Dendrite initiation and propagation in lithium metal solid-state batteries

Open access
Ning, Ziyang, Li, Guanchen, Melvin, Dominic L. R., Chen, Yang, Bu, Junfu, Spencer-Jolly, Dominic, Liu, Junliang, Hu, Bingkun, Gao, Xiangwen, Perera, Johann, Gong, Chen, Pu, Shengda D., Zhang, Shengming, Liu, Boyang, Hartley, Gareth O., Bodey, Andrew J., Todd, Richard I., Grant, Patrick S., Armstrong, David E. J., Marrow, T. James, Monroe, Charles W., Bruce, Peter G. · 2023 · Nature

Abstract

Analysis of dendrite initiation, owing to filling of pores with lithium by means of microcracks, and propagation, caused by wedge opening, shows that there are two separate processes during dendrite failure of lithium metal solid-state batteries. All-solid-state batteries with a Li anode and ceramic electrolyte have the potential to deliver a step change in performance compared with today’s Li-ion batteries^ 1 , 2 . However, Li dendrites (filaments) form on charging at practical rates and penetrate the ceramic electrolyte, leading to short circuit and cell failure^ 3 , 4 . Previous models of dendrite penetration have generally focused on a single process for dendrite initiation and propagation, with Li driving the crack at its tip^ 5 – 9 . Here we show that initiation and propagation are separate processes. Initiation arises from Li deposition into subsurface pores, by means of microcracks that connect the pores to the surface. Once filled, further charging builds pressure in the pores owing to the slow extrusion of Li (viscoplastic flow) back to the surface, leading to cracking. By contrast, dendrite propagation occurs by wedge opening, with Li driving the dry crack from the rear, not the tip. Whereas initiation is determined by the local (microscopic) fracture strength at the grain boundaries, the pore size, pore population density and current density, propagation depends on the (macroscopic) fracture toughness of the ceramic, the length of the Li dendrite (filament) that partially occupies the dry crack, current density, stack pressure and the charge capacity accessed during each cycle. Lower stack pressures suppress propagation, markedly extending the number of cycles before short circuit in cells in which dendrites have initiated.

Overview

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1038/s41586-023-05970-4

Cites

17 of 17 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 17 references

Metadata

Authors
Ning, Z., Li, G., Melvin, D. L. R., Chen, Y., Bu, J., Spencer-Jolly, D., Liu, J., Hu, B., Gao, X., Perera, J., Gong, C., Pu, S. D., Zhang, S., Liu, B., Hartley, G. O., Bodey, A. J., Todd, R. I., Grant, P. S., Armstrong, D. E. J., Marrow, T. J., Monroe, C. W., & Bruce, P. G.
Venue
Nature
Published
2023-06-07
Volume
618
Issue
7964
Pages
287-293
ISSN
  • 0028-0836 (ISSN-L)
  • 1476-4687
OpenAlex
W4379740411
Cited by
584
References
17
FWCI
42.81
Type
journal article
Language
en
Open access
green

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Dendrite initiation and propagation in lithium metal solid-state batteries. https://app.cochat.ai/papers/10.1038/s41586-023-05970-4
The paper
Ning, Z., Li, G., Melvin, D. L. R., Chen, Y., Bu, J., Spencer-Jolly, D., Liu, J., Hu, B., Gao, X., Perera, J., Gong, C., Pu, S. D., Zhang, S., Liu, B., Hartley, G. O., Bodey, A. J., Todd, R. I., Grant, P. S., Armstrong, D. E. J., . . . Bruce, P. G. (2023). Dendrite initiation and propagation in lithium metal solid-state batteries. Nature. https://doi.org/10.1038/s41586-023-05970-4

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.