CoChat

Synthesis of FAU(Y)- and MFI(ZSM5)-nanosized crystallites for catalytic cracking of 1,3,5-triisopropylbenzene

Open access
Morales-Pacheco, P., Domínguez, J.M., Bucio, L., Alvarez, F., Sedran, U., Falco, M. · 2011 · Catalysis Today
Cited by 64

The DOI matches its Crossref record; 1 of the 1 references it cites were found in a registry or an index.

Abstract

Abstract Nanocrystals of FAU(Y) and MFI(ZSM5) zeolites were synthesized from clear solutions at 80–95 °C under autogen and atmospheric pressures, respectively. The X-ray diffraction (XRD) patterns confirm the structural features reported for FAU(Y) and MFI(ZSM5). Similarly, Fourier transform infrared spectroscopy (FTIR) with KBr shows the bands arising from typical structural groups of FAU(Y) and MFI(ZSM5), i.e., 455–462 cm−1 and 555–560 cm−1. The mean crystallites size was measured by transmission electron microscopy (TEM) and it was determined also by Rietveld's method using Scherrer's equation; with similar results between 20 and 40 nm. Also, a cubic morphology for FAU(Y) crystallites and a disk-like habit for MFI(ZSM5) were verified together with the typical dimensions of the pore system and symmetry, i.e., pore diameters were between 0.74 and 0.56 nm for FAU(Y) and MFI(ZSM5). Theoretical images were calculated using HRTEM (Cerius2) program and these were compared with the experimental ones, thus matching the corresponding typical structural parameters. The textural properties were determined by N2 adsorption–desorption (BET) and typical surface areas of 658 and 495 m2/g were obtained for the nanosized materials. After ion-exchanging NH4NO3 ammonia was removed by calcination (i.e., 550 °C) and the total acidity was measured, i.e. 1190 and 1084 μmol(Py)/g (cat) at 25 °C and 84 and 34 μmol(Py)/g (cat) at 400 °C for FAU(Y) and MFI(ZSM5), respectively. Thermal gravimetric analysis (TGA) and differential scanning calorimetry (DSC) in air and N2 atmospheres showed a thermal stability of these materials up to about 1000 °C. The catalytic activity of FAU(Y) and MFI(ZSM5) was tested by means of the cracking of 1,3,5-triisopropylbenzene (1,3,5-TIPBz) in a CREC Riser Simulator Reactor at 350 °C; the cracking of 1,3,5-TIPBz increased to about 0.6 and 1.3 times from big (108.9 and 82.8 nm) to small (18 and 20.7 nm) crystallites of FAU(HY) and MFI(HZSM5), respectively, while diffusivity increased to about 3 and 4.6 times, which demonstrates a correlation between the mean crystallite size of these zeolites with cracking activity from the external crystallite surface and the diffusivity of large reactive molecules, i.e., 1,3,5-TIPBz.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1016/j.cattod.2010.07.005

Cites

1 of 1 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cited by

Metadata

Authors
Morales-Pacheco, P., Domínguez, J. M., Bucio, L., Alvarez, F., Sedran, U., & Falco, M.
Venue
Catalysis Today
Publisher
Elsevier BV
Published
2011-05
Volume
166
Issue
1
Pages
25-38
ISSN
0920-5861 (ISSN-L)
OpenAlex
W2017089206
Cited by
64
References
1
FWCI
1.55
Type
journal article
Language
en
Open access
bronze

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.