The DOI matches its Crossref record; 87 of the 87 references it cites were found in a registry or an index.
A review of PEM fuel cell durability: materials degradation, local heterogeneities of aging and possible mitigation strategies
Abstract
Through a tight collaboration between chemical engineers, polymer scientists, and electrochemists, we address the degradation mechanisms of membrane electrode assemblies (MEAs) during proton exchange membrane fuel cell (PEMFC) operation in real life (industrial stacks). A special attention is paid to the heterogeneous nature of the aging and performances degradation in view of the hardware geometry of the stack and MEA. Macroscopically, the MEA is not fuelled evenly by the bipolar plates and severe degradations occur during start‐up and shut‐down events in the region that remains/becomes transiently starved in hydrogen. Such transients are dramatic to the cathode catalyst layer, especially for the carbon substrate supporting the Pt‐based nanoparticles. Another level of heterogeneity is observed between the channel and land areas of the cathode catalyst layer. The degradation of Pt 3 Co/C nanocrystallites employed at the cathode cannot be avoided in stationary operation either. In addition to the electrochemical Ostwald ripening and to crystallite migration, these nanomaterials undergo severe corrosion of their high surface area carbon support. The mother Pt 3 Co/C nanocrystallites are continuously depleted in Co, generating Co 2+ cations that pollute the ionomer and depreciate the performance of the cathode. Such cationic pollution has also a negative effect on the physicochemical properties of the proton‐exchange membrane (proton conductivity and resistance to fracture), eventually leading to hole formation. These defects were localized with the help of an infrared camera. The mechanical fracture‐resistance of various perfluorosulfonated membranes further demonstrated that polytetrafluoroethylene‐reinforced membranes better resist hole formation, due to their high resistance to crack initiation and propagation. WIREs Energy Environ 2014, 3:540–560. doi: 10.1002/wene.113 This article is categorized under: Fuel Cells and Hydrogen > Science and Materials Fuel Cells and Hydrogen > Systems and Infrastructure Energy Research & Innovation > Science and Materials
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Tuinstra, F., & Koenig, J. L. (1970) · The Journal of Chemical Physics · doi:10.1063/1.1674108 · Cited by 10,717
Gasteiger, H. A., Kocha, S. S., Sompalli, B., & Wagner, F. T. (2005) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2004.06.021 · Cited by 4,876
Scientific Aspects of Polymer Electrolyte Fuel Cell Durability and Degradation
Borup, R., Meyers, J., Pivovar, B., Kim, Y. S., Mukundan, R., Garland, N., Myers, D., Wilson, M., Garzon, F., Wood, D., et al. (2007) · Chemical Reviews · doi:10.1021/cr050182l · Cited by 3,402
Wang, Y., Chen, K. S., Mishler, J., Cho, S. C., & Adroher, X. C. (2011) · Applied Energy · doi:10.1016/j.apenergy.2010.09.030 · Cited by 3,329
Cançado, L. G., Takai, K., Enoki, T., Endo, M., Kim, Y. A., Mizusaki, H., Jorio, A., Coelho, L. N., Magalhães-Paniago, R., & Pimenta, M. A. (2006) · Applied Physics Letters · doi:10.1063/1.2196057 · Cited by 2,628
Characterization of diamond films by Raman spectroscopy
Knight, D. S., & White, W. B. (1989) · Journal of Materials Research · doi:10.1557/jmr.1989.0385 · Cited by 2,512
A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies
Wu, J., Yuan, X. Z., Martin, J. J., Wang, H., Zhang, J., Shen, J., Wu, S., & Merida, W. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.006 · Cited by 1,587
Instability of Pt∕C Electrocatalysts in Proton Exchange Membrane Fuel Cells
Ferreira, P. J., la O’, G. J., Shao-Horn, Y., Morgan, D., Makharia, R., Kocha, S., & Gasteiger, H. A. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.2050347 · Cited by 1,491
Carbon: Electrochemical and Physicochemical Properties
Kinoshita, K. (1988) · Medical Entomology and Zoology · Cited by 1,367
Carbon—Electrochemical and Physicochemical Properties
Brown, O. R. (1989) · Electrochimica Acta · doi:10.1016/0013-4686(89)87066-5 · Cited by 1,211
Understanding and approaches for the durability issues of Pt-based catalysts for PEM fuel cell
Shao, Y., Yin, G., & Gao, Y. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.004 · Cited by 1,197
Recent advances in activity and durability enhancement of Pt/C catalytic cathode in PEMFC
Yu, X., & Ye, S. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.048 · Cited by 1,098
Review: Durability and Degradation Issues of PEM Fuel Cell Components
de Bruijn, F. A., Dam, V. A. T., & Janssen, G. J. M. (2008) · Fuel Cells · doi:10.1002/fuce.200700053 · Cited by 1,001
A Reverse-Current Decay Mechanism for Fuel Cells
Reiser, C. A., Bregoli, L., Patterson, T. W., Yi, J. S., Yang, J. D., Perry, M. L., & Jarvi, T. D. (2005) · Electrochemical and Solid-State Letters · doi:10.1149/1.1896466 · Cited by 976
Instability of Supported Platinum Nanoparticles in Low-Temperature Fuel Cells
Shao-Horn, Y., Sheng, W. C., Chen, S., Ferreira, P. J., Holby, E. F., & Morgan, D. (2007) · Topics in Catalysis · doi:10.1007/s11244-007-9000-0 · Cited by 939
Atlas D-Equilibres Electrochimiques
Pourbaix, M., & Burbank, J. (1964) · Journal of The Electrochemical Society · doi:10.1149/1.2426051 · Cited by 883
Three-dimensional computational analysis of transport phenomena in a PEM fuel cell
Berning, T., Lu, D. M., & Djilali, N. (2002) · Journal of Power Sources · doi:10.1016/s0378-7753(01)01057-6 · Cited by 711
A review of platinum-based catalyst layer degradation in proton exchange membrane fuel cells
Zhang, S., Yuan, X.-Z., Hin, J. N. C., Wang, H., Friedrich, K. A., & Schulze, M. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.06.073 · Cited by 661
The Bond-Valence Method: An Empirical Approach to Chemical Structure and Bonding
(1981) · Industrial Chemistry Library · doi:10.1016/b978-0-12-525102-0.50007-4 · Cited by 589
A review of accelerated stress tests of MEA durability in PEM fuel cells
ZHANG, S., YUAN, X., WANG, H., MERIDA, W., ZHU, H., SHEN, J., WU, S., & ZHANG, J. (2009) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.10.012 · Cited by 525
Visualization of Liquid Water Transport in a PEFC
Yang, X. G., Zhang, F. Y., Lubawy, A. L., & Wang, C. Y. (2004) · Electrochemical and Solid-State Letters · doi:10.1149/1.1803051 · Cited by 384
Mechanical endurance of polymer electrolyte membrane and PEM fuel cell durability
Huang, X., Solasi, R., Zou, Y., Feshler, M., Reifsnider, K., Condit, D., Burlatsky, S., & Madden, T. (2006) · Journal of Polymer Science Part B: Polymer Physics · doi:10.1002/polb.20863 · Cited by 369
Kreuer, K. D., Schuster, M., Obliers, B., Diat, O., Traub, U., Fuchs, A., Klock, U., Paddison, S. J., & Maier, J. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.11.011 · Cited by 365
Chen, S., Gasteiger, H. A., Hayakawa, K., Tada, T., & Shao-Horn, Y. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3258275 · Cited by 360
Mechanical response of fuel cell membranes subjected to a hygro-thermal cycle
Kusoglu, A., Karlsson, A. M., Santare, M. H., Cleghorn, S., & Johnson, W. B. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.05.020 · Cited by 323
Tang, Y., Karlsson, A. M., Santare, M. H., Gilbert, M., Cleghorn, S., & Johnson, W. B. (2006) · Materials Science and Engineering: A · doi:10.1016/j.msea.2006.03.055 · Cited by 316
Water Management in Cathode Catalyst Layers of PEM Fuel Cells
Eikerling, M. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2160435 · Cited by 295
A Nonisothermal, Two-Phase Model for Polymer Electrolyte Fuel Cells
Wang, Y., & Wang, C.-Y. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2193403 · Cited by 288
Bárány, T., Czigány, T., & Karger-Kocsis, J. (2010) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2010.07.001 · Cited by 277
Kusoglu, A., Karlsson, A. M., Santare, M. H., Cleghorn, S., & Johnson, W. B. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.03.063 · Cited by 274
Detection of Pt[sup z+] Ions and Pt Nanoparticles Inside the Membrane of a Used PEMFC
Guilminot, E., Corcella, A., Charlot, F., Maillard, F., & Chatenet, M. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2388863 · Cited by 250
Self-citationCoupled Thermal and Water Management in Polymer Electrolyte Fuel Cells
Weber, A. Z., & Newman, J. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2352039 · Cited by 249
Triblock copolymer ionomer membranes
Elabd, Y. A., Napadensky, E., Sloan, J. M., Crawford, D. M., & Walker, C. W. (2003) · Journal of Membrane Science · doi:10.1016/s0376-7388(03)00127-3 · Cited by 231
Influence of heat transfer on gas and water transport in fuel cells
Djilali, N., & Lu, D. (2002) · International Journal of Thermal Sciences · doi:10.1016/s1290-0729(01)01301-1 · Cited by 230
Membrane and Active Layer Degradation upon PEMFC Steady-State Operation
Guilminot, E., Corcella, A., Chatenet, M., Maillard, F., Charlot, F., Berthomé, G., Iojoiu, C., Sanchez, J.-Y., Rossinot, E., & Claude, E. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2775218 · Cited by 211
Self-citationIon Percolation and Insulator-to-Conductor Transition in Nafion Perfluorosulfonic Acid Membranes
Hsu, W. Y., Barkley, J. R., & Meakin, P. (1980) · Macromolecules · doi:10.1021/ma60073a041 · Cited by 197
Durst, J., Lamibrac, A., Charlot, F., Dillet, J., Castanheira, L. F., Maranzana, G., Dubau, L., Maillard, F., Chatenet, M., & Lottin, O. (2013) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2013.03.021 · Cited by 173
Self-citationHigh-resolution in-plane investigation of the water evolution and transport in PEM fuel cells
Hartnig, C., Manke, I., Kuhn, R., Kleinau, S., Goebbels, J., & Banhart, J. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.12.023 · Cited by 168
Segmented polymer electrolyte membrane fuel cells—A review
Pérez, L. C., Brandão, L., Sousa, J. M., & Mendes, A. M. M. (2010) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2010.08.024 · Cited by 157
Investigation of ionomer structure through its dependence on ion exchange capacity (IEC)
Moukheiber, E., Moor, G. D., Flandin, L., & Bas, C. (2011) · Journal of Membrane Science · doi:10.1016/j.memsci.2011.10.041 · Cited by 153
Self-citationSchneider, A., Colmenares, L. C., Seidel, Y. E., Jusys, Z., Wickman, B., Kasemo, B., & Behm, R. J. (2008) · Physical Chemistry Chemical Physics · doi:10.1039/b719775f · Cited by 153
Thermal conductivities from temperature profiles in the polymer electrolyte fuel cell
Vie, P. J. S., & Kjelstrup, S. (2003) · Electrochimica Acta · doi:10.1016/j.electacta.2003.10.018 · Cited by 148
Contaminant absorption and conductivity in polymer electrolyte membranes
Kelly, M. J., Fafilek, G., Besenhard, J. O., Kronberger, H., & Nauer, G. E. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.01.064 · Cited by 147
Dubau, L., Durst, J., Maillard, F. M., Guétaz, L., Chatenet, M., André, J., & Rossinot, E. (2011) · Electrochimica Acta · doi:10.1016/j.electacta.2011.03.073 · Cited by 145
Self-citationDubau, L., López‐Haro, M., Castanheira, L., Durst, J., Chatenet, M., Bayle‐Guillemaud, P., Guétaz, L., Caqué, N., Rossinot, E., & Maillard, F. M. (2013) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2013.06.011 · Cited by 136
Self-citationHara, M., Lee, M., Liu, C., Chen, B., Yamashita, Y., Uchida, M., Uchida, H., & Watanabe, M. (2012) · Electrochimica Acta · doi:10.1016/j.electacta.2012.03.043 · Cited by 132
Zhang, S., Yuan, X., Hin, J. N. C., Wang, H., Wu, J., Friedrich, K. A., & Schulze, M. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.08.070 · Cited by 130
Study on the processes of start-up and shutdown in proton exchange membrane fuel cells
Shen, Q., Hou, M., Liang, D. S., Zhou, Z., Li, X., Shao, Z., & Yi, B. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.12.075 · Cited by 129
Maillard, F. M., Dubau, L., Durst, J., Chatenet, M., André, J., & Rossinot, E. (2010) · Electrochemistry Communications · doi:10.1016/j.elecom.2010.06.007 · Cited by 127
Self-citationDubau, L., Maillard, F. M., Chatenet, M., André, J., & Rossinot, E. (2010) · Electrochimica Acta · doi:10.1016/j.electacta.2010.09.038 · Cited by 123
Self-citationPEM Fuel Cell Diagnostic Tools
Wang, H., Yuan, X., & Li, H. (2011) · CRC Press eBooks · doi:10.1201/b11100 · Cited by 123
Liu, Z. Y., Zhang, J. L., Yu, P., Zhang, J. X., Makharia, R. R., More, K. L., & Stach, E. A. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3391737 · Cited by 119
Dubau, L., Maillard, F. M., Chatenet, M., Guétaz, L., André, J., & Rossinot, E. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3485104 · Cited by 97
Self-citationDillet, J., Spernjak, D., Lamibrac, A., Maranzana, G., Mukundan, R., Fairweather, J. D., Didierjean, S., Borup, R. L., & Lottin, O. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.10.141 · Cited by 93
Self-citationRuvinskiy, P. S., Bonnefont, A., Pham‐Huu, C., & Savinova, E. R. (2011) · Langmuir · doi:10.1021/la2006343 · Cited by 91
Lamibrac, A., Maranzana, G., Lottin, O., Dillet, J., Mainka, J., Didierjean, S., Thomas, A., & Moyne, C. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.07.013 · Cited by 89
Self-citationCarbon corrosion and platinum nanoparticles ripening under open circuit potential conditions
Zhao, Z., Castanheira, L., Dubau, L., Berthomé, G., Crisci, A., & Maillard, F. M. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.12.053 · Cited by 89
Self-citationModeling the steady-state effects of cationic contamination on polymer electrolyte membranes
Kienitz, B. L., Baskaran, H., & Zawodzinski, T. A. (2008) · Electrochimica Acta · doi:10.1016/j.electacta.2008.09.058 · Cited by 85
Measuring the Current Distribution in PEFCs with Sub-Millimeter Resolution
Freunberger, S. A., Reum, M., Evertz, J., Wokaun, A. J., & Büchi, F. N. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2345591 · Cited by 84
Durst, J., Chatenet, M., & Maillard, F. M. (2012) · Physical Chemistry Chemical Physics · doi:10.1039/c2cp42191g · Cited by 83
Self-citationMagnetic resonance imaging of water distribution and production in a 6cm2 PEMFC under operation
Bedet, J., Maranzana, G., Leclerc, S., Lottin, O., Moyne, C., Stemmelen, D., Mutzenhardt, P., & Canet, D. (2008) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.01.053 · Cited by 80
Self-citationMembrane and Active Layer Degradation Following PEMFC Steady-State Operation
Iojoiu, C., Guilminot, É., Maillard, F. M., Chatenet, M., Sanchez, J., Claude, E., & Rossinot, E. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2775282 · Cited by 77
Self-citationPolymer electrolytes for a hydrogen economy
Noto, V. D., Zawodzinski, T. A., Herring, A. M., Giffin, G. A., Negro, E., & Lavina, S. (2012) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2012.01.080 · Cited by 77
Diagnosis of MEA degradation under accelerated relative humidity cycling
Vengatesan, S., Fowler, M. W., Yuan, X., & Wang, H. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.01.088 · Cited by 70
Moor, G. D., Bas, C., Charvin, N., Moukheiber, E., Niepceron, F., Breilly, N., André, J., Rossinot, E., Claude, E., Albérola, N. D., et al. (2012) · Fuel Cells · doi:10.1002/fuce.201100161 · Cited by 65
Self-citationMaranzana, G., Lottin, O., Colinart, T., Chupin, S., & Didierjean, S. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.03.002 · Cited by 63
Self-citationBurlatsky, S. F., Gummalla, M., O'Neill, J., Atrazhev, V. V., Varyukhin, A. N., Dmitriev, D. V., & Erikhman, N. S. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.05.005 · Cited by 62
Understanding the formation of pinholes in PFSA membranes with the essential work of fracture (EWF)
Moukheiber, E., Bas, C., & Flandin, L. (2013) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2013.03.031 · Cited by 60
Self-citationDescription of gasket failure in a 7 cell PEMFC stack
Husar, A., Serra, M., & Kunusch, C. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.01.078 · Cited by 60
Siroma, Z., Fujiwara, N., Ioroi, T., Yamazaki, S., Senoh, H., Yasuda, K., & Tanimoto, K. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.062 · Cited by 60
Morin, A., Xu, F., Gebel, G., & Diat, O. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.11.070 · Cited by 57
Zhao, Z., Dubau, L., & Maillard, F. M. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.06.016 · Cited by 57
Self-citationFactors Impacting Chemical Degradation Of Perfluorinated Sulfonic Acid Ionomers
Liu, H., Gasteiger, H. A., LaConti, A. B., & Zhang, J. (2006) · ECS Transactions · doi:10.1149/1.2214561 · Cited by 55
Measuring the Current Distribution with Sub-Millimeter Resolution in PEFCs
Reum, M., Freunberger, S. A., Wokaun, A. J., & Büchi, F. N. (2009) · Journal of The Electrochemical Society · doi:10.1149/1.3043422 · Cited by 46
Heterogeneities of Aging within a PEMFC MEA
Dubau, L., Durst, J., Maillard, F. M., Chatenet, M., André, J., & Rossinot, E. (2012) · Fuel Cells · doi:10.1002/fuce.201100073 · Cited by 44
Self-citationBas, C., Flandin, L., Danerol, A.-S., Claude, E., Rossinot, E., & Albérola, N. D. (2010) · Journal of Applied Polymer Science · doi:10.1002/app.31386 · Cited by 43
Self-citationJia, R., Han, B., Levi, K., Hasegawa, T., Ye, J., & Dauskardt, R. H. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.12.066 · Cited by 42
Chupin, S., Colinart, T., Didierjean, S., Dubé, Y., Agbossou, K., Maranzana, G., & Lottin, O. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.03.027 · Cited by 38
Self-citationKey counter ion parameters governing polluted nafion membrane properties
Bas, C., Reymond, L., Danerol, A.-S., Albérola, N. D., Rossinot, E., & Flandin, L. (2009) · Journal of Polymer Science Part B Polymer Physics · doi:10.1002/polb.21737 · Cited by 38
Self-citationA Half Cell Model to Study Performance Degradation of a PEMFC due to Cationic Contamination
Kienitz, B. L., Baskaran, H., Zawodzinski, T. A., & Pivovar, B. S. (2007) · ECS Transactions · doi:10.1149/1.2780991 · Cited by 35
Lamibrac, A., Maranzana, G., Dillet, J., Lottin, O., Didierjean, S., Durst, J., Dubau, L., Maillard, F. M., & Chatenet, M. (2012) · Energy Procedia · doi:10.1016/j.egypro.2012.09.038 · Cited by 34
Self-citationJia, Q., Ramaker, D. E., Ziegelbauer, J. M., Ramaswamy, N., Halder, A., & Mukerjee, S. (2013) · The Journal of Physical Chemistry C · doi:10.1021/jp311353u · Cited by 33
Start-Stop Phenomena in Channel and Land Areas of a Polymer Electrolyte Fuel Cell
Schneider, I., & von Dahlen, S. (2010) · Electrochemical and Solid-State Letters · doi:10.1149/1.3518520 · Cited by 31
Effects of contaminant on thermal properties in perfluorinated sulfonic acid membranes
Bas, C., Albérola, N. D., & Flandin, L. (2010) · Journal of Membrane Science · doi:10.1016/j.memsci.2010.07.001 · Cited by 25
Self-citationInternal currents in response to a load change during fuel cell start-up
Didierjean, S., Lamibrac, A., Geneston, T., Rakotondrainibé, A., Maranzana, G., Rozier, E., Beille, F., & Lottin, O. (2012) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2012.01.064 · Cited by 18
Self-citationFlandin, L., Danerol, A.-S., Bas, C., Claude, E., Moor, G. D., & Albérola, N. D. (2009) · Journal of The Electrochemical Society · doi:10.1149/1.3177202 · Cited by 10
Self-citationInfrared and thermal behaviour of proton exchange membrane (PEM) after cationic contamination
Moukheiber, E., Bas, C., Albérola, N. D., & Flandin, L. (2012) · Journal of Membrane Science · doi:10.1016/j.memsci.2012.12.024 · Cited by 9
Self-citation
Cited by
Designing the next generation of proton-exchange membrane fuel cells
Jiao, K., Xuan, J., Du, Q., Bao, Z., Xie, B., Wang, B., Zhao, Y., Fan, L., Wang, H., Hou, Z., et al. (2021) · Nature · doi:10.1038/s41586-021-03482-7 · Cited by 2,947
Chatenet, M., Pollet, B. G., Dekel, D. R., Dionigi, F., Deseure, J., Millet, P., Braatz, R. D., Bazant, M. Z., Eikerling, M., Staffell, I., et al. (2022) · Chemical Society Reviews · doi:10.1039/d0cs01079k · Cited by 2,025
Self-citationElectrocatalysis in Alkaline Media and Alkaline Membrane-Based Energy Technologies
Yang, Y., Peltier, C. R., Zeng, R., Schimmenti, R., Li, Q., Huang, X., Yan, Z., Potsi, G., Selhorst, R., Lu, X., et al. (2022) · Chemical Reviews · doi:10.1021/acs.chemrev.1c00331 · Cited by 544
Cunanan, C., Tran, M.-K., Lee, Y., Kwok, S., Leung, V., & Fowler, M. (2021) · Clean Technologies · doi:10.3390/cleantechnol3020028 · Cited by 398
Durability of platinum-based fuel cell electrocatalysts: Dissolution of bulk and nanoscale platinum
Cherevko, S., Kulyk, N., & Mayrhofer, K. J. J. (2016) · Nano Energy · doi:10.1016/j.nanoen.2016.03.005 · Cited by 377
Metadata
- Authors
- Dubau, L., Castanheira, L., Maillard, F., Chatenet, M., Lottin, O., Maranzana, G., Dillet, J., Lamibrac, A., Perrin, J., Moukheiber, E., ElKaddouri, A., De Moor, G., Bas, C., Flandin, L., & Caqué, N.
- Venue
- WIREs Energy and Environment
- Publisher
- Wiley
- Published
- 2014-03-05
- Volume
- 3
- Issue
- 6
- Pages
- 540-560
- ISSN
- 2041-8396 (ISSN-L)
- 2041-840X
- OpenAlex
- W1815912381
- Cited by
- 349
- References
- 87
- FWCI
- 11.50
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.