Abstract
We develop strategies to improve the crystallinity and mechanical properties of PLA, without compromising its hydrolytic degradation behaviour. These include reactive extrusion, and addition of a novel type of cross-linked PLA-based nucleating agent (biofiller, BF). The crystallinity is further increased by annealing at temperatures between 80 and 120 °C. Maximum crystallinities of 55% were achieved in the presence of 7 wt% of the BF at 100 °C. The increases in crystallinity upon annealing translated to a 42% increase in the flexural modulus relative to the base PLA, while impact strength was maintained. Annealing temperatures of 100 °C are optimum, because of thermal degradation taking place above this temperature. Annealing also results in increases in the glass transition temperatures followed by improvements in the heat deflection temperature by as much as 7 °C. The nucleated and annealed PLA degraded to the same extent as the untreated PLA, when subjected to hydrolysis over a 12-week period.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
A Literature Review of Poly(Lactic Acid)
Garlotta, D. (2001) · Journal of Polymers and the Environment · doi:10.1023/a:1020200822435 · Cited by 3,707
An Overview of Polylactides as Packaging Materials
Auras, R., Harte, B., & Selke, S. (2004) · Macromolecular Bioscience · doi:10.1002/mabi.200400043 · Cited by 3,454
Processing technologies for poly(lactic acid)
Lim, L.-T., Auras, R., & Rubino, M. (2008) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2008.05.004 · Cited by 2,766
Poly(lactic acid) modifications
Rasal, R. M., Janorkar, A. V., & Hirt, D. E. (2010) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2009.12.003 · Cited by 2,204
Fischer, E. W., Sterzel, H. J., & Wegner, G. (1973) · Kolloid-Zeitschrift und Zeitschrift für Polymere · doi:10.1007/bf01498927 · Cited by 1,704
Zhang, J., Tashiro, K., Tsuji, H., & Domb, A. J. (2008) · Macromolecules · doi:10.1021/ma0706071 · Cited by 913
Zhang, J., Duan, Y., Sato, H., Tsuji, H., Noda, I., Yan, S., & Ozaki, Y. (2005) · Macromolecules · doi:10.1021/ma051232r · Cited by 893
Pan, P., Kai, W., Zhu, B., Dong, T., & Inoue, Y. (2007) · Macromolecules · doi:10.1021/ma071258d · Cited by 679
Polymorphism and isomorphism in biodegradable polyesters
Pan, P., & Inoue, Y. (2009) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2009.01.003 · Cited by 611
Tsuji, H., & Ikada, Y. (2000) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(99)00111-1 · Cited by 329
Thermal and Rheological Properties of Commercial-Grade Poly(Lactic Acid)s
Dorgan, J. R., Lehermeier, H., & Mang, M. (2000) · Journal of Polymers and the Environment · doi:10.1023/a:1010185910301 · Cited by 294
Enthalpy of melting of α′- and α-crystals of poly(l-lactic acid)
Righetti, M. C., Gazzano, M., Di Lorenzo, M. L., & Androsch, R. (2015) · European Polymer Journal · doi:10.1016/j.eurpolymj.2015.07.024 · Cited by 215
Cited by
Yang, W., Zhou, Q., Pan, W., Zhu, S., Wei, C., Lu, H., Yang, W., & Yuen, A. C. Y. (2023) · Chemical Engineering Journal · doi:10.1016/j.cej.2023.143935 · Cited by 95
Wahbi, M., Wen, Y., Kontopoulou, M., & De France, K. J. (2025) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2025.124471 · Cited by 8
Metadata
- Authors
- Simmons, H., Tiwary, P., Colwell, J. E., & Kontopoulou, M.
- Venue
- Polymer Degradation and Stability
- Publisher
- Elsevier BV
- Published
- 2019-08
- Volume
- 166
- Pages
- 248-257
- ISSN
- 0141-3910 (ISSN-L)
- OpenAlex
- W2948576786
- Cited by
- 190
- References
- 12
- FWCI
- 3.16
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.