Quantifying inactive lithium in lithium metal batteries
Open accessThe DOI matches its Crossref record; 43 of the 43 references it cites were found in a registry or an index.
Abstract
Lithium metal anodes offer high theoretical capacities (3,860 milliampere-hours per gram)1, but rechargeable batteries built with such anodes suffer from dendrite growth and low Coulombic efficiency (the ratio of charge output to charge input), preventing their commercial adoption2,3. The formation of inactive (‘dead’) lithium— which consists of both (electro)chemically formed Li+ compounds in the solid electrolyte interphase and electrically isolated unreacted metallic Li0 (refs 4,5)—causes capacity loss and safety hazards. Quantitatively distinguishing between Li+ in components of the solid electrolyte interphase and unreacted metallic Li0 has not been possible, owing to the lack of effective diagnostic tools. Optical microscopy6, in situ environmental transmission electron microscopy7,8, X-ray microtomography9 and magnetic resonance imaging10 provide a morphological perspective with little chemical information. Nuclear magnetic resonance11, X-ray photoelectron spectroscopy12 and cryogenic transmission electron microscopy13,14 can distinguish between Li+ in the solid electrolyte interphase and metallic Li0, but their detection ranges are limited to surfaces or local regions. Here we establish the analytical method of titration gas chromatography to quantify the contribution of unreacted metallic Li0 to the total amount of inactive lithium. We identify the unreacted metallic Li0, not the (electro)chemically formed Li+ in the solid electrolyte interphase, as the dominant source of inactive lithium and capacity loss. By coupling the unreacted metallic Li0 content to observations of its local microstructure and nanostructure by cryogenic electron microscopy (both scanning and transmission), we also establish the formation mechanism of inactive lithium in different types of electrolytes and determine the underlying cause of low Coulombic efficiency in plating and stripping (the charge and discharge processes, respectively, in a full cell) of lithium metal anodes. We propose strategies for making lithium plating and stripping more efficient so that lithium metal anodes can be used for next-generation high-energy batteries. Titration gas chromatography is developed as an analytical method of distinguishing between lithium metal and lithium compounds within a cycled battery and assessing the amount of unreacted metallic lithium available.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“In addition, formation of mossy structures results in poor Coulombic efficiency: this is due to the loss of capacity involved in the formation of a new SEI on the increasing lithium surface area, and also due to formation of electrically isolated lithium metal structures that are, thus, electrochemically inactive.[247][248][249]”
From Current Challenges and Routes Forward for Nonaqueous Lithium–Air Batteries (2020) · cites this paper as [247]
In the citing paper
“When the Li + salt concentration drops to zero at the Li metalelectrolyte interface (which happens at a time known as the Sand's time), 250 the scarcity of Li + ions supply promotes the deposition onto surface protrusions (tip growth mode), over the growth of mossy deposits that grow from their roots (Fig. 17a).247”
From Current Challenges and Routes Forward for Nonaqueous Lithium–Air Batteries (2020) · cites this paper as [247]
In the citing paper
“The formation of Li dendrites is associated to depletion of Li + ions in the vicinity of the Li metal surface in Li plating experiments.”
From Current Challenges and Routes Forward for Nonaqueous Lithium–Air Batteries (2020) · cites this paper as [247]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Issues and challenges facing rechargeable lithium batteries
Tarascon, J.-M., & Armand, M. (2001) · Nature · doi:10.1038/35104644 · Cited by 21,130
Nonaqueous Liquid Electrolytes for Lithium-Based Rechargeable Batteries
Xu, K. (2004) · Chemical Reviews · doi:10.1021/cr030203g · Cited by 7,437
Self-citationReviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
Toward Safe Lithium Metal Anode in Rechargeable Batteries: A Review
Cheng, X.-B., Zhang, R., Zhao, C.-Z., & Zhang, Q. (2017) · Chemical Reviews · doi:10.1021/acs.chemrev.7b00115 · Cited by 6,197
Lithium metal anodes for rechargeable batteries
Xu, W., Wang, J., Ding, F., Chen, X., Nasybulin, E., Zhang, Y., & Zhang, J.-G. (2014) · Energy Environ. Sci. · doi:10.1039/c3ee40795k · Cited by 4,704
Self-citationHigh rate and stable cycling of lithium metal anode
Qian, J., Henderson, W. A., Xu, W., Bhattacharya, P., Engelhard, M., Borodin, O., & Zhang, J.-G. (2015) · Nature Communications · doi:10.1038/ncomms7362 · Cited by 2,561
Dendrite-Free Lithium Deposition via Self-Healing Electrostatic Shield Mechanism
Ding, F., Xu, W., Graff, G. L., Zhang, J., Sushko, M. L., Chen, X., Shao, Y., Engelhard, M. H., Nie, Z., Xiao, J., et al. (2013) · Journal of the American Chemical Society · doi:10.1021/ja312241y · Cited by 2,107
Electrical Energy Storage and Intercalation Chemistry
Whittingham, M. S. (1976) · Science · doi:10.1126/science.192.4244.1126 · Cited by 1,919
A Review of Solid Electrolyte Interphases on Lithium Metal Anode
Cheng, X., Zhang, R., Zhao, C., Wei, F., Zhang, J., & Zhang, Q. (2016) · Advanced Science · doi:10.1002/advs.201500213 · Cited by 1,786
Transition of lithium growth mechanisms in liquid electrolytes
Bai, P., Li, J., Brushett, F. R., & Bazant, M. Z. (2016) · Energy & Environmental Science · doi:10.1039/c6ee01674j · Cited by 1,591
Self-citation
Cited by
Mitigating Thermal Runaway of Lithium-Ion Batteries
Feng, X., Ren, D., He, X., & Ouyang, M. (2020) · Joule · doi:10.1016/j.joule.2020.02.010 · Cited by 1,735
Interfaces and Interphases in All-Solid-State Batteries with Inorganic Solid Electrolytes
Banerjee, A., Wang, X., Fang, C., Wu, E. A., & Meng, Y. S. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00101 · Cited by 1,526
Self-citationYu, Z., Wang, H., Kong, X., Huang, W., Tsao, Y., Mackanic, D. G., Wang, K., Wang, X., Huang, W., Choudhury, S., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0634-5 · Cited by 1,228
Self-citationCarbon-free high-loading silicon anodes enabled by sulfide solid electrolytes
Tan, D. H. S., Chen, Y., Yang, H., Bao, W., Sreenarayanan, B., Doux, J., Li, W., Lu, B., Ham, S., Sayahpour, B., et al. (2021) · Science · doi:10.1126/science.abg7217 · Cited by 1,062
Self-citationUnderstanding and applying coulombic efficiency in lithium metal batteries
Xiao, J., Li, Q., Bi, Y., Cai, M., Dunn, B., Glossmann, T., Liu, J., Osaka, T., Sugiura, R., Wu, B., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0648-z · Cited by 1,053
Self-citation
Metadata
- Authors
- Fang, C., Li, J., Zhang, M., Zhang, Y., Yang, F., Lee, J. Z., Lee, M.-H., Alvarado, J., Schroeder, M. A., Yang, Y., Lu, B., Williams, N., Ceja, M., Yang, L., Cai, M., Gu, J., Xu, K., Wang, X., & Meng, Y. S.
- Venue
- Nature
- Published
- 2019-08-21
- Volume
- 572
- Issue
- 7770
- Pages
- 511-515
- ISSN
- 0028-0836 (ISSN-L)
- 1476-4687
- OpenAlex
- W2899054965
- Cited by
- 1,413
- References
- 43
- FWCI
- 53.13
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.