CoChat

In-situ atomic tracking of intermetallic compound formation during thermal annealing

Open access

The DOI matches its Crossref record; 44 of the 44 references it cites were found in a registry or an index.

Abstract

Intermetallic compounds (IMCs) with ordered atomic structure have gained great attention as nanocatalysts for its enhanced activity and stability. Although the reliance of IMC preparation on high-temperature annealing is well known, a comprehensive understanding of the formation mechanisms of IMCs in this process is currently lacking. Here, we employ aberration-corrected high-angle annular dark-field scanning transmission electron microscopy (AC-HAADF-STEM) to track the formation process of IMCs on carbon supports during in-situ annealing, by taking PtFe as a case study within an industry-relevant impregnation synthesis framework. We directly discern five different stages at the atomic level: initial atomic precursors; Pt cluster formation; Pt-Fe disordered alloying; structurally ordered Pt3Fe formation, and final Pt3Fe-PtFe IMC conversion. In particular, we find that the crucial role of high-temperature annealing resides in facilitating the diffusion of Fe towards Pt, enabling the creation of alloys with the targeted stoichiometric ratio, which in turn provides the thermodynamic driving force for the disorder-to-order transition. The mechanisms of intermetallic compound (IMC) formation during annealing are poorly understood. Here, the authors identify five stages of PtFe-IMC formation at the atomic level using in-situ STEM, emphasizing the role of high temperature in achieving the targeted stoichiometric ratio.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1038/s41467-024-51541-0

Cites

44 of 44 references verified0 citation errors · 0 not checkable

Statistics

Figures

Fig. 1 Formation process of PtFe IMC. a–e Time-series AC-HAADF-STEM images of a specific nanoparticle. Scale bar: 2 nm. f–h FFT pattern of the nanoparticle in c–e and corresponding schematic crystal structure (i–k), respectively. l Ex-situ XRD pattern after heating at different temperatures compared with PtFe (ICSD No.42589) and Pt3Fe (ICSD No.56275). m The normalized in-situ X-ray absorption near-edge spectra (XANES) at the Pt L3-edge of samples annealed at different temperatures. Note: the XX in PtFe-XX represents the annealing temperature. n The k3-weighted Fourier transform extended X-ray absorption fine structure spectra (EXAFS) in R-space. The dotted lines indicate the fitting results. o The change of Pt-Fe, Pt-Pt coordination number and corresponding ratio with the annealing temperature. Source data are provided as a Source Data file.
Fig. 1 Formation process of PtFe IMC. a–e Time-series AC-HAADF-STEM images of a specific nanoparticle. Scale bar: 2 nm. f–h FFT pattern of the nanoparticle in c–e and corresponding schematic crystal structure (i–k), respectively. l Ex-situ XRD pattern after heating at different temperatures compared with PtFe (ICSD No.42589) and Pt3Fe (ICSD No.56275). m The normalized in-situ X-ray absorption near-edge spectra (XANES) at the Pt L3-edge of samples annealed at different temperatures. Note: the XX in PtFe-XX represents the annealing temperature. n The k3-weighted Fourier transform extended X-ray absorption fine structure spectra (EXAFS) in R-space. The dotted lines indicate the fitting results. o The change of Pt-Fe, Pt-Pt coordination number and corresponding ratio with the annealing temperature. Source data are provided as a Source Data file.CC BY-NC-ND · PubMed Central
Fig. 2 Representative atomic arrangements of Pt3Fe and PtFe IMC. a, c, g, i Nanoparticles with ordered Pt3Fe or PtFe IMC phases in typical zone axis direction during heating: (a) Pt3Fe IMC nanoparticle along [100] zone axis after heating to 750 °C and corresponding FFT pattern (b). c Pt3Fe IMC nanoparticle along [110] zone axis and corresponding FFT pattern (d). e 3D atom-overlapping Gaussian-function fitting mapping of c. f Simulated STEM image of Pt3Fe IMC along [110] zone axis, inset is the corresponding 3D atom-overlapping Gaussian-function fitting mapping. g PtFe IMC nanoparticle along [110] zone axis and corresponding FFT pattern (h). i PtFe IMC nanoparticle along [100] zone axis after heating to 950 °C and corresponding FFT pattern (j). k 3D atom-overlapping Gaussian-function fitting mapping of i. l Simulated STEM image of PtFe IMC along [100] zone axis, inset is the corresponding 3D atom-overlapping Gaussian-function fitting mapping. The inset in a, c, g, i is the corresponding schematic diagram of atomic structure.
Fig. 2 Representative atomic arrangements of Pt3Fe and PtFe IMC. a, c, g, i Nanoparticles with ordered Pt3Fe or PtFe IMC phases in typical zone axis direction during heating: (a) Pt3Fe IMC nanoparticle along [100] zone axis after heating to 750 °C and corresponding FFT pattern (b). c Pt3Fe IMC nanoparticle along [110] zone axis and corresponding FFT pattern (d). e 3D atom-overlapping Gaussian-function fitting mapping of c. f Simulated STEM image of Pt3Fe IMC along [110] zone axis, inset is the corresponding 3D atom-overlapping Gaussian-function fitting mapping. g PtFe IMC nanoparticle along [110] zone axis and corresponding FFT pattern (h). i PtFe IMC nanoparticle along [100] zone axis after heating to 950 °C and corresponding FFT pattern (j). k 3D atom-overlapping Gaussian-function fitting mapping of i. l Simulated STEM image of PtFe IMC along [100] zone axis, inset is the corresponding 3D atom-overlapping Gaussian-function fitting mapping. The inset in a, c, g, i is the corresponding schematic diagram of atomic structure.CC BY-NC-ND · PubMed Central
Fig. 3 In-situ analysis of elemental distribution during conversion. HAADF-STEM images and corresponding EDS elemental mapping of the same region annealing at different temperatures: (a–d) 750 °C, (f–i) 850 °C, and (k–n) 950 °C. e, j, o Statistic analysis of Pt/Fe ratio in each particle at different temperatures: (e) 750 °C, (j) 850 °C, and (o) 950 °C. HAADF-STEM images and corresponding EDS elemental mappings of the same nanoparticle at 750 °C (p, q), 850 °C (r, s) and 950 °C (t, u). v Quantitative analysis of the atomic percentage of Pt and Fe elements corresponding to the white square area at different temperatures. Source data are provided as a Source Data file.
Fig. 3 In-situ analysis of elemental distribution during conversion. HAADF-STEM images and corresponding EDS elemental mapping of the same region annealing at different temperatures: (a–d) 750 °C, (f–i) 850 °C, and (k–n) 950 °C. e, j, o Statistic analysis of Pt/Fe ratio in each particle at different temperatures: (e) 750 °C, (j) 850 °C, and (o) 950 °C. HAADF-STEM images and corresponding EDS elemental mappings of the same nanoparticle at 750 °C (p, q), 850 °C (r, s) and 950 °C (t, u). v Quantitative analysis of the atomic percentage of Pt and Fe elements corresponding to the white square area at different temperatures. Source data are provided as a Source Data file.CC BY-NC-ND · PubMed Central
Fig. 4 Transition from Pt3Fe to PtFe IMC. a–d Time-series AC-HAADF-STEM images. e–h FFT patterns correspond to the orange and blue dashed squares in a–d, respectively. False color is added to guide the vision. i HAADF-STEM image imposed with iFFT image (orange color), generated from the superlattice spots of Pt3Fe {001}. j–l HAADF-STEM images imposed with iFFT image (yellow color), generated from the superlattice spots of PtFe {011}. Inset is the FFT pattern used to generate the iFFT image. m–p Atomic models corresponding a–d to illustrate the orientation relationship and structure evolution. q–t HAADF-STEM images of nanoparticles that are transforming from Pt3Fe to PtFe through Fe diffusion. Scale bar: 2 nm.
Fig. 4 Transition from Pt3Fe to PtFe IMC. a–d Time-series AC-HAADF-STEM images. e–h FFT patterns correspond to the orange and blue dashed squares in a–d, respectively. False color is added to guide the vision. i HAADF-STEM image imposed with iFFT image (orange color), generated from the superlattice spots of Pt3Fe {001}. j–l HAADF-STEM images imposed with iFFT image (yellow color), generated from the superlattice spots of PtFe {011}. Inset is the FFT pattern used to generate the iFFT image. m–p Atomic models corresponding a–d to illustrate the orientation relationship and structure evolution. q–t HAADF-STEM images of nanoparticles that are transforming from Pt3Fe to PtFe through Fe diffusion. Scale bar: 2 nm.CC BY-NC-ND · PubMed Central
Fig. 5 Theoretical understanding of the formation of PtFe IMC. a Calculated energy analysis of a Fe atom alloying with a Pt9 cluster. b Calculated energy analysis of a Fe atom alloying with a Pt45Fe14 cluster. CI-NEB: climbing image-nudged elastic band. c Binary phase diagrams of Pt-Fe. d Schematic illustration of the formation process of PtFe IMC. Source data are provided as a Source Data file.
Fig. 5 Theoretical understanding of the formation of PtFe IMC. a Calculated energy analysis of a Fe atom alloying with a Pt9 cluster. b Calculated energy analysis of a Fe atom alloying with a Pt45Fe14 cluster. CI-NEB: climbing image-nudged elastic band. c Binary phase diagrams of Pt-Fe. d Schematic illustration of the formation process of PtFe IMC. Source data are provided as a Source Data file.CC BY-NC-ND · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 44 references

Cited by

See all 62

Metadata

Authors
Han, X., Zhou, Y., Tai, X., Wu, G., Chen, C., Hong, X., Tong, L., Xu, F., Liang, H.-W., & Lin, Y.
Affiliations
  • University of Science and Technology of China (CN)
  • Ningbo University (CN)
  • Chinese Academy of Sciences (CN)
Corresponding author
  • Tong, Lei
  • Xu, Fangfang
  • Lin, Yue
Venue
Nature Communications
Published
2024-08-22
Volume
15
Issue
1
Pages
7200-7200
ISSN
2041-1723 (ISSN-L)
OpenAlex
W4401793951
Cited by
53
References
44
Citations by year
2026: 23 · 2025: 29 · 2024: 1
FWCI
5.17
Type
journal article
Language
en
Open access
Licence
Locations
  • Nature Communications (publishedVersion, cc-by-nc-nd)
  • PubMed Central (publishedVersion, cc-by-nc-nd)
  • PubMed (publishedVersion)
  • RePEc: Research Papers in Economics (submittedVersion)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
Funders
China Postdoctoral Science Foundation ((2023M743348)
Topics
  • Physical Sciences › Materials Science › Materials Chemistry › Catalytic Processes in Materials Science
  • Life Sciences › Biochemistry, Genetics and Molecular Biology › Structural Biology › Advanced Electron Microscopy Techniques and Applications
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
Keywords
intermetallic compound formation, Pt3Fe, annealing, disorder-to-order transition, iron diffusion, impregnation synthesis, carbon support, platinum clusters, alloy stoichiometry

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: In-situ atomic tracking of intermetallic compound formation during thermal annealing. https://app.cochat.ai/papers/10.1038/s41467-024-51541-0
The paper
Han, X., Zhou, Y., Tai, X., Wu, G., Chen, C., Hong, X., Tong, L., Xu, F., Liang, H.-W., & Lin, Y. (2024). In-situ atomic tracking of intermetallic compound formation during thermal annealing. Nature Communications. https://doi.org/10.1038/s41467-024-51541-0

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.