CoChat

Review of the Corrosion of Nickel-Based Alloys and Stainless Steels in Strongly Oxidizing Pressurized High-Temperature Solutions at Subcritical and Supercritical Temperatures

Kritzer, P., Boukis, N., Dinjus, E. · 2000 · Corrosion
Cited by 98

The DOI matches its Crossref record; 1 of the 1 references it cites were found in a registry or an index.

Abstract

The corrosion phenomena of nickel-based Alloy 625 (UNS N06625), which in the present content is representative of other nickel-based alloys and stainless steels in strongly oxidizing solutions of different acids, salts, and bases, was reviewed. Acids include hydrofluoric acid (HF), hydrochloric acid (HCl), hydrobromic acid (HBr), sulfuric acid (H2SO4), nitric acid (HNO3), and phosphoric acid (H3PO4). Salts and bases are sodium chloride (NaCl), sodium hydrogen sulfate (NaHSO4), sodium sulfate (Na2SO4), and sodium hydroxide (NaOH). Concentrations of these species are typically ~ 0.1 mol/kg and that of oxygen > ~ 0.5 mol/kg (16,000 ppm). Temperatures (up to 500°C) and pressures (up to ~ 40 MPa) reach into the supercritical region of water. In acidic solutions, Cr(III) oxides or hydroxides are the thermodynamically stable compounds and thus form the oxide layer at temperatures up to ~ 250°C to 300°C. Under these conditions, serious general corrosion is not observed, but anion-induced localized attack can occur. This is the case in solutions of HCl and HBr, where pitting with penetration rates up to 1,000 μm in 100 h is observed. At higher temperatures, the transpassive conversion of solid Cr(III) compounds toward soluble Cr(VI) species is favored. At the same time, other components of the alloys—nickel, iron, molybdenum, cobalt, or niobium—cannot form a stable, protective layer since all of their oxides are also soluble in the acidic solution. The corrosion morphology of this transpassive dissolution is a uniformly attacked surface. Corrosion rates are up to ~ 500 μm in 100 h and depend strongly on the solubility of the corrosion products (not the oxides). Corrosion is negligibly low in solutions of HF and H3PO4. Surprisingly, an upper limit of severe corrosion is observed. This can be explained by the sharp drop of density, ionic product, and dielectric constant of water when increasing the temperature at constant pressure. At higher pressures, the drop shifts toward higher temperatures. Dissociation constants of acids present in the solution show the same behavior; they are extremely low in low-density, high-temperature solutions, leading to neutral conditions. The upper temperature limit of severe corrosion can be related to that drop in physical properties. The low corrosion in the low-density—and thus neutral—supercritical solutions can be explained by the stability of Ni(II) oxide, which forms the protective oxide layer. Chromium and molybdenum are still dissolved by forming their hexavalent acids, H2CrO4 or H2MoO4, respectively. In H3PO4 solution, additional corrosion mechanisms may occur. In alkaline solutions, no significant general corrosion occurs at subcritical temperatures. However, supercritical solutions of NaOH and oxygen are highly corrosive because of the formation of an oxidizing melt with a high solvency for salts. Attributing observed corrosion mechanisms on solubilities of the protecting oxides and the other corrosion products, the corrosion behavior of Alloy 625 can be generalized to other nickel-based alloys and stainless steels.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.5006/1.3294394

Cites

1 of 1 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Cited by

See all 98

Metadata

Authors
Kritzer, P., Boukis, N., & Dinjus, E.
Venue
Corrosion
Published
2000-11-01
Volume
56
Issue
11
Pages
1093-1104
ISSN
  • 0010-9312 (ISSN-L)
  • 1938-159X
OpenAlex
W2097032651
Cited by
98
References
1
FWCI
3.31
Type
journal article
Language
en
Open access
closed

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.