Carbonation of Stainless Steel Slag as a Process for CO2 Storage and Slag Valorization
The DOI matches its Crossref record; 45 of the 45 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The mechanism of the effect of carbonation on the leaching characteristics of chromium in the EAF slag is still unclear.”
From Carbonation of EAF Stainless Steel Slag and Its Effect on Chromium Leaching Characteristics (2021) · cites this paper as [12]
Citations
Cites
Carbon dioxide disposal in carbonate minerals
Lackner, K. S., Wendt, C. H., Butt, D. P., Joyce, E. L., & Sharp, D. H. (1995) · Energy · doi:10.1016/0360-5442(95)00071-n · Cited by 1,021 · cited 1×
“[11–13]).”
Mineral CO 2 Sequestration by Steel Slag Carbonation
Huijgen, W. J. J., Witkamp, G.-J., & Comans, R. N. J. (2005) · Environmental Science & Technology · doi:10.1021/es050795f · Cited by 858 · cited 5×
“Only Ca phases were considered in the calculation of the conversion yields, since the Mg content of the slag was an order of magnitude lower than the Ca content, and secondly because relevant CO2 uptakes by Mg oxide or silicate phases has not been reported in prior carbonation studies on steel slag, neither under mild…”
BackgroundMethodInfluentialProducts of steel slags an opportunity to save natural resources
Motz, H., & Geiseler, J. (2001) · Waste Management · doi:10.1016/s0956-053x(00)00102-1 · Cited by 823 · cited 3×
“as an aggregate or as a filler in cement production [5].”
BackgroundInfluentialSteel Slag—Its Production, Processing, Characteristics, and Cementitious Properties
Shi, C. (2004) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)0899-1561(2004)16:3(230 · Cited by 734
An overview of recovery of metals from slags
Shen, H., & Forssberg, E. (2003) · Waste Management · doi:10.1016/s0956-053x(02)00164-2 · Cited by 592 · cited 5×
“Steel slag is usually regarded as a non-hazardous waste owing to its limited release of trace contaminants, as mirrored by compliance with standard leaching criteria [3]; however, some types of stainless steel slag, such as that produced during steel refining, may release non negligible amounts of Cr [6].”
BackgroundResultInfluentialProctor, D. M., Fehling, K. A., Shay, E. C., Wittenborn, J. L., Green, J. J., Avent, C., Bigham, R. D., Connolly, M., Lee, B., Shepker, T. O., et al. (2000) · Environmental Science & Technology · doi:10.1021/es9906002 · Cited by 493 · cited 2×
“Steel slag is usually regarded as a non-hazardous waste owing to its limited release of trace contaminants, as mirrored by compliance with standard leaching criteria [3]; however, some types of stainless steel slag, such as that produced during steel refining, may release non negligible amounts of Cr [6].”
BackgroundCarbon dioxide sequestration in cement kiln dust through mineral carbonation
Huntzinger, D. N., Gierke, J. S., Kawatra, S. K., Eisele, T. C., & Sutter, L. L. (2009) · Environmental Science & Technology · doi:10.1021/es802910z · Cited by 442 · cited 2×
“5 w/w) [14, 15, 17, 19–21, 24, 25, 27, 28, 30].”
BackgroundMineral sequestration of CO2 by aqueous carbonation of coal combustion fly-ash
Montes-Hernandez, G., Pérez-López, R., Renard, F., Nieto, J. M., & Charlet, L. (2009) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2008.04.104 · Cited by 403 · cited 1×
“Direct aqueous carbonation studies have been performed in two different modes, either in slurry phase at Liquid to Solid (L/S) ratios between 5 and 50 w/w [18, 22, 23, 35, 36] (in particular for waste materials with high silicate contents), or at lower water contents (L/S ratios \ 1.”
BackgroundAccelerated Curing of Compacted Calcium Silicate Mortars on Exposure to CO 2
YOUNG, J. F., BERGER, R. L., & BREESE, J. (1974) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1974.tb11420.x · Cited by 356 · cited 1×
“[37, 38]).”
Experimental investigation and mathematical modeling of the concrete carbonation problem
Papadakis, V. G., Vayenas, C. G., & Fardis, M. N. (1991) · Chemical Engineering Science · doi:10.1016/0009-2509(91)85060-b · Cited by 346 · cited 1×
“[37, 38]).”
Research works printed but not linked: 1
- OECD (Organization for Economic Cooperation and Development): Iron and steel industry report 2000. OECD, Paris (2002)
Cited by
An overview of utilizing CO2 for accelerated carbonation treatment in the concrete industry
Li, L., & Wu, M. (2022) · Journal of CO2 Utilization · doi:10.1016/j.jcou.2022.102000 · Cited by 305
Direct mineral carbonation of coal fly ash for CO 2 sequestration
Tamilselvi Dananjayan, R. R., Kandasamy, P., & Andimuthu, R. (2016) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2015.05.145 · Cited by 261
Santos, R. M., Van Bouwel, J., Vandevelde, E., Mertens, G., Elsen, J., & Van Gerven, T. (2013) · International Journal of Greenhouse Gas Control · doi:10.1016/j.ijggc.2013.04.004 · Cited by 257
“(2005) and EAF slag as reported by Baciocchi et al. (2011); it was possible to reach 21–24 wt%,CO2 with AOD and CC slags compared to a maximum ~15 wt%,CO2 with finely milled BOF and EAF slags.”
BackgroundMethodInfluentialThe role of β-C2S and γ-C2S in carbon capture and strength development
Chang, J., Fang, Y., & Shang, X. (2016) · Materials and Structures · doi:10.1617/s11527-016-0797-5 · Cited by 228
Ho, H.-J., Iizuka, A., & Shibata, E. (2019) · Industrial & Engineering Chemistry Research · doi:10.1021/acs.iecr.9b01213 · Cited by 200
Accelerated carbonation of steel slag: A review of methods, mechanisms and influencing factors
Huang, X., Zhang, J., & Zhang, L. (2024) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.134603 · Cited by 195
Environmental benefit assessment of steel slag utilization and carbonation: A systematic review
Li, L., Ling, T.-C., & Pan, S.-Y. (2022) · Science of The Total Environment · doi:10.1016/j.scitotenv.2021.150280 · Cited by 193
Polettini, A., Pomi, R., & Stramazzo, A. (2016) · Chemical Engineering Journal · doi:10.1016/j.cej.2016.04.015 · Cited by 189
Self-citationSalman, M., Cizer, Ö., Pontikes, Y., Santos, R. M., Snellings, R., Vandewalle, L., Blanpain, B., & Van Balen, K. (2014) · Chemical Engineering Journal · doi:10.1016/j.cej.2014.02.051 · Cited by 171
“[7] have demonstrated that even under mild operating conditions of temperature and pressure, carbonation of humidified AOD slag is possible.”
BackgroundPolettini, A., Pomi, R., & Stramazzo, A. (2016) · Journal of Environmental Management · doi:10.1016/j.jenvman.2015.11.042 · Cited by 151
Self-citationThin-film versus slurry-phase carbonation of steel slag: CO2 uptake and effects on mineralogy
Baciocchi, R., Costa, G., Di Gianfilippo, M., Polettini, A., Pomi, R., & Stramazzo, A. (2015) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2014.09.016 · Cited by 147
Self-citationKazemian, M., & Shafei, B. (2023) · Journal of CO2 Utilization · doi:10.1016/j.jcou.2023.102443 · Cited by 170
Ultrasound-intensified mineral carbonation
Santos, R. M., François, D., Mertens, G., Elsen, J., & Van Gerven, T. (2013) · Applied Thermal Engineering · doi:10.1016/j.applthermaleng.2012.03.035 · Cited by 141
State-of-the-art review on capture of CO2 using adsorbents prepared from waste materials
Ochedi, F. O., Liu, Y., & Adewuyi, Y. G. (2020) · Process Safety and Environmental Protection · doi:10.1016/j.psep.2020.03.036 · Cited by 140
Ben Ghacham, A., Pasquier, L.-C., Cecchi, E., Blais, J.-F., & Mercier, G. (2017) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2017.08.015 · Cited by 130
“Baciocchi et al. (2010) investigated the carbonation of steel slags under less extreme pressure (3 Bar) and temperature (50 °C) conditions for a reaction duration of 2 h using 100% CO2.”
MethodA review on ex situ mineral carbonation
Yadav, S., & Mehra, A. (2021) · Environmental Science and Pollution Research · doi:10.1007/s11356-020-12049-4 · Cited by 152
Ebrahimi, A., Saffari, M., Milani, D., Montoya, A., Valix, M., & Abbas, A. (2017) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2017.04.037 · Cited by 129
Production of cement-free construction blocks from industry wastes
Mahoutian, M., & Shao, Y. (2016) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2016.08.012 · Cited by 139
Teo, P. T., Zakaria, S. K., Salleh, S. Z., Taib, M. A. A., Sharif, N. M., Seman, A. A., Mohamed, J. J., Yusoff, M. B., Yusoff, A. H., Mohamad, M., et al. (2020) · Metals · doi:10.3390/met10101347 · Cited by 150
Advances in state-of-art valorization technologies for captured CO2toward sustainable carbon cycle
Pan, S.-Y., Chiang, P.-C., Pan, W., & Kim, H. (2018) · Critical Reviews in Environmental Science and Technology · doi:10.1080/10643389.2018.1469943 · Cited by 114
“Furthermore, oxidant states of heavy metals in solid wastes would lead to different leaching behaviours (Baciocchi et al., 2010).”
BackgroundEnvironmental assessment of CO2 mineralisation for sustainable construction materials
Di Maria, A., Snellings, R., Alaerts, L., Quaghebeur, M., & Van Acker, K. (2020) · International Journal of Greenhouse Gas Control · doi:10.1016/j.ijggc.2019.102882 · Cited by 108
Effects of thin-film accelerated carbonation on steel slag leaching
Baciocchi, R., Costa, G., Polettini, A., & Pomi, R. (2015) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2014.12.059 · Cited by 97
Self-citationDirect mineral carbonation of steelmaking slag for CO2 sequestration at room temperature
Revathy, T. D. R., Palanivelu, K., & Ramachandran, A. (2015) · Environmental Science and Pollution Research · doi:10.1007/s11356-015-5893-5 · Cited by 100
“3 and 4, diffusion of both the gas molecules and leaching of metal cations present in the waste depends on the amount of water present inside the reactor (Baciocchi et al. 2010).”
BackgroundResultBodor, M., Santos, R. M., Kriskova, L., Elsen, J., Vlad, M., & Van Gerven, T. (2013) · European Journal of Mineralogy · doi:10.1127/0935-1221/2013/0025-2300 · Cited by 92
A review on steel slag valorisation via mineral carbonation
Ragipani, R., Bhattacharya, S., & Suresh, A. K. (2021) · Reaction Chemistry & Engineering · doi:10.1039/d1re00035g · Cited by 99
Valorization of steel slag by a combined carbonation and granulation treatment
Morone, M., Costa, G., Polettini, A., Pomi, R., & Baciocchi, R. (2013) · Minerals Engineering · doi:10.1016/j.mineng.2013.08.009 · Cited by 91
Self-citationLadle furnace slag as a partial replacement of Portland cement
Araos, P., Aponte, D., Ibáñez, J., & Bizinotto, M. B. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123106 · Cited by 91
“121 To solve these problems associated to the use of LFS as a cement replacement in general, three types 122 of methods have been proposed: an accelerated weathering of LFS with different hydration process 123 [35], a stabilization system subjecting the material to a carbonation process [55-57], and an air rapid 124 c…”
Accelerated Carbonation of Steel Slag Compacts: Development of High-Strength Construction Materials
Quaghebeur, M., Nielsen, P., Horckmans, L., & Van Mechelen, D. (2015) · Frontiers in Energy Research · doi:10.3389/fenrg.2015.00052 · Cited by 83
“For SS slags, raising the temperature from 20 to 140°C had a positive effect on the CO2 uptake, strength development, and the environmental properties (i.e., leaching of Cr and Mo) of the carbonated slag compacts.”
BackgroundJo, H., Park, S.-H., Jang, Y.-N., Chae, S.-C., Lee, P.-K., & Jo, H. Y. (2014) · Chemical Engineering Journal · doi:10.1016/j.cej.2014.05.129 · Cited by 82
Monitoring of Stainless-Steel Slag Carbonation Using X-ray Computed Microtomography
Boone, M. A., Nielsen, P., De Kock, T., Boone, M. N., Quaghebeur, M., & Cnudde, V. (2014) · Environmental Science & Technology · doi:10.1021/es402767q · Cited by 74
Bodor, M., Santos, R., Gerven, T., & Vlad, M. (2013) · Open Engineering · doi:10.2478/s13531-013-0115-8 · Cited by 71
“[25, 59].”
Wang, Y.-J., Zeng, Y.-N., Li, J.-G., Zhang, Y.-Z., Zhang, Y.-J., & Zhao, Q.-Z. (2020) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2020.120377 · Cited by 71
Teir, S., Kotiranta, T., Pakarinen, J., & Mattila, H. (2016) · Journal of CO2 Utilization · doi:10.1016/j.jcou.2016.02.004 · Cited by 79
Fang, Y., Su, W., Zhang, Y., Zhang, M., Ding, X., & Wang, Q. (2021) · Journal of Thermal Analysis and Calorimetry · doi:10.1007/s10973-021-10914-z · Cited by 67
Atmospheric Carbon Capture Performance of Legacy Iron and Steel Waste
Pullin, H., Bray, A. W., Burke, I. T., Muir, D., Sapsford, D., Mayes, W. M., & Renforth, P. (2019) · Environmental Science & Technology · doi:10.1021/acs.est.9b01265 · Cited by 73
Yang, J. J., Firsbach, F., & Sohn, I. (2021) · Resources Conservation and Recycling · doi:10.1016/j.resconrec.2021.106021 · Cited by 71
Solid‐waste‐Derived carbon dioxide‐capturing materials
Wang, J., Yang, Y., Jia, Q., Shi, Y., Guan, Q., Yang, N., Ning, P., & Wang, Q. (2019) · ChemSusChem · doi:10.1002/cssc.201802655 · Cited by 60
Zhao, Q. L., Chu, X., Mei, X., Meng, Q., Li, J., Liu, C., Saxén, H., & Zevenhoven, R. (2020) · Frontiers in Chemistry · doi:10.3389/fchem.2020.571504 · Cited by 64
“4 mL·g−1) can promote metal cations leaching from the SS (Baciocchi et al., 2010), while the presence of excessive water would block the diffusion of CO2 in the slurry (Fernández Bertos et al.”
BackgroundLoncnar, M., van der Sloot, H. A., Mladenovič, A., Zupančič, M., Kobal, L., & Bukovec, P. (2016) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2016.05.046 · Cited by 66
Maria, A. D., Muhammad, S., Dubois, M., & Acker, K. V. (2018) · The International Journal of Life Cycle Assessment · doi:10.1007/s11367-018-1440-1 · Cited by 65
Zhang, X., Zhao, J., Liu, Y., & Li, J. (2024) · Journal of CO2 Utilization · doi:10.1016/j.jcou.2024.102947 · Cited by 66
Baciocchi, R., Corti, A., Costa, G., Lombardi, L., & Zingaretti, D. (2011) · Energy Procedia · doi:10.1016/j.egypro.2011.02.469 · Cited by 57
Self-citationLeaching modelling of slurry-phase carbonated steel slag
Costa, G., Polettini, A., Pomi, R., & Stramazzo, A. (2016) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2015.10.005 · Cited by 50
Self-citationWang, X., Lu, X., Turvey, C., Dipple, G. M., & Ni, W. (2022) · Resources Conservation and Recycling · doi:10.1016/j.resconrec.2022.106590 · Cited by 52
El‐Naas, M. H., Gamal, M. M. E., Hameedi, S. M., & Mohamed, A. O. (2015) · Journal of Environmental Management · doi:10.1016/j.jenvman.2015.03.040 · Cited by 51
“resulting in a reduction of pH and leached metals, leading to solid stabilization (Baciocchi et al., 2010).”
BackgroundBiava, G., Zacco, A., Zanoletti, A., Sorrentino, G. P., Capone, C., Princigallo, A., Depero, L. E., & Bontempi, E. (2023) · Materials · doi:10.3390/ma16114055 · Cited by 48
“AOD slag belongs to the LF slag group and is produced during the argon oxygen decarburization process [32].”
BackgroundWet versus slurry carbonation of EAF steel slag
Baciocchi, R., Costa, G., Di Bartolomeo, E., Polettini, A., & Pomi, R. (2011) · Greenhouse Gases: Science and Technology · doi:10.1002/ghg.38 · Cited by 43
Self-citationHigh-capacity adsorbents from stainless steel slag for the control of dye pollutants in water
Plaza, L., Castellote, M., Nevshupa, R. A., & Jiménez-Relinque, E. (2021) · Environmental Science and Pollution Research · doi:10.1007/s11356-020-12174-0 · Cited by 42
“…convert slag into a product with new potentialities is focused on exploring the effect of accelerated carbonation for storing point-source emissions of CO2 (Baciocchi et al. 2010; Bonenfant et al. 2008; Huijgen et al. 2005; Johnson 2000; Kodama et al. 2008; Lekakh et al. 2008; Santos et al. 2013).”
BackgroundInfluentialChandel, S. S., Singh, P. K., Katiyar, P. K., & Randhawa, N. S. (2023) · Mining Metallurgy & Exploration · doi:10.1007/s42461-023-00886-z · Cited by 53
Remediation of stainless steel slag with MnO for CO2 mineralization
Zhao, Q. L., Liu, C., Gao, T.-C., Gao, L., Saxén, H., & Zevenhoven, R. (2019) · Process Safety and Environmental Protection · doi:10.1016/j.psep.2019.04.025 · Cited by 35
Feedstocks study on CO2 mineralization technology
Xie, H., Tang, L., Wang, Y., Liu, T., Hou, Z., Wang, J., Wang, T., Jiang, W., & Were, P. (2016) · Environmental Earth Sciences · doi:10.1007/s12665-016-5352-8 · Cited by 36
“Calcium (CaO: 30–60 %), silicon (SiO2: 8–35 %), aluminum (Al2O3: 1–35 %), magnesium (MgO: 1–15 %) and iron (FeO: 1–35 %) are the major chemical species (Baciocchi et al. 2010; Shi 2004; Shih et al. 2004).”
BackgroundInfluentialGeorgakopoulos, E., Santos, R. M., Chiang, Y. W., & Manovic, V. M. (2016) · Greenhouse Gases Science and Technology · doi:10.1002/ghg.1608 · Cited by 41
“=3 bar, L/S=0.4 L/kg) Baciocchi et al. (2010)38 EAF Steady (50 °C) (reaction time < 1 hour) At 1 bar, 30% less CO2 uptake than at higher pressures (3 and 10 bar) (reaction time > 1hour) Steady (0.4 L/kg) 49.1 % (after 24h,T=50 °C, part. size<150 µm, PCO₂=0.3 bar, L/S=0.4 L/kg,) AOD Steady (50 °C) Steady (0.4 L/kg) 69.…”
BackgroundMethodResultInfluentialAssessment of Accelerated Carbonation Processes for CO2 Storage Using Alkaline Industrial Residues
Zingaretti, D., Costa, G., & Baciocchi, R. (2013) · Industrial & Engineering Chemistry Research · doi:10.1021/ie403692h · Cited by 36
Self-citationEnvironmental Characteristics and Utilization Potential of Metallurgical Slag
Piatak, N. M. (2017) · Elsevier eBooks · doi:10.1016/b978-0-444-63763-5.00020-3 · Cited by 44
Using nondestructive techniques in mineral carbonation for understanding reaction fundamentals
Haque, F., Santos, R. M., & Chiang, Y. W. (2019) · Powder Technology · doi:10.1016/j.powtec.2019.08.089 · Cited by 38
Salman, M., Dubois, M., Maria, A. D., Acker, K. V., & Balen, K. V. (2015) · Journal of Industrial Ecology · doi:10.1111/jiec.12314 · Cited by 38
“Also, although there have been several works studying SS slag as a source of mineral sequestration of CO2 (Baciocchi et al. 2010; Santos et al. 2013), none have focused on developing construction materials as an end product.”
BackgroundBaciocchi, R., Costa, G., Polettini, A., Pomi, R., Stramazzo, A., & Zingaretti, D. (2016) · Frontiers in Energy Research · doi:10.3389/fenrg.2015.00056 · Cited by 32
Self-citationCarbonation of stainless steel slag in the context of in situ Brownfield remediation
Capobianco, O., Costa, G., Thuy, L., Magliocco, E., Hartog, N., & Baciocchi, R. (2013) · Minerals Engineering · doi:10.1016/j.mineng.2013.11.005 · Cited by 34
Self-citationKassim, D., Lamaa, G., Silva, R. V., & de Brito, J. (2022) · Applied Sciences · doi:10.3390/app12031662 · Cited by 29
“Exploiting the possibility of curing the EAFS concrete with CO 2 [40–42], by taking advantage of its CaO-rich chemistry, will not only lead to better mechanical performance but also an added value to CO 2 -capturing revolutionary technologies.”
BackgroundKurusta, T., Mucsi, G., Kumar, S., & Kristály, F. (2022) · Fuel · doi:10.1016/j.fuel.2023.128951 · Cited by 35
Influence of NaCl on mineral carbonation of CO2 using cement material in aqueous solutions
Jo, H., Jang, Y.-N., & Jo, H. Y. (2012) · Chemical Engineering Science · doi:10.1016/j.ces.2012.06.034 · Cited by 34
Slurry-Phase Carbonation Reaction Characteristics of AOD Stainless Steel Slag
Tao, M., Wang, Y.-J., Li, J., Zeng, Y., Liu, S., & Qin, S. (2021) · Processes · doi:10.3390/pr9122266 · Cited by 27
“Salman et al. [13] and Baciocchi et al. [14,15] also systematically studied the product leaching and reaction mechanism of steel slag carbonation and investigated the different degrees of steel slag carbonation to prove the possibility of CO 2 sequestration through steel slag carbonation.”
BackgroundCarbonation of EAF Stainless Steel Slag and Its Effect on Chromium Leaching Characteristics
Wang, Y.-J., Tao, M.-J., Li, J.-G., Zeng, Y.-N., Qin, S., & Liu, S.-H. (2021) · Crystals · doi:10.3390/cryst11121498 · Cited by 27
“[12] found that carbonation could increase the chromium leachability in the process of studying the carbonation mechanism of stainless steel slag, and pointed out that this was related to the presence of chromium in different valence states after carbonation.”
BackgroundLeventaki, E., Queiroz, E. C., Pisharody, S. K., Kumar, A. K. S., Ho, P. H., Andersson-Sarning, M., Haase, B., Baena‐Moreno, F. M., Cuin, A., & Bernin, D. (2024) · Environmental Research · doi:10.1016/j.envres.2024.118903 · Cited by 27
He, Y.-L., Jia, S., Yi, H., Tang, X., Yu, Q., Gao, F., Kang, D., & Zhao, S. (2024) · Journal of environmental chemical engineering · doi:10.1016/j.jece.2024.114090 · Cited by 26
Shear-Force Based Stainless Steel Slag Modification for Chromium Immobilization
Zhao, Q. L., Liu, C., Cao, L., Jiang, M., Li, B., Saxén, H., & Zevenhoven, R. (2018) · ISIJ International · doi:10.2355/isijinternational.isijint-2017-678 · Cited by 25
Granulation–Carbonation Treatment of Alkali Activated Steel Slag for Secondary Aggregates Production
Morone, M., Costa, G., Georgakopoulos, E., Manovic, V. M., Stendardo, S., & Baciocchi, R. (2016) · Waste and Biomass Valorization · doi:10.1007/s12649-016-9781-0 · Cited by 28
“These specific conditions were selected since in previous works carried out on steelmaking slag they allowed to achieve significant CO2 uptakes applying the wet carbonation route [25, 26, 29].”
Self-citationAhmed, A., & Hassan, Z. F. A. (2025) · The Science of The Total Environment · doi:10.1016/j.scitotenv.2025.179544 · Cited by 28
Wang, H., Zhou, G., Mu, Y., Zhang, M., & Guo, M. (2024) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2024.141181 · Cited by 24
CO2 Sequestration Through Aqueous Carbonation of Electric Arc Furnace Slag
Bonfante, F., Ferrara, G., Humbert, P., Garufi, D., Tulliani, J., & Palmero, P. (2024) · Journal of Advanced Concrete Technology · doi:10.3151/jact.22.207 · Cited by 26
Schnabel, K., Brück, F., Pohl, S., Mansfeldt, T., & Weigand, H. (2021) · Greenhouse Gases Science and Technology · doi:10.1002/ghg.2063 · Cited by 21
Utilization of steelmaking slag for carbon capture and storage with flue gas
Revathy, T. D. R., Ramachandran, A., & Palanivelu, K. (2021) · Environmental Science and Pollution Research · doi:10.1007/s11356-021-17493-4 · Cited by 19
Yuan, J., Chang, J. S., & Du, X. (2024) · Sustainable Chemistry and Pharmacy · doi:10.1016/j.scp.2024.101819 · Cited by 26
Carbonation of BOF Slag in a Rotary Kiln Reactor in View of the Scale‐Up of the Wet Route Process
Librandi, P., Costa, G., Stendardo, S., & Baciocchi, R. (2019) · Environmental Progress & Sustainable Energy · doi:10.1002/ep.13140 · Cited by 18
“CO2 in a solid and stable form [5,6] and yields a solid product that may be used for specific applications.”
BackgroundSelf-citationBouargane, B., Pérez-Moreno, S. M., Barba-Lobo, A., Bakiz, B., Atbir, A., & Bolívar, J. P. (2023) · Chemical Engineering Science · doi:10.1016/j.ces.2023.119013 · Cited by 17
Pusparizkita, Y. M., Schmahl, W. W., Ambarita, M., Kholid, H. N., Sadewa, A. Y., Ismail, R., Jamari, J., & Bayuseno, A. P. (2023) · Cleaner Engineering and Technology · doi:10.1016/j.clet.2023.100602 · Cited by 21
You, I., Park, J.-J., Lee, N., Ryu, G.-S., & Kwark, J.-W. (2024) · Journal of Building Engineering · doi:10.1016/j.jobe.2024.108631 · Cited by 18
Accelerated Carbonation Processes for Carbon Dioxide Capture, Storage and Utilisation
Baciocchi, R., Costa, G., & Zingaretti, D. (2014) · Green chemistry and sustainable technology · doi:10.1007/978-3-642-44988-8_11 · Cited by 16
“150 mm) and were related to the differences in the mineralogy of the two slags: the AOD residues mostly made up by γ-dicalcium silicate, while the others containing various Ca and Mg silicates [48].”
BackgroundSelf-citationTest methods for CO2 mineralization in cement-based materials: A review by RILEM TC 309-MCP
Matschei, T., Braymand, S., Garg, N., Huet, B., Jansen, D. C., Myers, R. J., Scruggs, B. E., Bernard, E., Bertola, J., Cazacliu, B. G., et al. (2026) · Materials and Structures · doi:10.1617/s11527-026-03064-x · Cited by 22
“When pressurized CO 2 is used, carbonation of CaSO 4 [105] and MgO can occur, even though MgO carbonation is usually limited [106].”
Wang, L., & Fan, Y. (2025) · Journal of Building Engineering · doi:10.1016/j.jobe.2025.111862 · Cited by 28
Costa, G., Polettini, A., Pomi, R., Stramazzo, A., & Zingaretti, D. (2016) · Greenhouse Gases Science and Technology · doi:10.1002/ghg.1659 · Cited by 18
Self-citationMatino, I., Colla, V., & Baragiola, S. (2018) · Waste and Biomass Valorization · doi:10.1007/s12649-018-0264-3 · Cited by 14
Evaluation of electrical properties of glass-ceramics obtained from mill scale
Montedo, O. R. K., Alves, I. T., Faller, C. A., Bertan, F. M., Piva, D. H., & Piva, R. H. (2015) · Materials Research Bulletin · doi:10.1016/j.materresbull.2015.07.040 · Cited by 20
Bonfante, F., Ferrara, G., Humbert, P., Garufi, D., Tulliani, J., & Palmero, P. (2025) · Materials and Structures · doi:10.1617/s11527-025-02661-6 · Cited by 19
Contribution mechanism of MgO doping to strength enhance of steel slag products during carbonation
Li, W., Wang, D., Cao, M., Xiong, C., & Chang, J. S. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2025.140272 · Cited by 14
Dudhaiya, A., & Santos, R. M. (2018) · Geosciences · doi:10.3390/geosciences8070260 · Cited by 15
“[35] Argon Oxygen Decarburization (AOD) The AOD slag, as received, as sieved to a particle size <150 μm, with 90% of the slag passing this mesh size.”
MethodFree CaO stabilisation by mixing of BF slag and BOF slag in molten state
Yin, X. M., Zhang, C., Wang, G., Yang, J., Cai, Y., & Zhao, C. (2018) · Ironmaking & Steelmaking Processes Products and Applications · doi:10.1080/03019233.2017.1419656 · Cited by 12
“far, several available even commercial processes for stabilising BOF slag have been developed, such as aging in slag pits [11], hydration by steam [12], carbonation via CO2 absorption [13,14] and additions of materials containing SiO2 coupled with O2 blowing [15,16].”
BackgroundZingaretti, D., Costa, G., & Baciocchi, R. (2013) · Energy Procedia · doi:10.1016/j.egypro.2013.06.509 · Cited by 17
“For all the considered types of residues used in the slurry phase and wet route, the chemical composition of the alkaline material and the operating condition applied in the carbonation experiments are reported in [6], [7], [9], [11] and [22]”
MethodSelf-citationGeorget, F., Caprai, V., Belli, A., Keulen, A., & Matschei, T. (2025) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2025.106179 · Cited by 12
Lee, O., Parr, J.-L. M., Zi, G., & Yoon, Y. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2025.142654 · Cited by 10
Properties of ten-year-aged argon oxygen decarburization stainless steel slag
Wang, Y.-J., Zeng, Y., Li, J., Zhang, Y., & Wang, W. (2021) · Journal of Iron and Steel Research International · doi:10.1007/s42243-021-00635-w · Cited by 11
The Properties of Steel Slag Bricks Prepared by both Alkali Activation and Accelerated Carbonation
Zhang, W. S., Shi, D., Shao, Z. J., Ye, J., & Wang, Y. (2012) · Key engineering materials · doi:10.4028/www.scientific.net/kem.509.113 · Cited by 10
“A large number of investigations have been respectively conducted in the alkali activation and accelerated carbonation of steel slag over the past decades [6-9].”
BackgroundCarbonation curing of alkaline industrial waste for binders: comparison of different wastes
Fang, Y., Zhang, Y., Zhang, M., Zhao, M., & Wang, Q. (2020) · Magazine of Concrete Research · doi:10.1680/jmacr.20.00133 · Cited by 9
Baciocchi, R., Capobianco, O., Costa, G., Morone, M., & Zingaretti, D. (2014) · Energy Procedia · doi:10.1016/j.egypro.2014.11.621 · Cited by 9
“: [8],[9]).”
Self-citationProperties of Carbonated Steel Slag Admixture in the Cementitious System
Sun, L., Wang, H., & Wang, Y. (2023) · Advances in Civil Engineering · doi:10.1155/2023/5547591 · Cited by 16
Direct Aqueous Mineral Carbonation of Waste Slate Using Ammonium Salt Solutions
Jo, H., Jo, H. Y., Rha, S., & Lee, P.-K. (2015) · Metals · doi:10.3390/met5042413 · Cited by 10
Stabilization of carbon dioxide and chromium slag via carbonation
Wu, X., Yu, B., Xu, W. M., Fan, Z. Y., Wu, Z., & Zhang, H. (2016) · Environmental Technology · doi:10.1080/09593330.2016.1244566 · Cited by 6
“So far, many alkaline wastes, such as cement kiln dust [26] and stainless steel slag [27] have been already studied,”
BackgroundReynes, J. F., Mercier, G., Blais, J., & Pasquier, L.-C. (2021) · Applied Geochemistry · doi:10.1016/j.apgeochem.2021.105029 · Cited by 7
Mechanochemical Activation of Argon Oxygen Decarburization Slags for Improved Mineral Carbonation
Ceyssens, L., Miladinović, N., Granata, G., & Gerven, T. V. (2025) · Chemical Engineering & Technology · doi:10.1002/ceat.12004 · Cited by 7
Wang, S., Zhang, Y.-F., Zhao, K., Long, H., & Rufei, W. E. I. (2025) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2025.146631 · Cited by 7
Metadata
- Authors
- Baciocchi, R., Costa, G., Di Bartolomeo, E., Polettini, A., & Pomi, R.
- Affiliations
- University of Rome Tor Vergata (IT)
- Sapienza University of Rome (IT)
- Corresponding author
- Costa, Giulia
- Venue
- Waste and Biomass Valorization
- Published
- 2010-10-20
- Volume
- 1
- Issue
- 4
- Pages
- 467-477
- ISSN
- 1877-2641 (ISSN-L)
- 1877-265X
- OpenAlex
- W2017861769
- Cited by
- 126
- References
- 45
- Citations by year
- 2026: 5 · 2025: 13 · 2024: 9 · 2023: 10 · 2022: 6 · 2021: 14 · 2020: 7 · 2019: 8 · 2018: 6 · 2017: 4 · 2016: 14 · 2015: 9 · 2014: 5 · 2013: 10 · 2012: 3
- FWCI
- 4.92
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.springer.com/tdm (tdm)
- Locations
- Waste and Biomass Valorization (publishedVersion)
- Cineca Institutional Research Information System (Tor Vergata University) (submittedVersion)
- IRIS Research product catalog (Sapienza University of Rome) (submittedVersion)
- Topics
- Physical Sciences › Environmental Science › Environmental Engineering › CO2 Sequestration and Geologic Interactions
- Physical Sciences › Engineering › Civil and Structural Engineering › Concrete and Cement Materials Research
- Physical Sciences › Engineering › Building and Construction › Recycling and utilization of industrial and municipal waste in materials production
- Keywords
- stainless steel slag, carbonation, CO2 sequestration, CO2 uptake, electric arc furnace slag, slag valorization, calcite formation, leaching behavior, slag mineralogy, milling, size fractionation
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.