Degradation of poly (D,L-lactic acid) microspheres: Effect of molecular weight
The DOI matches its Crossref record; 20 of the 21 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Polymers with higher molecular weight have generally exhibited lower degradation rates [83].”
From Poly Lactic-co-Glycolic Acid (PLGA) as Biodegradable Controlled Drug Delivery Carrier (2011) · cites this paper as [83]
Citations
Cites
Crystal structure, conformation and morphology of solution-spun poly(L-lactide) fibers
Hoogsteen, W., Postema, A. R., Pennings, A. J., Ten Brinke, G., & Zugenmaier, P. (1990) · Macromolecules · doi:10.1021/ma00204a041 · Cited by 864
Controlled Delivery Systems for Proteins Based on Poly(Lactic/Glycolic Acid) Microspheres
Cohen, S., Yoshioka, T., Lucarelli, M., Hwang, L. H., & Langer, R. (1991) · Pharmaceutical Research · doi:10.1023/a:1015841715384 · Cited by 843
Li, S. M., Garreau, H., & Vert, M. (1990) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00700871 · Cited by 733
Thermal characterization of polylactides
Jamshidi, K., Hyon, S.-H., & Ikada, Y. (1988) · Polymer · doi:10.1016/0032-3861(88)90116-4 · Cited by 692
Reed, A. M., & Gilding, D. K. (1981) · Polymer · doi:10.1016/0032-3861(81)90168-3 · Cited by 502
Biodegradable Polymers as Drug Delivery Systems
(1991) · Drug Development and Industrial Pharmacy · doi:10.3109/03639049109043830 · Cited by 431
Jalil, R., & Nixon, J. R. (1990) · Journal of Microencapsulation · doi:10.3109/02652049009021842 · Cited by 401
Biodegradable microspheres as a vaccine delivery system
Eldridge, J. H., Staas, J. K., Meulbroek, J. A., McGhee, J. R., Tice, T. R., & Gilley, R. M. (1991) · Molecular Immunology · doi:10.1016/0161-5890(91)90076-v · Cited by 399
Li, S. M., Garreau, H., & Vert, M. (1990) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00700872 · Cited by 383
Controlled release of bioactive agents from lactide/glycolide polymers
Lewis, D. H. (1990) · Drugs and the pharmaceutical sciences · Cited by 370
Cited by
Items 101–200 of 358
Berkland, C. J., Pollauf, E. J., Raman, C., Silverman, R., Kim, K., & Pack, D. W. (2007) · Journal of Pharmaceutical Sciences · doi:10.1002/jps.20948 · Cited by 79
Li, P., Feng, X., Jia, X., & Fan, Y. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2010.02.023 · Cited by 72
Jain, G. K., Pathan, S. A., Akhter, S., Ahmad, N., Jain, N., Talegaonkar, S., Khar, R. K., & Ahmad, F. J. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.08.015 · Cited by 78
Mylonaki, I., Allémann, É., Delié, F., & Jordan, O. (2018) · Journal of Controlled Release · doi:10.1016/j.jconrel.2018.07.044 · Cited by 68
“As Mw is known to largely influence the erosion profile [22], a comparative study was conducted with polymers of various Mw.”
BackgroundLange, J., de Souza, F. G., Nele, M., Tavares, F. W., Segtovich, I. S. V., da Silva, G. C. Q., & Pinto, J. C. (2015) · Macromolecular Theory and Simulations · doi:10.1002/mats.201500049 · Cited by 68
Poly-DL-lactide-co-glycolide microspheres as a controlled release antigen delivery system
Lima, K. M., & Rodrigues Júnior, J. M. (1999) · Brazilian Journal of Medical and Biological Research · doi:10.1590/s0100-879x1999000200005 · Cited by 65
Reich, G. (1998) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/s0939-6411(97)00152-5 · Cited by 65
“Its possibly negative effect during the microsphere formation process on the molecular weight ( Mw) of the polymer [15] and thus on the performance of the resulting microspheres has so far not been investigated in detail.”
BackgroundIn vitro degradation and erosion behavior of commercial PLGAs used for controlled drug delivery
Walker, J., Albert, J., Liang, D., Sun, J., Schutzman, R., Kumar, R., White, C., Beck‐Broichsitter, M., & Schwendeman, S. P. (2022) · Drug Delivery and Translational Research · doi:10.1007/s13346-022-01177-8 · Cited by 69
Yoo, J. Y., Kim, J. M., Seo, K. S., Jeong, Y. K., Lee, H. B., & Khang, G. (2005) · PubMed · Cited by 64
Matsusaki, M., Kishida, A., Stainton, N. M., Ansell, C. W. G., & Akashi, M. (2001) · Journal of Applied Polymer Science · doi:10.1002/app.2085 · Cited by 65
MPEG–PCL copolymeric nanoparticles in drug delivery systems
Danafar, H. (2016) · Cogent Medicine · doi:10.1080/2331205x.2016.1142411 · Cited by 73
“PUBLIC INTEREST STATEMENT Tremendous progress has been attained in evaluating and optimizing the application of mPEG–PCL copolymers in DDS. mPEG–PCL copolymers are biodegradable, biocompatible copolymers having a very low glass transition temperature.”
MethodInfluentialDetermination of water‐soluble acid distribution in poly(lactide‐co‐glycolide)
Ding, A. G., & Schwendeman, S. P. (2003) · Journal of Pharmaceutical Sciences · doi:10.1002/jps.10524 · Cited by 68
Gan, Z., Jim, T. F., Jing, X., Wu, C. C., & Kuliche, W. K. (1999) · Polymer · doi:10.1016/s0032-3861(98)00414-5 · Cited by 67
Oh, J.-Y., Nam, Y. S., Lee, K. H., & Park, T. G. (1999) · Journal of Controlled Release · doi:10.1016/s0168-3659(98)00123-0 · Cited by 67
Chen, C., Cui, Y., Mao, X., Pan, X., & Wu, J. (2016) · Macromolecules · doi:10.1021/acs.macromol.6b02271 · Cited by 66
Huang, X. D., Nayak, B. R., & Lowe, T. L. (2004) · Journal of Polymer Science Part A Polymer Chemistry · doi:10.1002/pola.20327 · Cited by 65
Surfactants influence polymer nanoparticle fate within the brain
Joseph, A., Simo, G. M., Gao, T. A., Alhindi, N., Xu, N., Graham, D. J., Gamble, L. J., & Nance, E. A. (2021) · Biomaterials · doi:10.1016/j.biomaterials.2021.121086 · Cited by 62
Some insight into hydrolytic scission mechanisms in bioerodible polyesters
Alexis, F., Venkatraman, S. S., Rath, S. K., & Gan, L. (2006) · Journal of Applied Polymer Science · doi:10.1002/app.23888 · Cited by 69
Fujiyama, J., Nakase, Y., Osaki, K., Sakakura, C., Yamagishi, H., & Hagiwara, A. (2003) · Journal of Controlled Release · doi:10.1016/s0168-3659(03)00131-7 · Cited by 63
Polymer degradation induced drug precipitation in PLGA implants – Why less is sometimes more
Zlomke, C., Barth, M., & Mäder, K. (2019) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/j.ejpb.2019.03.016 · Cited by 60
Long-term delivery of all-trans-retinoic acid using biodegradable PLLA/PEG-PLLA blended microspheres
Choi, Y., Kim, S. Y., Kim, S. H., Lee, K.-S., Kim, C., & Byun, Y. (2001) · International Journal of Pharmaceutics · doi:10.1016/s0378-5173(00)00676-1 · Cited by 54
“For PLA, the critical molecular weight which can be solubilized in water was found to be around 1100 Da (Park, 1994).”
BackgroundQuantitative analysis of three‐dimensional fluid flow in rotating bioreactors for tissue engineering
Botchwey, E. A., Pollack, S. R., Levine, E. M., Johnston, E. D., & Laurencin, C. T. (2004) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.10163 · Cited by 54
Bertram, J. P., Rauch, M. F., Chang, K., & Lavik, E. (2009) · Pharmaceutical Research · doi:10.1007/s11095-009-0009-x · Cited by 61
“acid to lactic acid ratio will still play a dominant role in dictating themicrosphere release kinetics (41, 42).”
BackgroundSingh, V. V., Singh, S., Das, S., Kumar, A., Self, W. T., & Seal, S. (2012) · Nanoscale · doi:10.1039/c2nr12131j · Cited by 54
Ravivarapu, H. B., Lee, H., & DeLuca, P. P. (2000) · Pharmaceutical Development and Technology · doi:10.1081/pdt-100100543 · Cited by 51
Ultrasound degradation of novel polymer contrast agents
El‐Sherif, D. M., Lathia, J. D., Le, N. T., & Wheatley, M. A. (2003) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.20032 · Cited by 51
Rivas, D., Ginebreda, A., Pérez, S., Quero, C., & Barceló, . (2016) · The Science of The Total Environment · doi:10.1016/j.scitotenv.2016.05.090 · Cited by 53
Vey, E., Rodger, C., Meehan, L., Booth, J., Claybourn, M., Miller, A. F., & Saiani, A. (2011) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2011.12.010 · Cited by 54
Netti, P. A., Biondi, M., & Frigione, M. (2020) · Polymers · doi:10.3390/polym12092042 · Cited by 50
Bertram, J. P., Jay, S. M., Hynes, S. R., Robinson, R., Criscione, J. M., & Lavik, E. B. (2009) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.04.012 · Cited by 47
“By conserving these properties, one can infer from literature how variations such as molecular weight or copolymer ratio may influence drug release rates or encapsulation [21, 22].”
BackgroundWang, N., & Wu, X. S. (1998) · Journal of Biomaterials Science Polymer Edition · doi:10.1163/156856297x00272 · Cited by 47
Understanding and utilizing the biomolecule/nanosystems interface
Chen, E. Y., Liu, W. F., Megido, L., Díez, P., Fuentes, M., Fager, C., Olsson, E., Gessner, I., & Mathur, S. (2017) · Elsevier eBooks · doi:10.1016/b978-0-323-48063-5.00003-4 · Cited by 63
Effects of mechanical load on the degradation of poly(d,l-lactic acid) foam
Fan, Y., Li, P., Zeng, L., & Huang, X. (2008) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.12.015 · Cited by 49
Abdullah, K. K., & Molnár, K. (2025) · Journal of Polymer Science · doi:10.1002/pol.20241010 · Cited by 56
Study of the emulsion‐diffusion of solvent: preparation and characterization of nanocapsules
Guinebretière, S., Briançon, S., Liéto, J., Mayer, C., & Fessi, H. (2002) · Drug Development Research · doi:10.1002/ddr.10054 · Cited by 46
Facile and efficient chemical functionalization of aliphatic polyesters by cross metathesis
Fournier, L., Robert, C., Pourchet, S., Gonzalez, A., Williams, L. G., Prunet, J. A., & Thomas, C. M. (2016) · Polymer Chemistry · doi:10.1039/c6py00664g · Cited by 49
Felder, C. B., Vorlaender, N., Gander, B. A., Merkle, H. P., & Bertschinger, H. U. (2000) · Vaccine · doi:10.1016/s0264-410x(00)00264-4 · Cited by 45
Functional Hybrid Materials with Polymer Nanoparticles as Templates
Ethirajan, A., & Landfester, K. (2010) · Chemistry - A European Journal · doi:10.1002/chem.201001477 · Cited by 50
Layer-by-layer polyelectrolyte coating of low molecular weight poly(lactic acid) nanoparticles
Hirsjärvi, S., Peltonen, L., & Hirvonen, J. J. (2006) · Colloids and Surfaces B Biointerfaces · doi:10.1016/j.colsurfb.2006.03.009 · Cited by 45
Balmert, S. C., Zmolek, A. C., Glowacki, A. J., Knab, T. D., Rothstein, S. N., Wokpetah, J., Fedorchak, M. V., & Little, S. R. (2015) · Journal of Materials Chemistry B · doi:10.1039/c5tb00515a · Cited by 52
Zhou, X., Cai, Q., Yan, N. J., Deng, X., & Yang, X. (2010) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.32896 · Cited by 48
“This was consistent with the previous investigations that the weight loss would not take place until the molecular weight of samples had decreased to a critical value and become soluble in water.(25,26) Different from the bimodal GPC profiles of hydrolytic specimens, the enzymatic-degraded samples remained one broad s…”
ResultUnintended potential impact of perfect sink conditions on PLGA degradation in microparticles
Klose, D., Delplace, C., & Siepmann, J. (2010) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2010.10.054 · Cited by 53
“…al., 2000; Berkland et al., 2003; Siepmann et al., 2005), system’s porosity (Kang and Schwendeman, 2007; Klose et al., 2006), polymer molecular weight (Park, 1994; Ravivarapu et al., 2000), monomer ratio (lactic acid:glycolic acid) (Ravivarapu et al., 2000), and type of drug (Frank et al., 2005).”
BackgroundTamani, F., Bassand, C., Hamoudi, M., Danède, F., Willart, J., Siepmann, F., & Siepmann, J. (2019) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2019.118819 · Cited by 43
“…waterfilled pores, swollen PLGA gel and/or slightly hydrated polymer networks, polyester hydrolysis (Grizzi et al., 1995), drug – PLGA interactions (Park, 1994; Blasi et al., 2007), the creation of water-soluble monomers and oligomers and the latter’s diffusion into the surrounding bulk fluid,…”
BackgroundTaddei, P., Monti, P., & Simoni, R. (2002) · Journal of Materials Science Materials in Medicine · doi:10.1023/a:1014742003146 · Cited by 46
Pore formation and pore closure in poly(D,L-lactide-co-glycolide) films
Fredenberg, S., Wahlgren, M., Reslow, M., & Axelsson, A. (2010) · Journal of Controlled Release · doi:10.1016/j.jconrel.2010.11.020 · Cited by 56
A review on latest innovations in physical modifications of galactomannans
Kian-Pour, N., Yıldırım-Yalçın, M., Kurt, A., Özmen, D., & Toker, Ö. S. (2023) · Food Hydrocolloids · doi:10.1016/j.foodhyd.2023.108470 · Cited by 46
Stability Studies of Microparticulate System with Piroxicam as Model Drug
Puthli, S. P., & Vavia, P. R. (2009) · AAPS PharmSciTech · doi:10.1208/s12249-009-9280-8 · Cited by 45
Alemrayat, B., Elhissi, A. M. A., & Younes, H. M. (2018) · Pharmaceutical Development and Technology · doi:10.1080/10837450.2018.1455698 · Cited by 40
“DOI:10.1080/ 10837450.2016.1264415 Park TG. 1994.”
InfluentialImmunoisolation of pancreatic islets via thin-layer surface modification
Pathak, S., Pham, T. T., Jeong, J., & Byun, Y. (2019) · Journal of Controlled Release · doi:10.1016/j.jconrel.2019.04.034 · Cited by 42
Mogi, T., Ohtake, N., Yoshida, M., Chimura, R., Kamaga, Y., Ando, S., Tsukamoto, T., Nakajima, T., Uenodan, H., Otsuka, M., et al. (2000) · Colloids and Surfaces B Biointerfaces · doi:10.1016/s0927-7765(99)00105-8 · Cited by 46
Healing kinetics of microneedle-formed pores in PLGA films
Mazzara, J. M., Balagna, M. A., Thouless, M. D., & Schwendeman, S. P. (2013) · Journal of Controlled Release · doi:10.1016/j.jconrel.2013.06.035 · Cited by 39
Ouchi, T., Toyohara, M., Arimura, H., & Ohya, Y. (2002) · Biomacromolecules · doi:10.1021/bm0200231 · Cited by 42
Synthesis and Characterization of Low Molecular Weight Polylactic Acid
Proikakis, C. S., Tarantili, P. A., & Andreopoulos, A. G. (2002) · Journal of Elastomers & Plastics · doi:10.1106/009524402021336 · Cited by 39
Rothen-Weinhold, A., Besseghir, K., & Gurny, R. (1997) · European Journal of Pharmaceutical Sciences · doi:10.1016/s0928-0987(97)00022-5 · Cited by 38
Use of DSC to Study the Degradation Behavior of PLA and PLGA Microparticles
Reich, G. (1997) · Drug Development and Industrial Pharmacy · doi:10.3109/03639049709146155 · Cited by 41
Dwivedi, V., Manickam, C., Binjawadagi, B., Dechamma, H. J., & Renukaradhya, G. J. (2012) · PLoS ONE · doi:10.1371/journal.pone.0051794 · Cited by 35
“long-period of time, thus avoiding the need of a booster dose [2].”
BackgroundA novel method of studying polymer biodegradation
Wu, C., & Gan, Z. (1998) · Polymer · doi:10.1016/s0032-3861(97)10199-9 · Cited by 42
Lu, W., & Park, T. G. (1995) · Biotechnology Progress · doi:10.1021/bp00032a016 · Cited by 35
Self-citationProspects for polymer therapeutics in Parkinson's disease and other neurodegenerative disorders
Newland, B., Newland, H., Werner, C., Rosser, A., & Wang, W. (2015) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2014.12.002 · Cited by 39
Synthesis and Properties of Feather Keratin-Based Superabsorbent Hydrogels
Wattie, B., Dumont, M., & Lefsrud, M. G. (2016) · Waste and Biomass Valorization · doi:10.1007/s12649-016-9773-0 · Cited by 34
The degradation behavior of silk fibroin derived from different ionic liquid solvents
You, R., Zhang, Y., Liu, Y., Liu, G., & Li, M. (2013) · Natural Science · doi:10.4236/ns.2013.56a002 · Cited by 34
Xiao, Y., Cummins, D., Palmans, A. R. A., Koning, C. E., & Heise, A. (2008) · Soft Matter · doi:10.1039/b717059a · Cited by 34
Modeling drug release from bioerodible microspheres using a cellular automaton
Bertrand, N., Leclair, G., & Hildgen, P. (2007) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2007.05.050 · Cited by 38
Polymeric lamellar substrate particles for intranasal vaccination
Jabbal‐Gill, I., Wu, L., Kistner, O., Davis, S. S., & Illum, L. (2001) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(01)00173-9 · Cited by 37
Mayer, J. B., Patil, S. M., Shin, S.-H., Yoo, J., & Won, Y.-Y. (2025) · ACS Biomaterials Science & Engineering · doi:10.1021/acsbiomaterials.5c00419 · Cited by 38
Steele, T. W. J., Huang, C. L., Kumar, S., Iskandar, A., Baoxin, A., Boey, F. Y. C., Loo, S. C. J., & Venkatraman, S. S. (2013) · NPG Asia Materials · doi:10.1038/am.2013.9 · Cited by 35
Palamoor, M., & Jablonski, M. M. (2013) · Molecular Pharmaceutics · doi:10.1021/mp300488s · Cited by 35
Ko, Y., Park, J. H., Lee, J. B., Oh, H. H., Park, W. H., Cho, D., & Kwon, O. H. (2016) · Tissue Engineering and Regenerative Medicine · doi:10.1007/s13770-016-0053-7 · Cited by 37
Biodegradable Polymers in Drug Delivery
Jain, J. P., Ayen, W. Y., Domb, A. J., & Kumar, N. (2011) · Wiley eBooks · doi:10.1002/9781118015810.ch1 · Cited by 45
Silk Hydrogel for Tissue Engineering: A Review
Patil, S., Ealla, K. K. R., Panta, P., Veeraraghavan, V. P., Ravula, N. R., Durga, C. S., Ramani, P., Sahu, V., & Poola, P. K. (2022) · The Journal of Contemporary Dental Practice · doi:10.5005/jp-journals-10024-3322 · Cited by 35
“74 Natural silks show high molecular weights, and by processing silk, lower molecular weights can be acquired.”
Clements, A. E. B., & Murphy, W. L. (2019) · Acta Biomaterialia · doi:10.1016/j.actbio.2019.04.051 · Cited by 34
Investigation of Mucoadhesion and Degradation of PCL and PLGA Microcontainers for Oral Drug Delivery
Abid, Z., Mosgaard, M. D., Manfroni, G., Petersen, R. S., Nielsen, L. H., Müllertz, A., Boisen, A., & Keller, S. S. (2019) · Polymers · doi:10.3390/polym11111828 · Cited by 33
“PLGA 50:50 is expected to have the highest degradation rate compared to PLGA 75:25, which typically is approximately twice as slow due to the higher content of hydrophobic groups [27].”
BackgroundChimisso, V., Aleman‐Garcia, M. A., Avsar, S. Y., Dinu, I. A., & Palivan, C. G. (2020) · Molecules · doi:10.3390/molecules25184090 · Cited by 32
Novel Pentablock Copolymer-Based Nanoparticulate Systems for Sustained Protein Delivery
Patel, S. P., Vaishya, R. D., Pal, D., & Mitra, A. K. (2014) · AAPS PharmSciTech · doi:10.1208/s12249-014-0196-6 · Cited by 36
The effect of the type of HA on the degradation of PLGA/HA composites
Naik, A., Shepherd, D. V., Shepherd, J. H., Best, S. M., & Cameron, R. E. (2016) · Materials Science and Engineering C · doi:10.1016/j.msec.2016.09.048 · Cited by 35
Perspectives On: Local and Sustained Delivery of Angiogenic Growth Factors
Lee, H., Chung, H. J., & Park, T. G. (2007) · Journal of Bioactive and Compatible Polymers · doi:10.1177/0883911506073363 · Cited by 36
Self-citationFormulation and Characterization of Immunoreactive Tetanus Toxoid Biodegradable Polymer Particles
Raghuvanshi, O. S. (2001) · Drug Delivery · doi:10.1080/107175401750177089 · Cited by 32
“This might be the cause of the slow release pattern of TT observed with PLA particles (Park 1994).”
BackgroundDrug release mechanisms of high-drug-load, melt-extruded dexamethasone intravitreal implants
Costello, M. A., Liu, J., Chen, B., Wang, Y., Qin, B., Xu, X., Li, Q., Lynd, N. A., & Zhang, F. (2023) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/j.ejpb.2023.04.003 · Cited by 33
Carrier mediated protein and peptide stabilization
Tiwari, A. K., Gajbhiye, V., Sharma, R. K., & Jain, N. K. (2010) · Drug Delivery · doi:10.3109/10717544.2010.509359 · Cited by 34
“For example, increase in polymer Mw results in longer degradation times and slower release (Park, 1994; 1995; Ramirez et al., 1999).”
BackgroundIn situ forming risperidone implants: Effect of PLGA attributes on product performance
Wang, X., Bao, Q., Wang, R., Kwok, O., Maurus, K., Wang, Y., Qin, B., & Burgess, D. J. (2023) · Journal of Controlled Release · doi:10.1016/j.jconrel.2023.08.029 · Cited by 29
Novel method to characterize the hydrolytic decomposition of biopolymer surfaces
Kiss, É., & Vargha-Butler, E. I. (1999) · Colloids and Surfaces B Biointerfaces · doi:10.1016/s0927-7757(99)00009-6 · Cited by 31
Ma, C. H., Zhang, H., Yang, S., Yin, R., Yao, X., & Zhang, W. (2018) · Biomicrofluidics · doi:10.1063/1.5021394 · Cited by 30
Qodratnama, R., Serino, L. P., Cox, H. C., Qutachi, O., & White, L. J. (2014) · Materials Science and Engineering C · doi:10.1016/j.msec.2014.11.003 · Cited by 32
Chu, Z., Zheng, Q. S., Guo, M., Yao, J., Xu, P. F., Feng, W., Hou, Y., Zhou, G., Wang, L., Li, X., et al. (2016) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.35766 · Cited by 31
Mechanical, physical, and degradation properties of 3D printed PLA + Mg composites
Zeynivandnejad, M., Moradi, M., & Sadeghi, A. (2023) · Journal of Manufacturing Processes · doi:10.1016/j.jmapro.2023.05.099 · Cited by 29
Thompson, C. J., Hansford, D., Higgins, S. J., Hutcheon, G. A., Rostron, C., & Munday, D. L. (2006) · Journal of Microencapsulation · doi:10.1080/02652040500444123 · Cited by 30
Cho, K. Y., Choi, S. H., Kim, C.-H., Nam, Y. S., Park, T. G., & Park, J. (2001) · Journal of Controlled Release · doi:10.1016/s0168-3659(01)00442-4 · Cited by 33
Self-citationMethodology to nanoencapsulate hepatoprotective components from Picrorhiza kurroa as food supplement
Jia, D., Barwal, I., Thakur, S., & Yadav, S. C. (2014) · Food Bioscience · doi:10.1016/j.fbio.2014.10.005 · Cited by 28
“A study of degradation mechanism (Gopferich, 1996; Park, 1994, 1995) showed that change in composition leads to size changes in a three phase way.”
BackgroundPoh, P. S. P., Hege, C. S., Chhaya, M. P., Balmayor, E. R., Foehr, P., Burgkart, R., Schantz, J., Schiller, S., Schilling, A. F., & Hutmacher, D. W. (2016) · Polymer International · doi:10.1002/pi.5181 · Cited by 31
Drug-Eluting Biodegradable Implants for the Sustained Release of Bisphosphonates
Dharmayanti, C., Gillam, T. A., Williams, D. B., & Blencowe, A. (2020) · Polymers · doi:10.3390/polym12122930 · Cited by 30
“At the onset of bulk erosion, macroscopic pores appeared throughout the PLGA implants (Figure 4), possibly attributed to differences in the erosion rate within the polymer, where complete hydrolysis of lower Mw chains occurs more rapidly [56,57].”
BackgroundWang, W., Zhou, S., Sun, L., & Huang, C. (2009) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2009.08.031 · Cited by 30
“For example, increase in polymer Mw results in longer degradation times and slower drug release (Park, 1994, 1995; Ramirez, Pastoriza, & Herrero-Vanrell, 1999).”
BackgroundStereochemistry Determines Immune Cellular Responses to Polylactide Implants
Maduka, C. V., Alhaj, M., Ural, E. E., Kuhnert, M. M., Habeeb, O. M., Schilmiller, A. L., Hankenson, K. D., Goodman, S. B., Narayan, R., & Contag, C. H. (2023) · ACS Biomaterials Science & Engineering · doi:10.1021/acsbiomaterials.2c01279 · Cited by 30
Wang, Y., Molin, D. G. M., Sevrin, C., Grandfils, C., van den Akker, N. M. S., Gagliardi, M., Knetsch, M. L. W., Delhaas, T., & Koole, L. H. (2016) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2016.03.002 · Cited by 29
García, J. T., Fariña, J. B., Munguía, O., & Llabrés, M. (1999) · Journal of Microencapsulation · doi:10.1080/026520499289338 · Cited by 32
Novel biodegradable Round Window Disks for inner ear delivery of dexamethasone
Lehner, E., Liebau, A., Syrowatka, F., Knolle, W., Plontke, S. K., & Mäder, K. (2020) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2020.120180 · Cited by 27
Boimvaser, S., Mariano, R. N., Turino, L. N., & Vega, J. R. (2015) · Polymer Bulletin · doi:10.1007/s00289-015-1481-6 · Cited by 30
Busatto, C. A., Pesoa, J., Helbling, I. M., Luna, J. A., & Estenoz, D. A. (2017) · Journal of Applied Polymer Science · doi:10.1002/app.45464 · Cited by 27
Vancomycin release from poly(d,l-lactic acid) spray-coated hydroxyapatite fibers
Ravelingien, M., Mullens, S., Luyten, J., D’Hondt, M., Boonen, J., Spiegeleer, B. M. J. D., Coenye, T., Vervaet, C., & Remon, J. P. (2010) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/j.ejpb.2010.08.010 · Cited by 31
“Mw of 17 kDa lasts 53 days [14].”
BackgroundBiodegradable polymers: An update
Shikanov, A., Kumar, N., & Domb, A. J. (2005) · Israel Journal of Chemistry · doi:10.1560/atqm-mq02-gldu-ef6l · Cited by 29
DEGRADITION OF POLY (D,L-LACTIDE-CO-GLYCOLIDE) 50:50 IMPLANT IN AQUEOUS MEDIUM
Farahani, T. D., Abtahi, M., Entezami, A. A., & Mobedi, H. (2005) · Cited by 61
Metadata
- Authors
- Park, T. G.
- Affiliations
- Temple University (US)
- Corresponding author
- Park, Tae Gwan
- ORCID
- Park, Tae Gwan
- Venue
- Journal of Controlled Release
- Publisher
- Elsevier BV
- Published
- 1994-05
- Volume
- 30
- Issue
- 2
- Pages
- 161-173
- ISSN
- 0168-3659 (ISSN-L)
- OpenAlex
- W1985019144
- Cited by
- 359
- References
- 21
- Citations by year
- 2026: 2 · 2025: 12 · 2024: 13 · 2023: 12 · 2022: 9 · 2021: 11 · 2020: 13 · 2019: 13 · 2018: 9 · 2017: 14 · 2016: 16 · 2015: 14 · 2014: 18 · 2013: 11 · 2012: 14
- FWCI
- 8.32
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- Journal of Controlled Release (publishedVersion)
- Topics
- Life Sciences › Pharmacology, Toxicology and Pharmaceutics › Pharmaceutical Science › Advanced Drug Delivery Systems
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Materials Science › Biomaterials › Hydrogels: synthesis, properties, applications
- Keywords
- poly(D,L-lactide), biodegradable microspheres, polymer degradation, molecular weight effects, oligomers, glass transition temperature, water hydration, polymer morphology, controlled release
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.