In Situ Observation of the Electrochemical Lithiation of a Single SnO 2 Nanowire Electrode
Abstract
Fragile Tin Oxide Electrodes: While tin oxide has a high energy density, and would thus make an attractive anode material for a Li-ion battery, it undergoes significant volume changes when Li is intercalated. The large strains cause cracking, pulverization, and a resultant loss of electrical conduction. Huang et al. (p. 1515 ; see the Perspective by Chiang ) used in situ transmission electron microscopy on a single tin oxide nanowire to identify the physical changes that occur during intercalation and observed a moving cloud of dislocations that separated the reacted and unreacted sections. Upon completion of the electrochemical charging, the nanowire showed up to 90% elongation and a 35% increase in diameter.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Issues and challenges facing rechargeable lithium batteries
Tarascon, J.-M., & Armand, M. (2001) · Nature · doi:10.1038/35104644 · Cited by 21,130
Mechanical alloying and milling
Suryanarayana, C. (2001) · Progress in Materials Science · doi:10.1016/s0079-6425(99)00010-9 · Cited by 8,075
Phospho‐olivines as Positive‐Electrode Materials for Rechargeable Lithium Batteries
Padhi, A. K., Nanjundaswamy, K. S., & Goodenough, J. B. (1997) · Journal of The Electrochemical Society · doi:10.1149/1.1837571 · Cited by 7,933
Piezoelectric Nanogenerators Based on Zinc Oxide Nanowire Arrays
Wang, Z. L., & Song, J. (2006) · Science · doi:10.1126/science.1124005 · Cited by 7,922
High-performance lithium battery anodes using silicon nanowires
Chan, C. K., Peng, H., Liu, G., McIlwrath, K., Zhang, X. F., Huggins, R. A., & Cui, Y. (2008) · Nature Nanotechnology · doi:10.1038/nnano.2007.411 · Cited by 6,683
Battery materials for ultrafast charging and discharging
Kang, B., & Ceder, G. (2009) · Nature · doi:10.1038/nature07853 · Cited by 3,480
Dowsland, K. A., & Thompson, J. M. (2012) · Handbook of Natural Computing · doi:10.1007/978-3-540-92910-9_49 · Cited by 2,432
High-performance lithium-ion anodes using a hierarchical bottom-up approach
Magasinski, A., Dixon, P., Hertzberg, B., Kvit, A., Ayala, J., & Yushin, G. (2010) · Nature Materials · doi:10.1038/nmat2725 · Cited by 2,044
Virus-Enabled Synthesis and Assembly of Nanowires for Lithium Ion Battery Electrodes
Nam, K. T., Kim, D.-W., Yoo, P. J., Chiang, C.-Y., Meethong, N., Hammond, P. T., Chiang, Y.-M., & Belcher, A. M. (2006) · Science · doi:10.1126/science.1122716 · Cited by 1,855
Park, M., Wang, G., Kang, Y., Wexler, D., Dou, S., & Liu, H. (2007) · Angewandte Chemie International Edition · doi:10.1002/anie.200603309 · Cited by 861
Zhu, T., & Li, J. (2010) · Progress in Materials Science · doi:10.1016/j.pmatsci.2010.04.001 · Cited by 828
Self-citationKim, H., & Cho, J. (2008) · Nano Letters · doi:10.1021/nl801853x · Cited by 513
Limthongkul, P., Jang, Y.-I., Dudney, N. J., & Chiang, Y. (2003) · Acta Materialia · doi:10.1016/s1359-6454(02)00514-1 · Cited by 511
Atomic resolution of lithium ions in LiCoO2
Shao-Horn, Y., Croguennec, L., Delmas, C., Nelson, E. C., & O'Keefe, M. A. (2003) · Nature Materials · doi:10.1038/nmat922 · Cited by 273
Defect-induced melting and solid-state amorphization
Fecht, H. J. (1992) · Nature · doi:10.1038/356133a0 · Cited by 269
Bhandakkar, T. K., & Gao, H. (2010) · International Journal of Solids and Structures · doi:10.1016/j.ijsolstr.2010.02.001 · Cited by 202
Lai, W., Erdonmez, C. K., Marinis, T. F., Bjune, C. K., Dudney, N. J., Xu, F., Wartena, R., & Chiang, Y. (2010) · Advanced Materials · doi:10.1002/adma.200903650 · Cited by 178
Self-supported SnO2nanowire electrodes for high-power lithium-ion batteries
Ko, Y.-D., Kang, J. G., Park, J., Lee, S., & Kim, D. (2009) · Nanotechnology · doi:10.1088/0957-4484/20/45/455701 · Cited by 129
Brazier, A., Dupont, L., Laffont, L., Kuwata, N., Kawamura, J., & Tarascon, J. ‐. (2008) · Chemistry of Materials · doi:10.1021/cm7033933 · Cited by 128
Self-supported SnO2 nanowire electrodes for high-power lithium-ion batteries
김동완, 고영대, Park, J., 강진구, & 이성준 (2009) · Cited by 127
Nanorobots for Medicine: How Close Are We?
Kostarelos, K. (2010) · Nanomedicine · doi:10.2217/nnm.10.19 · Cited by 26
Power sources for nanotechnology
Curtright, A. E., Bouwman, P. J., Wartena, R. C., & Lyons, K. S. (2004) · International Journal of Nanotechnology · doi:10.1504/ijnt.2004.003726 · Cited by 14
Cited by
Li-ion battery materials: present and future
Nitta, N., Wu, F., Lee, J. T., & Yushin, G. (2015) · Materials Today · doi:10.1016/j.mattod.2014.10.040 · Cited by 7,389
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
Electrolytes and Interphases in Li-Ion Batteries and Beyond
Xu, K. (2014) · Chemical Reviews · doi:10.1021/cr500003w · Cited by 5,566
Metal Oxides and Oxysalts as Anode Materials for Li Ion Batteries
Reddy, M. V., Subba Rao, G. V., & Chowdari, B. V. R. (2013) · Chemical Reviews · doi:10.1021/cr3001884 · Cited by 2,921
A pomegranate-inspired nanoscale design for large-volume-change lithium battery anodes
Liu, N., Lu, Z., Zhao, J., McDowell, M. T., Lee, H.-W., Zhao, W., & Cui, Y. (2014) · Nature Nanotechnology · doi:10.1038/nnano.2014.6 · Cited by 2,491
Metadata
- Authors
- Huang, J. Y., Zhong, L., Wang, C. M., Sullivan, J. P., Xu, W., Zhang, L. Q., Mao, S. X., Hudak, N. S., Liu, X. H., Subramanian, A., Fan, H., Qi, L., Kushima, A., & Li, J.
- Venue
- Science
- Published
- 2010-12-10
- Volume
- 330
- Issue
- 6010
- Pages
- 1515-1520
- ISSN
- 0036-8075 (ISSN-L)
- 1095-9203
- OpenAlex
- W2007084362
- Cited by
- 1,563
- References
- 22
- FWCI
- 64.54
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.