translucent zirconias
Yan, J., Kaizer, M. R., & Zhang, Y. (2018) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2018.08.023 · Cited by 113
Effect of the microstructure on the lifetime of dental ceramics
Borba, M., de Araújo, M. D., Fukushima, K. A., Yoshimura, H. N., Cesar, P. F., Griggs, J. A., & Bona, Á. D. (2011) · Dental Materials · doi:10.1016/j.dental.2011.04.003 · Cited by 110
Long‐term strength of ceramics for biomedical applications
Zhang, Y., & Lawn, B. R. (2004) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.20039 · Cited by 102
Shyam, A., & Lara‐Curzio, E. (2006) · Journal of Materials Science · doi:10.1007/s10853-005-5553-0 · Cited by 96
Metadata
- Authors
- Zhang, F., Reveron, H., Spies, B. C., Van Meerbeek, B., & Chevalier, J.
- Venue
- Acta Biomaterialia
- Publisher
- Elsevier BV
- Published
- 2019-06
- Volume
- 91
- Pages
- 24-34
- ISSN
- 1742-7061 (ISSN-L)
- OpenAlex
- W2942146468
- Cited by
- 238
- References
- 32
- FWCI
- 29.31
- Type
- journal article
- Language
- en
- Open access
- bronze
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.