Zeta potential, gel formation and compressive strength of low calcium fly ash geopolymers
Open accessThe DOI matches its Crossref record; 31 of the 31 references it cites were found in a registry or an index.
Abstract
A major challenge in the specification of geopolymer mix designs is the variability in the fly ash used and the impact of that variability on the performance of the geopolymer produced. The factors affecting the performance of geopolymers made from a total of five chemically and physically distinct fly ashes are reported. The key factor identified as influencing the strength was the workability, with a flow in the range between 110 ± 5% and 140 ± 5% required for optimal performance. In this flow range, the strength of geopolymer is governed by the specific surface area of precursor fly ash coupled with the quantity of the 10 lm and 20 lm particles. In addition a negative zeta potential of the fly ash was identified as assisting gel formation with the smaller the negative zeta potential of the geopolymer product the more gel formation and high compressive strength observed.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Palomo, A., Grutzeck, M. W., & Blanco, M. T. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(98)00243-9 · Cited by 2,319 · cited 1×
“It is recognised that alkali additions to fly ash can activate this material to set and harden thereby forming an alkali-activated system, widely known as geopolymer [9–11].”
BackgroundIndustrially interesting approaches to “low-CO2” cements
Gartner, E. (2004) · Cement and Concrete Research · doi:10.1016/j.cemconres.2004.01.021 · Cited by 2,016 · cited 1×
“Cement production alone contributes between 4% and 8% of the current anthropogenic carbon dioxide (CO2) emissions worldwide [2–4], with the production of 1 tonne of cement producing from 0.”
BackgroundCosts and carbon emissions for geopolymer pastes in comparison to ordinary portland cement
McLellan, B. C., Williams, R. P., Lay, J., van Riessen, A., & Corder, G. D. (2011) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2011.02.010 · Cited by 1,949 · cited 1×
“The most emphasized advantage of this is the reduction of CO2 emission by 26–45% with the replacement of Portland cement with no adverse economic effects [12–14].”
BackgroundSustainable cement production—present and future
Schneider, M., Romer, M., Tschudin, M., & Bolio, H. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.03.019 · Cited by 1,643
The greening of the concrete industry
Meyer, C. (2009) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2008.12.010 · Cited by 1,548 · cited 1×
“Cement production alone contributes between 4% and 8% of the current anthropogenic carbon dioxide (CO2) emissions worldwide [2–4], with the production of 1 tonne of cement producing from 0.”
BackgroundMechanism of geopolymerization and factors influencing its development: a review
Khale, D., & Chaudhary, R. (2007) · Journal of Materials Science · doi:10.1007/s10853-006-0401-4 · Cited by 1,463 · cited 1×
“Thus, an added benefit is to convert a waste product into a useful by-product, conserving landfills and storage lagoons [16].”
BackgroundHabert, G., d’Espinose de Lacaillerie, J. B., & Roussel, N. (2011) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2011.03.012 · Cited by 1,407 · cited 1×
“The most emphasized advantage of this is the reduction of CO2 emission by 26–45% with the replacement of Portland cement with no adverse economic effects [12–14].”
BackgroundHuntzinger, D. N., & Eatmon, T. D. (2009) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2008.04.007 · Cited by 1,392 · cited 1×
“6 up to1 tonne of CO2, depending on the power plant [5–7].”
BackgroundComposition and microstructure of alkali activated fly ash binder: Effect of the activator
Fernández-Jiménez, A., & Palomo, A. (2005) · Cement and Concrete Research · doi:10.1016/j.cemconres.2005.03.003 · Cited by 1,144 · cited 4×
“Extensive research has been published on the development of fly ash based geopolymer using a wide range of mix designs and activators with distinct variations in compressive strength being noted [11,17–19].”
BackgroundInfluentialResistance of geopolymer materials to acid attack
Bakharev, T. (2005) · Cement and Concrete Research · doi:10.1016/j.cemconres.2004.06.005 · Cited by 1,109 · cited 1×
“The AM is defined as the SiO2 to Na2O ratio in alkali activator solution and the Na2O dosage is described as the percentage of Na2O to fly ash ratio in the alkali activator solution, while previously the activator dosage was considered in terms of the mass ratio of Na to fly ash [25].”
Background
Cited by
Review of leaching behavior of municipal solid waste incineration (MSWI) ash
Luo, H., Cheng, Y., He, D., & Yang, E.-H. (2019) · Science of The Total Environment · doi:10.1016/j.scitotenv.2019.03.004 · Cited by 407
John, S. K., Nadir, Y., & Girija, K. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.122443 · Cited by 290
Comparison of long term performance between alkali activated slag and fly ash geopolymer concretes
Wardhono, A., Gunasekara, C., Law, D. W., & Setunge, S. (2017) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2017.03.153 · Cited by 270
Self-citationChemical Stability and Leaching Behavior of One-Part Geopolymer from Soil and Coal Fly Ash Mixtures
Tigue, A. A. S., Malenab, R. A. J., Dungca, J. R., Yu, D. E. C., & Promentilla, M. A. B. (2018) · Minerals · doi:10.3390/min8090411 · Cited by 67
Metadata
- Authors
- Gunasekara, C., Law, D. W., Setunge, S., & Sanjayan, J. G.
- Venue
- Construction and Building Materials
- Publisher
- Elsevier BV
- Published
- 2015-10
- Volume
- 95
- Pages
- 592-599
- ISSN
- 0950-0618 (ISSN-L)
- OpenAlex
- W1948963376
- Cited by
- 181
- References
- 31
- FWCI
- 20.91
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.