Wear debris related osteolysis is recognised as being the main cause of failure in joint replacements based on UHMWPE inserts. However, many solutions and “new” polyethylenes have been suggested in order to address this issue. This review discusses “historical” issues associated with UHMWPE, such as oxidation, sterilization method and storage, as well as “new” topics, such as crosslinking and stabilization. The final aim is to aid orthopaedic surgeons in their selection of polyethylene inserts and in the information given to the patients. The main problem for the polymer is degradative oxidation, which is caused by the combination of the irradiation used for sterilization and oxygen, and which leads to a decrease in wear resistance and mechanical properties. Irradiation and packaging in the absence of oxygen can only reduce the oxidation, while sterilization with gas (EtO or gas plasma) is the only method that effectively eliminates it. Manufacturing processes are of great relevance to the clinical duration and must be considered by surgeons. Crosslinked polyethylene has been developed for joint inserts due to its superior wear resistance compared to conventional UHMWPE; to prevent the oxidation, crosslinked polyethylene requires post-irradiation thermal treatment, which reduces its mechanical properties and which depends on the producer. Several good clinical results from the use of crosslinked acetabular cups have reported at mid-term, while early results for knee replacements are also encouraging. Recently, the use of the antioxidant vitamin E (alpha-tocopherol) has been introduced for joint prostheses in order to prevent the oxidation of both crosslinked and noncrosslinked UHMWPE.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Kurtz, S. (1999) · Biomaterials · doi:10.1016/s0142-9612(99)00053-8 · Cited by 847 · cited 2×
“Medical-grade UHMWPE orthopaedic implants are machined from stocks and sheets made from UHMWPE powders by compression moulding or ram extrusion and subsequent annealing [1]; the ASTM F 648-07 designation (standard specification for UHMWPE powder and fabricated form for surgical implants) defines the characteristics re…”
BackgroundGreen, T. (1998) · Biomaterials · doi:10.1016/s0142-9612(98)00140-9 · Cited by 569 · cited 1×
“3–10 lm in size are phagocytable and are therefore the most biologically active [21, 22].”
BackgroundUnified wear model for highly crosslinked ultra-high molecular weight polyethylenes (UHMWPE)
Muratoglu, O. K., Bragdon, C. R., O’Connor, D., Jasty, M., Harris, W. H., Gul, R. M., & Garry, F. J. M. (1999) · Biomaterials · doi:10.1016/s0142-9612(99)00039-3 · Cited by 455
Wear and Periprosthetic Osteolysis: The Problem
Harris, W. H. (2001) · Clinical Orthopaedics and Related Research · doi:10.1097/00003086-200112000-00007 · Cited by 433 · cited 1×
“The particles of polyethylene removed induce aseptic loosening, through a mechanism involving the formation of reactive tissue and consequently osteolysis, which has been recognized as being the main cause of implant failure [4, 19].”
BackgroundWear particles, periprosthetic osteolysis and the immune system
Goodman, S. B. (2007) · Biomaterials · doi:10.1016/j.biomaterials.2007.06.035 · Cited by 340 · cited 1×
“A foreign-body, granulomatous response to UHMWPE particles denotes a nonspecific chronic inflammatory reaction involving activated mononucleated macrophages and fibroblasts but few T lymphocytes [20].”
Backgroundα-Tocopherol-doped irradiated UHMWPE for high fatigue resistance and low wear
Oral, E., Wannomae, K. K., Hawkins, N., Harris, W. H., & Muratoglu, O. K. (2004) · Biomaterials · doi:10.1016/j.biomaterials.2003.12.048 · Cited by 301
Oxidation in orthopaedic UHMWPE sterilized by gamma-radiation and ethylene oxide
Costa, L., Cortemiglia, M. P. L. D., Trossarelli, L., Prever, E. M. B. D., Crova, M., & GALLINARO, P. (1998) · Biomaterials · doi:10.1016/s0142-9612(97)00160-9 · Cited by 300
Self-citationPruitt, L. A. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2004.03.022 · Cited by 282
McKELLOP, H., SHEN, F.-W., LU, B., CAMPBELL, P., & SALOVEY, R. (2000) · The Journal of Bone and Joint Surgery-American Volume · doi:10.2106/00004623-200012000-00004 · Cited by 264 · cited 2×
“abrasive wear and the post-oxidative reduction in molecular weight [2, 3].”
BackgroundMechanisms of decrease in fatigue crack propagation resistance in irradiated and melted UHMWPE
Oral, E., Malhi, A. S., & Muratoglu, O. K. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2005.06.025 · Cited by 241
Baker, D., Bellare, A., & Pruitt, L. A. (2003) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.10606 · Cited by 215 · cited 1×
“trast, the problem with complete melting is the resulting deterioration in mechanical properties like elongationto-break, tensile modulus, tensile strength [28, 32] and J-integral fracture toughness [32], and resistance to fatigue crack propagation [33–37].”
BackgroundFisher, J., McEwen, H. M. J., Tipper, J. L., Galvin, A. L., Ingram, J., Kamali, A., Stone, M. H., & Ingham, E. (2004) · Clinical Orthopaedics & Related Research · doi:10.1097/01.blo.0000148783.20469.4c · Cited by 185 · cited 1×
“Crosslinking would generate a larger percentage of small particles [39, 40], which would lead to a higher release of tumor necrosis factor-alpha and therefore to a higher reactivity [ 41 ].”
BackgroundSurface reactivity in the pathogenic response to particulates.
Fubini, B. (1997) · Environmental Health Perspectives · doi:10.1289/ehp.97105s51013 · Cited by 175 · cited 2×
“Many modifications can occur: freshly detached particles are different from particles that have been in contact with biological tissues for some time [23], and the debris may be not only fragments of UHMWPE but fragments of an oxidized, lower molecular mass polyethylene [24].”
BackgroundSimis, K., Bistolfi, A., Bellare, A., & Pruitt, L. A. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2005.09.033 · Cited by 143
Self-citationIn vivo UHMWPE biodegradation of retrieved prosthesis
Costa, L., Cortemiglia, M. P. L. D., Trossarelli, L., Prever, E. M. B. D., Crova, M., & GALLINARO, P. (1998) · Biomaterials · doi:10.1016/s0142-9612(98)00013-1 · Cited by 142 · cited 4×
“Sterilization of UHMWPE components deserves a special mention since, as described above, it is known that this process can modify the mechanical and wear properties of UHMWPE [1, 6–9, 16].”
BackgroundInfluentialSelf-citationComparative fatigue behavior and toughness of remelted and annealed highly crosslinked polyethylenes
Medel, F. J., Peña, P., Cegoñino, J., Gómez‐Barrena, E., & Puértolas, J. A. (2007) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.30807 · Cited by 136
Gencur, S. J., Rimnac, C. M., & Kurtz, S. M. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2005.09.010 · Cited by 130
Macrophage response to cross-linked and conventional UHMWPE
Sethi, R. K., Neavyn, M. J., Rubash, H. E., & Shanbhag, A. S. (2003) · Biomaterials · doi:10.1016/s0142-9612(03)00056-5 · Cited by 115 · cited 1×
“However, crosslinked and conventional polyethylenes would cause similar levels of cytokines, IL6, IL-1a, IL-1b and TNF-a [42], and the degree of crosslinking-related osteolysis would be reduced compared to conventional osteolysis [43].”
BackgroundA study of the nanostructure and tensile properties of ultra-high molecular weight polyethylene
Turell, M. B., & Bellare, A. (2003) · Biomaterials · doi:10.1016/j.biomaterials.2003.10.027 · Cited by 91 · cited 1×
“Medical-grade polyethylene (UHMWPE with an average molecular mass of [2,000,000 a.m.u.) is a semicrystalline polymer that can be depicted as a set of ordered regions (crystalline lamellae) embedded in a disordered amorphous phase [ 12 ].”
BackgroundUnacceptable biodegradation of polyethylene in vivo
Prever, E. B. D., Crova, M., Costa, L., Dallera, A., Camino, G., & GALLINARO, P. (1996) · Biomaterials · doi:10.1016/0142-9612(96)83282-0 · Cited by 90
Self-citationBracco, P., Brunella, V., Luda, M. P., Zanetti, M., & Costa, L. (2005) · Polymer · doi:10.1016/j.polymer.2005.08.095 · Cited by 86 · cited 1×
“Such reactions result in polymer chains with stable C–C chemical bonds, theoretically increasing the molecular mass to infinity [13, 25].”
BackgroundSelf-citationBracco, P., Prever, E. M. B. D., Cannas, M. F., Cortemiglia, M. P. L. D., & Costa, L. (2006) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2006.02.003 · Cited by 82 · cited 2×
“It is well established that such irradiation, as well as electron beam irradiation, causes crosslinking, chain scission and long-term oxidative degradation of polyethylene, and that long-term post-irradiation aging can have detrimental effects on the morphology and mechanical properties of UHMWPE [1, 14, 16, 17].”
BackgroundSelf-citationWear of high-dose gamma-irradiated polyethylene in total hip replacements
Oonishi, H., & Kadoya, Y. (2000) · Journal of Orthopaedic Science · doi:10.1007/s007760050155 · Cited by 69 · cited 1×
“The potential benefits of reduced particulate wear generation led to the introduction of crosslinked UHMWPE in orthopaedics during the late 1970s [27].”
BackgroundPost-γ-irradiation reactions in vitamin E stabilised and unstabilised HDPE
Mallégol, J., Carlsson, D. J., & Deschênes, L. (2001) · Nuclear Instruments and Methods in Physics Research Section B Beam Interactions with Materials and Atoms · doi:10.1016/s0168-583x(01)00944-2 · Cited by 62 · cited 1×
“In several applications, such as food packaging and preservation, polyethylene is currently stabilized against oxidative degradation by adding a suitable biocompatible stabilizer: vitamin E or (better) its synthetic derivative, alpha-tocopherol [ 59 , 60].”
Bracco, P., Brunella, V., Cortemiglia, M. P. L. D., Prever, E. M. B. D., Zanetti, M., & Costa, L. (2006) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2006.08.002 · Cited by 60 · cited 1×
“continue during storage and in vivo implantation [14, 15].”
BackgroundSelf-citationWolf, C., Maninger, J., Lederer, K., Frühwirth-Smounig, H., Gamse, T., & Marr, R. J. (2006) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-006-0607-7 · Cited by 57
Highly cross-linked polyethylene bearing surfaces in total hip arthroplasty.
Atienza, C. A., & Maloney, W. J. (2008) · PubMed · Cited by 24
Mechanisms of Crosslinking and Oxidative Degradation of UHMWPE
Costa, L., & Bracco, P. (2004) · Elsevier eBooks · doi:10.1016/b978-012429851-4/50012-7 · Cited by 10
Self-citation
Cited by
González-Henríquez, C. M., Sarabia-Vallejos, M. A., & Rodriguez-Hernandez, J. (2019) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2019.03.001 · Cited by 562
Biomaterials for Bone Regenerative Engineering
Yu, X., Tang, X., Gohil, S. V., & Laurencin, C. T. (2015) · Advanced Healthcare Materials · doi:10.1002/adhm.201400760 · Cited by 418
Patel, K., Chikkali, S. H., & Sivaram, S. (2020) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2020.101290 · Cited by 320
Additive manufacturing of polymer melts for implantable medical devices and scaffolds
Youssef, A., Hollister, S. J., & Dalton, P. D. (2017) · Biofabrication · doi:10.1088/1758-5090/aa5766 · Cited by 190
“Moreover, re-melting UHMWPE can be a method to decrease the amount of free radicals that are a residual by-product of crosslinking by irradiation [37].”
BackgroundInfluentialRecent updates for biomaterials used in total hip arthroplasty
Hu, C. Y., & Yoon, T.-R. (2018) · Biomaterials Research · doi:10.1186/s40824-018-0144-8 · Cited by 186
Metadata
- Authors
- Brach del Prever, E. M., Bistolfi, A., Bracco, P., & Costa, L.
- Venue
- Journal of Orthopaedics and Traumatology
- Published
- 2008-12-24
- Volume
- 10
- Issue
- 1
- Pages
- 1-8
- ISSN
- 1590-9921 (ISSN-L)
- 1590-9999
- OpenAlex
- W2164574353
- Cited by
- 188
- References
- 28
- FWCI
- 4.85
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.