Kinetics of dissolution and Sr release during biotite and phlogopite weathering

Open access
Taylor, Aaron S., Blum, Joel D., Lasaga, Antonio C., MacInnis, Ian N. · 2000 · Geochimica et Cosmochimica Acta
Cited by 134

The DOI matches its Crossref record; 2 of the 2 references it cites were found in a registry or an index.

Abstract

The dissolution kinetics and isotopic composition of Sr released during the weathering of biotite and phlogopite were measured under experimental conditions at pH ∼ 3 and 25°C. Although the overall release of Sr was essentially stoichiometric, the 87Sr/86Sr ratios of weathering solutions were generally higher than the reacting mineral. The initial phase of dissolution was characterized by the simultaneous rapid release of Sr from the sheet silicate and from trace amounts of calcite inclusions. During the initial phase, the 87Sr/86Sr ratios of the output solutions were lower than either the bulk mineral or the later, steady-state ratios. After the early stages of the experiments, calcite dissolution became limited by the rate at which it was exposed to the weathering solution and the 87Sr/86Sr of the output solutions increased to values above those of the biotite and phlogopite (after correction for the calcite inclusions). Differences in the location of Sr and Rb within the mica structure may cause the Sr isotopic ratio of the effluent to increase above the mineral ratio. The log values of the steady-state Sr release rate constants (moles per meter per second) were determined to be −15.1 for biotite and −15.9 for phlogopite under our experimental conditions. Cation release rates indicate that different sites within the sheet silicate structure reacted at different rates. Interlayer cations were generally released more rapidly than octahedral cations, which reacted slightly faster than the tetrahedral cations. Interlayer potassium release was considered to be controlled by diffusion with a moving boundary condition. Diffusion coefficients calculated from this model were 3.5 × 10−19 cm2/s for biotite and 1.9 × 10−18 cm2/s for phlogopite. Iron oxidation appeared to limit the overall biotite dissolution rate. Iron-free phlogopite reacted nearly twice as fast as biotite. The log values of the overall dissolution rates (moles per meter per second) were determined to be −11.6 for biotite and −11.2 for phlogopite. Cation release during phlogopite dissolution was also much less stoichiometric than during biotite weathering.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1016/s0016-7037(99)00369-5

Cites

2 of 2 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 2 references

Cited by

See all 134

Metadata

Authors
Taylor, A. S., Blum, J. D., Lasaga, A. C., & MacInnis, I. N.
Venue
Geochimica et Cosmochimica Acta
Publisher
Elsevier BV
Published
2000-04
Volume
64
Issue
7
Pages
1191-1208
ISSN
0016-7037 (ISSN-L)
OpenAlex
W2008560323
Cited by
134
References
2
FWCI
8.37
Type
journal article
Language
en
Open access
hybrid

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Kinetics of dissolution and Sr release during biotite and phlogopite weathering. https://app.cochat.ai/papers/10.1016/s0016-7037(99)00369-5
The paper
Taylor, A. S., Blum, J. D., Lasaga, A. C., & MacInnis, I. N. (2000). Kinetics of dissolution and Sr release during biotite and phlogopite weathering. Geochimica et Cosmochimica Acta. https://doi.org/10.1016/s0016-7037(99)00369-5

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.