This paper systematically studied the modification of cement-based materials by nano-SiO2 particles with an average diameter of about 20 nm. In order to obtain the effect of nano-SiO2 particles on the mechanical properties, hydration, and pore structure of cement-based materials, adding 1%, 3%, and 5% content of nano-SiO2 in cement paste, respectively. The results showed that the reaction of nano-SiO2 particles with Ca(OH)2 (crystal powder) started within 1 h, and formed C–S–H gel. The reaction speed was faster after aging for three days. The mechanical properties of cement-based materials were improved with the addition of 3% nano-SiO2, and the early strength enhancement of test pieces was obvious. Three-day compressive strength increased 33.2%, and 28-day compressive strength increased 18.5%. The exothermic peak of hydration heat of cement increased significantly after the addition of nano-SiO2. Appearance time of the exothermic peak was advanced and the total heat release increased. Thermogravimetric-differential scanning calorimetry (TG-DSC) analysis showed that nano-SiO2 promoted the formation of C–S–H gel. The results of mercury intrusion porosimetry (MIP) showed that the total porosity of cement paste with 3% nano-SiO2 was reduced by 5.51% and 5.4% at three days and 28 days, respectively, compared with the pure cement paste. At the same time, the pore structure of cement paste was optimized, and much-detrimental pores and detrimental pores decreased, while less harmful pores and innocuous pores increased.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
2 retracted
RETRACTED: Al2O3 nanoparticles in concrete and different curing media
Nazari, A., & Riahi, S. (2011) · Energy and Buildings · doi:10.1016/j.enbuild.2011.02.018 · Cited by 145
RetractedNazari, A., & Riahi, S. (2010) · Energy and Buildings · doi:10.1016/j.enbuild.2010.12.025 · Cited by 114
RetractedNanotechnology in concrete – A review
Sanchez, F., & Sobolev, K. (2010) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2010.03.014 · Cited by 1,834 · cited 1×
“Recently, many nanomaterials, such as nano-TiO2 [4–8], nano-CaCO3 [9,10], nano-Al2O3 [11–13], and carbon nano-tubes [14] have been added in cement-based materials to improve various properties of cement.”
BackgroundMicrostructure of cement mortar with nano-particles
Li, H., Xiao, H.-G., Yuan, J., & Ou, J. (2004) · Composites Part B: Engineering · doi:10.1016/s1359-8368(03)00052-0 · Cited by 1,226 · cited 2×
“Nano-SiO2 can also be a nucleation point to promote cement hydration and strengthen the connection of cement hydration products [23,27].”
BackgroundYu, R., Spiesz, P., & Brouwers, H. J. H. (2014) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2014.04.063 · Cited by 630 · cited 3×
“It as found that the hy ration rocess of ce ent ith nano-Si 2 as si ilar to ortlan ce ent [17,28].”
BackgroundResultModification of cement-based materials with nanoparticles
Kawashima, S., Hou, P., Corr, D. J., & Shah, S. P. (2013) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.06.012 · Cited by 560 · cited 1×
“Recently, many nanomaterials, such as nano-TiO2 [4–8], nano-CaCO3 [9,10], nano-Al2O3 [11–13], and carbon nano-tubes [14] have been added in cement-based materials to improve various properties of cement.”
BackgroundA study on mechanical and pressure-sensitive properties of cement mortar with nanophase materials
Li, H., Xiao, H.-G., & Ou, J.-P. (2004) · Cement and Concrete Research · doi:10.1016/j.cemconres.2003.08.025 · Cited by 499 · cited 3×
“Nano-SiO2 can also be a nucleation point to promote cement hydration and strengthen the connection of cement hydration products [23,27].”
BackgroundLi, Z., Wang, H., He, S., Lu, Y., & Wang, M. (2005) · Materials Letters · doi:10.1016/j.matlet.2005.08.061 · Cited by 396
Influences of nano-TiO2 on the properties of cement-based materials: Hydration and drying shrinkage
Zhang, R., Cheng, X. Y., Hou, P., & Ye, Z. (2015) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2015.02.003 · Cited by 390 · cited 1×
“The nano-SiO2 has poor degree of crystallization, so the diffraction peak of Ca(OH)2 should be focused and the intensity reflected the contained of Ca(OH)2 [4].”
BackgroundInfluence of nano-SiO2 on the Portland cement pastes
Stefanidou, M., & Papayianni, I. (2012) · Composites Part B Engineering · doi:10.1016/j.compositesb.2011.12.015 · Cited by 380 · cited 1×
“5% 25% 28 days Stefanidou [22] 15 nm 1.”
Cited by
Stabilization of expansive soils using chemical additives: A review
Barman, D., & Dash, S. K. (2022) · Journal of Rock Mechanics and Geotechnical Engineering · doi:10.1016/j.jrmge.2022.02.011 · Cited by 418
Wang, Y., Hughes, P., Niu, H., & Fan, Y. (2019) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2019.07.077 · Cited by 222
Sustainability of nanomaterials based self-healing concrete: An all-inclusive insight
Huseien, G. F., Shah, K. W., & Sam, A. R. M. (2019) · Journal of Building Engineering · doi:10.1016/j.jobe.2019.01.032 · Cited by 210
Onaizi, A. M., Huseien, G. F., Lim, N. H. A. S., Amran, M., & Samadi, M. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.124850 · Cited by 202
Majeed, S. S., Othuman Mydin, M. A., Bahrami, A., Dulaimi, A., Özkılıç, Y. O., Omar, R., & Jagadesh, P. (2024) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2024.01.282 · Cited by 37
Metadata
- Authors
- Wang, L., Zheng, D., Zhang, S., Cui, H., & Li, D.
- Venue
- Nanomaterials
- Publisher
- MDPI AG
- Published
- 2016-12-15
- Volume
- 6
- Issue
- 12
- Pages
- 241
- ISSN
- 2079-4991 (ISSN-L)
- OpenAlex
- W2565986892
- Cited by
- 163
- References
- 21
- FWCI
- 12.23
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.