Electrochemical study on hot corrosion of Si-modified aluminide coated In-738LC in Na2SO4–20 wt.% NaCl melt at 750 °C
The DOI matches its Crossref record; 6 of the 6 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“However, the dissolution of Al2O3 in the molten salt [121] and the formation of cavities in aluminide coatings during thermal cycling processes [122] can cause spallation and cracks, leading to the failure of aluminide coatings.”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [122]
Citations
Cites
Chemical Reactions Involved in the Initiation of Hot Corrosion of B‐1900 and NASA‐TRW VIA
Fryburg, G. C., Kohl, F. J., Stearns, C. A., & Fielder, W. L. (1982) · Journal of The Electrochemical Society · doi:10.1149/1.2123928 · Cited by 80
Chemical Reactions Involved in the Initiation of Hot Corrosion of IN‐738
Fryburg, G. C., Kohl, F. J., & Stearns, C. A. (1984) · Journal of The Electrochemical Society · doi:10.1149/1.2115455 · Cited by 78
Use of Anodic Polarization in Fused Na2SO4 for Estimating Hot Corrosion Rates
Shores, D. A. (1975) · Corrosion · doi:10.5006/0010-9312-31.12.434 · Cited by 38
An experimental low cost silicon/aluminide high temperature coating for superalloys
Young, S. G., & DEADMORE, D. L. (1980) · Thin Solid Films · doi:10.1016/0040-6090(80)90502-7 · Cited by 28
Swadźba, L. (1994) · Materials science forum · doi:10.4028/www.scientific.net/msf.163-165.619 · Cited by 12
Rapid Evaluation of Corrosion Resistance of Ni-Base Alloys in Molten Salts Using AC Impedance Method
Nishikata, A., Zhang, G., & Tsuru, T. (1997) · Materials Transactions JIM · doi:10.2320/matertrans1989.38.312 · Cited by 5
Self-citation
Research works printed but not linked: 1
- M.C. Meelu et al., US patent no. 6,126,758 (2000)
Cited by
A review on molten sulfate salts induced hot corrosion
Hu, S., Finklea, H., & Liu, X. (2021) · Journal of Materials Science & Technology · doi:10.1016/j.jmst.2021.03.013 · Cited by 183
Oxidation behavior of a single-crystal Ni-base superalloy between 900 and 1000°C in air
Liu, C. T., Ma, J., & Sun, X. (2009) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2009.10.261 · Cited by 137
Influence of micro-structure on corrosion behavior of a Ni-based superalloy in 3.5% NaCl
Liu, L., Li, Y., & Wang, F. (2007) · Electrochimica Acta · doi:10.1016/j.electacta.2007.05.043 · Cited by 133
Preparation and hot corrosion behaviour of a MCrAlY+AlSiY composite coating
Jiang, S. M., Peng, X., Bao, Z. B., Liu, S. C., Wang, Q., Gong, J., & Sun, C. (2008) · Corrosion Science · doi:10.1016/j.corsci.2008.08.018 · Cited by 100
Pei, H., Wen, Z., & Yue, Z. (2017) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2017.02.031 · Cited by 86
Shirvani, K., Firouzi, S., & Rashidghamat, A. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.10.037 · Cited by 83
Self-citationHe, H., Liu, Z., Wang, W., & Zhou, C. (2015) · Corrosion Science · doi:10.1016/j.corsci.2015.08.011 · Cited by 80
Liu, Z., Zhao, X., & Zhou, C. (2014) · Corrosion Science · doi:10.1016/j.corsci.2014.11.043 · Cited by 64
Zhao, X., & Zhou, C. (2014) · Corrosion Science · doi:10.1016/j.corsci.2014.05.018 · Cited by 60
Sun, J., Jiang, S. M., Yu, H., Liu, S. B., Gong, J., & Sun, C. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.02.007 · Cited by 58
Yu, X. H., Song, P. Y., He, X., Khan, A., Huang, T., Li, C., Li, Q., Lü, K., Chen, K., & Lu, J. (2019) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2019.03.165 · Cited by 57
Sun, J., Liu, S. B., Li, W., Yu, H. J., Jiang, S. M., Gong, J., & Sun, C. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.01.014 · Cited by 54
Li, P., Jin, X., Zhao, J., Lu, P., Hu, N., Liu, D., Dong, J., & Fan, X. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110684 · Cited by 53
Firouzi, A., & Shirvani, K. (2010) · Corrosion Science · doi:10.1016/j.corsci.2010.06.026 · Cited by 49
Self-citationJiang, S. M., Xu, C. Z., Li, H. Q., Liu, S. C., Gong, J., & Sun, C. (2009) · Corrosion Science · doi:10.1016/j.corsci.2009.09.032 · Cited by 44
Yuwen, P., & Zhou, C. (2016) · Corrosion Science · doi:10.1016/j.corsci.2016.09.011 · Cited by 43
Oxidation of the single-crystal Ni-base superalloy DD32 containing rhenium in air at 900 and 1000 °C
Liu, C. T., Sun, X., Guan, H. R., & Hu, Z. Q. (2005) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2004.06.003 · Cited by 40
Latief, F. H., Kakehi, K., & Tashiro, Y. (2013) · Journal of Industrial and Engineering Chemistry · doi:10.1016/j.jiec.2013.02.039 · Cited by 37
The effect of silicon on thermal shock performance of aluminide-thermal barrier coatings
Shirvani, K., Mastali, S., Rashidghamat, A., & Abdollah-Pour, H. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.05.025 · Cited by 35
Self-citationDevelopment of a new slurry coating design for the surface protection of gas turbine components
Grégoire, B., Bonnet, G., & Pedraza, F. (2019) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2019.06.020 · Cited by 29
Yu, H., Fan, Q., Li, J., Ma, D., Gong, J., & Sun, C. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110937 · Cited by 32
Reactive air aluminizing of a nickel-based superalloy (IN738LC): Coating formation mechanism
Sarraf, S. H., Soltanieh, M., & Rastegari, S. (2023) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2023.129229 · Cited by 28
Balashadehi, M. M., Nourpour, P., Rouhaghdam, A. S., Allahyarzadeh, M. H., Heydarzadeh, A., & Hamdi, M. (2020) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2020.126283 · Cited by 30
Yu, M., Sun, Q., Wang, Q., Li, X., Zhou, D., Pu, J., Chen, B., & Li, C. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110224 · Cited by 27
Li, H., Qiao, M., & Zhou, C. (2013) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2013.09.016 · Cited by 27
High Temperature Cyclic Oxidation Behavior of Ni and Co Based Superalloys
Mudgal, D., Singh, S., & Prakash, S. (2012) · Journal of Minerals and Materials Characterization and Engineering · doi:10.4236/jmmce.2012.113017 · Cited by 27
He, J., Guo, H., Zhang, Y., & Gong, S. (2014) · Corrosion Science · doi:10.1016/j.corsci.2014.04.027 · Cited by 28
Yang, R., Wu, Y., Wu, Q., Li, S., Ma, Y., & Gong, S. (2012) · Chinese Journal of Aeronautics · doi:10.1016/s1000-9361(11)60451-2 · Cited by 24
The Effect of Silicon on Cyclic Oxidation Behavior of Aluminide Coatings on Superalloy IN-738LC
Shirvani, K., Saremi, M., Nishikata, A., & Tsuru, T. (2004) · Materials science forum · doi:10.4028/www.scientific.net/msf.461-464.335 · Cited by 23
Self-citationSulphidation Behavior of a Non Harmful Water-Based Al and Al–Si Slurry Coating on CM247 Superalloy
Montero, X., Galetz, M. C., & Schütze, M. (2013) · Oxidation of Metals · doi:10.1007/s11085-013-9412-0 · Cited by 21
Codeposition of Co–Al–Y on nickel base superalloys by pack cementation process
Qiao, M., & Zhou, C. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.06.033 · Cited by 21
Gonzalez-Rodriguez, J. G., Mejía, E., Lucio-García, M. A., Salinas-Bravo, V. M., Porcayo-Calderón, J., & Martínez-Villafañe, A. (2009) · Corrosion Science · doi:10.1016/j.corsci.2009.04.012 · Cited by 21
Targhi, V. T., Omidvar, H., Sharifianjazi, F., & Pakseresht, A. (2020) · Surfaces and Interfaces · doi:10.1016/j.surfin.2020.100599 · Cited by 25
Liu, L., Li, Y., & Wang, F. (2008) · Materials Letters · doi:10.1016/j.matlet.2008.05.068 · Cited by 18
Azarmehr, S. A., Shirvani, K., Solimani, A., Schütze, M., & Galetz, M. C. (2019) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2019.01.116 · Cited by 17
Self-citationMa, H., Liu, Y., Zheng, S., Liu, X., & Li, J. (2023) · Applied Surface Science · doi:10.1016/j.apsusc.2023.157805 · Cited by 16
Role of Aluminide Coating on Oxidation Resistance of Ni-Based Single Crystal Superalloy at 900 °C
Latief, F. H., Sherif, E. M., & Kakehi, K. (2015) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)05118-0 · Cited by 16
Zarei, F., Nuranian, H., & Shirvani, K. (2020) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2020.125901 · Cited by 15
Self-citationLi, P., Fan, X., Lu, P., Wang, H., & Jin, X. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111548 · Cited by 15
Latief, F. H., Kakehi, K., & Sherif, E. M. (2014) · Progress in Natural Science Materials International · doi:10.1016/j.pnsc.2014.03.006 · Cited by 15
Cyclic oxidation behavior of Ni 3 Al‐based single crystal alloy IC21
Yang, T., Zhou, X. C., Li, S., Pei, Y., & Gong, S. (2017) · Rare Metals · doi:10.1007/s12598-016-0854-9 · Cited by 14
Research Status of Aluminum Base Coating on Titanium Alloy
Zeng, S., & Li, F. (2023) · Coatings · doi:10.3390/coatings13091525 · Cited by 15
“In addition, the dissolution of Al 2 O 3 in molten salt [58] and the formation of holes in the aluminide coating during thermal cycling [59] would lead to spalling and cracking of the aluminide coating, resulting in the failure of the coating.”
Hot Corrosion Behavior of Hf-Doped NiAl Coating in the Mixed Salt of Na2SO4 + K2SO4 at 900 °C
Zhang, W. L., Li, W., Fu, L. B., Peng, X., Sun, J., Jiang, S. M., Gong, J., & Sun, C. (2023) · Acta Metallurgica Sinica (English Letters) · doi:10.1007/s40195-023-01563-2 · Cited by 11
Mo, W., Shao, M., Wu, Y. H., Sun, Q., Xia, S., Wen, F., & Wang, Y. (2023) · Journal of Vacuum Science & Technology A Vacuum Surfaces and Films · doi:10.1116/6.0002654 · Cited by 11
Zhang, L., & Zhou, Y. (2022) · CORROSION · doi:10.5006/4150 · Cited by 10
Sarraf, S. H., Soltanieh, M., & Rastegari, S. (2024) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2024.178123 · Cited by 10
Elhelaly, M. A., El-Zomor, M. A., Ahmed, M. H., & Youssef, A. O. (2018) · Oxidation of Metals · doi:10.1007/s11085-018-9871-4 · Cited by 10
Improved oxidation and hot corrosion resistance of the NiSiAlY alloy at 750 ℃
Yu, M., Cui, T., Zhou, D., Li, R., Pu, J., & Li, C. (2021) · Materials Today Communications · doi:10.1016/j.mtcomm.2021.102939 · Cited by 15
Shirvani, K., Saremi, M., & Yamamoto, Y. (2006) · Materials and Corrosion · doi:10.1002/maco.200503907 · Cited by 10
Self-citationEnhancing Corrosion Resistance of Type 310S Stainless Steel in Carbonate Melt by Hot-Dip Aluminizing
Sah, S. P., Tada, E., & Nishikata, A. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.1241807jes · Cited by 10
Self-citationMicrostructure and hot corrosion resistance of Si-Al-Y coated TiAl alloy
Li, Y., Xie, F., & Yang, S. (2020) · Journal of Central South University · doi:10.1007/s11771-020-4478-8 · Cited by 9
Latief, F. H., Kakehi, K., & Fu, X. (2012) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)15809-3 · Cited by 9
Latief, F. H., Kakehi, K., Fu, X., & Tashiro, Y. (2012) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)18000-x · Cited by 9
Anisotropic Oxidation Resistance in a Ni-Base Single Crystal Superalloy
Latief, F. H., & Alrasheedi, N. H. (2015) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)04839-3 · Cited by 7
Maurya, S. S., Grain, A. K., Kar, I. P., Kumar, S., Sharma, S., Singh, N. K., Pandey, K. K., & Keshri, A. K. (2025) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-025-07735-2 · Cited by 6
Effect of Minor Alloying Elements on the Corrosion Behavior of Fe40Al in NaCl-KCl Molten Salts
Salinas, G., Gonzalez-Rodriguez, J. G., Porcayo-Calderón, J., Salinas-Bravo, V. M., & Espinosa-Medina, M. A. (2012) · International Journal of Corrosion · doi:10.1155/2012/185842 · Cited by 6
“[17] used polarization curves to study the corrosion performance of the slurry Si-modified aluminide coating on the nickel base super alloy In-738LC exposed to Na2SO4—20 wt.”
MethodCharacterization and Growth Kinetics Modelling of Nickel Silicides Formed on Inconel 738 Alloy
Yener, T., Efe, G. C., Keddam, M., & Erdoğan, A. (2025) · Metals and Materials International · doi:10.1007/s12540-025-01942-7 · Cited by 5
“However, when alloys are utilized at high temperatures for extended periods of time, degradation of the alloy is unavoidable due to the presence of combustion gasses, which creates an extreme environment [1–3].”
Dai, Y., Zou, J., Ning, X., Wei, H., & Li, F. (2024) · Colloids and Surfaces A Physicochemical and Engineering Aspects · doi:10.1016/j.colsurfa.2024.134420 · Cited by 5
Hot corrosion behavior of the spray-formed nickel-based superalloy
Xia, M., Tian-Fu, G., Jia, C., & Ge, C. (2016) · Chinese Physics B · doi:10.1088/1674-1056/25/12/128103 · Cited by 4
Corrosion behavior of the NiCrAlY and NiSiAlY alloys with salt mixtures of NaCl/Na2SO4
Zheng, H., Cui, T., Zhu, B., Yu, X., & Yu, M. (2024) · Journal of Vacuum Science & Technology A Vacuum Surfaces and Films · doi:10.1116/6.0003383 · Cited by 4
Corrosion Behavior of Fe40Al Alloy with Additions of Ti, Ag, and Cr in Molten KCl + ZnCl2
Ademar, R., Gonzalez-Rodriguez, J. G., Uruchurtu, J., Porcayo-Calderón, J., Salinas-Bravo, V. M., Dominguez‐Patiño, G., & Bedolla-Jacuinde, A. (2012) · International Journal of Corrosion · doi:10.1155/2012/146486 · Cited by 4
Cyclic Oxidation Performance of Si-Aluminide/MCrAlY Coating on Ni-Base GTD-111 Superalloy
Shirvani, K., & Miraboutalebi, S. V. (2017) · Materials science forum · doi:10.4028/www.scientific.net/msf.889.159 · Cited by 3
Self-citationInternal surface protection of gas turbine blade by Si‐aluminide coating
Firouzi, A., & Shirvani, K. (2010) · Materials and Corrosion · doi:10.1002/maco.201005854 · Cited by 3
Self-citationLow‐Energy X‐ray Shielding Performance of Silicide Coatings on Inconel 738 Alloy
Yener, T., KALKAN, Y., & Yener, Ş. Ç. (2025) · Advanced Engineering Materials · doi:10.1002/adem.202500289 · Cited by 2
The Role of Silicon in the Protection Against Type I Hot Corrosion
Pedraza, F., Piel, D., Kepa, T., Gossart, C., & Mondet, M. (2024) · The minerals, metals & materials series · doi:10.1007/978-3-031-63937-1_65 · Cited by 2
Yan-zhang, D., Jian-peng, Z., Qian, S., Li, X., & Hong-ming, W. (2024) · Colloids and Surfaces A Physicochemical and Engineering Aspects · doi:10.1016/j.colsurfa.2024.135732 · Cited by 2
Li, P., Hou, C., Jin, X., Lu, P., Li, Z., Xiong, K., & Fan, X. (2024) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2024.130463 · Cited by 2
Wang, C., Xu, G., Ouyang, Z., Xu, K., Xu, J. M., Jiang, L. K., Wang, Y., Su, S., Hu, S., & Xiang, J. H. (2025) · Advanced Engineering Materials · doi:10.1002/adem.202402825 · Cited by 1
The oxidation and hot corrosion behaviors of the Pt-modified NiSiAlY coating at 750 ℃
Yu, M., Zhu, B., Wang, F., Wang, S., Du, S., & Xu, K. (2025) · High Temperature Corrosion of Materials · doi:10.1007/s11085-025-10347-1 · Cited by 1
“Shirvani et al.[13] showed that Si-modified aluminide coatings provided superior protection to nickel-based superalloys in mixed salt (75 wt.% Na ₂ SO ₄ and 20 wt.% NaCl) environments during high-temperature corrosion tests.”
Saminathan, R., Fageehi, Y. A., Ramalingam, K., Vidhya, D., Bhuvaneshwari, D., Manickam, R. B. M., kumar, P. L., & Vasudevan, A. (2020) · Materials Today Proceedings · doi:10.1016/j.matpr.2020.09.799 · Cited by 1
Metadata
- Authors
- Shirvani, K., Saremi, M., Nishikata, A., & Tsuru, T.
- Affiliations
- University of Tehran (IR)
- Tokyo Institute of Technology (JP)
- Corresponding author
- Shirvani, K
- Venue
- Corrosion Science
- Publisher
- Elsevier BV
- Published
- 2003-05
- Volume
- 45
- Issue
- 5
- Pages
- 1011-1021
- ISSN
- 0010-938X (ISSN-L)
- OpenAlex
- W2014463885
- Cited by
- 70
- References
- 6
- Citations by year
- 2025: 5 · 2024: 6 · 2023: 6 · 2022: 4 · 2021: 2 · 2020: 5 · 2019: 4 · 2018: 3 · 2017: 3 · 2016: 2 · 2015: 3 · 2014: 4 · 2013: 5 · 2012: 6
- FWCI
- 1.71
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- Corrosion Science (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Engineering › Mechanical Engineering › High Temperature Alloys and Creep
- Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
- Keywords
- hot corrosion, aluminide coatings, low temperature hot corrosion, anodic polarization, passive film, SiO2 thin films, pitting corrosion, corrosion products, sulfidation, nickel-based superalloy
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.