Abstract

Water oxidation is a crucial reaction for renewable energy conversion and storage. Among the alkaline oxygen evolution reaction (OER) catalysts, NiFe based oxyhydroxides show the highest catalytic activity. However, the details of their OER mechanism are still unclear, due to the elusive nature of the OER intermediates. Here, using a novel differential electrochemical mass spectrometry (DEMS) cell interface, we performed isotope‐labelling experiments in 18 O‐labelled aqueous alkaline electrolyte on Ni(OH) 2 and NiFe layered double hydroxide nanocatalysts. Our experiments confirm the occurrence of Mars‐van‐Krevelen lattice oxygen evolution reaction mechanism in both catalysts to various degrees, which involves the coupling of oxygen atoms from the catalyst and the electrolyte. The quantitative charge analysis suggests that the participating lattice oxygen atoms belong exclusively to the catalyst surface, confirming DFT computational hypotheses. Also, DEMS data suggest a fundamental correlation between the magnitude of the lattice oxygen mechanism and the faradaic efficiency of oxygen controlled by pseudocapacitive oxidative metal redox charges.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1002/anie.202101698

Cites

46 of 46 references verified0 citation errors · 0 not checkable

Statistics

Figures

Figure 1 Electrochemical flow cells for differential electrochemical mass spectrometry (DEMS) setup. a) the DEMS dual thin‐layer electrolyte flow cell with close up of main components: working electrode, WE, reversible hydrogen electrode (RHE) as reference electrode, RE, and the Pt counter electrode, CE; 1) Teflon gasket between each cell stack, 2) the inlet channel, 3) the outlet channel, 4) the internal channel and 5) the bulk flow channel stack. b) Illustration of the DEMS hanging droplet cell design showing the actual electrolyte droplet and the main components working electrode (WE) and Teflon mask, the glass capillary, the Ag/AgCl reference electrode, RE, and the Pt counter electrode, CE.
Figure 1 Electrochemical flow cells for differential electrochemical mass spectrometry (DEMS) setup. a) the DEMS dual thin‐layer electrolyte flow cell with close up of main components: working electrode, WE, reversible hydrogen electrode (RHE) as reference electrode, RE, and the Pt counter electrode, CE; 1) Teflon gasket between each cell stack, 2) the inlet channel, 3) the outlet channel, 4) the internal channel and 5) the bulk flow channel stack. b) Illustration of the DEMS hanging droplet cell design showing the actual electrolyte droplet and the main components working electrode (WE) and Teflon mask, the glass capillary, the Ag/AgCl reference electrode, RE, and the Pt counter electrode, CE.CC BY · PubMed Central
Figure 2 Mass spectrometric cyclic voltammograms (MSCVs), iMS, of a) the NiFe LDH and b) the β‐Ni(OH)2 OER electrocatalyst. The data was obtained in the dual thin‐layer DEMS flow cell setup in 0.1 M K16OH at a scan rate 5 mV s−1 up to current density around 6 mA cm−2. Plotted are signals of m/z=32 of 16O16O (green line), and m/z=34 and 36 corresponding to the naturally abundant isotopes 16O18O (grey line, intensity ×10) and 18O18O (blue line, intensity ×10).
Figure 2 Mass spectrometric cyclic voltammograms (MSCVs), iMS, of a) the NiFe LDH and b) the β‐Ni(OH)2 OER electrocatalyst. The data was obtained in the dual thin‐layer DEMS flow cell setup in 0.1 M K16OH at a scan rate 5 mV s−1 up to current density around 6 mA cm−2. Plotted are signals of m/z=32 of 16O16O (green line), and m/z=34 and 36 corresponding to the naturally abundant isotopes 16O18O (grey line, intensity ×10) and 18O18O (blue line, intensity ×10).CC BY · PubMed Central
Figure 3 a–d) MSCV and faradic CV curves in time domain of a) 16O‐NiFe LDH (MSCV top, CV bottom) and b) Ni(16OH)2 (MSCV top, CV bottom) recorded in 18O ‐enriched 0.1 M KOH electrolyte prepared using H2 18O (99.3 % 18O). a) and b) show the mass ion currents, iMS, of m/z=36 18O2 (blue line), m/z=34 18O16O (grey line) and m/z=32 16O2 (green line) related to the faradaic current iF (red line) and the applied potential E (black line). The experimental m/z=34 MSCVs, inside the dashed square boxes in (a) and (b), are shown enlarged in panels c) and d). Beside the experimental m/z=34 18O16O (grey line) traces, panels (c) and (d) show the experimental mass current of m/z=36 normalized to the maximum m/z=34 mass current (dotted blue line), as well as the theoretically expected m/z=34 18O16O ion current based on the 16O atomic abundance of 0.78 % in the 0.1 M K16OH/H2 18O electrolyte (dotted black line). e) Comparison of the ratios of mass spectrometric charges of evolved 16O18O (m/z=34) and 18O18O (m/z=36) over the first three potential cycles for the Ni(OH)2 (cyan) and NiFe LDH (orange) (see details in Figure S5 and S6 and corresponding 16O abundance in Figure S7). The dashed areas corresponds to the expected 16O18O/18O18O ratio, 1.58 %, based on the 16O atomic abundance of 0.78 %. Error bars represent standard deviation from the average of two measurements of the same catalysts on two different electrodes.
Figure 3 a–d) MSCV and faradic CV curves in time domain of a) 16O‐NiFe LDH (MSCV top, CV bottom) and b) Ni(16OH)2 (MSCV top, CV bottom) recorded in 18O ‐enriched 0.1 M KOH electrolyte prepared using H2 18O (99.3 % 18O). a) and b) show the mass ion currents, iMS, of m/z=36 18O2 (blue line), m/z=34 18O16O (grey line) and m/z=32 16O2 (green line) related to the faradaic current iF (red line) and the applied potential E (black line). The experimental m/z=34 MSCVs, inside the dashed square boxes in (a) and (b), are shown enlarged in panels c) and d). Beside the experimental m/z=34 18O16O (grey line) traces, panels (c) and (d) show the experimental mass current of m/z=36 normalized to the maximum m/z=34 mass current (dotted blue line), as well as the theoretically expected m/z=34 18O16O ion current based on the 16O atomic abundance of 0.78 % in the 0.1 M K16OH/H2 18O electrolyte (dotted black line). e) Comparison of the ratios of mass spectrometric charges of evolved 16O18O (m/z=34) and 18O18O (m/z=36) over the first three potential cycles for the Ni(OH)2 (cyan) and NiFe LDH (orange) (see details in Figure S5 and S6 and corresponding 16O abundance in Figure S7). The dashed areas corresponds to the expected 16O18O/18O18O ratio, 1.58 %, based on the 16O atomic abundance of 0.78 %. Error bars represent standard deviation from the average of two measurements of the same catalysts on two different electrodes.CC BY · PubMed Central
Figure 4 The evolution in the atomic fraction of 18O of the total DEMS charge of evolved oxygen measured in non‐enriched H2 16O‐based electrolyte for a) NiFe LDH and b) Ni(OH)2. The catalysts were previously cycled into the OER range in 18O isotope‐enriched electrolyte. A rinsing step with non‐enriched H2 16O was conducted before the experiments shown here. Shown are data obtained from MSCVs over the first four cycles (see also Figure S8 and S9). The bars represent the experimental 18O fraction (full blue bars) and the expected 18O fraction based on the natural isotope abundance (hashed bars).
Figure 4 The evolution in the atomic fraction of 18O of the total DEMS charge of evolved oxygen measured in non‐enriched H2 16O‐based electrolyte for a) NiFe LDH and b) Ni(OH)2. The catalysts were previously cycled into the OER range in 18O isotope‐enriched electrolyte. A rinsing step with non‐enriched H2 16O was conducted before the experiments shown here. Shown are data obtained from MSCVs over the first four cycles (see also Figure S8 and S9). The bars represent the experimental 18O fraction (full blue bars) and the expected 18O fraction based on the natural isotope abundance (hashed bars).CC BY · PubMed Central
Figure 5 a) Mass spectrometric cyclic voltammograms (MSCVs) of the IrOx catalyst during OER in 0.5 M HCl in 18O isotope labelled electrolyte (97 % abundance). Plotted are the experimental mass currents iMS of m/z=36 18O2 (blue line, top), experimental iMS of m/z=34 18O16O (grey line, center), the expected iMS of m/z=34 18O16O (dotted black line, center) based on the 18O abundance in the electrolyte, and the applied electrode potential sweep (black line, bottom). b) Trend in mean faradaic efficiency of O2 (FEO2), evaluated over the entire potential cycle shown in Figure 2 plotted versus 18O16O/18O2 percentage ratio of IrOx, NiFe LDH and Ni(OH)2. FEO2 data of IrOx catalyst taken from referencer [18].
Figure 5 a) Mass spectrometric cyclic voltammograms (MSCVs) of the IrOx catalyst during OER in 0.5 M HCl in 18O isotope labelled electrolyte (97 % abundance). Plotted are the experimental mass currents iMS of m/z=36 18O2 (blue line, top), experimental iMS of m/z=34 18O16O (grey line, center), the expected iMS of m/z=34 18O16O (dotted black line, center) based on the 18O abundance in the electrolyte, and the applied electrode potential sweep (black line, bottom). b) Trend in mean faradaic efficiency of O2 (FEO2), evaluated over the entire potential cycle shown in Figure 2 plotted versus 18O16O/18O2 percentage ratio of IrOx, NiFe LDH and Ni(OH)2. FEO2 data of IrOx catalyst taken from referencer [18].CC BY · PubMed Central
Figure 6 Deconvolution of the total faradaic charge under iF (red line) into faradaic charge and pseudocapacitive oxidative metal charge: The charge under the faradic mass spectrometric cyclic voltammogram (MSCV, blue line) of Ni(OH)2, QF,O2DEMS , splits into QF,OERDEMS (grey area, 86 % of QF,O2DEMS ) and the LOER‐derived QF,LOERDEMS (cyan color, 14 % of QF,O2DEMS . The percentage of QF,LOERDEMS in respect to the total QF,O2DEMS might represent a lower limit due to the exchange of surface lattice hydroxides with electrolyte). The faradaic O2 efficiency, FEO2, is dependent on the potential window considered in the integration of iF : FEO2=82 % for purple potential range, that is, without the Ni redox wave 1; FEO2=62 % for pink potential range including the Ni redox waves. Only anodic faradaic currents were included in the analysis to exclusively account for anodic processes (molecular O2).
Figure 6 Deconvolution of the total faradaic charge under iF (red line) into faradaic charge and pseudocapacitive oxidative metal charge: The charge under the faradic mass spectrometric cyclic voltammogram (MSCV, blue line) of Ni(OH)2, QF,O2DEMS , splits into QF,OERDEMS (grey area, 86 % of QF,O2DEMS ) and the LOER‐derived QF,LOERDEMS (cyan color, 14 % of QF,O2DEMS . The percentage of QF,LOERDEMS in respect to the total QF,O2DEMS might represent a lower limit due to the exchange of surface lattice hydroxides with electrolyte). The faradaic O2 efficiency, FEO2, is dependent on the potential window considered in the integration of iF : FEO2=82 % for purple potential range, that is, without the Ni redox wave 1; FEO2=62 % for pink potential range including the Ni redox waves. Only anodic faradaic currents were included in the analysis to exclusively account for anodic processes (molecular O2).CC BY · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 46 references

Research works printed but not linked: 1

  1. L. Demourgues-Guerlou, L. Fournes, C. Delmas, J. Solid State Chem. 1995, 114, 6– 14;

Cited by

Metadata

Authors
Ferreira de Araújo, J., Dionigi, F., Merzdorf, T., Oh, H., & Strasser, P.
Affiliations
  • Department of Chemistry Chemical Engineering Division Technical University of Berlin Straße des 17. June 124 10623 Berlin Germany
  • Technische Universität Berlin (DE)
Corresponding author
Strasser, Peter
Venue
Angewandte Chemie International Edition
Publisher
Wiley
Published
2021-05-26
Volume
60
Issue
27
Pages
14981-14988
ISSN
  • 1433-7851 (ISSN-L)
  • 1521-3773
OpenAlex
W3143272023
Cited by
155
References
46
Citations by year
2026: 26 · 2025: 34 · 2024: 31 · 2023: 34 · 2022: 22 · 2021: 8
FWCI
4.46
Type
journal article
Language
en
Open access
Locations
  • Angewandte Chemie International Edition (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
Funders
Deutsche Forschungsgemeinschaft (STR 596/12-1, EXC 2008/1 - 390540038)
Topics
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › CO2 Reduction Techniques and Catalysts
  • Physical Sciences › Materials Science › Materials Chemistry › Iron oxide chemistry and applications
Keywords
Mars-van Krevelen mechanism, oxygen evolution reaction, NiFe layered double hydroxide, nickel hydroxide, alkaline water oxidation, lattice oxygen, differential electrochemical mass spectrometry, Faradaic efficiency, electrocatalysis

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.