Local pH and Its Evolution Near Mg Alloy Surfaces Exposed to Simulated Body Fluids
The DOI matches its Crossref record; 1 of the 1 references it cites were found in a registry or an index.
Abstract
Many reports are available on degradation rates and corrosion product characterization of magnesium alloys for implant application. Typically, the data are obtained ex situ, as post factum analysis of occurred degradation processes or in bulk electrolyte that does not fully reflect concentration gradients at the interface and in the diffusion layer. Meanwhile, these local conditions are essential for tissue‐implant compatibility. Only a limited number of studies employ the techniques that visualize ongoing degradation and are localized enough to observe the changes in the electrolyte layer directly adjacent to corroding magnesium. Here, local pH in Hank's solution is studied in operando, with potentiometric micro‐probes (d = 2 µm) located 10–50 µm above the surface of four Mg alloys potentially relevant for implant applications. A significant difference in local pH is observed for Mg in simple Hank's solution (near surface pH 9.9–10.5) or Hank's solution modified with 2.5 × 10−3 m Ca 2+ (pH 7.8–8.5). The corresponding pH values are established during the first seconds of immersion. These findings indicate different degradation kinetics in electrolytes with or without Ca 2+. The degradation rate of Mg alloys decreases by almost two times in Ca 2+ containing Hank's solution. Calcium‐phosphate/carbonate protective layer stabilizes the surface pH below 8.5 controlling Mg degradation.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Zhang, Y., Xu, J., Ruan, Y. C., Yu, M. K., O'Laughlin, M., Wise, H., Chen, D., Tian, L., Shi, D., Wang, J., et al. (2016) · Nature Medicine · doi:10.1038/nm.4162 · Cited by 1,051
Cited by
Mei, D., Lamaka, S. V., Lu, X., & Zheludkevich, M. L. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108722 · Cited by 284
Self-citationKovacevic, S., Ali, W., Mandal, T. K., Martínez-Pañeda, E., & LLorca, J. (2025) · Acta Biomaterialia · doi:10.1016/j.actbio.2025.03.034 · Cited by 31
Kwesiga, M. P., Gillette, A. A., Razaviamri, F., Plank, M. E., Canull, A. L., Alesch, Z., He, W., Lee, B. P., & Guillory, R. J. (2023) · Bioactive Materials · doi:10.1016/j.bioactmat.2022.10.017 · Cited by 25
“degradation have been demonstrated near Mg discs in solution [59,60] and our viability data shows a differential toxicity environment near and far away from the degrading discs.”
BackgroundMartinez, D. C., Borkam-Schuster, A., Helmholz, H., Dobkowska, A., Luthringer-Feyerabend, B., Płociński, T., Willumeit-Römer, R., & Święszkowski, W. (2024) · Acta Biomaterialia · doi:10.1016/j.actbio.2024.08.015 · Cited by 21
Self-citation
Metadata
- Authors
- Lamaka, S. V., Gonzalez, J., Mei, D., Feyerabend, F., Willumeit‐Römer, R., & Zheludkevich, M. L.
- Venue
- Advanced Materials Interfaces
- Publisher
- Wiley
- Published
- 2018-06-19
- Volume
- 5
- Issue
- 18
- ISSN
- 2196-7350 (ISSN-L)
- OpenAlex
- W2809032984
- Cited by
- 95
- References
- 1
- FWCI
- 2.69
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.