Abstract
Abstract Current research into the causes of macro-cracks in the debinding of light-cured ceramic body is predominantly focused on heating rate and holding time. In this paper, we propose a novel approach to analyze the causes of defects in the ceramic body during the debinding process via the interconnected channels formed in the process of the binder discharged from the inside to the outside. The physical and chemical changes, and related reaction products of the binder were analyzed by the TG-FTIR using a specific resin as the binder in the low temperature debinding stage (200–300 °C) and high temperature debinding stage (300–600 °C). Based on the result, a novel approach is proposed to illustrate the process of the formation of interconnected channels and defects. The samples of green bodies debond at different holding time were analyzed by the SEM and μ-CT. The experimental results prove the formation of interconnected channels, and it is found that the holding temperature of 237 °C is favorable for the formation of the channel and the discharge of the gas products. The defect-free samples after low temperature debinding process were debond in the high temperature debinding process at three different holding temperatures of 360 °C, 430 °C, and 550 °C obtained by analyzing the DTG curve and the absorption curve of CO2 in the infrared spectrum, and samples after high temperature debinding process were analyzed by the SEM and μ-CT. The experimental results show that these holding temperatures favor the stable discharge of CO2 and the binder pyrolysis products from the channels, thereby avoiding cracks due to severe gas expansion. The research results in this paper have important reference value for the preparation of defect-free ceramic samples.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cited by
Additive manufacturing by digital light processing: a review
Chaudhary, R., Fabbri, P., Leoni, E., Mazzanti, F., Akbari, R., & Antonini, C. (2023) · Progress in Additive Manufacturing · doi:10.1007/s40964-022-00336-0 · Cited by 450
The recent development of vat photopolymerization: A review
Zhang, F., Zhu, L., Li, Z., Wang, S., Shi, J., Tang, W., Li, N., & Yang, J. (2021) · Additive Manufacturing · doi:10.1016/j.addma.2021.102423 · Cited by 375
Zhou, S., Liu, G., Wang, C., Zhang, Y., Yan, C., & Shi, Y. (2024) · Materials & Design · doi:10.1016/j.matdes.2024.112632 · Cited by 150
Self-citationGu, Q., Wang, H., Gao, W., Yu, J., & Zhou, X. (2023) · Ceramics International · doi:10.1016/j.ceramint.2023.06.142 · Cited by 78
DLP of Translucent Alumina: In-Depth Investigation on Slurry Development and Debinding Regimes
De Lisi, M., Shu, C., Attia, U. M., & Essa, K. (2023) · Machines · doi:10.3390/machines11030321 · Cited by 16
Metadata
- Authors
- Wang, K., Qiu, M., Jiao, C., Gu, J., Xie, D., Wang, C., Tang, X., Wei, Z., & Shen, L.
- Venue
- Ceramics International
- Publisher
- Elsevier BV
- Published
- 2020-02
- Volume
- 46
- Issue
- 2
- Pages
- 2438-2446
- ISSN
- 0272-8842 (ISSN-L)
- OpenAlex
- W2975186898
- Cited by
- 167
- References
- 0
- FWCI
- 5.27
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Study on defect-free debinding green body of ceramic formed by DLP technology. https://app.cochat.ai/papers/10.1016/j.ceramint.2019.09.237
- The paper
- Wang, K., Qiu, M., Jiao, C., Gu, J., Xie, D., Wang, C., Tang, X., Wei, Z., & Shen, L. (2020). Study on defect-free debinding green body of ceramic formed by DLP technology. Ceramics International. https://doi.org/10.1016/j.ceramint.2019.09.237
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.