Abstract

The objective of this work was to develop and study new biodegradable thermoplastics with improved mechanical properties for potential use as temporary implantable biomaterials. Linear poloxamer and star-shaped poloxamine have been used as macroinitiators for the ring-opening polymerization (ROP) of lactide to yield high molecular weight PLA-based thermoplastic block copolymers. The influence of the nature of the macroinitiator, PLA crystallinity and initial molecular weight on the copolymers properties was investigated by performing a 7-week degradation test in PBS. The evaluation of water uptakes and molecular weights during the degradation pointed out an early hydrolytic degradation of the 100-kg∙mol(-1) copolymers compared to the 200-kg∙mol(-1) ones (molecular weight decrease of ca. 40% and 20%, respectively). A dramatic loss of tensile mechanical properties was also observed for the 100-kg∙mol(-1) copolymers, whereas the 200-kg∙mol(-1) copolymers showed stable or even slightly improved properties with Young's moduli around 500 MPa and yield strains around 3% to 4%. Finally, the cytocompatibility of the more stable 200 kg∙mol(-1) copolymers was confirmed by murine mesenchymal stem cells (MSCs) culture.

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1016/j.msec.2013.06.001

Cites

Statistics

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

  • For amorphous PLA, there is a period in the earlier stages of degradation during which Young's modulus and tensile strength remain constant before decreasing.

    “However, many authors observed that it exists a period, especially for amorphous PLA, in the earlier stages of degradation, for which Young's modulus and tensile strength remain constant before decreasing (Tsuji, 2002; Karjalainen et al., 1996; Leroy et al., 2013).”

    From Mechanical behaviour׳s evolution of a PLA-b-PEG-b-PLA triblock copolymer during hydrolytic degradation (2016) · cites this paper as Leroy et al., 2013

    Section 3.5 (page unavailable) reports that, for the studied PLA-based copolymers, Young’s modulus stayed stable and stress at failure remained in the same range early in degradation, before mechanical properties decreased. It does not establish that pattern specifically for amorphous PLA; stress at failure also increased slightly during the initial period rather than remaining constant. (LLM, conf=0.86)

    Experimental — accuracy not yet measured
  • The induction period in mass loss is commonly observed during degradation of aliphatic polyesters and is due to the difficulty for degraded chains to diffuse out of the sample.

    “This induction period is commonly observed during the degradation of aliphatic polyesters and is due to the dif fi culty, At fi rst, for the degraded chains to diffuse out of the sample (Leroy et al., 2013; Li et al., 1990).”

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

The citation lists haven’t been fetched yet

References 37 · Cited by 22

Research works printed but not linked: 1

  1. P. Aizawa, G. Karlsson, C. Benemar, V. Segl, K. Martinelle, E. Lindner, R. Smith, Ef- fect of different materials used in bioreactor equipments on cell growth of human embryonic kidney (HEK293) cells cultivated in a protein-free medium cell tech- nology for cell products, Springer, Netherlands, 2007. 459-462.

Authors
Leroy, A., Pinese, C., Bony, C., Garric, X., Noël, D., Nottelet, B., & Coudane, J.
Affiliations
  • Centre National de la Recherche Scientifique (FR)
  • Inserm (FR)
Corresponding author
Nottelet, Benjamin
Venue
Materials Science and Engineering C
Publisher
Elsevier BV
Published
2013-10
Volume
33
Issue
7
Pages
4133-4139
ISSN
0928-4931 (ISSN-L)
OpenAlex
W2006148138
Cited by
22
References
37
Citations by year
2025: 1 · 2022: 1 · 2021: 1 · 2020: 5 · 2019: 3 · 2018: 1 · 2017: 1 · 2016: 7 · 2015: 1
FWCI
1.02
Type
journal article
Language
en
Open access
Locations
  • Materials Science and Engineering C (publishedVersion, other-oa)
  • PubMed (publishedVersion)
  • HAL (submittedVersion, cc-by-nc-nd)
Topics
  • Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
  • Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
  • Physical Sciences › Materials Science › Biomaterials › Magnesium Alloys: Properties and Applications
Keywords
polylactic acid, poloxamer, poloxamine, star block copolymers, linear block copolymers, ring-opening polymerization, macroinitiator, biodegradable thermoplastics, temporary implants, hydrolytic degradation, molecular weight effects, tensile properties, water absorption, cytocompatibility, mesenchymal stem cells
MeSH terms
Animals, Cell Line, Chromatography, Gel, Ethylenediamines, Materials Testing, Microscopy, Fluorescence, Molecular Weight, Polyesters, Polymers, Temperature, Water, Cell Death, Lactic Acid, Poloxamer, Biomedical Technology, Cell Proliferation, Mice, Mechanical Phenomena, Mesenchymal Stem Cells

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review