Durability Study of Pt∕C and Pt∕CNTs Catalysts under Simulated PEM Fuel Cell Conditions
Abstract
The durability of carbon black supported Pt ( Pt ∕ C ) and multiwalled carbon nanotubes supported Pt (Pt/CNTs) catalysts for potential application in polymer electrolyte membrane fuel cells are investigated using an accelerated durability test. The electrochemical surface area of Pt ∕ C degrades by 49.8% during the 192 - h test time, compared with 26.1% for Pt/CNTs, which is due to Pt particle growth and Pt loss from the support in the form of Pt ions and Pt particles. Transmission electron microscopy and X-ray diffraction analysis show that Pt particles in Pt ∕ CNTs present higher sintering resistance. X-ray photoelectron spectroscopy characterization indicates that CNTs in Pt ∕ CNTs are more resistant to electrochemical oxidation than carbon black in Pt ∕ C . It can be concluded that Pt ∕ CNTs are more stable under electrochemical operation, which can be attributed to specific interaction between Pt and the support and the higher resistance of the support to electrochemical oxidation.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Modification of the surface chemistry of activated carbons
Figueiredo, J. L., Pereira, M. F. R., Freitas, M. M. A., & Órfão, J. J. M. (1999) · Carbon · doi:10.1016/s0008-6223(98)00333-9 · Cited by 2,935
The role of carbon materials in heterogeneous catalysis
Rodríguez-reinoso, F. (1998) · Carbon · doi:10.1016/s0008-6223(97)00173-5 · Cited by 1,760
Instability of Pt∕C Electrocatalysts in Proton Exchange Membrane Fuel Cells
Ferreira, P. J., la O’, G. J., Shao-Horn, Y., Morgan, D., Makharia, R., Kocha, S., & Gasteiger, H. A. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.2050347 · Cited by 1,491
Li, W., Liang, C., Zhou, W., Qiu, J., Zhou, Sun, G., & Xin, Q. (2003) · The Journal of Physical Chemistry B · doi:10.1021/jp022505c · Cited by 1,126
A Reverse-Current Decay Mechanism for Fuel Cells
Reiser, C. A., Bregoli, L., Patterson, T. W., Yi, J. S., Yang, J. D., Perry, M. L., & Jarvi, T. D. (2005) · Electrochemical and Solid-State Letters · doi:10.1149/1.1896466 · Cited by 976
Comparison of high surface Pt/C catalysts by cyclic voltammetry
Pozio, A., De Francesco, M., Cemmi, A., Cardellini, F., & Giorgi, L. (2002) · Journal of Power Sources · doi:10.1016/s0378-7753(01)00921-1 · Cited by 906
Aging mechanisms and lifetime of PEFC and DMFC
Knights, S. D., Colbow, K. M., St-Pierre, J., & Wilkinson, D. P. (2004) · Journal of Power Sources · doi:10.1016/j.jpowsour.2003.09.033 · Cited by 753
Kinetic Model of Platinum Dissolution in PEMFCs
Darling, R. M., & Meyers, J. P. (2003) · Journal of The Electrochemical Society · doi:10.1149/1.1613669 · Cited by 688
Electrocatalytic Corrosion of Carbon Support in PEMFC Cathodes
Roen, L. M., Paik, C. H., & Jarvi, T. D. (2004) · Electrochemical and Solid-State Letters · doi:10.1149/1.1630412 · Cited by 658
Xing, Y. (2004) · The Journal of Physical Chemistry B · doi:10.1021/jp046697i · Cited by 619
Characterization of Vulcan Electrochemically Oxidized under Simulated PEM Fuel Cell Conditions
Kangasniemi, K. H., Condit, D. A., & Jarvi, T. D. (2004) · Journal of The Electrochemical Society · doi:10.1149/1.1649756 · Cited by 599
Surface Area Loss of Supported Platinum in Polymer Electrolyte Fuel Cells
Wilson, M. S., Garzon, F. H., Sickafus, K. E., & Gottesfeld, S. (1993) · Journal of The Electrochemical Society · doi:10.1149/1.2220925 · Cited by 411
Durability of PEFCs at High Humidity Conditions
Xie, J., Wood, D. L., Wayne, D. M., Zawodzinski, T. A., Atanassov, P., & Borup, R. L. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.1830355 · Cited by 382
Sonochemical Oxidation of Multiwalled Carbon Nanotubes
Xing, Y., Li, L., Chusuei, C. C., & Hull, R. V. (2005) · Langmuir · doi:10.1021/la047268e · Cited by 343
Degradation Study of MEA for PEMFCs under Low Humidity Conditions
Endoh, E., Terazono, S., Widjaja, H., & Takimoto, Y. (2004) · Electrochemical and Solid-State Letters · doi:10.1149/1.1739314 · Cited by 321
Durability study of Pt3Ni1 catalysts as cathode in PEM fuel cells
Colón-Mercado, H. R., Kim, H., & Popov, B. N. (2004) · Electrochemistry Communications · doi:10.1016/j.elecom.2004.05.028 · Cited by 222
Preparation of Platinum Supported on Pregraphitized Carbon Blacks
Coloma, F., Sepulveda-Escribano, A., Fierro, J. L. G., & Rodriguez-Reinoso, F. (1994) · Langmuir · doi:10.1021/la00015a025 · Cited by 195
In Situ Analysis of Performance Degradation of a PEMFC under Nonsaturated Humidification
Yu, J., Matsuura, T., Yoshikawa, Y., Islam, M. N., & Hori, M. (2005) · Electrochemical and Solid-State Letters · doi:10.1149/1.1854781 · Cited by 173
Guerrero-Ruiz, A. R., Badenes, P., & Rodríguez-Ramos, I. (1998) · Applied Catalysis A General · doi:10.1016/s0926-860x(98)00187-2 · Cited by 166
Purification of Single-Wall Carbon Nanotubes by Electrochemical Oxidation
Fang, H.-T., Liu, C.-G., Liu, C., Li, F., Liu, M., & Cheng, H.-M. (2004) · Chemistry of Materials · doi:10.1021/cm035263h · Cited by 165
Studies on performance degradation of a direct methanol fuel cell (DMFC) in life test
Liu, J., Zhou, Z., Zhao, X., et al. (2003) · Physical Chemistry Chemical Physics · doi:10.1039/b313478d · Cited by 150
Heat-Treated Carbon-Blacks as Supports for Platinum Catalysts
Coloma-Pascual, F., Sepúlveda‐Escribano, A., & Rodríguez-Reinoso, F. (1995) · Journal of Catalysis · doi:10.1006/jcat.1995.1171 · Cited by 143
Kim, C., Kim, Y. J., Kim, Y. A., Yanagisawa, T., Park, K. C., Endo, M., & Dresselhaus, M. S. (2004) · Journal of Applied Physics · doi:10.1063/1.1804242 · Cited by 125
Performance and lifetime analysis of the kW-class PEMFC stack
Ahn, S., Shin, S.-J., Ha, H. Y., Hong, S.-A., Lee, Y.-C., Lim, T.-W., & Oh, I. (2002) · Journal of Power Sources · doi:10.1016/s0378-7753(01)01032-1 · Cited by 125
Chalkova, E., Pague, M. B., Fedkin, M. V., Wesolowski, D. J., & Lvov, S. N. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.1895225 · Cited by 113
Catalyst Microstructure Examination of PEMFC Membrane Electrode Assemblies vs. Time
Cheng, X., Chen, L., Cheng, P., Chen, Z., Zhang, Y., & Fan, Q. (2003) · Journal of The Electrochemical Society · doi:10.1149/1.1625944 · Cited by 113
Li, G., & Pickup, P. G. (2004) · Electrochimica Acta · doi:10.1016/j.electacta.2004.04.005 · Cited by 111
Dissolution of Nafion® membrane and recast Nafion® film in mixtures of methanol and water
Siroma, Z., Fujiwara, N., Ioroi, T., Yamazaki, S., Yasuda, K., & Miyazaki, Y. (2003) · Journal of Power Sources · doi:10.1016/j.jpowsour.2003.08.024 · Cited by 95
Novel Pt–Ru–Ni/C Catalysts for Methanol Electro-oxidation in Acid Medium
Wang, Z. B., Yin, G., Shi, P. F., & Sun, Y. (2006) · Electrochemical and Solid-State Letters · doi:10.1149/1.2133722 · Cited by 85
Self-citationEffect of heat treatment of activated carbon supports on the loading and activity of Pt catalyst
Kang, M. S., Bae, Y., & Lee, C. (2005) · Carbon · doi:10.1016/j.carbon.2005.01.035 · Cited by 72
In situ FTIR characterization of the electrooxidation of glassy carbon electrodes
Yang, Y., & Lin, Z. G. (1995) · Journal of Applied Electrochemistry · doi:10.1007/bf00262965 · Cited by 62
Degradation Study of MEA for PEMFC under Low Humidity Conditions
Endoh, E. (2004) · ECS Proceedings Volumes · doi:10.1149/200421.0363pv · Cited by 62
Wang, Z. B., Yin, G., & Shi, P. F. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.2120287 · Cited by 46
Self-citationWell-Dispersed Multiwalled Carbon Nanotubes Supported Platinum Nanocatalysts for Oxygen Reduction
Li, X., Ge, S., Hui, C. L., & Hsing, I. (2004) · Electrochemical and Solid-State Letters · doi:10.1149/1.1783111 · Cited by 44
Pt/C obtained from carbon with different treatments and (NH4)2PtCl6 as a Pt precursor
Verde‐Gómez, Y., Alonso-Núñez, G., Ramos, V., Zhang, H., Jacobson, A. J., & Keer, A. (2004) · Applied Catalysis A General · doi:10.1016/j.apcata.2004.09.013 · Cited by 38
Cited by
A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies
Wu, J., Yuan, X. Z., Martin, J. J., Wang, H., Zhang, J., Shen, J., Wu, S., & Merida, W. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.006 · Cited by 1,587
Understanding and approaches for the durability issues of Pt-based catalysts for PEM fuel cell
Shao, Y., Yin, G., & Gao, Y. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.004 · Cited by 1,197
Self-citationNitrogen-doped graphene and its electrochemical applications
Shao, Y., Zhang, S., Engelhard, M. H., Li, G., Shao, G., Wang, Y., Liu, J., Aksay, I. A., & Lin, Y. (2010) · Journal of Materials Chemistry · doi:10.1039/c0jm00782j · Cited by 1,123
Self-citationNanostructured carbon for energy storage and conversion
Candelaria, S. L., Shao, Y., Zhou, W., Li, X., Xiao, J., Zhang, J.-G., Wang, Y., Liu, J., Li, J., & Cao, G. (2012) · Nano Energy · doi:10.1016/j.nanoen.2011.11.006 · Cited by 975
Self-citationShao, Y., Sui, J., Yin, G., & Gao, Y. (2008) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2007.09.047 · Cited by 763
Self-citation
Metadata
- Authors
- Shao, Y., Yin, G., Gao, Y., & Shi, P.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2006
- Volume
- 153
- Issue
- 6
- Pages
- A1093
- ISSN
- 0013-4651 (ISSN-L)
- OpenAlex
- W1998120740
- Cited by
- 411
- References
- 35
- FWCI
- 27.67
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.