Toward Dendrite-Free Lithium Deposition via Structural and Interfacial Synergistic Effects of 3D Graphene@Ni Scaffold
Abstract
Owing to its ultrahigh specific capacity and low electrochemical potential, lithium (Li) metal is regarded as one of the most attractive anode materials for next-generation lithium batteries. Nevertheless, the commercialization of Li–metal-based rechargeable batteries (LiMBs) has been retarded by the uncontrollable growth of Li dendrites, as well as the resulting poor cycle stability and safety hazards. In this work, a 3D graphene@Ni scaffold has been proposed to accomplish dendrite-free Li deposition via structural and interfacial synergistic effects. Due to the intrinsic high surface area used to reduce the effective electrode current density and the surface-coated graphene working as an artificial protection layer to provide high cycle stability as well as suppress the growth of Li dendrites, the Coulombic efficiencies of Li deposition on 3D graphene@Ni foam after 100 cycles can be sustained as high as 96, 98, and 92% at the current densities of 0.25, 0.5, and 1.0 mA cm –2, respectively, which shows more excellent cycle stability than that of its planar Cu foil and bare Ni foam counterparts. The results obtained here demonstrate that the comprehensive consideration of multiaspect factors could be more help to enhance the performance of Li metal anode so as to achieve its real application in next-generation LiMBs.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
High rate and stable cycling of lithium metal anode
Qian, J., Henderson, W. A., Xu, W., Bhattacharya, P., Engelhard, M., Borodin, O., & Zhang, J.-G. (2015) · Nature Communications · doi:10.1038/ncomms7362 · Cited by 2,561
Cited by
Lithium Metal Anodes with Nonaqueous Electrolytes
Zhang, J.-G., Xu, W., Xiao, J., Cao, X., & Liu, J. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00275 · Cited by 730
Advanced Micro/Nanostructures for Lithium Metal Anodes
Zhang, R., Li, N., Cheng, X., Yin, Y., Zhang, Q., & Guo, Y. (2017) · Advanced Science · doi:10.1002/advs.201600445 · Cited by 549
Li-S Batteries: Challenges, Achievements and Opportunities
Raza, H., Bai, S., Cheng, J., Majumder, S., Zhu, H., Liu, Q., Zheng, G., Li, X., & Chen, G. (2023) · Electrochemical Energy Reviews · doi:10.1007/s41918-023-00188-4 · Cited by 406
Perspectives for restraining harsh lithium dendrite growth: Towards robust lithium metal anodes
Wu, F., Yuan, Y.-X., Cheng, X.-B., Bai, Y., Li, Y., Wu, C., & Zhang, Q. (2018) · Energy Storage Materials · doi:10.1016/j.ensm.2018.03.024 · Cited by 319
Anode Improvement in Rechargeable Lithium–Sulfur Batteries
Tao, T., Lu, S., Fan, Y., Lei, W., Huang, S., & Chen, Y. (2017) · Advanced Materials · doi:10.1002/adma.201700542 · Cited by 304
Metadata
- Authors
- Xie, K., Wei, W., Yuan, K., Lu, W., Guo, M., Li, Z., Song, Q., Liu, X., Wang, J.-G., & Shen, C.
- Venue
- ACS Applied Materials & Interfaces
- Publisher
- American Chemical Society (ACS)
- Published
- 2016-09-26
- Volume
- 8
- Issue
- 39
- Pages
- 26091-26097
- ISSN
- 1944-8244 (ISSN-L)
- 1944-8252
- OpenAlex
- W2520144272
- Cited by
- 158
- References
- 1
- FWCI
- 12.04
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Toward Dendrite-Free Lithium Deposition via Structural and Interfacial Synergistic Effects of 3D Graphene@Ni Scaffold. https://app.cochat.ai/papers/10.1021/acsami.6b09031
- The paper
- Xie, K., Wei, W., Yuan, K., Lu, W., Guo, M., Li, Z., Song, Q., Liu, X., Wang, J.-G., & Shen, C. (2016). Toward Dendrite-Free Lithium Deposition via Structural and Interfacial Synergistic Effects of 3D Graphene@Ni Scaffold. ACS Applied Materials & Interfaces. https://doi.org/10.1021/acsami.6b09031
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.