CoChat

Formation of Green Rust and Immobilization of Nickel in Response to Bacterial Reduction of Hydrous Ferric Oxide

Parmar, Y. A. Gorby, T. J. Beveridg, N. · 2001 · Geomicrobiology Journal
Cited by 72

The DOI matches its Crossref record; 2 of the 2 references it cites were found in a registry or an index.

Abstract

This investigation documents the formation of Green Rust (GR) and immobilization of Ni 2+ in response to bacterial reduction of hydrous ferric oxide (HFO). In the absence of Ni 2+ , 79% of the total Fe(III) present as HFO was reduced; at 10 -3 and 10 -4 M Ni 2+ , 36% of the total Fe(III) was reduced, whereas 45 to 50% of the total Fe(III) was reduced at 10 -5 M Ni 2+ . The inhibitory effect of 10 -3 and 10 -4 M Ni 2+ on Fe(III)-reduction corresponded to a 50% decrease in number of viable cells relative to the Ni 2+ -free condition, and a 25% decrease at 10 -5 M Ni 2+ . A prominent GR peak at d = 10.9 nm was evident in X-ray diffraction patterns of postreduction residual solids from the cultures. Minor peaks arising for vivianite and magnetite were also present. In samples prepared for scanning electron microscopy, thin hexagonal plates of GR were easily distinguished as a solid phase transformation product of HFO. Small hexagonal sheets and fragments of larger GR plates were also observed in transmission electron microscopy whole mounts together with bacteria that were mineralized by surface precipitates of microcrystalline magnetite. Energy dispersive spectroscopy (EDS) confirmed that GR contained Fe and P, as well as Ni in those samples taken from the Ni 2+ -amended experiments. EDS detected neither P nor Ni in the magnetite precipitates associated with the bacterial cells. Dissolved Ni2 + concentrations decreased in an exponential fashion with respect to time in all experimental systems, corresponding to an overall first-order rate constant k of -0.030 day -1 . At the same time, a strong linear relationship (r 2 = 0.99) between the dissolved and solid phase Ni 2+ /Fe 2+ ratios over the entire period of the Fe(III)reduction experiments provided evidence that the solid-phase partitioning of Ni 2+ in GR extended from equilibrium solid-solution behavior.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1080/014904501753210549

Cites

2 of 2 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 2 references

Cited by

See all 72

Metadata

Authors
Parmar, Y. A. G.
Venue
Geomicrobiology Journal
Published
2001-10
Volume
18
Issue
4
Pages
375-385
ISSN
  • 0149-0451 (ISSN-L)
  • 1521-0529
OpenAlex
W2158513804
Cited by
72
References
2
FWCI
5.69
Type
journal article
Language
en
Open access
closed

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Formation of Green Rust and Immobilization of Nickel in Response to Bacterial Reduction of Hydrous Ferric Oxide. https://app.cochat.ai/papers/10.1080/014904501753210549
The paper
Parmar, Y. A. G. (2001). Formation of Green Rust and Immobilization of Nickel in Response to Bacterial Reduction of Hydrous Ferric Oxide. Geomicrobiology Journal. https://doi.org/10.1080/014904501753210549

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.