Abstract
Bentonite, biotite, illite, kaolin, vermiculite and zeolite were acidified or alkalized with hydrochloric acid or sodium hydroxide at concentrations of 0.1, 1.0 and 5.0 mole dm−3 at room temperature for two weeks. In acid treatments, dissolution of Al prevailed over Si and the opposite was observed in alkali treatments. The XRD patterns showed severe alteration of the crystal structure after acid treatments, whereas sharpening of the XRD peaks after alkali treatments was observed. Illite and kaolin were most resistant to acid attack. with a few exceptions, the surface areas of the minerals computed from both water and nitrogen adsorption isotherms increased with acid and alkali treatments. with increasing reagent concentration, the nitrogen surface area increased faster than the water surface area. well-defined trends were not noted in either changes of average water or nitrogen adsorption energies or in relative amounts of adsorption sites, indicating that the effects of acid and alkali attack are controlled by the individual character of the minerals.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Adsorption of Gases in Multimolecular Layers
Brunauer, S., Emmett, P. H., & Teller, E. (1938) · Journal of the American Chemical Society · doi:10.1021/ja01269a023 · Cited by 28,156
Adsorption Surface Area and Porosity
Gregg, S. J., Sing, K. S. W., & Salzberg, H. W. (1967) · Journal of The Electrochemical Society · doi:10.1149/1.2426447 · Cited by 9,507 · cited 4×
“Silicon oxides, products of mineral destruction, also have low adsorption energy (Gregg and Sing, 1967).”
BackgroundInfluential(1977) · Ceramurgia International · doi:10.1016/0390-5519(77)90076-x · Cited by 2,673
An Introduction to Clay Colloid Chemistry
OLPHEN, H. V. (1964) · Soil Science · doi:10.1097/00010694-196404000-00013 · Cited by 2,573
Agricultural Salinity Assessment and Management
(2011) · American Society of Civil Engineers eBooks · doi:10.1061/9780784411698 · Cited by 910
Adsorption of Gases on Heterogeneous Surfaces
(1992) · Elsevier eBooks · doi:10.1016/c2009-0-21554-6 · Cited by 848 · cited 1×
“imation used for evaluation of energy distribution functions is considered to be precise only at 0 K (Rudzinski and Everett, 1991), one can suspect that the nitrogen adsorption distribution is more realistic because of the low temperature of measurement.”
BackgroundChemistry of clays and clay minerals
Hunter, K. A. (1988) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(88)90287-6 · Cited by 774
An introduction to clay colloid chemistry
Zettlemoyer, A. C. (1978) · Advances in Colloid and Interface Science · doi:10.1016/0001-8686(78)80005-0 · Cited by 637
Lagaly, G. (1978) · Berichte der Bunsengesellschaft für physikalische Chemie · doi:10.1002/bbpc.197800022 · Cited by 501
Pretreatment for Mineralogical Analysis
Kunze, G. W., & Dixon, J. B. (1986) · SSSA Book Series · doi:10.2136/sssabookser5.1.2ed.c5 · Cited by 310
Madejová, J., Bujdák, J., Janek, M., & Komadel, P. (1998) · Spectrochimica Acta Part A Molecular and Biomolecular Spectroscopy · doi:10.1016/s1386-1425(98)00040-7 · Cited by 297
Chemical Weathering of Minerals in Soils
Jackson, M. L., & Sherman, G. D. (1953) · Advances in agronomy · doi:10.1016/s0065-2113(08)60231-x · Cited by 296
Christidis, G. E., Scott, P. W., & DUNHAM, A. C. (1997) · Applied Clay Science · doi:10.1016/s0169-1317(97)00017-3 · Cited by 295 · cited 2×
“The HCl activation of two bentonites leads to a 5-fold increase of the surface area of the raw materials (Christidis et al., 1997).”
BackgroundSurface modification of clay minerals
Bergaya, F., & Lagaly, G. (2001) · Applied Clay Science · doi:10.1016/s0169-1317(01)00063-1 · Cited by 280 · cited 1×
“Treatment of minerals with inorganic acids of rather high concentrations and usually at elevated temperatures, referred to as ‘acid activation’, is commonly used for production of sorbents or catalysts (white carbon blacks) used in industry or environmental protection measures (Bandosz et al., 1992; Bergaya and Lagaly…”
BackgroundThomas, G. W., & Hargrove, W. L. (1984) · Agronomy Monographs · doi:10.2134/agronmonogr12.2ed.c1 · Cited by 242
Localized adsorption on heterogeneous surfaces
Cerofolini, G. F. (1974) · Thin Solid Films · doi:10.1016/0040-6090(74)90235-1 · Cited by 229
Barrios, M. S., González, L. V. F., Rodríguez, M. A. V., & Pozas, J. M. M. (1995) · Applied Clay Science · doi:10.1016/0169-1317(95)00007-q · Cited by 205 · cited 6×
“partial dissolution of the octahedral Mg cations, generating amorphous silica from the tetrahedral sheet (Suárez Barrios et al., 2001). Kooyman et al. (1997) observed a progressive dealumination of various samples of synthetic ZSM-5”
BackgroundInfluentialAdsorption of cadmium and copper by modified kaolinites
Suraj, G., Iyer, C. S. P., & Lalithambika, M. (1998) · Applied Clay Science · doi:10.1016/s0169-1317(98)00043-x · Cited by 169 · cited 1×
“preferentially the octahedral Al ions from the clay structure and forms additional Al OH and Si OH bonds, without disturbing the mineral structure (Suraj et al., 1998).”
BackgroundSmectite Transformation in High Molar KOH Solutions
Bauer, A., & Velde, B. (1999) · Clay Minerals · doi:10.1180/000985599546226 · Cited by 158
Synthesis of illite-smectite from smectite at Earth surface temperatures and high pH
Eberl, D. D., Velde, B., & Mccormick, T. (1993) · Clay Minerals · doi:10.1180/claymin.1993.028.1.06 · Cited by 154
Recent progress in determination of energetic heterogeneity of solids from adsorption data
Jaroniec, M., & Bräuer, P. (1986) · Surface Science Reports · doi:10.1016/0167-5729(86)90004-x · Cited by 143 · cited 1×
“geneous surfaces (Jaroniec et al., 1975; Jaroniec and Brauer, 1986; Rudzinski et al., 1982) the total adsorption at a given pressure P can be expressed as a sum of local adsorptions ai on given sites of energy Ei = (Ea,i Ec), where Ea,i is adsorption energy of i-th site:”
BackgroundStructural and Textural Modifications of Palygorskite and Sepiolite Under Acid Treatment
Myriam, M., Suárez, M., & Martín-Pozas, J. M. (1998) · Clays and Clay Minerals · doi:10.1346/ccmn.1998.0460301 · Cited by 141 · cited 1×
“Myriam (1998) found that under acid treatment, sepiolite is destroyed more rapidly than palygorskite because of its magnesian composition and larger structural microchannels.”
BackgroundAn Ecosystem Approach to Soil Acidification
Ulrich, B. (1991) · Springer eBooks · doi:10.1007/978-3-642-74442-6_3 · Cited by 134
Properties and Catalytic Activity of Acid-Modified Montmorillonite and Vermiculite
Ravichandran, J., & Sivasankar, B. (1997) · Clays and Clay Minerals · doi:10.1346/ccmn.1997.0450609 · Cited by 130 · cited 1×
“Treatment of minerals with inorganic acids of rather high concentrations and usually at elevated temperatures, referred to as ‘acid activation’, is commonly used for production of sorbents or catalysts (white carbon blacks) used in industry or environmental protection measures (Bandosz et al. , 1992; Bergaya and Lagal…”
Harris, L. B. (1968) · Surface Science · doi:10.1016/0039-6028(68)90015-0 · Cited by 126
Adsorption of water vapor on X and Y zeolites exchanged with barium
Moïse, J.-C., Bellat, J. P., & Méthivier, A. (2001) · Microporous and Mesoporous Materials · doi:10.1016/s1387-1811(00)00352-8 · Cited by 126 · cited 1×
“Surface areas of illites from 50 to 200, of zeolites from 100 to 400 and for vermiculites up to 700 mg 1 are found (Newman, 1987; Moise et al., 2001; Volzone et al., 1999).”
BackgroundRudziński, W., Jagiełło, J., & Grillet, Y. (1982) · Journal of Colloid and Interface Science · doi:10.1016/0021-9797(82)90345-9 · Cited by 119 · cited 1×
“geneous surfaces (Jaroniec et al., 1975; Jaroniec and Brauer, 1986; Rudzinski et al., 1982) the total adsorption at a given pressure P can be expressed as a sum of local adsorptions ai on given sites of energy Ei = (Ea,i Ec), where Ea,i is adsorption energy of i-th site:”
BackgroundEffect of Heating and Acid Pre-Treatment on Pore Size Distribution of Sepiolite
Balcı, S. (1999) · Clay Minerals · doi:10.1180/000985599546406 · Cited by 109
Soil acidification from use of too much fertilizer
Wallace, A. M. (1994) · Communications in Soil Science and Plant Analysis · doi:10.1080/00103629409369010 · Cited by 92
Kooyman, P. J., van der Waal, P., & van Bekkum, H. (1997) · Zeolites · doi:10.1016/s0144-2449(96)00106-6 · Cited by 89
Zeolitization of a bentonite and its application to the removal of ammonium ion from waste water
Ruiz, R., Blanco, C., Pesquera, C., González, F., Benito, I., & López, J. L. (1997) · Applied Clay Science · doi:10.1016/s0169-1317(96)00038-5 · Cited by 87 · cited 1×
“by Ruiz et al. (1997) who found that the laminar”
Breen, C., Madejová, J., & Komadel, P. (1995) · Applied Clay Science · doi:10.1016/0169-1317(95)00024-x · Cited by 82
Filippidis, A., Godelitsas, A., Charistos, D., Misaelides, P., & Kassoli-fournaraki, A. (1996) · Applied Clay Science · doi:10.1016/s0169-1317(96)00025-7 · Cited by 79
Ylagan, R. F., Altaner, S. P., & Pozzuoli, A. (2000) · Clays and Clay Minerals · doi:10.1346/ccmn.2000.0480603 · Cited by 69
Textural properties of acid activated glauconite
Srasra, E., & Trabelsi‐Ayadi, M. (2000) · Applied Clay Science · doi:10.1016/s0169-1317(00)00008-9 · Cited by 66 · cited 1×
“(Suárez Barrios et al., 2001). Kooyman et al. (1997) observed a progressive dealumination of various samples of synthetic ZSM-5 zeolites in mineral acids with increase in concentration, temperature and duration of the treatment.”
BackgroundDetermination of energy distribution function from observed adsorption isotherms
Jaroniec, M., Rudziński, W., Sokołowski, S., & Smarzewski, R. (1975) · Colloid & Polymer Science · doi:10.1007/bf01775683 · Cited by 63 · cited 1×
“geneous surfaces (Jaroniec et al., 1975; Jaroniec and Brauer, 1986; Rudzinski et al., 1982) the total adsorption at a given pressure P can be expressed as a sum of local adsorptions ai on given sites of energy Ei = (Ea,i Ec), where Ea,i is adsorption energy of i-th site:”
BackgroundThe theory of polymolecular adsorption
Aranovich, G. L. (1992) · Langmuir · doi:10.1021/la00038a071 · Cited by 58 · cited 1×
“Surface area values were calculated from adsorption data using the linear form of the Aranovich (1992) isotherm: x/[a(1 x)1/2] = 1/(amC) + x/am (1) where x = P/P0, am (kg/kg) is the statistical monolayer capacity and C = exp((Ea-Ec)/RT) is the constant related to the adsorption energy, Ea (J), and…”
MethodBiotite Flakes: Alteration by Chemical and Biological Treatment
Boyle, J. R., Voigt, G. K., & Sawhney, B. L. (1967) · Science · doi:10.1126/science.155.3759.193 · Cited by 58 · cited 1×
“observations (Boyle et al., 1967).”
Textural and structural modifications of saponite from Cerro del Aguila by acid treatment
Barrios, M. S., Buey, C. D. S., Romero, E. G., & Pozas, J. M. M. (2001) · Clay Minerals · doi:10.1180/0009855013640003 · Cited by 27
Drief, A., Nieto, F., & Sánchez‐Navas, A. (2001) · Clays and Clay Minerals · doi:10.1346/ccmn.2001.0490108 · Cited by 20 · cited 1×
“Acid and alkali effects are important controls over mineral weathering (Frank and Gebhardt, 1991; Jackson and Sherman, 1952, 1989; Yatsu, 1988) and genesis (Chermak and Rimstidt, 1987; Drief et al., 2001; Eberl et al., 1993; Huang, 1993).”
BackgroundCharacterization of natural phillipsite modified with orthophosphoric acid
Notario, J. S., García, J. E., Cáceres, J. M., Arteaga, I. J., & González, M. M. (1995) · Applied Clay Science · doi:10.1016/0169-1317(95)00025-y · Cited by 19 · cited 1×
“Natural phillipsite treated with orthophosphoric acid increased the surface area with increasing concentrations of the acid (Notario et al., 1995).”
Background
Cited by
Adsorption of a few heavy metals on natural and modified kaolinite and montmorillonite: A review
Bhattacharyya, K. G., & Gupta, S. S. (2008) · Advances in Colloid and Interface Science · doi:10.1016/j.cis.2007.12.008 · Cited by 1,525
CO2 capture adsorbents functionalized by amine – bearing polymers: A review
Varghese, A. M., & Karanikolos, G. N. (2020) · International Journal of Greenhouse Gas Control · doi:10.1016/j.ijggc.2020.103005 · Cited by 363
Pawar, R. R., Lalhmunsiama, Bajaj, H. C., & Lee, S.-M. (2016) · Journal of Industrial and Engineering Chemistry · doi:10.1016/j.jiec.2015.11.014 · Cited by 232
Bhattacharyya, K. G., & Gupta, S. S. (2008) · Chemical Engineering Journal · doi:10.1016/j.cej.2007.03.005 · Cited by 232
Adsorption of Chromium(VI) from Water by Clays
Bhattacharyya, K. G., & Sen Gupta, S. (2006) · Industrial & Engineering Chemistry Research · doi:10.1021/ie060586j · Cited by 231
Metadata
- Authors
- Jozefaciuk, G., & Bowanko, G.
- Venue
- Clays and Clay Minerals
- Publisher
- Cambridge University Press (CUP)
- Published
- 2002-12
- Volume
- 50
- Issue
- 6
- Pages
- 771-783
- ISSN
- 0009-8604 (ISSN-L)
- 1552-8367
- OpenAlex
- W2136217206
- Cited by
- 211
- References
- 41
- FWCI
- 1.06
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.