Characterisation of thermally modified hard- and softwoods by C CPMAS NMR
The DOI matches its Crossref record; 14 of the 14 references it cites were found in a registry or an index.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Characterisation of thermally modified wood: molecular reasons for wood performance improvement
Tjeerdsma, B. F., Boonstra, M., Pizzi, A., Tekely, P., & Militz, H. (1998) · Holz als Roh- und Werkstoff · doi:10.1007/s001070050287 · Cited by 672
Studies of microstructure in native celluloses using solid-state carbon-13 NMR
VanderHart, D. L., & Atalla, R. H. (1984) · Macromolecules · doi:10.1021/ma00138a009 · Cited by 613
Magnetic Resonance Studies of Thermally Modified Wood
Sivonen, H., Maunu, S. L., Sundholm, F., Jämsä, S., & Viitaniemi, P. (2002) · Holzforschung · doi:10.1515/hf.2002.098 · Cited by 300
Thermal Modifications in Softwood Studied by FT‐IR and UV Resonance Raman Spectroscopies
Nuopponen, M., Vuorinen, T., Jämsä, S., & Viitaniemi, P. (2005) · Journal of Wood Chemistry and Technology · doi:10.1081/wct-120035941 · Cited by 263
Hatcher, P. G. (1987) · Organic Geochemistry · doi:10.1016/0146-6380(87)90049-0 · Cited by 227
Thermochemical behavior of Norway spruce ( Picea abies ) at 180-225 °C
Alén, R., Kotilainen, R., & Zaman, A. (2002) · Wood Science and Technology · doi:10.1007/s00226-001-0133-1 · Cited by 196
The role of solid state 13 C NMR spectroscopy in studies of the nature of native celluloses
Atalla, R. H., & VanderHart, D. L. (1999) · Cited by 142
Heat‐treated softwood exposed to weathering
Nuopponen, M. H., Wikberg, H., Vuorinen, T., Maunu, S. L., Jämsä, S., & Viitaniemi, P. (2003) · Journal of Applied Polymer Science · doi:10.1002/app.13351 · Cited by 133
Self-citationStudies of crystallinity of Scots pine and Norway spruce cellulose
Andersson, S., Wikberg, H., Pesonen, E., Maunu, S. L., & Serimaa, R. E. (2004) · Trees · doi:10.1007/s00468-003-0312-9 · Cited by 105
Self-citationSolid-state spectroscopic analysis of lignins from several Austral hardwoods
Martı́nez, Á. T., Almendros, G., González-Vila, F. J., & Fründ, R. (1999) · Solid State Nuclear Magnetic Resonance · doi:10.1016/s0926-2040(99)00045-4 · Cited by 92
Cited by
Wood modification by heat treatment: A review
Esteves, B. M., & Pereira, H. M. (2008) · BioResources · doi:10.15376/biores.4.1.370-404 · Cited by 1,270
Pseudo-lignin and pretreatment chemistry
Sannigrahi, P., Kim, D. H., Jung, S., & Ragauskas, A. (2011) · Energy Environ. Sci. · doi:10.1039/c0ee00378f · Cited by 535
Kim, H.-S., Lee, B.-H., Choi, S.-W., Kim, S., & Kim, H.-J. (2007) · Composites Part A: Applied Science and Manufacturing · doi:10.1016/j.compositesa.2007.01.004 · Cited by 426
Thermal modification of wood—a review: chemical changes and hygroscopicity
Hill, C., Altgen, M., & Rautkari, L. (2021) · Journal of Materials Science · doi:10.1007/s10853-020-05722-z · Cited by 378
Esteves, B., Marques, A. V., Domingos, I., & Pereira, H. (2007) · Wood Science and Technology · doi:10.1007/s00226-006-0099-0 · Cited by 304
Falco, C., Perez Caballero, F., Babonneau, F., Gervais, C., Laurent, G., Titirici, M.-M., & Baccile, N. (2011) · Langmuir · doi:10.1021/la202361p · Cited by 301
Catalytic transformation of cellulose into platform chemicals
Yabushita, M., Kobayashi, H., & Fukuoka, A. (2014) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2013.01.052 · Cited by 289
Structural Changes of Oak Wood Main Components Caused by Thermal Modification
Kubovský, I., Kačíková, D., & Kačík, F. (2020) · Polymers · doi:10.3390/polym12020485 · Cited by 289
Ionic liquids and deep eutectic solvents for lignocellulosic biomass fractionation
van Osch, D. J. G. P., Kollau, L. J. B. M., van den Bruinhorst, A., Asikainen, S., Rocha, M. A. A., & Kroon, M. C. (2017) · Physical Chemistry Chemical Physics · doi:10.1039/c6cp07499e · Cited by 288
Transformation of lignocellulosic biomass during torrefaction
Park, J., Meng, J., Lim, K. H., Rojas, O. J., & Park, S. (2013) · Journal of Analytical and Applied Pyrolysis · doi:10.1016/j.jaap.2012.12.024 · Cited by 200
Composition and structure of balsa (Ochroma pyramidale) wood
Borrega, M., Ahvenainen, P., Serimaa, R., & Gibson, L. (2015) · Wood Science and Technology · doi:10.1007/s00226-015-0700-5 · Cited by 189
“Considering that the cellulose content in balsa was between 40-45%, then cellulose crystallinity was about 80-90%, significantly higher than the 40-60% determined for other hardwoods such as birch, aspen and oak (Wikberg and Maunu 2004, Penttilä et al. 2013).”
InfluentialGonzález-Peña, M. M., & Hale, M. D. C. (2009) · hfsg · doi:10.1515/hf.2009.078 · Cited by 186
“This may be linked to the production and subsequent destruction of chromophoric species, probably originated from extractives, and/or due to condensation and re-polymerisation of the lignin substance (Wikberg and Maunu 2004).”
BackgroundEffects of aging on wood: a literature review
Kránitz, K., Sonderegger, W., Bues, C.-T., & Niemz, P. (2016) · Wood Science and Technology · doi:10.1007/s00226-015-0766-0 · Cited by 181
“However, some degradation in the amorphous regions occurs, consequently decreasing the accessibility of hydroxyl groups and resulting in higher crystallinity of cellulose (Nakao et al. 1989; Wikberg and Maunu 2004).”
BackgroundInvestigation of the chemical modifications of beech wood lignin during heat treatment
Brosse, N., El Hage, R., Chaouch, M., Pétrissans, M., Dumarçay, S., & Gérardin, P. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.05.018 · Cited by 164
Deep Eutectic Solvents (DESs) for the Isolation of Willow Lignin (Salix matsudana cv. Zhuliu)
Li, T., Lyu, G., Liu, Y., Lou, R., Lucia, L., Yang, G., Chen, J., & Saeed, H. (2017) · International Journal of Molecular Sciences · doi:10.3390/ijms18112266 · Cited by 149
“The existence of the β-O-4 ethe linkage and β-β linkage were indicated by signals at 57 to 61 ppm, 52 to 54 ppm [34].”
MethodThe influence of thermal treatment on color response of wood materials
Aydemir, D., Gunduz, G., & Ozden, S. (2012) · Color Research & Application · doi:10.1002/col.20655 · Cited by 29
“The main mechanical function of hemicelluloses and lignin is to buttress the cellulose fibrils.(1) Wood materials can be degraded by attacks by numerous biological species and by environmental conditions, so they are protected by the use of various treatment processes.”
BackgroundEffect of natural aging on wood
Kránitz, K. (2014) · ETH Zurich · doi:10.3929/ethz-a-010388674 · Cited by 20
Analytical Pyrolysis Characteristics of Enzymatic/Mild Acidolysis Lignin (EMAL)
Li, T., Lyu, G., Saeed, H. A. M., Liu, Y., Wu, Y., Yang, G., & Lucia, L. A. (2018) · BioResources · doi:10.15376/biores.13.2.4484-4496 · Cited by 15
Yan, C., Sun, T., Jia, H., Xu, Y., & Sun, Y. (2021) · Desalination and Water Treatment · doi:10.5004/dwt.2021.27022 · Cited by 4
Metadata
- Authors
- WIKBERG, H., & LIISAMAUNU, S.
- Venue
- Carbohydrate Polymers
- Publisher
- Elsevier BV
- Published
- 2004-12-07
- Volume
- 58
- Issue
- 4
- Pages
- 461-466
- ISSN
- 0144-8617 (ISSN-L)
- OpenAlex
- W1984865019
- Cited by
- 424
- References
- 14
- FWCI
- 32.68
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.