Synthesis and characteristics of fly ash and bottom ash based geopolymers–A comparative study
The DOI matches its Crossref record; 21 of the 21 references it cites were found in a registry or an index.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Barbosa, V. F. F., MacKenzie, K. J. D., & Thaumaturgo, C. (2000) · International Journal of Inorganic Materials · doi:10.1016/s1466-6049(00)00041-6 · Cited by 1,128 · cited 1×
“geopolymers compared to ashes, due to use of sodium silicate in geopolymer processing [23–25].”
MethodInfluence of NaOH solution on the synthesis of fly ash geopolymer
Rattanasak, U., & Chindaprasirt, P. (2009) · Minerals Engineering · doi:10.1016/j.mineng.2009.03.022 · Cited by 939 · cited 1×
“The geopolymerization level is lower in BAG compared to FAG, but still the polymerization level is higher than previous achieved results till date for BAG [26].”
ResultComparative study on the characteristics of fly ash and bottom ash geopolymers
Chindaprasirt, P., Jaturapitakkul, C., Chalee, W., & Rattanasak, U. (2009) · Waste Management · doi:10.1016/j.wasman.2008.06.023 · Cited by 735 · cited 2×
“Although bottom ash and fly ash have similar chemical compositions, bottom ash is found to be less reactive compared to fly ash thus having little or almost no use in the manufacturing of geopolymer [11].”
BackgroundResultWorkability and strength of lignite bottom ash geopolymer mortar
Sathonsaowaphak, A., Chindaprasirt, P., & Pimraksa, K. (2009) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2009.01.120 · Cited by 507 · cited 1×
“On the other side, instead of calcite peak, anorthite (JCPDS 891462) and albite (JCPDS 20-0554) (plagioclase feldspar member) are present in the XRD pattern of bottom ash as well as in its geopolymer [12,13].”
BackgroundThermal behaviour of geopolymers prepared using class F fly ash and elevated temperature curing
Bakharev, T. (2006) · Cement and Concrete Research · doi:10.1016/j.cemconres.2006.03.022 · Cited by 494 · cited 1×
“The whole process is helped by molecular thermal agitation which can be successfully provided by heating at 60–80 1C in the humid atmosphere for 24–48 h to complete the reaction, although the strength continues to increase as the time passes and the reaction goes to completion [4].”
BackgroundÁlvarez-Ayuso, E., Querol, X., Plana, F., Alastuey, A., Moreno, N., Izquierdo, M., Font, O., Moreno, T., Diez, S., Vázquez, E., et al. (2008) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2007.10.008 · Cited by 480
Temuujin, J., Williams, R. P., & van Riessen, A. (2009) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2009.03.016 · Cited by 465
Mechanical and microstructural properties of alkali-activated fly ash geopolymers
Komljenović, M., Baščarević, Z., & Bradić, V. (2010) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2010.04.064 · Cited by 446 · cited 1×
“9 GPa and these values are higher than the previously reported results [9,27].”
ResultPreparation and characterisation of fly ash based geopolymer mortars
Temuujin, J., van Riessen, A., & MacKenzie, K. J. D. (2010) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2010.04.012 · Cited by 354
Coal fly ash-slag-based geopolymers: Microstructure and metal leaching
Izquierdo, M., Querol, X., Davidovits, J., Antenucci, D., Nugteren, H. W., & Fernández‐Pereira, C. (2008) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2008.11.063 · Cited by 265 · cited 1×
“012 Si–O–Al bonds, (iii) formation of three dimensional aluminosilicate structures by polycondensation of the oligomers and (iv) bonding of the remaining solid filler particles to the aluminosilicate network for further enhancing the strength and stability [2,3].”
BackgroundStability in the system CaO–Al2O3–H2O
Lothenbach, B., Pelletier-Chaignat, L., & Winnefeld, F. (2012) · Cement and Concrete Research · doi:10.1016/j.cemconres.2012.09.002 · Cited by 259 · cited 1×
“These cementing compounds are formed by calcium present in the ashes during geopolymerization [18–20].”
BackgroundAlkali-activated complex binders from class C fly ash and Ca-containing admixtures
Guo, X., Shi, H., Chen, L., & Dick, W. A. (2010) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2009.08.110 · Cited by 166 · cited 1×
“FeO is present in the form of wustite (JCPDS 43-1312) while belite (Ca2SiO4) (JCPDS 9-351) peaks were also detected [14,15].”
BackgroundSynthesis of geopolymer composites from blends of CFBC fly and bottom ashes
Li, Q., Xu, H., Li, F., Li, P., Shen, L., & Zhai, J. (2012) · Fuel · doi:10.1016/j.fuel.2012.02.059 · Cited by 151 · cited 1×
“This is because the fly ash contains physically absorbed water or moisture which is lost at lower temperature whilst its geopolymer (FAG) has chemically bonded hydroxyl group to silicon (Si–OH), which is released at higher temperatures and gives Si–O–Si structure [16].”
BackgroundAnalysis of geopolymer concrete columns
Sarker, P. K. (2008) · Materials and Structures · doi:10.1617/s11527-008-9415-5 · Cited by 127 · cited 2×
“The concentration of sodium silicate is found to be the best around 14 M in water [9–10].”
BackgroundMethodHuang, Y., & Han, M. (2011) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2011.07.029 · Cited by 123
Response of alkali activated fly ash mortars to microwave curing
Somaratna, J., Ravikumar, D., & Neithalath, N. (2010) · Cement and Concrete Research · doi:10.1016/j.cemconres.2010.08.010 · Cited by 117 · cited 1×
“There are evidences showing that same process can be accomplished by microwave radiations for few minutes of curing [5–6].”
BackgroundZhang, Y. J., Liu, L. C., Xu, Y., Wang, Y., & Xu, D. L. (2012) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2012.01.001 · Cited by 106
Synthesis of thermostable geopolymer from circulating fluidized bed combustion (CFBC) bottom ashes
Xu, H., Li, Q., Shen, L., Wang, W., & Zhai, J. (2009) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2009.09.149 · Cited by 99 · cited 2×
“4 MPa) and is higher comparing to previously reported strength for BAG [11,12].”
BackgroundResultIzquierdo, M., Querol, X., Philippart, C., Antenucci, D., & Towler, M. R. (2009) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2009.11.075 · Cited by 91
Thakur, R., & Ghosh, S. (2014) · Cited by 69
Jaarsveld, J. G. S. V., van Deventer, J. S. J., & Lukey, G. C. (2004) · Chemical Engineering Communications · doi:10.1080/00986440490277974 · Cited by 51
Cited by
Progressive utilisation prospects of coal fly ash: A review
Gollakota, A. R. K., Volli, V., & Shu, C.-M. (2019) · Science of The Total Environment · doi:10.1016/j.scitotenv.2019.03.337 · Cited by 548
Amran, M., Debbarma, S., & Ozbakkaloglu, T. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.121857 · Cited by 532
An overview of geopolymers derived from industrial by-products
Mehta, A., & Siddique, R. (2016) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2016.09.136 · Cited by 391
Behavior of low-calcium fly and bottom ash-based geopolymer concrete cured at ambient temperature
Xie, T., & Ozbakkaloglu, T. (2015) · Ceramics International · doi:10.1016/j.ceramint.2015.01.031 · Cited by 344
Long-term durability properties of geopolymer concrete: An in-depth review
Amran, M., Al-Fakih, A., Chu, S. H., Fediuk, R., Haruna, S., Azevedo, A., & Vatin, N. (2021) · Case Studies in Construction Materials · doi:10.1016/j.cscm.2021.e00661 · Cited by 280
Metadata
- Authors
- ul Haq, E., Kunjalukkal Padmanabhan, S., & Licciulli, A.
- Venue
- Ceramics International
- Publisher
- Elsevier BV
- Published
- 2014-03
- Volume
- 40
- Issue
- 2
- Pages
- 2965-2971
- ISSN
- 0272-8842 (ISSN-L)
- OpenAlex
- W2074064941
- Cited by
- 240
- References
- 21
- FWCI
- 19.59
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.