Improvements to the Quantitative Assay of Nonrefractory Minerals for Fe(II) and Total Fe Using 1,10-Phenanthroline
Abstract
A method using 1,10-phenanthroline (phen) to quantify Fe(II) and total Fe in nonrefractory minerals was modified to improve the accuracy and precision and to eliminate the inconvenience of performing much of the analysis under darkroom conditions. Reagents were combined to minimize solution-handling errors, volumes of the reagent additions were determined gravimetrically and the acid-matrix solution was preheated to near-boiling before sample contact. The darkness requirement, which stems from the photoreduction of Fe(III) to Fe(II) in the presence of phen, was eliminated by the use of opaque amber-colored high-density-polyethylene bottles during the digestion step and for storage of the digestate and subsequent dilutions before Fe(II) analysis. Reduction of Fe(III) for total-Fe analysis was accomplished either by exposure to light from a Hg-vapor lamp or by reaction with hydroxylamine, NH 2 OH. Although the minimum periods required for adequate reduction ranged from 1.5 to 4 h, the optimum reduction periods were between 6 and 10 h. When standard samples containing Fe(II) and MnCl 2 were digested and analyzed for total-Fe using the light treatment (with incidental heating to 35–45 °C), significant decreases and in some instances, oscillations, in absorptivity were obtained. Similar experiments with NH 2 OH, or with CrCl 3 showed no effect. The absorptivity of most digestates stored in opaque bottles was stable for at least 2 weeks, although digestates with Mn concentrations above 3 µg mL−1 showed proportional decreases in absorptivity. Analysis of 8 geochemical reference materials by the modified method (using NH 2 OH) yielded excellent agreement with published values and a mean relative standard deviation of 0.6%. Total-Fe results obtained using the light treatment, however, were generally lower (∼2% relative) than the NH 2 OH values, although this difference decreased with longer irradiation periods. Use of NH 2 OH was deemed preferable because it was simpler, faster, minimized interferences from Mn and eliminated the need for specialized apparatus. Lastly, MICA Fe was shown to be unreliable as a primary reference material for Fe(II) determinations.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cited by
Zhang, C., Zhou, M., Ren, G., Yu, X., Ma, L., Yang, J., & Yu, F. (2015) · Water Research · doi:10.1016/j.watres.2014.12.022 · Cited by 295
Reductive capacity of natural reductants
Lee, W., & Batchelor, B. (2003) · Environmental Science & Technology · doi:10.1021/es025830m · Cited by 96
Effects of citrate on hexavalent chromium reduction by structural Fe (II) in nontronite
Liu, X., Dong, H., Yang, X., Kovarik, L., Chen, Y., & Zeng, Q. (2018) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2017.09.038 · Cited by 59
Chen, N., Fang, G., Liu, G., Zhou, D., Gao, J., & Gu, C. (2018) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2018.06.030 · Cited by 51
Metadata
- Authors
- Amonette, J. E., & Charles Templeton, J.
- Venue
- Clays and Clay Minerals
- Publisher
- Cambridge University Press (CUP)
- Published
- 1998-02
- Volume
- 46
- Issue
- 1
- Pages
- 51-62
- ISSN
- 0009-8604 (ISSN-L)
- 1552-8367
- OpenAlex
- W2100838242
- Cited by
- 216
- References
- 0
- FWCI
- 0.38
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.