Sulfonated cellulose nanofibrils obtained from wood pulp through regioselective oxidative bisulfite pre-treatment
The DOI matches its Crossref record; 22 of the 22 references it cites were found in a registry or an index.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Segal, L., Creely, J. J., Martin, A. E., & Conrad, C. M. (1959) · Textile Research Journal · doi:10.1177/004051755902901003 · Cited by 8,613 · cited 1×
“…(I002) at 22.2 and from the peak intensity at 18.0 associated with the amorphous fraction of cellulose (Iam) according to following equation (Segal et al. 1959): CrI ¼ I002 Iam I002 100% Field-emission scanning electron microscopy (FESEM) FESEM (Zeiss ULTRA plus) images of the freezedried…”
MethodInfluentialCellulose nanofibers prepared by TEMPO-mediated oxidation of native cellulose
Saito, T., Kimura, S., Nishiyama, Y., & Isogai, A. (2007) · Biomacromolecules · doi:10.1021/bm0703970 · Cited by 2,493 · cited 3×
“Compared to TEMPO oxidation, which has been reported to result in individual nanofibrils, the obtained nanofibrils presumably existed mainly in bundles because the width of a single fibril has been reported to be 3–5 nm (Saito et al. 2007, 2009).”
BackgroundResultPääkkö, M., Ankerfors, M., Kosonen, H., Nykänen, A., Ahola, S., Österberg, M., Ruokolainen, J., Laine, J., Larsson, P. T., Ikkala, O., et al. (2007) · Biomacromolecules · doi:10.1021/bm061215p · Cited by 1,962 · cited 1×
“The viscosities exhibited typical shear thinning behavior (Pääkkö et al. 2007; Lasseuguette et al. 2008), except for the sample with the highest content of sulfonated groups which possessed notably lower and almost constant viscosity after five passes through homogenizer.”
BackgroundSaito, T., Nishiyama, Y., Putaux, J.-L., Vignon, M., & Isogai, A. (2006) · Biomacromolecules · doi:10.1021/bm060154s · Cited by 1,796 · cited 3×
“(Saito et al. 2006) and periodate-chlorite (Liimatainen et al.”
BackgroundInfluentialCellulose Nanopaper Structures of High Toughness
Henriksson, M., Berglund, L. A., Isaksson, P., Lindström, T., & Nishino, T. (2008) · Biomacromolecules · doi:10.1021/bm800038n · Cited by 1,299 · cited 1×
“These values are comparable to those previously reported for nanofibril films (Henriksson et al. 2008) and suggest that nanofibrils maintained their high strength properties also after oxidative sulfonation treatment.”
ResultProperties and modification methods for vegetable fibers for natural fiber composites
Bledzki, A. K., Reihmane, S., & Gassan, J. (1996) · Journal of Applied Polymer Science · doi:10.1002/(sici)1097-4628(19960222)59:8<1329::aid-app17>3.0.co;2-0 · Cited by 906 · cited 2×
“The nanofibrils, which possess unique mechanical and chemical properties such as superior strength (Chakraborty et al. 2006), low density (Bledzki et al. 1996), and high water retention capacity (Herrick et al. 1983), can be liberated from the matrix using intensive mechanical treatments such as…”
BackgroundObtaining Cellulose Nanofibers with a Uniform Width of 15 nm from Wood
Abe, K., Iwamoto, S., & Yano, H. (2007) · Biomacromolecules · doi:10.1021/bm700624p · Cited by 885 · cited 2×
“liberated from the matrix using intensive mechanical treatments such as grinding (Abe et al. 2007) and refining (Nakagaito and Yano 2004).”
BackgroundMethodSaito, T., Hirota, M., Tamura, N., Kimura, S., Fukuzumi, H., Heux, L., & Isogai, A. (2009) · Biomacromolecules · doi:10.1021/bm900414t · Cited by 807 · cited 2×
“Compared to TEMPO oxidation, which has been reported to result in individual nanofibrils, the obtained nanofibrils presumably existed mainly in bundles because the width of a single fibril has been reported to be 3–5 nm (Saito et al. 2007, 2009).”
BackgroundNakagaito, A. N., & Yano, H. (2004) · Applied Physics A: Materials Science & Processing · doi:10.1007/s00339-003-2453-5 · Cited by 608 · cited 2×
“2007) and refining (Nakagaito and Yano 2004).”
BackgroundNanofibrillated cellulose from TEMPO-oxidized eucalyptus fibres: Effect of the carboxyl content
Besbes, I., Alila, S., & Boufi, S. (2011) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2010.12.052 · Cited by 421 · cited 1×
“These values were comparable to those previously reported for individual TEMPO-oxidized nanofibrils (Saito et al. 2007; Besbes et al. 2011), but the required anionic charge density of sulfonated cellulose was only 30–50 % that of the TEMPO samples.”
ResultClay Nanopaper with Tough Cellulose Nanofiber Matrix for Fire Retardancy and Gas Barrier Functions
Liu, A., Walther, A., Ikkala, O., Belova, L., & Berglund, L. A. (2011) · Biomacromolecules · doi:10.1021/bm101296z · Cited by 412 · cited 2×
“A vacuum-filtration method was used to prepare a thin film from sulfonated nanofibrils (Liu et al. 2011).”
MethodLiimatainen, H., Visanko, M., Sirviö, J. A., Hormi, O. E. O., & Niinimaki, J. (2012) · Biomacromolecules · doi:10.1021/bm300319m · Cited by 329 · cited 8×
“The fpotential in deionized water (conductivity\5 lS/cm, pH 5.5) was determined to be -125 mV on a Mütek SZP-06 device, and the degree of polymerization (DP) was 3817, as determined using a procedure similar to that previously described (Liimatainen et al. 2012b).”
BackgroundMethodResultSelf-citationPeriodate oxidation of cellulose at elevated temperatures using metal salts as cellulose activators
Sirvio, J., Hyvakko, U., Liimatainen, H., Niinimaki, J., & Hormi, O. (2011) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2010.09.036 · Cited by 282 · cited 6×
“…excesses of oxidant with long reaction times have traditionally been used in the periodate reaction, the reaction efficacy can be markedly improved using mechanical treatments, high temperatures, and metal salts as activators, as previously shown (Liimatainen et al. 2011; Sirviö et al. 2011).”
BackgroundMethodSelf-citationRheological properties of microfibrillar suspension of TEMPO-oxidized pulp
Lasseuguette, E., Roux, D., & Nishiyama, Y. (2008) · Cellulose · doi:10.1007/s10570-007-9184-2 · Cited by 273 · cited 1×
“The viscosities exhibited typical shear thinning behavior (Pääkkö et al. 2007; Lasseuguette et al. 2008), except for the sample with the highest content of sulfonated groups which possessed notably lower and almost constant viscosity after five passes through homogenizer.”
BackgroundFahlén, J., & Salmén, L. (2005) · Biomacromolecules · doi:10.1021/bm040068x · Cited by 212 · cited 2×
“Cellulose nanofibrils are fibrous hydrogen-bonded constituents of plant cellulose existing embedded in a matrix of hemicellulose and lignin in fiber cell walls (Fahlén and Salmén 2005).”
BackgroundReinforcing potential of wood pulp-derived microfibres in a PVA matrix
Chakraborty, A., Sain, M., & Kortschot, M. T. (2006) · Holzforschung · doi:10.1515/hf.2006.010 · Cited by 126 · cited 2×
“The nanofibrils, which possess unique mechanical and chemical properties such as superior strength (Chakraborty et al. 2006), low density (Bledzki et al. 1996), and high water retention capacity (Herrick et al. 1983), can be liberated from the matrix using intensive mechanical treatments such as…”
BackgroundOxidation and sulfonation of cellulosics
Zhang, J., Jiang, N., Dang, Z., Elder, T., & Ragauskas, A. J. (2007) · Cellulose · doi:10.1007/s10570-007-9193-1 · Cited by 124 · cited 3×
“Previously consecutive oxidation and sulfonation of cellulose have been used to prepare sulfonated celluloses from pre-fabricated nanodimensional cellulosics, but these techniques have not been used as a pre-treatment method to enhance nanofibrillation (Zhang et al. 2008).”
BackgroundMethodInfluentialProduction of nanocellulose from native cellulose – Various options utilizing ultrasound
Mishra, S., Manent, A.-S., Chabot, B., & Daneault, C. (2011) · BioResources · doi:10.15376/biores.7.1.422-436 · Cited by 101 · cited 2×
“…residual aldehydes can be decreased by increasing the bisulfite concentration during the reaction, as previously shown by Nikiforova et al. (2011) or aldehydes can be efficiently converted back to alcohols using, e.g., NaBH4 to increase the stability of the cellulosic material (Mishra et al. 2012).”
BackgroundCellulose nanofibres by sonocatalysed-TEMPO-oxidation
Rattaz, A., Mishra, S., Chabot, B., & Daneault, C. (2011) · Cellulose · doi:10.1007/s10570-011-9529-8 · Cited by 100 · cited 1×
“Conductometric titration was used to analyze the amount of sulfonated (anionic) groups in the cellulose, using a procedure described by Katz et al. (1984) and by Rattaz et al. (2011).”
MethodCharacterization of highly accessible cellulose microfibers generated by wet stirred media milling
Liimatainen, H., Sirviö, J. A., Haapala, A., Hormi, O. E. O., & Niinimäki, J. (2010) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2010.11.007 · Cited by 97 · cited 3×
“…excesses of oxidant with long reaction times have traditionally been used in the periodate reaction, the reaction efficacy can be markedly improved using mechanical treatments, high temperatures, and metal salts as activators, as previously shown (Liimatainen et al. 2011; Sirviö et al. 2011).”
BackgroundMethodSelf-citationLiimatainen, H., Sirviö, J. A., Sundman, O., Hormi, O. E. O., & Niinimäki, J. (2012) · Water Research · doi:10.1016/j.watres.2012.01.035 · Cited by 87 · cited 8×
“The fpotential in deionized water (conductivity\5 lS/cm, pH 5.5) was determined to be -125 mV on a Mütek SZP-06 device, and the degree of polymerization (DP) was 3817, as determined using a procedure similar to that previously described (Liimatainen et al. 2012b).”
BackgroundMethodResultSelf-citationMishra, S., Manent, A.-S., Chabot, B., & Daneault, C. (2012) · Journal of Wood Chemistry and Technology · doi:10.1080/02773813.2011.624666 · Cited by 49 · cited 1×
“…residual aldehydes can be decreased by increasing the bisulfite concentration during the reaction, as previously shown by Nikiforova et al. (2011) or aldehydes can be efficiently converted back to alcohols using, e.g., NaBH4 to increase the stability of the cellulosic material (Mishra et al. 2012).”
Background
Cited by
Production of cellulose nanofibrils: A review of recent advances
Nechyporchuk, O., Belgacem, M. N., & Bras, J. (2016) · Industrial Crops and Products · doi:10.1016/j.indcrop.2016.02.016 · Cited by 1,687
Key advances in the chemical modification of nanocelluloses
Habibi, Y. (2014) · Chem. Soc. Rev. · doi:10.1039/c3cs60204d · Cited by 1,561
Abdul Khalil, H. P. S., Davoudpour, Y., Islam, M. N., Mustapha, A., Sudesh, K., Dungani, R., & Jawaid, M. (2014) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2013.08.069 · Cited by 1,333
Klemm, D., Cranston, E. D., Fischer, D., Gama, M., Kedzior, S. A., Kralisch, D., Kramer, F., Kondo, T., Lindström, T., Nietzsche, S., et al. (2018) · Materials Today · doi:10.1016/j.mattod.2018.02.001 · Cited by 936
Recent advances in surface-modified cellulose nanofibrils
Rol, F., Belgacem, M. N., Gandini, A., & Bras, J. (2019) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2018.09.002 · Cited by 698
Metadata
- Authors
- Liimatainen, H., Visanko, M., Sirviö, J., Hormi, O., & Niinimäki, J.
- Venue
- Cellulose
- Published
- 2013-01-22
- Volume
- 20
- Issue
- 2
- Pages
- 741-749
- ISSN
- 0969-0239 (ISSN-L)
- 1572-882X
- OpenAlex
- W2064272795
- Cited by
- 184
- References
- 22
- FWCI
- 3.59
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.