Electrochromism in Anodic Iridium Oxide Films: II . pH Effects on Corrosion Stability and the Mechanism of Coloration and Bleaching
Abstract
The oxidation state of iridium ions in an oxide film, grown electrochemically on an Ir metal reflector electrode, can be rapidly and reversibly modulated according to the electrochromic redox reaction Ir OH n transparent ⇄ IrO x OH n − x blue ‐ black + x H + + xe By suitable choice of electrolyte composition and potential limits, the coloration and bleaching processes can be effected without causing oxide film growth or dissolution, or electrolyte decomposition. Color‐bleach (c‐b) cycles exhibit reflectance contrast changes, Δ R / R , and charging times, τ, suitable for electrooptic display devices, e.g. , for a film 320 nm thick, Δ R / R = 70 % at λ = 546 nm and τ ≤ 80 msec . Long term corrosion stability is obtainable in mildly acidic sulfate electrolytes, e.g. , 0.5 M Na 2 SO 4 at p H 3.5. Sulfate electrolytes are also apparently unique in preventing degradation of c‐b response times owing to changes in film structure. East write‐erase times are made possible by the highly porous and hydrated nature of the oxide film and the ready availability of the protons required for bleaching from an ‘internal’ source—free H 2 O molecules in the electrolyte contained within the film pores and/or bound H 2 O or OH groups on the oxide surface. The kinetics and mechanism of the electrochromic reaction in anodic iridium oxide films are discussed with particular reference to the requirement for preserving electroneutrality within the bulk oxide. Recent claims that this redox reaction can occur without exchange of protons with the electrolyte are shown not to be substantiated. Attractive features of the electrochromic iridium oxide system for display devices include: ( i ) broad spectral absorption; ( ii ) good contrast ratio; ( iii ) fast response; ( iv ) good corrosion stability; ( v ) good open‐circuit memory in the presence of water and dissolved O 2 ; ( vi ) suitable threshold and switching voltage levels; and ( vii ) the ability to grow and reform the oxide layer in situ in the electrooptic display cell. The charge (∼20 mC cm −2 ) and energy (∼30 mJ cm −2 ) required for coloration and bleaching are similar to those required for other electrochromic oxide systems, e.g. , the tungsten bronzes.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cited by
Electrochemical oxide film formation at noble metals as a surface-chemical process
Conway, B. E. (1995) · Progress in Surface Science · doi:10.1016/0079-6816(95)00040-6 · Cited by 630
Electrochromic materials and devices for energy efficient windows
Lampert, C. M. (1984) · Solar Energy Materials · doi:10.1016/0165-1633(84)90024-8 · Cited by 575
Cherevko, S., Geiger, S., Kasian, O., Mingers, A., & Mayrhofer, K. J. J. (2016) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2016.05.015 · Cited by 332
Tarasevich, M. R., Sadkowski, A., & Yeager, E. (1983) · Comprehensive Treatise of Electrochemistry · doi:10.1007/978-1-4613-3584-9_6 · Cited by 286
Oxygen evolution activity and stability of iridium in acidic media. Part 1. – Metallic iridium
Cherevko, S., Geiger, S., Kasian, O., Mingers, A., & Mayrhofer, K. J. J. (2016) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2016.04.033 · Cited by 272
Metadata
- Authors
- Gottesfeld, S., & McIntyre, J. D. E.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 1979-05-01
- Volume
- 126
- Issue
- 5
- Pages
- 742-750
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W1595808117
- Cited by
- 201
- References
- 0
- FWCI
- 17.58
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Electrochromism in Anodic Iridium Oxide Films: II . pH Effects on Corrosion Stability and the Mechanism of Coloration and Bleaching. https://app.cochat.ai/papers/10.1149/1.2129131
- The paper
- Gottesfeld, S., & McIntyre, J. D. E. (1979). Electrochromism in Anodic Iridium Oxide Films: II . pH Effects on Corrosion Stability and the Mechanism of Coloration and Bleaching. Journal of The Electrochemical Society. https://doi.org/10.1149/1.2129131
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.