Effect of Grain Size on Hertzian Contact Damage in Alumina
The DOI matches its Crossref record; 14 of the 14 references it cites were found in a registry or an index.
Abstract
The role of microstructural scale on deformation‐micro fracture damage induced by contact with spheres is investigated in monophase alumina ceramics over a range 3–48 μ in grain size. Measurement of a universal indentation stress–strain curve indicates a critical contact pressure ≅5 GPa, above which irreversible deformation occurs in alumina. A novel sectioning technique identifies the deformation elements as intragrain shear faults, predominantly crystallographic twins, within a confining subsurface zone of intense compression‐shear stress. The twins concentrate the shear stresses at the grain boundaries and, above a threshold grain size, initiate tensile intergranular microcracks. Below this threshold size, classical Hertzian cone fractures initiate outside the contact circle. Above the threshold, the density and scale of subsurface‐zone microcracks increase dramatically with increasing grain size, ultimately dominating the cone fractures. The damage process is stochastic, highlighting the microstructural discreteness of the initial deformation field; those grains which lie in the upper tail of the grain‐size distribution and which have favorable crystallographic orientation relative to local shear stresses in the contact field are preferentially activated. Initial flaw state is not an important factor, because the contact process creates its own flaw population. These and other generic features of the damage process will be discussed in relation to microstructural design of polycrystalline ceramics.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Johnson, K. L. (1985) · Cambridge University Press eBooks · doi:10.1017/cbo9781139171731 · Cited by 7,796
Fundamentals of rock mechanics
(1974) · International Journal of Rock Mechanics and Mining Sciences & Geomechanics Abstracts · doi:10.1016/0148-9062(74)92205-0 · Cited by 4,907
Lawn, B. (1993) · Cambridge University Press eBooks · doi:10.1017/cbo9780511623127 · Cited by 4,759
Self-citationIndentation fracture: principles and applications
Lawn, B., & Wilshaw, R. (1975) · Journal of Materials Science · doi:10.1007/bf00823224 · Cited by 1,321
Self-citationPowder Processing Science and Technology for Increased Reliability
Lange, F. F. (1989) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1989.tb05945.x · Cited by 1,188
Hardness, Toughness, and Brittleness: An Indentation Analysis
Lawn, B. R., & Marshall, D. B. (1979) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1979.tb19075.x · Cited by 889
Self-citationMicrofracture beneath point indentations in brittle solids
Lawn, B. R., & Swain, M. V. (1975) · Journal of Materials Science · doi:10.1007/bf00541038 · Cited by 717
Self-citationPlastic deformation of single crystals of sapphire: Basal slip and twinning
Kronberg, M. L. (1957) · Acta Metallurgica · doi:10.1016/0001-6160(57)90090-1 · Cited by 577
SWANSON, P. L., FAIRBANKS, C. J., LAWN, B. R., MAI, Y., & HOCKEY, B. J. (1987) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1987.tb04982.x · Cited by 534
Self-citationOn the theory of Hertzian fracture
Frank, F. C., & Lawn, B. R. (1967) · Proceedings of the Royal Society of London. Series A. Mathematical and Physical Sciences · doi:10.1098/rspa.1967.0137 · Cited by 500
Self-citation
Cited by
Indentation of Ceramics with Spheres: A Century after Hertz
Lawn, B. R. (1998) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1998.tb02580.x · Cited by 734
Self-citationContact-damage-resistant ceramic/single-wall carbon nanotubes and ceramic/graphite composites
Wang, X., Padture, N. P., & Tanaka, H. (2004) · Nature Materials · doi:10.1038/nmat1161 · Cited by 403
Self-citationMechanical properties of cathode materials for lithium-ion batteries
Stallard, J. C., Wheatcroft, L., Booth, S. G., Boston, R., Corr, S. A., De Volder, M. F. L., Inkson, B. J., & Fleck, N. A. (2022) · Joule · doi:10.1016/j.joule.2022.04.001 · Cited by 336
Toughness Properties of a Silicon Carbide with an in Situ Induced Heterogeneous Grain Structure
Padture, N. P., & Lawn, B. R. (1994) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1994.tb04637.x · Cited by 257
Self-citationOverview: Damage in brittle layer structures from concentrated loads
Lawn, B. R., Deng, Y., Miranda, P., Pajares, A., Chai, H., & Kim, D. K. (2002) · Journal of Materials Research · doi:10.1557/jmr.2002.0440 · Cited by 194
Self-citationBrittle Fracture versus Quasi Plasticity in Ceramics: A Simple Predictive Index
Rhee, Y., Kim, H., Deng, Y., & Lawn, B. R. (2001) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2001.tb00698.x · Cited by 166
Self-citationFracture mode transitions in brittle coatings on compliant substrates as a function of thickness
Chai, H., & Lawn, B. R. (2004) · Journal of Materials Research · doi:10.1557/jmr.2004.0219 · Cited by 81
Self-citation
Metadata
- Authors
- Guiberteau, F., Padture, N. P., & Lawn, B. R.
- Venue
- Journal of the American Ceramic Society
- Publisher
- Wiley
- Published
- 1994-07
- Volume
- 77
- Issue
- 7
- Pages
- 1825-1831
- ISSN
- 0002-7820 (ISSN-L)
- 1551-2916
- OpenAlex
- W1982560934
- Cited by
- 254
- References
- 14
- FWCI
- 25.31
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.