Twin boundary defect engineering improves lithium-ion diffusion for fast-charging spinel cathode materials
Open accessThe DOI matches its Crossref record; 48 of the 48 references it cites were found in a registry or an index.
Abstract
Defect engineering on electrode materials is considered an effective approach to improve the electrochemical performance of batteries since the presence of a variety of defects with different dimensions may promote ion diffusion and provide extra storage sites. However, manipulating defects and obtaining an in-depth understanding of their role in electrode materials remain challenging. Here, we deliberately introduce a considerable number of twin boundaries into spinel cathodes by adjusting the synthesis conditions. Through high-resolution scanning transmission electron microscopy and neutron diffraction, the detailed structures of the twin boundary defects are clarified, and the formation of twin boundary defects is attributed to agminated lithium atoms occupying the Mn sites around the twin boundary. In combination with electrochemical experiments and first-principles calculations, we demonstrate that the presence of twin boundaries in the spinel cathode enables fast lithium-ion diffusion, leading to excellent fast charging performance, namely, 75% and 58% capacity retention at 5 C and 10 C, respectively. These findings demonstrate a simple and effective approach for fabricating fast-charging cathodes through the use of defect engineering.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Double-slit photoelectron interference in strong-field ionization of the neon dimer
Kunitski, M., Eicke, N., Huber, P., Köhler, J., Zeller, S., Voigtsberger, J., Schlott, N., Henrichs, K., Sann, H., Trinter, F., et al. (2019) · Nature Communications · doi:10.1038/s41467-018-07882-8 · Cited by 8,162
Double-slit photoelectron interference in strong-field ionization of the neon dimer
Kunitski, M., Eicke, N., Huber, P., Köhler, J., Zeller, S., Voigtsberger, J., Schlott, N., Henrichs, K., Sann, H., Trinter, F., et al. (2019) · Institutional Repository of Leibniz Universität Hannover (Leibniz Universität Hannover) · doi:10.15488/5174 · Cited by 8,161
Li-ion battery materials: present and future
Nitta, N., Wu, F., Lee, J. T., & Yushin, G. (2015) · Materials Today · doi:10.1016/j.mattod.2014.10.040 · Cited by 7,389
Research on Advanced Materials for Li‐ion Batteries
Li, H., Wang, Z., Chen, L., & Huang, X. (2009) · Advanced Materials · doi:10.1002/adma.200901710 · Cited by 1,803
Ultrastrong steel via minimal lattice misfit and high-density nanoprecipitation
Jiang, S., Wang, H., Wu, Y., Liu, X., Chen, H., Yao, M., Gault, B., Ponge, D., Raabe, D., Hirata, A., et al. (2017) · Nature · doi:10.1038/nature22032 · Cited by 1,441 · cited 1×
“As shown in equation (1), DLi has a positive correlation with the slopes of the IP/ν curves (Fig.”
BackgroundJiang, H., Gu, J., Zheng, X., Liu, M., Qiu, X., Wang, L., Li, W., Chen, Z., Ji, X., & Li, J. (2019) · Energy & Environmental Science · doi:10.1039/c8ee03276a · Cited by 1,399
High dislocation density–induced large ductility in deformed and partitioned steels
He, B., Hu, B., Yen, H., Cheng, G.-J., Wang, Z., Luo, H., & Huang, M. (2017) · Science · doi:10.1126/science.aan0177 · Cited by 1,241
Oxygen Vacancy‐Mediated Photocatalysis of BiOCl: Reactivity, Selectivity, and Perspectives
Li, H., Li, J., Ai, Z., Jia, F., & Zhang, L. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201705628 · Cited by 1,207
Defect Graphene as a Trifunctional Catalyst for Electrochemical Reactions
Jia, Y., Zhang, L., Du, A., Gao, G., Chen, J., Yan, X., Brown, C. L., & Yao, X. (2016) · Advanced Materials · doi:10.1002/adma.201602912 · Cited by 1,169
Self-citationWan, J., Chen, W., Jia, C., Zheng, L., Dong, J., Zheng, X., Wang, Y., Yan, W., Chen, C., Peng, Q., et al. (2018) · Advanced Materials · doi:10.1002/adma.201705369 · Cited by 1,036
Cited by
Ji, G., Wang, J., Liang, Z., Jia, K., Ma, J., Zhuang, Z., Zhou, G., & Cheng, H.-M. (2023) · Nature Communications · doi:10.1038/s41467-023-36197-6 · Cited by 518
Fast-charging cathode materials for lithium & sodium ion batteries
Yuan, M., Liu, H., & Ran, F. (2023) · Materials Today · doi:10.1016/j.mattod.2023.02.007 · Cited by 272
Metadata
- Authors
- Wang, R., Chen, X., Huang, Z., Yang, J., Liu, F., Chu, M., Liu, T., Wang, C., Zhu, W., Li, S., Li, S., Zheng, J., Chen, J., He, L., Jin, L., Pan, F., & Xiao, Y.
- Venue
- Nature Communications
- Published
- 2021-05-25
- Volume
- 12
- Issue
- 1
- Pages
- 3085-3085
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W3164681617
- Cited by
- 217
- References
- 48
- FWCI
- 8.57
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.