Bone bonding behavior of three kinds of apatite containing glass ceramics

Kitsugi, Toshiaki, Yamamuro, Takao, Nakamura, Takashi, Higashi, Shoichiro, Kakutani, Yoshiaki, Hyakuna, Katsufumi, Ito, Setsuro, Kokubo, Tadashi, Takagi, Masataka, Shibuya, Takehiro·1986·Journal of Biomedical Materials Research

Abstract

We have produced three kinds of apatite‐containing glass ceramics of the same chemical composition: MgO (4.6), CaO (44.9), SiO 2 (34.2), P 2 O 5 (16.3), CaF 2 (0.5) (in weight ratio). They contain different crystal combinations and have different mechanical properties. The first glass ceramic (A–;GC) was prepared by heating a glass plate to 870°C. It contains only oxy‐ and fluoroapatite (35 wt%). The second glass ceramic (A–W–GC), and the third (A–W–CP–GC), were prepared by heating glass powder compacts to 1050°C and 1200°C, respectively. A–W–GC contains oxyapatite and fluoroapatite (Ca 10(PO 4)6(O,F 2)) (35 wt%) and β‐wollastonite (40 wt%). A–W–CP–GC contains oxyapatite and fluoroapatite (20 wt%), β‐wollastonite (CaO·SiO 2) (55 wt%), and β‐whitlockite (3CaO·P 2 O 5) (15 wt%). The bending strengths of A–;GC, A–W–GC, and A–W–CP–GC were 88MPa, 178MPa, and 213MPa, respectively, in air. Rectangular ceramic plates (15mm × 10mm × 2mm) were implanted into a rabbit tibia. Ten and 25 weeks after implantation, the segment of tibia with implant was excised for examination. The segment was held by a special jig and the traction breaking load (failure load) was measured by an autograph. A–;GC showed a lower load than A–W–GC and A–W–CP–GC. The loads for A–W–GC and A–W–CP–GC were almost equal. The failure loads did not change significantly between 10 and 25 weeks for any of the materials. The interface was examined by Giemsa surface staining, contact micro‐radiography, and SEM‐EPMA. Giemsa surface staining and CMR revealed direct bonding between the materials and the bone for all the three materials. SEM‐EPMA showed that Si and Mg content decreased, Ca content did not change, and P content increased at the reaction zone between all three glass ceramics and bone. This was observed at 10 weeks, as well as at 25 weeks, after implantation. The reaction zone was narrowest with A–;GC, wider with A–W–GC, and widest with A–W–CP–GC.

Overview

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1002/jbm.820200906

Cites

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cited by

See all 178

Metadata

Authors
Kitsugi, T., Yamamuro, T., Nakamura, T., Higashi, S., Kakutani, Y., Hyakuna, K., Ito, S., Kokubo, T., Takagi, M., & Shibuya, T.
Venue
Journal of Biomedical Materials Research
Publisher
Wiley
Published
1986-11
Volume
20
Issue
9
Pages
1295-1307
ISSN
  • 0021-9304 (ISSN-L)
  • 1097-4636
OpenAlex
W2047722298
Cited by
178
References
0
FWCI
5.51
Type
journal article
Language
en
Open access
closed

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Bone bonding behavior of three kinds of apatite containing glass ceramics. https://app.cochat.ai/papers/10.1002/jbm.820200906
The paper
Kitsugi, T., Yamamuro, T., Nakamura, T., Higashi, S., Kakutani, Y., Hyakuna, K., Ito, S., Kokubo, T., Takagi, M., & Shibuya, T. (1986). Bone bonding behavior of three kinds of apatite containing glass ceramics. Journal of Biomedical Materials Research. https://doi.org/10.1002/jbm.820200906

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.