Porous Titania Ceramic Prepared by Mimicking Silicified Wood
The DOI matches its Crossref record; 1 of the 1 references it cites were found in a registry or an index.
Abstract
A porous titania ceramic with a woodlike microstructure that was analogous to silicified wood was prepared. The production of “titanified wood” was performed using the following process: (i) introduction of titanium tetraisopropoxide into wood materials via vacuum infiltration, (ii) hydrolysis of the titanium tetraisopropoxide in the cell structure to form a titania gel, and (iii) firing at a temperature of 600°–1400°C in air. The resulting titania ceramic had the same external and internal forms of the original wood.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The range of wood-templated ceramics has been extended to oxidic ceramics like titania (Ota et al. 2000), zirconia and alumina (Mizutani et al. 2005).”
From PETRIFACTIONS AND WOOD-TEMPLATED CERAMICS: COMPARISONS BETWEEN NATURAL AND ARTIFICIAL SILICIFICATION (2015) · cites this paper as Ota et al. 2000
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Leo, R. F., & Barghoorn, E. S. (1976) · Botanical Museum leaflets, Harvard University · doi:10.5962/p.295209 · Cited by 166
Research works printed but not linked: 5
- 10.1126/science.1546311 · DOI · Paper page
- 10.1111/j.1151-2916.1991.tb04047.x · doi:10.1111/j.1151-2916.1991.tb04047.x
- 10.1016/0025-5408(78)90161-7 · DOI · Paper page
- 10.1016/0025-5408(78)90185-X · DOI
- 10.1111/j.1151-2916.1995.tb07988.x · DOI · Paper page
Cited by
Processing Routes to Macroporous Ceramics: A Review
Studart, A. R., Gonzenbach, U. T., Tervoort, E., & Gauckler, L. J. (2006) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2006.01044.x · Cited by 1,839
Hierarchically Structured Porous Materials for Energy Conversion and Storage
Li, Y., Fu, Z., & Su, B. (2012) · Advanced Functional Materials · doi:10.1002/adfm.201200591 · Cited by 951
Porous electrode materials for lithium-ion batteries–how to prepare them and what makes them special
Vu, A., Qian, Y., & Stein, A. (2012) · Advanced Energy Materials · doi:10.1002/aenm.201200320 · Cited by 719
Macro-porous ceramics: processing and properties
Ohji, T., & Fukushima, M. (2012) · International Materials Reviews · doi:10.1179/1743280411y.0000000006 · Cited by 689
Three-Dimensional Titanium Dioxide Nanomaterials
Fattakhova-Rohlfing, D., Zaleska, A., & Bein, T. (2014) · Chemical Reviews · doi:10.1021/cr500201c · Cited by 418
Biomorphic mineralization: From biology to materials
Fan, T.-X., Chow, S.-K., & Zhang, D. (2009) · Progress in Materials Science · doi:10.1016/j.pmatsci.2009.02.001 · Cited by 349
Toward Strong and Tough Glass and Ceramic Scaffolds for Bone Repair
Fu, Q., Saiz, E., Rahaman, M. N., & Tomsia, A. P. (2013) · Advanced Functional Materials · doi:10.1002/adfm.201301121 · Cited by 247
Biotemplated Materials for Sustainable Energy and Environment: Current Status and Challenges
Zhou, H., Fan, T., & Zhang, D. (2011) · ChemSusChem · doi:10.1002/cssc.201100048 · Cited by 195
Hierarchically porous ZnO with high sensitivity and selectivity to H2S derived from biotemplates
Liu, Z., Fan, T., Zhang, D., Gong, X., & Xu, J. (2009) · Sensors and Actuators B: Chemical · doi:10.1016/j.snb.2008.10.043 · Cited by 194
PETRIFACTIONS AND WOOD-TEMPLATED CERAMICS: COMPARISONS BETWEEN NATURAL AND ARTIFICIAL SILICIFICATION
Dietrich, D., Viney, M., & Lampke, T. (2015) · IAWA Journal · doi:10.1163/22941932-00000094 · Cited by 19
Metadata
- Authors
- Ota, T., Imaeda, M., Takase, H., Kobayashi, M., Kinoshita, N., Hirashita, T., Miyazaki, H., & Hikichi, Y.
- Venue
- Journal of the American Ceramic Society
- Publisher
- Wiley
- Published
- 2000-06
- Volume
- 83
- Issue
- 6
- Pages
- 1521-1523
- ISSN
- 0002-7820
- 1551-2916
- Cited by
- 130
- References
- 1
- Language
- en
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.