The DOI matches its Crossref record; 30 of the 30 references it cites were found in a registry or an index.
Suppressing Li Dendrite Formation in Li2S‐P2S5 Solid Electrolyte by LiI Incorporation
Abstract
Solid electrolytes have been considered as a promising approach for Li dendrite prevention because of their high mechanical strength and high Li transference number. However, recent reports indicate that Li dendrites also form in Li 2 S‐P 2 S 5 based sulfide electrolytes at current densities much lower than that in the conventional liquid electrolytes. The methods of suppressing dendrite formation in sulfide electrolytes have rarely been reported because the mechanism for the “unexpected” dendrite formation is unclear, limiting the successful utilization of high‐energy Li anode with these electrolytes. Herein, the authors demonstrate that the Li dendrite formation in Li 2 S‐P 2 S 5 glass can be effectively suppressed by tuning the composition of the solid electrolyte interphase (SEI) at the Li/electrolyte interface through incorporating LiI into the electrolyte. This approach introduces high ionic conductivity but electronic insulation of LiI in the SEI, and more importantly, improves the mobility of Li atoms, promoting the Li depositon at the interface and thus suppresses dendrite growth. It is shown that the critical current density is improved significantly after incorporating LiI into Li 2 S‐P 2 S 5 glass, reaching 3.90 mA cm−2 at 100 °C after adding 30 mol% LiI. Stable cycling of the Li‐Li cells for 200 h is also achieved at 1.50 mA cm−2 at 100 °C.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
A solid future for battery development
Janek, J., & Zeier, W. G. (2016) · Nature Energy · doi:10.1038/nenergy.2016.141 · Cited by 3,979
High-power all-solid-state batteries using sulfide superionic conductors
Kato, Y., Hori, S., Saito, T., Suzuki, K., Hirayama, M., Mitsui, A., Yonemura, M., Iba, H., & Kanno, R. (2016) · Nature Energy · doi:10.1038/nenergy.2016.30 · Cited by 3,517
Zhu, Y., He, X., & Mo, Y. (2015) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.5b07517 · Cited by 1,936
Albertus, P., Babinec, S., Litzelman, S., & Newman, A. (2017) · Nature Energy · doi:10.1038/s41560-017-0047-2 · Cited by 1,888
The Impact of Elastic Deformation on Deposition Kinetics at Lithium/Polymer Interfaces
Monroe, C., & Newman, J. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.1850854 · Cited by 1,701
Stable lithium electrodeposition in liquid and nanoporous solid electrolytes
Lu, Y., Tu, Z., & Archer, L. A. (2014) · Nature Materials · doi:10.1038/nmat4041 · Cited by 1,592
Mechanism of Lithium Metal Penetration through Inorganic Solid Electrolytes
Porz, L., Swamy, T., Sheldon, B. W., Rettenwander, D., Frömling, T., Thaman, H. L., Berendts, S., Uecker, R., Carter, W. C., & Chiang, Y. (2017) · Advanced Energy Materials · doi:10.1002/aenm.201701003 · Cited by 1,117
Electrochemical Stability of Li10GeP2S12 and Li7La3Zr2O12 Solid Electrolytes
Han, F., Zhu, Y., He, X., Mo, Y., & Wang, C. (2016) · Advanced Energy Materials · doi:10.1002/aenm.201501590 · Cited by 1,095
Self-citationSulfide Solid Electrolyte with Favorable Mechanical Property for All-Solid-State Lithium Battery
Sakuda, A., Hayashi, A., & Tatsumisago, M. (2013) · Scientific Reports · doi:10.1038/srep02261 · Cited by 1,051
Dendritic growth mechanisms in lithium/polymer cells
Brissot, C., Rosso, M., Chazalviel, J.-N., & Lascaud, S. (1999) · Journal of Power Sources · doi:10.1016/s0378-7753(98)00242-0 · Cited by 945
Cited by
Fundamentals of inorganic solid-state electrolytes for batteries
Famprikis, T., Canepa, P., Dawson, J. A., Islam, M. S., & Masquelier, C. (2019) · Nature Materials · doi:10.1038/s41563-019-0431-3 · Cited by 2,525
High electronic conductivity as the origin of lithium dendrite formation within solid electrolytes
Han, F., Westover, A. S., Yue, J., Fan, X., Wang, F., Chi, M., Leonard, D. N., Dudney, N. J., Wang, H., & Wang, C. (2019) · Nature Energy · doi:10.1038/s41560-018-0312-z · Cited by 1,695
Self-citationTian, Y., Zeng, G., Rutt, A., Shi, T., Kim, H., Wang, J., Koettgen, J., Sun, Y., Ouyang, B., Chen, T., et al. (2021) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00767 · Cited by 1,614
Understanding interface stability in solid-state batteries
Xiao, Y., Wang, Y., Bo, S.-H., Kim, J. C., Miara, L. J., & Ceder, G. (2019) · Nature Reviews Materials · doi:10.1038/s41578-019-0157-5 · Cited by 1,219
Li, M., Wang, C., Chen, Z., Xu, K., & Lu, J. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00531 · Cited by 944
Self-citation
Metadata
- Authors
- Han, F., Yue, J., Zhu, X., & Wang, C.
- Venue
- Advanced Energy Materials
- Publisher
- Wiley
- Published
- 2018-03-12
- Volume
- 8
- Issue
- 18
- ISSN
- 1614-6832 (ISSN-L)
- 1614-6840
- OpenAlex
- W2792502627
- Cited by
- 400
- References
- 30
- FWCI
- 15.71
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Suppressing Li Dendrite Formation in Li2S‐P2S5 Solid Electrolyte by LiI Incorporation. https://app.cochat.ai/papers/10.1002/aenm.201703644
- The paper
- Han, F., Yue, J., Zhu, X., & Wang, C. (2018). Suppressing Li Dendrite Formation in Li2S‐P2S5 Solid Electrolyte by LiI Incorporation. Advanced Energy Materials. https://doi.org/10.1002/aenm.201703644
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.