Insights on the Proton Insertion Mechanism in the Electrode of Hexagonal Tungsten Oxide Hydrate

Jiang, Heng, Hong, Jessica J., Wu, Xianyong, Surta, T. Wesley, Qi, Yitong, Dong, Shengyang, Li, Zhifei, Leonard, Daniel P., Holoubek, John J., Wong, Jane C., Razink, Joshua James, Zhang, Xiaogang, Ji, Xiulei·2018·Journal of the American Chemical Society

Abstract

Abstract This study reveals the transport behavior of lattice water during proton (de)­insertion in the structure of the hexagonal WO3·0.6H2O electrode. By monitoring the mass evolution of this electrode material via electrochemical quartz crystal microbalance, we discovered (1) WO3·0.6H2O incorporates additional lattice water when immersing in the electrolyte at open circuit voltage and during initial cycling; (2) The reductive proton insertion in the WO3 hydrate is a three-tier process, where in the first stage 0.25 H+ is inserted per formula unit of WO3 while simultaneously 0.25 lattice water is expelled; then in the second stage 0.30 naked H+ is inserted, followed by the third stage with 0.17 H3O+ inserted per formula unit. Ex situ XRD reveals that protonation of the WO3 hydrate causes consecutive anisotropic structural changes: it first contracts along the c-axis but later expands along the ab planes. Furthermore, WO3·0.6H2O exhibits impressive cycle life over 20 000 cycles, together with appreciable capacity and promising rate performance.

Overview

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1021/jacs.8b03959

Cites

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cited by

See all 243

Metadata

Authors
Jiang, H., Hong, J. J., Wu, X., Surta, T. W., Qi, Y., Dong, S., Li, Z., Leonard, D. P., Holoubek, J. J., Wong, J. C., Razink, J. J., Zhang, X., & Ji, X.
Venue
Journal of the American Chemical Society
Published
2018-09-05
Volume
140
Issue
37
Pages
11556-11559
ISSN
  • 0002-7863 (ISSN-L)
  • 1520-5126
OpenAlex
W2891683159
Cited by
243
References
0
FWCI
6.45
Type
journal article
Language
en
Open access
closed

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Insights on the Proton Insertion Mechanism in the Electrode of Hexagonal Tungsten Oxide Hydrate. https://app.cochat.ai/papers/10.1021/jacs.8b03959
The paper
Jiang, H., Hong, J. J., Wu, X., Surta, T. W., Qi, Y., Dong, S., Li, Z., Leonard, D. P., Holoubek, J. J., Wong, J. C., Razink, J. J., Zhang, X., & Ji, X. (2018). Insights on the Proton Insertion Mechanism in the Electrode of Hexagonal Tungsten Oxide Hydrate. Journal of the American Chemical Society. https://doi.org/10.1021/jacs.8b03959

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.