Stable Black Phosphorus Encapsulation in Porous Mesh-like UiO-66 Promoted Charge Transfer for Photocatalytic Oxidation of Toluene and o-Dichlorobenzene: Performance, Degradation Pathway, and Mechanism
The DOI matches its Crossref record; 2 of the 2 references it cites were found in a registry or an index.
Abstract
This work presents a new strategy to enhance the charge transfer from Zr atoms in UiO-66 to black phosphorus (BP) via an atomic-level charge-transfer channel provided by Zr–P bonds for photocatalytic degradation of toluene and o-dichlorobenzene. The formation of Zr–P bonds is the key to covering BP with the UiO-66 encapsulation layer and improving the charge-transfer capability of BP–UiO, which is also verified by a series of characterization and theoretical calculations. The hydrophilic porous mesh-like UiO-66 encapsulation layer endows BP–UiO with enhanced visible-light-harvesting ability, charge transport capability, and photocatalytic activity. Additionally, BP–UiO demonstrates the promoted redox/acidity properties, significantly improving catalytic activity for the degradation of toluene and o -dichlorobenzene even in the presence of water. The degradation pathways of contaminants are investigated via the study of transient variations by in situ infrared (IR) methods, refined by the static analysis of intermates accumulated on the BP–UiO surface by gas chromatography–mass spectrometry (GC–MS). The electron transfer via bond construction and the combination of in situ IR and GC–MS are expected to provide a more complete theoretical basis for environmental catalysis.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
A Graphitic‐C 3 N 4 “Seaweed” Architecture for Enhanced Hydrogen Evolution
Han, Q., Wang, B., Zhao, Y., Hu, C., & Qu, L. (2015) · Angewandte Chemie International Edition · doi:10.1002/anie.201504985 · Cited by 472
Monolithic aerogel photocatalysts: a review
Wan, W., Zhang, R., Ma, M., & Zhou, Y. (2018) · Journal of Materials Chemistry A · doi:10.1039/c7ta09227j · Cited by 205
Cited by
Li, H., Yu, J., Gong, Y., Lin, N., Yang, Q., Zhang, X., & Wang, Y. (2023) · Separation and Purification Technology · doi:10.1016/j.seppur.2022.122716 · Cited by 155
Self-citation
Metadata
- Authors
- Chen, J., Yang, Y., Zhao, S., Bi, F., Song, L., Liu, N., Xu, J., Wang, Y., & Zhang, X.
- Venue
- ACS Catalysis
- Publisher
- American Chemical Society (ACS)
- Published
- 2022-06-22
- Volume
- 12
- Issue
- 13
- Pages
- 8069-8081
- ISSN
- 2155-5435 (ISSN-L)
- OpenAlex
- W4283321630
- Cited by
- 165
- References
- 2
- FWCI
- 6.62
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Stable Black Phosphorus Encapsulation in Porous Mesh-like UiO-66 Promoted Charge Transfer for Photocatalytic Oxidation of Toluene and o-Dichlorobenzene: Performance, Degradation Pathway, and Mechanism. https://app.cochat.ai/papers/10.1021/acscatal.2c01375
- The paper
- Chen, J., Yang, Y., Zhao, S., Bi, F., Song, L., Liu, N., Xu, J., Wang, Y., & Zhang, X. (2022). Stable Black Phosphorus Encapsulation in Porous Mesh-like UiO-66 Promoted Charge Transfer for Photocatalytic Oxidation of Toluene and o-Dichlorobenzene: Performance, Degradation Pathway, and Mechanism. ACS Catalysis. https://doi.org/10.1021/acscatal.2c01375
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.