Decomposition of synthesized ettringite by carbonation
The DOI matches its Crossref record; 3 of the 3 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“It is well established that gypsum is formed at high RH values of ~90% meanwhile bassanite forms at lower RH (e.g., 60-70%) [18,19,21].”
From X-ray Total Scattering Study of Phases Formed from Cement Phases Carbonation (2021) · cites this paper as [19]
In the citing paper
“In agreement with previous reports [18,19,21], only bassanite is observed here, as calcium sulphate crystalline phase, because the RH of the carbonation experiment was 65%.”
From X-ray Total Scattering Study of Phases Formed from Cement Phases Carbonation (2021) · cites this paper as [19]
Citations
Cites
Formation and carbonation of C-S-H in water
SUZUKI, K., NISHIKAWA, T., & Ito, S. (1985) · Cement and Concrete Research · doi:10.1016/0008-8846(85)90032-8 · Cited by 157
Self-citationThe analysis of ettringite in hardened cement paste
Uchikawa, H., & Uchida, S. (1974) · Cement and Concrete Research · doi:10.1016/0008-8846(74)90053-2 · Cited by 30
Analysis of Hydrated Phases for Evaluation the Durability of Concrete
SUZUKI, K., NISHIKAWA, T., YAMADE, Y., & Taniguchi, I. (1990) · Concrete Research and Technology · doi:10.3151/crt1990.1.2_39 · Cited by 30
Self-citation
Research works printed but not linked: 3
- Suzuki, 1989, 43, 18
- Kira, 1979, Gypsum & Lime No. 159, 48
- Kuzel, 1989, Zement-Kalk-Gips, 42, 413
Cited by
Items 101–200 of 270
Cheng, L., Kurihara, R., Ohkubo, T., Kitagaki, R., Teramoto, A., Suda, Y., & Maruyama, I. (2025) · Cement and Concrete Research · doi:10.1016/j.cemconres.2025.107898 · Cited by 36
Degradation of concrete by flue gases from coal combustion
Pavlík, V., Bajza, A., Rouseková, I., Unčík, S., & Dubík, M. (2007) · Cement and Concrete Research · doi:10.1016/j.cemconres.2007.04.008 · Cited by 36
Kim, H., Pei, J., Siddique, S., & Jang, J. G. (2021) · Sustainability · doi:10.3390/su13095175 · Cited by 37
“This may be due to the decomposition of ettringite to calcite upon carbonation [32].”
BackgroundMINERAL COMPOSITION OF ESTONIAN OIL SHALE SEMI-COKE SEDIMENTS
Mõtlep, R., Kirsimäe, K., Talviste, P., Puura, E., & JÜRGENSON, J. (2007) · Oil Shale · doi:10.3176/oil.2007.3.01 · Cited by 35
“However, at high CO2 partial pressure and relatively low pH level, ettringite decomposes into sulfates and aragonite [CaCO3] with vaterite [γ-CaCO3] as an intermediate phase [22].”
BackgroundKuusik, R., Uibu, M., Kirsimäe, K., Mõtlep, R., & Meriste, T. (2012) · Oil Shale · doi:10.3176/oil.2012.4.08 · Cited by 40
“7 ettringite dissolves incongruently to gypsum (6), (amorphous) Al-hydroxide and Ca-aluminate type phases; or in the presence of atmospheric CO2 into Ca-sulphate, Al-gel and calcium carbonate polymorph – aragonite or vaterite (γ-CaCO3) as an intermediate phase [56–58].”
BackgroundCarbon sequestration potential of cement kiln dust: Mechanisms, methodologies, and applications
Adekunle, S. K. (2024) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2024.141283 · Cited by 39
Gu, T., Min, Q., Zeng, X., Wu, L., Wang, M., Zhang, L., & Liu, L. (2024) · Journal of CO2 Utilization · doi:10.1016/j.jcou.2024.102835 · Cited by 38
Elkhaldi, I., Rozière, E., Turcry, P., & Loukili, A. (2022) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2022.134876 · Cited by 36
CARBONATION IN CONCRETE AND EFFECT ON STEEL CORROSION
Sagüés, A. A., Moreno, É. I., Morris, W., & Perdrix, C. A. (1997) · Cited by 31
Ndiaye, K., Ginestet, S., & Cyr, M. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.02.136 · Cited by 31
Saeki, N., Kurihara, R., & Maruyama, I. (2024) · Journal of Advanced Concrete Technology · doi:10.3151/jact.22.602 · Cited by 31
Ndiaye, K., Ginestet, S., & Cyr, M. (2016) · Applied Thermal Engineering · doi:10.1016/j.applthermaleng.2016.08.157 · Cited by 28
Suma, M. F., Santhanam, M., & Rahul, A. V. (2020) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2020.103806 · Cited by 26
Carbonation resistance of blended mortars and industrial by-products: A brief review
Singh, N., Sharma, B., & Rathee, M. (2022) · Cleaner Materials · doi:10.1016/j.clema.2022.100058 · Cited by 27
Sulfoaluminate cement behaviours in carbon dioxide, warm and moist environments
Mechling, J.-M., Lecomte, A., Roux, A., & Rolland, B. L. (2013) · Advances in Cement Research · doi:10.1680/adcr.12.00070 · Cited by 24
Guenanou, F., Khelafi, H., & Aattache, A. (2019) · Journal of Building Engineering · doi:10.1016/j.jobe.2019.100734 · Cited by 25
Biogenic acid resistance of calcium sulfoaluminate cement: Revelations from a field study
Damion, T., & Chaunsali, P. (2023) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2023.105324 · Cited by 25
Sealing process induced by carbonation of localized cracks in cementitious materials
Ranaivomanana, H., Verdier, J., Sellier, A., & Bourbon, X. (2012) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.12.008 · Cited by 23
Hydration and strength development of binder based on high-calcium oil shale fly ash
Freidin, C. (1998) · Cement and Concrete Research · doi:10.1016/s0008-8846(98)00058-1 · Cited by 23
Drouet, E. (2010) · theses.fr (ABES) · doi:10.70675/32c67da3z68acz420cz85e9zeb73da9dcad6 · Cited by 112
Liao, Y. C., Hu, M., Yao, J., Wang, K., Tang, S., & Zuo, Y. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2024.139795 · Cited by 23
The damage of calcium sulfoaluminate cement paste partially immersed in MgSO4 solution
Liu, Z., Li, X., Deng, D., & Schutter, G. D. (2015) · Materials and Structures · doi:10.1617/s11527-015-0532-7 · Cited by 22
“Ettringite would decompose to CaSO4 2H2O, CaCO3, and alumina gel as the following equation [13]:”
MethodHay, R., & Çelik, K. (2024) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2024.136428 · Cited by 25
Effect of different concrete materials on the corrosion of the embedded reinforcing steel
Holland, B., Alapati, P., Kurtis, K. E., & Kahn, L. F. (2023) · Elsevier eBooks · doi:10.1016/b978-0-12-821840-2.00007-9 · Cited by 24
Yue, Z., Dhandapani, Y., & Bernal, S. A. (2024) · Cement and Concrete Research · doi:10.1016/j.cemconres.2024.107713 · Cited by 23
Thermodynamic Modeling Study of Carbonation of Portland Cement
Reddy, K. C., Seifu, M. N., & Park, S. (2022) · Materials · doi:10.3390/ma15145060 · Cited by 23
“The kinetics of ettringite destabilization can be pressed with the following equation [44,45]: Ettringite + Carbon dioxide→ Calcium carbonate + gypsum + alumina gel + water (3CaO·Al2O3·3CaSO4·32H2O + 3CO2 → 3CaCO3 + 3( aSO4·2H2O) + Al2O3·xH2O + (26− x)H2O) (2)”
BackgroundSun, T., Xiao, X., Ouyang, G., Li, W., Tang, P., & Wang, Z. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.133644 · Cited by 21
Dwivedi, A., & Gupta, S. (2024) · The Science of The Total Environment · doi:10.1016/j.scitotenv.2024.170285 · Cited by 21
Development of a cementitious material for thermal energy storage at low temperature
Ndiaye, K., Cyr, M., & Ginestet, S. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.118130 · Cited by 23
Microstructural and Phase Characteristics of Phosphogypsum-Cement Mixtures
Roy, A. D., Kalvakaalava, R., & Seals, R. K. (1996) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)0899-1561(1996)8:1(11 · Cited by 20
Application of FTIR, Raman, and TGA in carbonation of cementitious materials: A review
Adem, J. K., Shimelis, E., Oumer, A., Park, S., Gwon, S., Yang, B., & Kim, G. M. (2025) · Journal of Building Engineering · doi:10.1016/j.jobe.2025.114228 · Cited by 40
Al-Mansour, A., Dai, Y., Xu, C., Yang, R., Lü, J., Peng, Y., Wang, J., Lv, Q., & Zeng, Q. (2023) · Materials Today Sustainability · doi:10.1016/j.mtsust.2023.100325 · Cited by 20
Ultra-lightweight foamed concrete for an automated facade application
Adams, T. F., Vollpracht, A., Haufe, J., Hildebrand, L., & Brell‐Çokcan, S. (2018) · Magazine of Concrete Research · doi:10.1680/jmacr.18.00272 · Cited by 19
Goyal, S., & Sharma, D. (2020) · Elsevier eBooks · doi:10.1016/b978-0-12-819946-6.00006-0 · Cited by 28
Yang, Z., Xue, N., Xu, L., Yu, L., Huang, L., & Wu, K. (2022) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2022.12.061 · Cited by 19
Lv, Y., Niu, D., Liu, X., Lin, M., & Li, Y.-C. (2023) · Scientific Reports · doi:10.1038/s41598-023-30015-1 · Cited by 18
CO2 sequestration and low carbon strategies in 3D printed concrete
Kopitha, K., Rajeev, P., Sanjayan, J., & Elakneswaran, Y. (2024) · Journal of Building Engineering · doi:10.1016/j.jobe.2024.111653 · Cited by 30
Davolio, M., Muciaccia, G., & Ferrara, L. (2025) · Cleaner Materials · doi:10.1016/j.clema.2025.100292 · Cited by 33
Guleria, H., & Goyal, S. (2025) · Innovative Infrastructure Solutions · doi:10.1007/s41062-025-02081-z · Cited by 17
“The reaction of C 3 S and C 2 S with CO 2 is exothermic in nature and releases 347 and 184 kJ/mol respectively [53].”
Caneda‐Martínez, L., Frías, M., Sánchez-Montero, J., Rebolledo, N., Flores, E., & Medina, C. (2022) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2022.104608 · Cited by 22
Performance of photocatalytic, carbonated calcium sulfoaluminate-belite cement
Baral, A., & Roesler, J. R. (2022) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2022.104787 · Cited by 18
Brahim, M.-N., Mechling, J.-M., Janvier-Badosa, S., & Marchetti, M. (2023) · Materials Today Communications · doi:10.1016/j.mtcomm.2023.105539 · Cited by 26
Accelerated carbonation curing of building mortars incorporating volcanic ash and brine sludge
Assaggaf, R. A., Alhajji, L., Siddique, S., & Adekunle, S. K. (2024) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2024.137267 · Cited by 19
Leaching Processes and Evaluation Tests for Inorganic Constituent Release from Cement-Based Matrices
Kosson, D. S., & Garrabrants, A. C. (2004) · CRC Press eBooks · doi:10.1201/9781420032789.ch10 · Cited by 17
Evaluating the Impact of CO2 on Calcium SulphoAluminate (CSA) Concrete
Akerele, D. D., & Aguayo, F. M. (2024) · Buildings · doi:10.3390/buildings14082462 · Cited by 20
CZECH FLUID SULFOCALCIC ASH AND FLY ASH
Škvára, F. (2016) · Ceramics - Silikaty · doi:10.13168/cs.2016.0051 · Cited by 16
Cementless building units based on oil shale and coal fly ash binder
Freidin, C., & Motzafi-Haller, W. (1999) · Construction and Building Materials · doi:10.1016/s0950-0618(99)00041-0 · Cited by 16
Kong, D., Zhang, S., Zhang, J., Liu, T., Wang, L., & Jin, L. (2024) · Journal of Building Engineering · doi:10.1016/j.jobe.2024.111275 · Cited by 22
Yue, Z., Su, Z., Paul, P. P., Marsh, A., Macente, A., Michiel, M. D., Provis, J. L., Withers, P. J., & Bernal, S. A. (2024) · Cement and Concrete Research · doi:10.1016/j.cemconres.2024.107716 · Cited by 17
Brocken, H. J. P., van der Pers, N. M., & Larbi, J. A. (2000) · Materials and Structures · doi:10.1007/bf02480603 · Cited by 15
Zhong, L., Qu, J., Li, X., He, X., & Zhang, Q. (2016) · RSC Advances · doi:10.1039/c6ra01253a · Cited by 16
Zhang, W., Gong, S., & Kang, B. (2017) · Advances in Materials Science and Engineering · doi:10.1155/2017/1464619 · Cited by 15
X-ray Total Scattering Study of Phases Formed from Cement Phases Carbonation
Cuesta, A., De la Torre, A. G., & Aranda, M. A. G. (2021) · Minerals · doi:10.3390/min11050519 · Cited by 14
“Calcium carbonate polymorph formation seems to depend upon the carbonation conditions with works reporting aragonite [16,19], vaterite [20], mixtures of vaterite and aragonite [18], calcite [17] and even the three CaCO3 polymorphs depending upon the investigated sample [15].”
BackgroundMethodEffect of CO2 capture on the performance of CaO-activated slag pastes and their acid resistance
Li, H., Zhang, S., Wang, K., Zhang, X., & Jiang, Y. (2022) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2022.130039 · Cited by 14
The role of carbonation in the occurrence of MgSO4 crystallization distress on concrete
Liu, Z., Hu, W., Pei, M., & Deng, D. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.10.127 · Cited by 13
Sedman, A., Talviste, P., Mõtlep, R., Jõeleht, A., & Kirsimäe, K. (2012) · Engineering Geology · doi:10.1016/j.enggeo.2012.02.002 · Cited by 13
“7, but at lower pH values it dissolves incongruently to gypsum, aragonite/calcite, Al-hydroxide and/or Ca-aluminate type phases (Nishikawa et al., 1992; Myneni et al., 1998).”
BackgroundAdem, J. K., Seo, J., Park, S., & Kim, G. M. (2025) · Journal of Building Engineering · doi:10.1016/j.jobe.2025.112683 · Cited by 25
Kitamura, H., Dahlan, A. V., Tian, Y. H., Shimaoka, T., Yamamoto, T., & Takahashi, F. (2018) · Environmental Science and Pollution Research · doi:10.1007/s11356-018-1959-5 · Cited by 15
Gypsum efflorescence on clay brick masonry: Analysis of potential efflorescence origins
Janßen, H., Chwast, J., & Elsen, J. (2019) · Journal of Building Physics · doi:10.1177/1744259119896083 · Cited by 12
“Synthetic ettringite and monosulphate do however decompose back to gypsum upon carbonation (Nishikawa et al., 1992; Xiantuo et al., 1994; among others).”
BackgroundSaikia, S. K., Rajput, A. S., & Saini, K. (2024) · Journal of Building Engineering · doi:10.1016/j.jobe.2024.110192 · Cited by 13
OBSERVATIONS OF PEAK STRENGTH BEHAVIOR IN CSA CEMENT MORTARS
Brien, J. V., Henke, K. R., & Mahboub, K. C. (2013) · Journal of Green Building · doi:10.3992/jgb.8.3.97 · Cited by 11
KAMEI, T., Ahmed, A., Horai, H., & Ugai, K. (2014) · Journal of Material Cycles and Waste Management · doi:10.1007/s10163-014-0251-0 · Cited by 12
“An increase of excess water in the mix of binders used in the formation of ettringite helps to slow down the carbonation reaction [35].”
BackgroundBehavior of iodate substituted ettringite during aqueous leaching
Avalos, N. M., Varga, T. R., Mergelsberg, S. T., Silverstein, J. A., & Saslow, S. A. (2020) · Applied Geochemistry · doi:10.1016/j.apgeochem.2020.104863 · Cited by 11
Beaupere, N., Malley‐Ernewein, A., Nahhas, T., Ginestet, S., Samson, G., & Cyr, M. (2024) · Solar Energy · doi:10.1016/j.solener.2024.112927 · Cited by 12
Shafique, M. T., Siddique, S., Khalid, H. R., Adekunle, S. K., Hanif, A., Ahmad, S., & Al-Dulaijan, S. U. (2025) · Journal of Building Engineering · doi:10.1016/j.jobe.2025.114087 · Cited by 13
Carbon dioxide sequestration in power plant Ca-rich ash waste deposits
Leben, K., Mõtlep, R., Konist, A., Pihu, T., & Kirsimäe, K. (2021) · Oil Shale · doi:10.3176/oil.2021.1.04 · Cited by 13
Hydration and strength development of binder based on high-calcium oil shale fly ash
Freidin, C. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(99)00139-8 · Cited by 10
Influence of absolute basicity and capillary porosity on carbonation of concrete
Ba, M., Qian, C., & Gao, G. (2010) · Journal of Wuhan University of Technology-Mater Sci Ed · doi:10.1007/s11595-010-0114-z · Cited by 10
“The reaction between CO2 and C-S-H produces CaCO3 and a silica gel [8, 9] . AFt and AFm decompose by carbonation to CaCO3 [ 10 , 12] . As is known that Ca(OH)2, C-S-H, AFm”
BackgroundMicrostructural Investigation of Carbonation of Calcium Silicate Hydrate in Hydrated Cement Paste
Chen, W., Xu, W. B., & Li, Y. (2011) · Advanced materials research · doi:10.4028/www.scientific.net/amr.261-263.601 · Cited by 10
“While the carbonation process of the Portlandite [2, 3] and ettringite [4] in the cement hydrates is well investigated, the carbonation process of calcium silicate hydrate (C-S-H) gel, the major product of hydrated cement responsible for the mechanical properties and durability of hardened concrete is not completely r…”
BackgroundUtilizing Ground Granulated Blast Furnace Slag during Carbon Sequestration in Concrete
Saikia, S. K., Rajput, A. S., & Saini, K. (2024) · Journal of Materials in Civil Engineering · doi:10.1061/jmcee7.mteng-18542 · Cited by 9
Wei, Y., Li, L., Li, Z., & Liu, S. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2025.139892 · Cited by 10
Wang, R., Fan, Y.-S., Wang, Z., Huang, T., & Zhang, T. (2021) · Journal of Zhejiang University. Science A · doi:10.1631/jzus.a2000526 · Cited by 9
“(5) (Nishikawa et al., 1992).”
Collier, N. C., Heyes, D. W., Butcher, E., Borwick, J., Milodowski, A. E., Field, L. P., Kemp, S. J., Mounteney, I., Bernal, S. A., Corkhill, C. L., et al. (2019) · Applied Geochemistry · doi:10.1016/j.apgeochem.2019.04.020 · Cited by 9
Lv, Y. H., Niu, D., Yang, R., Liu, X., Wang, Y., Fu, Q., Cao, Z., Huang, J., & Sun, Y. (2024) · Journal of Building Engineering · doi:10.1016/j.jobe.2024.110325 · Cited by 8
Alapati, P., & Kurtis, K. E. (2019) · Purdue e-Pubs (Purdue University System) · Cited by 16
Effect of Polycarboxylate Superplasticizer on Properties of Phosphogypsum-Based Cement
Lin, Z. S., Shi, H., & Beguedou, E. (2012) · Key engineering materials · doi:10.4028/www.scientific.net/kem.509.13 · Cited by 8
“2% samples strength has been increased after carbonation [8].”
BackgroundMa, C., Kong, D., Qin, Q., Yu, L., Yang, C., & Wang, C. (2023) · Journal of Building Engineering · doi:10.1016/j.jobe.2023.107456 · Cited by 8
How to Identify a Natural Cement: Case Study of the Vassy Church, France
Bouichou, M., Marie‐Victoire, E., Texier, A., & Blondiaux, T. (2018) · Springer eBooks · doi:10.1007/978-3-319-91606-4_1 · Cited by 8
“It should be noted that during carbonation, Ettringite decomposes into Calcite, Gypsum and alumina gel (Nishikawa 1992).”
BackgroundWen, X., Fu, J., & Wang, J. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2025.143610 · Cited by 8
Xiao, R., Prentice, D. P., Sarkar, M., Kumar, A., Rosner, F., Neithalath, N., Plante, E. C. L., Bauchy, M., & Sant, G. (2026) · Communications Sustainability · doi:10.1038/s44458-026-00116-9 · Cited by 7
Effect of carbonation on eco-friendly binders for marine infrastructures
Wesemann, C. A., Antoun, M., Teune, I. E., Schollbach, K., Rippen, J. C., Hylkema, A., Oosterhoff, B., & Brouwers, H. J. H. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2025.141293 · Cited by 6
Microstructure of Ettringite Binder Exposed to Natural Carbonation
Lam, N. N. (2020) · IOP Conference Series Earth and Environmental Science · doi:10.1088/1755-1315/505/1/012002 · Cited by 7
Quantifying Conservativeness of Water-Soluble Chloride Testing
Ahmed, A. A., & Trejo, D. (2023) · ACI Materials Journal · doi:10.14359/51738499 · Cited by 6
Reliability of chloride testing results in cementitious systems containing admixed chlorides
Ahmed, A. A., & Vaddey, N. P. (2021) · Sustainable and Resilient Infrastructure · doi:10.1080/23789689.2021.1917059 · Cited by 8
“Nishikawa et al. (1992) reported that CSA systems, when exposed to CO2, can result in disintegration of AFt into CASO4.”
BackgroundXu, N., Sa, R., He, Y., Guo, J., Chen, Y., Wang, N., Feng, Y., & Ma, S. (2025) · Materials · doi:10.3390/ma18153436 · Cited by 5
“In a high-pressure CO 2 environment, ettringite rapidly decomposes into CaCO 3 , gypsum, and aluminum gel [54].”
ACTIVATION OF METAKAOLIN BY CaO And CaSO₄ ANHYDRITE II
Škvára, F. (2022) · Ceramics - Silikaty · doi:10.13168/cs.2022.0054 · Cited by 5
Andrade, C., Martínez-Serrano, A., Sanjuán, M. Á., & Ríos, J. A. T. (2023) · Construction Materials · doi:10.3390/constrmater3030020 · Cited by 5
STUDY OF CARBONATION DURABILITY OF SEVERAL ETTRINGITE-ENRICHED PASTES
Chen, B., Horgnies, M., Morin, V., Boumaaza, M., Huet, B., Gengembre, E., Baco, I., Johannes, K., & Kuznik, F. (2019) · WIT transactions on engineering sciences · doi:10.2495/mc190031 · Cited by 5
Liu, Y., Lu, H., Wang, C., Liu, Y., Ma, J., & Liu, M. (2022) · Processes · doi:10.3390/pr10081641 · Cited by 8
The investigation of basic processes of rapidly hardening wood-cement-water mixture with CO2
Qi, H., Cooper, P. A., & Hooton, R. D. (2009) · European Journal of Wood and Wood Products · doi:10.1007/s00107-009-0351-z · Cited by 6
“After studying the carbonation kinetics of ettringite, Nishikawa et al. (1992) also found that the carbonation reaction could be modeled by a modified diffusion-controlled model.”
BackgroundMethodResultLiu, Z., Hou, L., Hu, W., Zhang, F., & Deng, D. (2017) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)mt.1943-5533.0002198 · Cited by 5
Durability of concrete prepared with low-carbon binders: Perspectives and insights
Machner, A., Suraneni, P., WEERDT, K. D., Krüger, M. E., Wilson, W., & Isgor, O. B. (2026) · Cement and Concrete Research · doi:10.1016/j.cemconres.2026.108273 · Cited by 5
Liu, Y., Lu, H., Liu, M., & Dong, Y. (2024) · Environment Development and Sustainability · doi:10.1007/s10668-024-05653-8 · Cited by 4
“As the samples underwent 1–10 wet–dry cycles, the diffraction peaks of calcite intensified, and new peaks corresponding to gypsum dihy - drate emerged, potentially signifying the carbonation of internal calcite transforming into gypsum and calcite (Zhou & Glasser, 2000; Nishikawa et al., 1992 ).”
Hydration and carbonation curing of high ferrite clinker (FePC) synthesized using EAF slag
Adesanya, E., Isteri, V., Baral, A., Rößler, C., Hanein, T., & Yliniemi, J. (2024) · Low-carbon Materials and Green Construction · doi:10.1007/s44242-024-00051-9 · Cited by 6
Wei, P., Wang, W., Yu, Y., Hu, X., Wang, B., Li, N., & Jiang, P. (2025) · Materials Research Express · doi:10.1088/2053-1591/adb543 · Cited by 4
Chemical resistance of the binder based on sulfocalcic fly ash
Formáček, P., Šulc, R., Vondráčková, D., Šídlová, M., & Polonská, A. (2020) · AIP conference proceedings · doi:10.1063/5.0000474 · Cited by 4
Creep behaviour of geopolymer concrete
Un, C. H. (2017) · Figshare · doi:10.25916/sut.26279014 · Cited by 12
Zhang, H., Chang, J. S., Hou, J., & Cui, K. (2025) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.5c06909 · Cited by 3
Zhao, B., Christodoulatos, C., Shi, Q., Ji, M., Sheets, S., & Meng, X. (2025) · Separation and Purification Technology · doi:10.1016/j.seppur.2025.135776 · Cited by 3
Chen, M., Wang, H., Liu, P., Liu, T., & Jiang, G. (2026) · Journal of Building Engineering · doi:10.1016/j.jobe.2026.115768 · Cited by 8
Metadata
- Authors
- Nishikawa, T., Suzuki, K., Ito, S., Sato, K., & Takebe, T.
- Affiliations
- Nagoya Institute of Technology (JP)
- ORCID
- Venue
- Cement and Concrete Research
- Publisher
- Elsevier BV
- Published
- 1992-01
- Volume
- 22
- Issue
- 1
- Pages
- 6-14
- ISSN
- 0008-8846 (ISSN-L)
- OpenAlex
- W2057425322
- Semantic Scholar
- 0a0e4b3d04a3426d9e995b260dfebb3f2b372787
- Cited by
- 272
- References
- 3
- Citations by year
- 2026: 18 · 2025: 31 · 2024: 30 · 2023: 22 · 2022: 18 · 2021: 14 · 2020: 21 · 2019: 14 · 2018: 15 · 2017: 10 · 2016: 8 · 2015: 6 · 2014: 3 · 2013: 5 · 2012: 6
- FWCI
- 18.26
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- www.elsevier.com/legal/tdmrep-license (tdm)
- Locations
- Cement and Concrete Research (publishedVersion)
- Topics
- Physical Sciences › Engineering › Civil and Structural Engineering › Concrete and Cement Materials Research
- Physical Sciences › Earth and Planetary Sciences › Earth-Surface Processes › Building materials and conservation
- Physical Sciences › Environmental Science › Environmental Engineering › CO2 Sequestration and Geologic Interactions
- Keywords
- ettringite, carbonation, ettringite decomposition, gypsum, calcium carbonate, alumina gel, water-to-solid ratio, carbonation kinetics, Jander equation, carbon dioxide, cement hydration products
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.