3D mesoporous rose-like nickel-iron selenide microspheres as advanced electrocatalysts for the oxygen evolution reaction
The DOI matches its Crossref record; 6 of the 6 references it cites were found in a registry or an index.
Abstract
The development of efficient and stable non-noble metal-based electrocatalysts for the oxygen evolution reaction (OER) is one of the essential challenges for the upcoming hydrogen economy. Herein, 3D mesoporous nickel iron selenide with rose-like microsphere architecture was directly grown on Ni foam via a successive two-step hydrothermal method. The unique 3D mesoporous rose-like morphology leads to a higher number of active sites as well as fast mass and electron transport through the entire electrode, and facilitates the release of O 2 bubbles formed during the OER catalysis. As a result, the synthesized Ni 0.76 Fe 0.24 Se exhibits superior OER performances, with an ultralow overpotential of 197 mV needed to produce a current density of 10 mA·cm –2 in 1 M KOH, outperforming all transition metal selenide OER catalysts reported to date.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Wang, D.-Y., Gong, M., Chou, H.-L., Pan, C.-J., Chen, H.-A., Wu, Y., Lin, M.-C., Guan, M., Yang, J., Chen, C.-W., et al. (2015) · Journal of the American Chemical Society · doi:10.1021/ja511572q · Cited by 874
Masa, J., Weide, P., Peeters, D., Sinev, I., Xia, W., Sun, Z., Somsen, C., Muhler, M., & Schuhmann, W. (2016) · Advanced Energy Materials · doi:10.1002/aenm.201502313 · Cited by 854
Long, X., Li, G., Wang, Z., Zhu, H., Zhang, T., Xiao, S., Guo, W., & Yang, S. (2015) · Journal of the American Chemical Society · doi:10.1021/jacs.5b07728 · Cited by 657
Selenide‐Based Electrocatalysts and Scaffolds for Water Oxidation Applications
Xia, C., Jiang, Q., Zhao, C., Hedhili, M. N., & Alshareef, H. N. (2016) · Advanced Materials · doi:10.1002/adma.201503906 · Cited by 614
Wu, Y., Liu, Y., Li, G.-D., Zou, X., Lian, X., Wang, D., Sun, L., Asefa, T., & Zou, X. (2017) · Nano Energy · doi:10.1016/j.nanoen.2017.03.024 · Cited by 387
Zhang, W., Wu, Y., Qi, J., Chen, M., & Cao, R. (2017) · Advanced Energy Materials · doi:10.1002/aenm.201602547 · Cited by 215
Cited by
Recent progress in transition metal selenide electrocatalysts for water splitting
Xia, X., Wang, L., Sui, N., Colvin, V. L., & Yu, W. W. (2020) · Nanoscale · doi:10.1039/d0nr02939d · Cited by 336
Kawashima, K., Márquez, R. A., Smith, L. A., Vaidyula, R. R., Carrasco-Jaim, O. A., Wang, Z., Son, Y. J., Cao, C. L., & Mullins, C. B. (2023) · Chemical Reviews · doi:10.1021/acs.chemrev.3c00005 · Cited by 295
Sivanantham, A., Ganesan, P., Vinu, A., & Shanmugam, S. (2020) · ACS Catalysis · doi:10.1021/acscatal.9b04216 · Cited by 270
Wang, K., Wang, X., Li, Z., Yang, B., Ling, M., Gao, X., Lu, J., Shi, Q., Lei, L., Wu, G., et al. (2020) · Nano Energy · doi:10.1016/j.nanoen.2020.105162 · Cited by 225
Hameed, A., Batool, M., Liu, Z., Nadeem, M. A., & Jin, R. (2022) · ACS Energy Letters · doi:10.1021/acsenergylett.2c01362 · Cited by 205
Metadata
- Authors
- Yu, J., Cheng, G., & Luo, W.
- Venue
- Nano Research
- Publisher
- Tsinghua University Press
- Published
- 2018-03-19
- Volume
- 11
- Issue
- 4
- Pages
- 2149-2158
- ISSN
- 1998-0000 (ISSN-L)
- 1998-0124
- OpenAlex
- W2762961053
- Cited by
- 75
- References
- 6
- FWCI
- 2.35
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.