Abstract
The objective of the study was to ascertain residual water levels in polylactide and polylactide-co-glycolide microspheres prepared using the solvent evaporation technique and to investigate the effects of that water on the glass transitional behaviour of the microspheres. Microspheres were prepared from polylactic acid (PLA) and polylactide-co-glycolide (PLGA) 50:50 and 75:25 using a standard solvent evaporation technique. The glass transition was measured as a function of drying conditions using modulated temperature DSC. The microspheres were found to contain very low levels of dichloromethane, while residual water levels of up to circa 3% w/w were noted after freeze or oven drying, these levels being higher for microspheres containing higher glycolic acid levels. The residual water was found to lower the T(g) following the Gordon-Taylor relationship. The data indicate that the microparticles may retain significant water levels following standard preparation and drying protocols and that this drying may markedly lower the T(g) of the spheres.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“It has been further reported that Tg of PLGAs decrease with a decrease of lactide content in the copolymer composition and with a decrease in molecular weight [13].”
From Poly Lactic-co-Glycolic Acid (PLGA) as Biodegradable Controlled Drug Delivery Carrier (2011) · cites this paper as [13]
Citations
Cites
Gordon, M., & Taylor, J. S. (1952) · Journal of Applied Chemistry · doi:10.1002/jctb.5010020901 · Cited by 2,621
Preparation of microspheres by the solvent evaporation technique
O'Donnell, P. B., & McGinity, J. W. (1997) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(97)00049-5 · Cited by 806
Hancock, B. C., & Zografi, G. (1994) · Pharmaceutical Research · doi:10.1023/a:1018941810744 · Cited by 714
Witschi, C., & Doelker, E. (1997) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/s0939-6411(96)00037-9 · Cited by 206
Aso, Y., Yoshioka, S., LIWANPO, A., & Terao, T. (1994) · Journal of Controlled Release · doi:10.1016/0168-3659(94)90248-8 · Cited by 131
Characterisation of the Glass Transition of an Amorphous Drug Using Modulated DSC
Royall, P. G., Craig, D. Q. M., & Doherty, C. G. (1998) · Pharmaceutical Research · doi:10.1023/a:1011902816175 · Cited by 84
Self-citationThomasin, C., Johansen, P., Alder, R., Bemsel, R., Hottinger, G., Altorfer, H. R., Wright, D. S., Wehrli, G., Merkle, H. P., & Gander, B. A. (1996) · European Journal of Pharmaceutics and Biopharmaceutics · Cited by 60
Investigation of Progesterone Loaded Poly(D,L-Lactide) Microspheres Using TMDSC, SEM and PXRD
Hill, V. L., Passerini, N., Craig, D. Q. M., Vickers, M., Anwar, J., & Feely, L. C. (1998) · Journal of Thermal Analysis and Calorimetry · doi:10.1023/a:1010167214806 · Cited by 26
Self-citationRoyall, P. G., Hill, V. L., Craig, D. Q. M., Price, D. M., & Reading, M. (2001) · Pharmaceutical Research · doi:10.1023/a:1011094611784 · Cited by 18
Self-citation
Cited by
Poly Lactic-co-Glycolic Acid (PLGA) as Biodegradable Controlled Drug Delivery Carrier
Makadia, H. K., & Siegel, S. J. (2011) · Polymers · doi:10.3390/polym3031377 · Cited by 4,816
“It has been further reported that Tg of PLGAs decrease with a decrease of lactide content in the copolymer composition and with a decrease in molecular weight [13].”
BackgroundThe mechanisms of drug release in poly(lactic-co-glycolic acid)-based drug delivery systems—A review
Fredenberg, S., Wahlgren, M., Reslow, M., & Axelsson, A. (2011) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2011.05.049 · Cited by 1,286
Freitas, S., Merkle, H. P., & Gander, B. (2005) · Journal of Controlled Release · doi:10.1016/j.jconrel.2004.10.015 · Cited by 923
“Thus, the conditions and rate of drying influence the amount of solvent and moisture residue [110], microsphere morphology and porosity as well as drug recrystallisation inside the spheres, and are therefore likely to affect the release behaviour of the final product.”
BackgroundPLGA-based nanoparticles: A new paradigm in biomedical applications
Sharma, S., Parmar, A., Kori, S., & Sandhir, R. (2016) · TrAC Trends in Analytical Chemistry · doi:10.1016/j.trac.2015.06.014 · Cited by 340
Plasticizing effect of water on poly(lactide-co-glycolide)
Blasi, P., D'Souza, S. S., Selmin, F., & DeLuca, P. P. (2005) · Journal of Controlled Release · doi:10.1016/j.jconrel.2005.07.009 · Cited by 321
Poly(lactic acid)/poly(lactic-co-glycolic acid)-based microparticles: an overview
Blasi, P. (2019) · Journal of Pharmaceutical Investigation · doi:10.1007/s40005-019-00453-z · Cited by 235
Peptide/protein vaccine delivery system based on PLGA particles
Allahyari, M., & Mohit, E. (2016) · Human Vaccines & Immunotherapeutics · doi:10.1080/21645515.2015.1102804 · Cited by 232
“It has been shown that a decline in lactide quantity and MW is associated with a decrease in the degree of crystalinity of PLGA polymer.(22,60)”
BackgroundAnalysis of initial burst in PLGA microparticles
Allison, S. D. (2008) · Expert Opinion on Drug Delivery · doi:10.1517/17425247.5.6.615 · Cited by 202
“The solubility of water in PLGA composed of 50% lactide and 50% glycolide is less than 3% [47] and increases with glycolide content [48] .”
BackgroundWu, J., Kong, T., Yeung, K. W. K., Shum, H. C., Cheung, K. M. C., Wang, L., & To, M. K. T. (2013) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.03.022 · Cited by 191
Poly(lactic-co-glycolic acid) microsphere production based on quality by design: a review
Hua, Y., Su, Y., Zhang, H., Liu, N., Wang, Z., Gao, X., Gao, J., & Zheng, A. (2021) · Drug Delivery · doi:10.1080/10717544.2021.1943056 · Cited by 175
“Hence, careful regulation of the monomer composition is crucial (Passerini & Craig, 2001; Wu et al., 2006).”
BackgroundTwenty-five years of polymersomes: lost in translation?
Matoori, S., & Leroux, J. (2020) · Materials Horizons · doi:10.1039/c9mh01669d · Cited by 161
Bouissou, C., Rouse, J. J., Price, R., & van der Walle, C. F. (2006) · Pharmaceutical Research · doi:10.1007/s11095-006-0180-2 · Cited by 145
“Comparative DSC data for polylactide microspheres showing aging of polylactide microspheres are provided by Passerini and Craig (44).”
MethodModulated Temperature Differential Scanning Calorimetry
Reading, M., & Hourston, D. J. (2006) · Hot topics in thermal analysis and calorimetry · doi:10.1007/1-4020-3750-3 · Cited by 142
Curcumin encapsulation in functional PLGA nanoparticles: A promising strategy for cancer therapies
Feltrin, F. D. S., Agner, T., Sayer, C., & Lona, L. M. F. (2021) · Advances in Colloid and Interface Science · doi:10.1016/j.cis.2021.102582 · Cited by 152
Molecular engineering solutions for therapeutic peptide delivery
Acar, H., Ting, J., Srivastava, S., LaBelle, J. L., & Tirrell, M. (2017) · Chemical Society Reviews · doi:10.1039/c7cs00536a · Cited by 145
Kang, J., & Schwendeman, S. P. (2006) · Molecular Pharmaceutics · doi:10.1021/mp060041n · Cited by 156
Glass Transition Temperature of PLGA Particles and the Influence on Drug Delivery Applications
Liu, G., & McEnnis, K. (2022) · Polymers · doi:10.3390/polym14050993 · Cited by 151
“Water, on the other hand, acts as a plasticizer which decreases the glass transition temperature of PLGA particles, thus PLGA particles would be softer than the dry polymer state [92].”
BackgroundColtelli, M., Maggiore, I. D., Bertoldo, M., Signori, F., Bronco, S., & Ciardelli, F. (2008) · Journal of Applied Polymer Science · doi:10.1002/app.28512 · Cited by 135
Physical properties of PLGA films during polymer degradation
Houchin, M. L., & Topp, E. M. (2009) · Journal of Applied Polymer Science · doi:10.1002/app.30813 · Cited by 133
Developments and Industrial Applications of Basalt Fibre Reinforced Composite Materials
Chowdhury, I. R., Pemberton, R., & Summerscales, J. (2022) · Journal of Composites Science · doi:10.3390/jcs6120367 · Cited by 130
“Structural composites are often exposed to environmental moisture during their service life period. of PLA matrix composites to be used in humid tropical environments [130].”
BackgroundAllison, S. D. (2008) · Journal of Pharmaceutical Sciences · doi:10.1002/jps.21124 · Cited by 129
“48 Water solubility in PLGA is expected to vary depending on copolymer composition, end group treatment, and molecular weight.(49) Plasticizers, such as emulsion stabilizers that are partially miscible with the polymer also decrease Tg.”
BackgroundTsouris, V., Joo, M. K., Kim, S. H., Kwon, I. C., & Won, Y. (2014) · Biotechnology Advances · doi:10.1016/j.biotechadv.2014.05.006 · Cited by 135
Cappellano, G., Comi, C., Chiocchetti, A., & Dianzani, U. (2019) · International Journal of Molecular Sciences · doi:10.3390/ijms20010204 · Cited by 126
“Low amounts of lactic acid and low molecular weight of PLGA decrease the glass transition temperature, which is usually above the physiological temperature for PLGA [48,49].”
BackgroundApplication of PLGA as a Biodegradable and Biocompatible Polymer for Pulmonary Delivery of Drugs
Mahar, R., Chakraborty, A., Nainwal, N., Bahuguna, R., Sajwan, M., & Jakhmola, V. (2023) · AAPS PharmSciTech · doi:10.1208/s12249-023-02502-1 · Cited by 137
“It is also reported that with a decrease in molecular weight and lactide content, the Tg (glass transition temperature) value of PLGA also decreases [52].”
BackgroundGlass Transitions in Polylactides
Baker, G., Vogel, E., & Smith, M. (2008) · Polymer Reviews · doi:10.1080/15583720701834208 · Cited by 111
Water-induced shape-memory poly(d,l-lactide)/microcrystalline cellulose composites
Liu, Y., Li, Y., Chen, H., Yang, G., Zheng, X., & Zhou, S. (2014) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2014.01.031 · Cited by 103
Ricci, M., Blasi, P., Giovagnoli, S., Rossi, C. R., Macchiarulo, G., Luca, G., Basta, G., & Calafiore, R. (2005) · Journal of Controlled Release · doi:10.1016/j.jconrel.2005.06.023 · Cited by 107
Panigrahi, D., Sahu, P. K., Swain, S., & Verma, R. K. (2021) · SN Applied Sciences · doi:10.1007/s42452-021-04609-1 · Cited by 109
“It has also been reported that the Tg of PLGA decreases under the wet condition, which leads to the plasticization of the polymer matrix and lessening in mechanical properties of PLGA [63, 67, 68].”
BackgroundPLGA microcapsules with novel dimpled surfaces for pulmonary delivery of DNA
Mohamed, F., & van der Walle, C. F. (2006) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2005.12.016 · Cited by 82
Damadzadeh, B., Jabari, H., Skrifvars, M., Airola, K., Moritz, N., & VALLITTU, P. K. (2010) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-010-4110-9 · Cited by 82
Key factors for tuning hydrolytic degradation of polylactide/zinc oxide nanocomposites
Benali, S., Aouadi, S., Dechief, A.-L., Murariu, M., & Dúbois, P. (2015) · Nanocomposites · doi:10.1179/2055033214y.0000000007 · Cited by 74
Polymeric nanoparticles – Influence of the glass transition temperature on drug release
Lappe, S., Mulac, D., & Langer, K. (2016) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2016.12.025 · Cited by 71
“With decreasing residual moisture Tg increased indicating that water appears to have a plasticising effect on the polymer (Passerini and Craig, 2001; Zweers et al., 2004; Blasi et al., 2005).”
BackgroundBrandhonneur, N., Hatahet, T., Amela‐Cortes, M., Molard, Y., Cordier, S., & Dollo, G. (2018) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/j.ejpb.2018.01.007 · Cited by 71
Lange, J., de Souza, F. G., Nele, M., Tavares, F. W., Segtovich, I. S. V., da Silva, G. C. Q., & Pinto, J. C. (2015) · Macromolecular Theory and Simulations · doi:10.1002/mats.201500049 · Cited by 68
Evaluation of ibuprofen-loaded microspheres prepared from novel copolyesters
Thompson, C. J., Hansford, D., Higgins, S. J., Rostron, C., Hutcheon, G. A., & Munday, D. L. (2006) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2006.08.019 · Cited by 84
Abrego, G., Alvarado, H. L., Egea, M. A., González‐Mira, E., Calpena, A. C., & García, M. L. (2014) · Journal of Pharmaceutical Sciences · doi:10.1002/jps.24101 · Cited by 69
Kianfar, F., Antonijević, M. D., Chowdhry, B. Z., & Boateng, J. S. (2012) · Colloids and Surfaces B Biointerfaces · doi:10.1016/j.colsurfb.2012.10.006 · Cited by 58
Physical ageing and thermal analysis of PLGA microspheres encapsulating protein or DNA
Rouse, J. J., Mohamed, F., & van der Walle, C. F. (2007) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2007.02.026 · Cited by 63
Kim, T. H., & Park, T. G. (2004) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2003.11.021 · Cited by 60
“The increased volume fraction of ice upon freezing was likely to induce the enlargement of liquid water-filled pore dimensions with a concomitant cracking of PLGA polymer walls surrounding the pores (Passerini and Craig, 2001).”
BackgroundEshaghi, B., Alsharif, N., An, X., Akiyama, H., Brown, K. A., Gummuluru, S., & Reinhard, B. M. (2020) · Advanced Science · doi:10.1002/advs.202000649 · Cited by 55
Garner, J., Skidmore, S., Park, H., Park, K., Choi, S. H., & Wang, Y. (2017) · Journal of Pharmaceutical Sciences · doi:10.1016/j.xphs.2017.10.027 · Cited by 54
Puccetti, M., Giovagnoli, S., Zelante, T., Romani, L., & Ricci, M. (2018) · Journal of Pharmaceutical Sciences · doi:10.1016/j.xphs.2018.04.023 · Cited by 45
Qin, Y., Summerscales, J., Graham‐Jones, J., Meng, M., & Pemberton, R. (2020) · Polymers · doi:10.3390/polym12122928 · Cited by 54
Accelerated ageing and degradation in poly-l-lactide/hydroxyapatite nanocomposites
Delabarde, C., Plummer, C., Bourban, P.-E., & Månson, J. (2011) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.12.018 · Cited by 40
Functional Nanofibrous Biomaterials of Tailored Structures for Drug Delivery—A Critical Review
Li, Z., Mei, S., Dong, Y., She, F., Li, Y., Li, P., & Kong, L. (2020) · Pharmaceutics · doi:10.3390/pharmaceutics12060522 · Cited by 46
“The glass transition temperature of PLGA has been demonstrated to decrease with decreasing lactide content and molecular weight [80].”
BackgroundZonal release of proteins within tissue engineering scaffolds
Suciati, T. A., Howard, D. J., Barry, J. J. A., Everitt, N. M., Shakesheff, K. M., & Rose, F. R. A. J. (2006) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-006-0443-9 · Cited by 42
Abulateefeh, S. R., & Alkilany, A. M. (2015) · AAPS PharmSciTech · doi:10.1208/s12249-015-0413-y · Cited by 39
Lakkireddy, H. R., & Bazile, D. (2016) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2016.08.012 · Cited by 39
“Decrease in lactide content and decrease in molecular weight of the polymer lead to a reduction of Tg of PLGA ([55,56]).”
Bhuiyan, D. B., Middleton, J. C., Tannenbaum, R., & Wick, T. M. (2016) · Journal of Biomaterials Science Polymer Edition · doi:10.1080/09205063.2016.1184121 · Cited by 36
“Increasing the ratio of glycolide in the PLGA chain would increase the initial strength and decrease the hydrolytic degradation rate of the polymer,[45] which will be favorable for load-bearing applications.”
BackgroundChlon, C., Guédon, C. M., Verhaagen, B., Shi, W. T., Hall, C. S., Lub, J., & Böhmer, M. R. (2009) · Biomacromolecules · doi:10.1021/bm801243u · Cited by 35
Noviendri, D., Jaswir, I., Taher, M., Mohamed, F., Salleh, H. M., Noorbatcha, I. A., Octavianti, F., Lestari, W., Hendri, R., Ahmad, H., et al. (2016) · Journal of Oleo Science · doi:10.5650/jos.ess16018 · Cited by 38
Blasi, P., Giovagnoli, S., Schoubben, A., Ricci, M., Rossi, C. R., Luca, G., Basta, G., & Calafiore, R. (2006) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2006.07.049 · Cited by 38
Worku, Z. A., Aarts, J., Singh, A. K., & den Mooter, G. V. (2014) · Molecular Pharmaceutics · doi:10.1021/mp4003943 · Cited by 31
Kazazi-Hyseni, F., Landín, M., Lathuile, A., Veldhuis, G. J., Rahimian, S., Hennink, W. E., Kok, R. J., & van Nostrum, C. F. (2014) · Pharmaceutical Research · doi:10.1007/s11095-014-1381-8 · Cited by 34
“In line with the results published, the pore closure is rather slow for the PLGAmicrospheres of this study (Tg in dry state is around 45°C and when hydrated it is depressed to about 30°C (9,61,62), allowing diffusion of entrapped blue dextran through these water-filled pores.”
Huang, J., Cao, Y., Huang, Z., Imbraguglio, S. A., Wang, Z., Peng, X., & Guo, Z. (2016) · Macromolecular Materials and Engineering · doi:10.1002/mame.201600172 · Cited by 31
Niclosamide encapsulated polymeric nanocarriers for targeted cancer therapy
Jain, N. K., Prabhuraj, R. S., Bavya, M. C., Prasad, R., Bandyopadhyaya, R., Naidu, V. G. M., & Srivastava, R. (2019) · RSC Advances · doi:10.1039/c9ra03407b · Cited by 30
Gopinathan, N., Yang, B., Lowe, J. P., Edler, K. J., & Rigby, S. P. (2014) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2014.04.018 · Cited by 30
“In addition to a sharp water peak at 373 K, the glass transition was also observed, which occurred at 316 K for batch A, for example, which is the same as that observed for similar PLGA particles (Passerini and Craig, 2001).”
ResultEffect of Hydration on Physicochemical Properties of End-Capped PLGA
D’Souza, S. S., Dorati, R., & DeLuca, P. P. (2014) · Advances in Biomaterials · doi:10.1155/2014/834942 · Cited by 32
“This parameter could be of considerable practical significance, particularly in view of the amorphous nature of the pharmaceutical solid with the concomitant possibility of plasticization effects [12].”
BackgroundMundhe, G. S., Mahanwar, P. A., Patil, J. R., & Sundaramoorthy, E. (2023) · International Journal for Research in Applied Science and Engineering Technology · doi:10.22214/ijraset.2023.50471 · Cited by 28
Vay, K., Frieß, W., & Scheler, S. (2012) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/j.ejpb.2012.02.019 · Cited by 30
Chemical Structure of Poly(Lactic Acid)
Jiang, X., Luo, Y., Tian, X., Huang, D., Reddy, N., & Yang, Y. (2010) · Wiley eBooks · doi:10.1002/9780470649848.ch6 · Cited by 34
Rial-Hermida, M. I., Oliveira, N. M., Concheiro, Á., Alvarez‐Lorenzo, C., & Mano, J. F. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2014.06.009 · Cited by 27
“DSC runs of PLGA powder revealed a glass transition temperature (Tg) at 45 C, which is in agreement with the literature [37] (Fig.”
ResultRecent biomedical applications and patents on biodegradable polymer
Kaur, T., Kaur, R., & Kaur, A. (2014) · Cited by 36
Characterization of an air‐spun poly( L ‐lactic acid) nanofiber mesh
François, S., Sarra‐Bournet, C., Jaffre, A., Chakfé, N., Durand, B., & Laroche, G. (2010) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.31612 · Cited by 27
Maenz, S., Hennig, M., Mühlstädt, M., Kunisch, E., Bungartz, M., Brinkmann, O., Bossert, J., Kinne, R. W., & Jandt, K. D. (2016) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2016.01.030 · Cited by 26
AFM Investigation of Liquid-Filled Polymer Microcapsules Elasticity
Sarrazin, B., Tsapis, N., Mousnier, L., Taulier, N., Urbach, W., & Guénoun, P. (2016) · Langmuir · doi:10.1021/acs.langmuir.6b00431 · Cited by 33
Novel biodegradable Round Window Disks for inner ear delivery of dexamethasone
Lehner, E., Liebau, A., Syrowatka, F., Knolle, W., Plontke, S. K., & Mäder, K. (2020) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2020.120180 · Cited by 27
Implantable biomedical materials for treatment of bone infection
Shuaishuai, W., Tongtong, Z., Wang, D., Zhang, M., Wang, X., Yu, Y., Dong, H., Wu, G., & Zhang, M. (2023) · Frontiers in Bioengineering and Biotechnology · doi:10.3389/fbioe.2023.1081446 · Cited by 28
“In general, PLGA degradation and drug release rates are accelerated by greater hydrophilicity, increased chemical interactions between hydrolyzed groups, less crystallinity, and greater volume-to-surface ratio (Passerini and Craig, 2001).”
BackgroundPasserini, N., & Craig, D. Q. M. (2002) · Journal of Pharmacy and Pharmacology · doi:10.1211/002235702760089027 · Cited by 25
“…water content of the formed spheres after drying was 1.12³ 0.09%, 1.28³ 0.11%, 1.63 ³ 0.07% and 1.51 ³ 0.06%, respectively, for 0, 10, 30 and 50% loading (determined by TGA, previous studies having established that dichloromethane levels are negligible using this protocol ; Passerini & Craig 2001).”
MethodSelf-citationPost-loading of proangiogenic growth factors in PLGA microspheres
Scheiner, K. C., Maas-Bakker, R. F., van Steenbergen, M. J., Schwendeman, S. P., Hennink, W. E., & Kok, R. J. (2020) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/j.ejpb.2020.10.022 · Cited by 24
Pharmaceutical Applications of Plasticized Polymers
Šnejdrová, E., & Dittrich, M. (2012) · InTech eBooks · doi:10.5772/36543 · Cited by 31
“Residual water markedly decreases Tg values according to GordonTaylor relationship (Passerini & Craig, 2001).”
BackgroundAltındal, D. Ç., & Gümüşderelı́oğlu, M. (2019) · Journal of Drug Delivery Science and Technology · doi:10.1016/j.jddst.2019.05.027 · Cited by 23
“In addition, the burst release may have caused due to the contribution of water that can depress the Tg up to 15 °C bringing the polymer to a rubbery state at the release temperature [33].”
BackgroundBiomedical applications of PLGA particles
Agrawal, A., Rellegadla, S., & Jain, S. (2019) · Elsevier eBooks · doi:10.1016/b978-0-12-816913-1.00004-0 · Cited by 31
Surve, D. H., Jirwankar, Y. B., Dighe, V. D., & Jindal, A. B. (2020) · Molecular Pharmaceutics · doi:10.1021/acs.molpharmaceut.0c00773 · Cited by 23
Patil, S. M., & Won, Y. (2024) · Macromolecules · doi:10.1021/acs.macromol.4c00106 · Cited by 22
Wiranidchapong, C., Ruangpayungsak, N., Suwattanasuk, P., Shuwisitkul, D., & Tanvichien, S. (2014) · Drug Development and Industrial Pharmacy · doi:10.3109/03639045.2014.925917 · Cited by 20
Manna, S., Augsburger, J. J., Corrêa, Z. M., Figueroa, J. A. L., & Banerjee, R. K. (2013) · Journal of Biomechanical Engineering · doi:10.1115/1.4026176 · Cited by 20
“experiment are consistent with previous work [33].”
ResultColoring of PLGA implants to better understand the underlying drug release mechanisms
Bode, C., Kranz, H., Siepmann, F., & Siepmann, J. (2019) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2019.118563 · Cited by 21
Zaghloul, N., Mahmoud, A. A. K., ElKasabgy, N. A., & Hoffy, N. M. E. (2022) · Drug Delivery · doi:10.1080/10717544.2022.2092239 · Cited by 20
“Furthermore, it has been reported that the Tg (glass transition temperature) of PLGA decreases with decreasing lactide content (Passerini & Craig, 2001) in the copolymer composition which is found to be 37 °C in case of PLGA with monomers ratio of 50:50 and 42 °C in case of PLGA with monomers ratio…”
BackgroundMicrobial Poly(hydroxybutyrate-co-hydroxyvalerate) Scaffold for Periodontal Tissue Engineering
Phuegyod, S., Pramual, S., Wattanavichean, N., Assawajaruwan, S., Amornsakchai, T., Sukho, P., Svasti, J., Surarit, R., & Niamsiri, N. (2023) · Polymers · doi:10.3390/polym15040855 · Cited by 21
“The water molecules could intersperse and intercalate among the polymer chains that finally spread the polymer chains apart by losing the crystalline network characteristics of the polymer [44].”
BackgroundSchoubben, A., Blasi, P., & DeLuca, P. P. (2011) · Journal of Pharmaceutical Sciences · doi:10.1002/jps.23029 · Cited by 20
Tanır, T. E., Hasırcı, V., & Hasırcı, N. (2014) · Polymer Composites · doi:10.1002/pc.23100 · Cited by 21
Sunazuka, Y., Ueda, K., Higashi, K., Wada, K., & Moribe, K. (2024) · Molecular Pharmaceutics · doi:10.1021/acs.molpharmaceut.3c01066 · Cited by 20
Longobardi, G., Moore, T. L., Conte, C., Ungaro, F., Satchi‐Fainaro, R., & Quaglia, F. (2024) · Wiley Interdisciplinary Reviews Nanomedicine and Nanobiotechnology · doi:10.1002/wnan.1990 · Cited by 22
Dorati, R., Genta, I., Tomasi, C., Modena, T., Colonna, C., Pavanetto, F., Perugini, P., & Conti, B. (2008) · Journal of Microencapsulation · doi:10.1080/02652040801996763 · Cited by 20
Yokoi, Y., Yonemochi, E., & Terada, K. (2004) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2004.05.005 · Cited by 17
Paakinaho, K., Heino, H., Pelto, M., Hannula, M., Törmälä, P. O., & Kellomäki, M. (2011) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-011-4538-6 · Cited by 19
Saquinavir Loaded Acetalated Dextran Microconfetti – a Long Acting Protease Inhibitor Injectable
Collier, M. A., Gallovic, M. D., Bachelder, E. M., Sykes, C., Kashuba, A. D. M., & Ainslie, K. M. (2016) · Pharmaceutical Research · doi:10.1007/s11095-016-1936-y · Cited by 19
“As mentioned previously, Ace-DEX has a glass transition temperature of roughly 160–190°C (22) while PLGA and PCL are closer to 50°C (27, 28).”
Physiologically Relevant Mechanics of Biodegradable Polyester Nanoparticles
Alsharif, N., Eshaghi, B., Reinhard, B. M., & Brown, K. A. (2020) · Nano Letters · doi:10.1021/acs.nanolett.0c03004 · Cited by 19
Samimi, R., Salarian, M., Xu, W. Z., Lui, E. M. K., & Charpentier, P. A. (2014) · Industrial & Engineering Chemistry Research · doi:10.1021/ie501118u · Cited by 17
Transport of Polymeric Nanoparticulate Drug Delivery Systems in the Proximity of Silica and Sand
Chen, I., Zhang, M., Teipel, B. R., de Araujo, I. S., Yegin, Y., & Akbulut, M. E. S. (2015) · Environmental Science & Technology · doi:10.1021/es504188a · Cited by 15
Hemelryck, S. V., Wens, R., van Poppel, H., Luijks, M., Shahidi, K., Marczak, M., Kahnt, A., Holm, R., Mannaert, E., & Langguth, P. (2021) · Pharmaceutics · doi:10.3390/pharmaceutics13081231 · Cited by 14
“Pore closure, promoted by a higher polymer chain mobility and lower glass transition temperature (Tg) of the more hydrophilic polymer PLGA5050A in formulation 1, may explain this observation [14,38].”
BackgroundShear yielding and crazing in dry and wet amorphous PLA at body temperature
Chen, H., Pan, Z., Yuan, D., Sulley, G. S., Oosterbeek, R. N., Williams, C. K., & Brassart, L. (2023) · Polymer · doi:10.1016/j.polymer.2023.126477 · Cited by 16
Accelerated degradation testing impacts the degradation processes in 3D printed amorphous PLLA
Malone, L. P., Best, S. M., & Cameron, R. E. (2024) · Frontiers in Bioengineering and Biotechnology · doi:10.3389/fbioe.2024.1419654 · Cited by 18
“Passerini and Craig previously reported that the lowering of Tg in fl uid obeyed the Gordon-Taylor relationship (Passerini and Craig, 2001).”
Formulation Strategies for Sustained Release of Proteins
Lewis, A. L., & Illum, L. (2010) · Therapeutic Delivery · doi:10.4155/tde.10.17 · Cited by 14
Modulated Temperature Differential Scanning Calorimetry
Kett, V. L., Murphy, J., Craig, D. Q. M., & Reading, M. (2006) · CRC Press eBooks · doi:10.1201/9781420014891.ch4 · Cited by 13
Self-citationNanogels: A New Dawn in Antimicrobial Chemotherapy
Sahu, P. K., Das, D., Kashaw, V., Iyer, A. K., & Kashaw, S. K. (2017) · Elsevier eBooks · doi:10.1016/b978-0-323-52733-0.00005-7 · Cited by 17
Characterization andin vitrodegradation of salicylate-derived poly(anhydride-ester microspheres)
Yeagy, B. A., Prudencio, A., Schmeltzer, R. C., Uhrich, K. E., & Cook, T. J. (2006) · Journal of Microencapsulation · doi:10.1080/02652040600776481 · Cited by 14
Sokol, M. B., Beganovskaya, V. A., Mollaeva, M. R., Yabbarov, N. G., Chirkina, M., Belykh, D. V., Startseva, O. M., Egorov, A. E., Kostyukov, A. A., Kuzmin, V. A., et al. (2024) · Pharmaceutics · doi:10.3390/pharmaceutics16010126 · Cited by 12
“Previous studies revealed that lyophilized nanoparticles still contained 3.5% of residual moisture [38], which is acceptable and results in only non-significant PLGA degradation [39].”
BackgroundInfluentialMaltodextrins as drying auxiliary agent for the preparation of easily resuspendable nanoparticles
Magri, G., Franzè, S., Musazzi, U. M., Selmin, F., & Cilurzo, F. (2019) · Journal of Drug Delivery Science and Technology · doi:10.1016/j.jddst.2019.01.019 · Cited by 12
“As an example, the moisture content can reduce the Tg of PLGA from about 45 °C to about 15 °C [11, 12].”
Background
Metadata
- Authors
- Passerini, N., & Craig, D. Q. M.
- Affiliations
- Queen's University Belfast (GB)
- Corresponding author
- Craig, D.Q.M
- Venue
- Journal of Controlled Release
- Publisher
- Elsevier BV
- Published
- 2001-05
- Volume
- 73
- Issue
- 1
- Pages
- 111-115
- ISSN
- 0168-3659 (ISSN-L)
- OpenAlex
- W2021468645
- Semantic Scholar
- 0c903721aa58894b62e667a8cd7158bb258d4bff
- Cited by
- 165
- References
- 9
- Citations by year
- 2026: 3 · 2025: 5 · 2024: 9 · 2023: 11 · 2022: 4 · 2021: 6 · 2020: 12 · 2019: 12 · 2018: 7 · 2017: 8 · 2016: 9 · 2015: 11 · 2014: 16 · 2013: 4 · 2012: 4
- FWCI
- 1.27
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- Journal of Controlled Release (publishedVersion)
- PubMed (publishedVersion)
- Archivio istituzionale della ricerca (Alma Mater Studiorum Università di Bologna) (submittedVersion)
- UCL Discovery (University College London) (submittedVersion)
- UEA Digital Repository (University of East Anglia) (submittedVersion)
- Topics
- Life Sciences › Pharmacology, Toxicology and Pharmaceutics › Pharmaceutical Science › Advanced Drug Delivery Systems
- Physical Sciences › Materials Science › Biomaterials › Hydrogels: synthesis, properties, applications
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Keywords
- polylactide-co-glycolide, residual water, glass transition temperature, solvent evaporation, drying conditions, freeze-drying, oven drying, temperature-modulated DSC, biodegradable microparticles
- MeSH terms
- Polylactic Acid-Polyglycolic Acid Copolymer, Calorimetry, Differential Scanning, Chemistry, Physical, Desiccation, Drug Carriers, Freeze Drying, Microspheres, Polyesters, Polyglycolic Acid, Polymers, Water, Lactic Acid, Chemical Phenomena
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.