Influence of clay organic modifier on the thermal-stability of PLA based nanocomposites
The DOI matches its Crossref record; 12 of the 12 references it cites were found in a registry or an index.
Abstract
Abstract Poly(lactic acid) (PLA) is a biodegradable aliphatic thermoplastic polyester well known for being a promising alternative to petroleum-based materials since it can be produced from renewable resources. Although this polymer has good properties when compared to other biodegradable polymers, it presents some limitations like poor thermal, mechanical resistance and gas barrier. The incorporation of clay minerals has been used as a way to overcome this problem. The present work aims to investigate the influence of clay organic modifier (Cloisite 30B, Cloisite 15A and Dellite 43B) and amount (3 and 5%) on PLA thermal stability. PLA and PLA nanocomposites were submitted to thermo-oxidative degradation at 140 °C during 120 h. Samples removed along the time were characterized by gel permeation chromatography (GPC), scanning electron microscopy (SEM), X-ray diffraction (XRD), nuclear magnetic resonance (1H NMR), Fourier transform infrared spectroscopy (FTIR) and differential scanning calorimetry (DSC). After degradation, even though all samples exhibited a significant decrease of molecular weight, it was smaller for nanocomposites. As a consequence of chain scission an increase in the crystallinity degree was observed for all nanocomposites. Results showed that clay mineral incorporation, mainly D43B enhanced the polymer thermal stability.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
An overview of the recent developments in polylactide (PLA) research
Madhavan Nampoothiri, K., Nair, N. R., & John, R. P. (2010) · Bioresource Technology · doi:10.1016/j.biortech.2010.05.092 · Cited by 2,448
SINHARAY, S., & BOUSMINA, M. (2005) · Progress in Materials Science · doi:10.1016/j.pmatsci.2005.05.002 · Cited by 1,611
Vroman, I., & Tighzert, L. (2009) · Materials · doi:10.3390/ma2020307 · Cited by 1,355
Nano-biocomposites: Biodegradable polyester/nanoclay systems
BORDES, P., POLLET, E., & AVEROUS, L. (2009) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2008.10.002 · Cited by 1,033
Carrasco, F., Pagès, P., Gámez-Pérez, J., Santana, O. O., & Maspoch, M. L. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.11.045 · Cited by 738
Paul, M.-A., Alexandre, M., Degée, P., Henrist, C., Rulmont, A., & Dubois, P. (2003) · Polymer · doi:10.1016/s0032-3861(02)00778-4 · Cited by 480
Biodegradation of poly(lactic acid) and its nanocomposites
Fukushima, K., Abbate, C., Tabuani, D., Gennari, M., & Camino, G. (2009) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.07.001 · Cited by 368
Polylactide/montmorillonite nanocomposites: study of the hydrolytic degradation
Paul, M.-A., Delcourt, C., Alexandre, M., Degée, P., Monteverde, F., & Dubois, P. (2005) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2004.10.011 · Cited by 326
New polylactide/layered silicate nanocomposites. 5. Designing of materials with desired properties
Sinha Ray, S., Yamada, K., Okamoto, M., Fujimoto, Y., Ogami, A., & Ueda, K. (2003) · Polymer · doi:10.1016/j.polymer.2003.08.021 · Cited by 317
Effect of tin on poly(l-lactic acid) pyrolysis
Nishida, H., Mori, T., Hoshihara, S., Fan, Y., Shirai, Y., & Endo, T. (2003) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(03)00152-6 · Cited by 176
Effect of natural weather on the structure and properties of polylactide/Cloisite 30B nanocomposites
Zaidi, L., Kaci, M., Bruzaud, S., Bourmaud, A., & Grohens, Y. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.05.014 · Cited by 150
Lewitus, D., McCarthy, S., Ophir, A., & Kenig, S. (2006) · Journal of Polymers and the Environment · doi:10.1007/s10924-006-0007-6 · Cited by 110
Cited by
Poly(lactic acid)—Mass production, processing, industrial applications, and end of life
Castro-Aguirre, E., Iñiguez-Franco, F., Samsudin, H., Fang, X., & Auras, R. (2016) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2016.03.010 · Cited by 1,329
Improvement of thermal behaviors of biodegradable poly(lactic acid) polymer: A review
Jin, F.-L., Hu, R.-R., & Park, S.-J. (2019) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2018.10.078 · Cited by 233
Mechanical recycling of polylactide, upgrading trends and combination of valorization techniques
Badia, J. D., & Ribes-Greus, A. (2016) · European Polymer Journal · doi:10.1016/j.eurpolymj.2016.09.005 · Cited by 161
“The use of nanoclay organic modifiers could also be considered since they prevent from thermal oxidation, even though this option may affect to crystallinity and thus affect to other physic-chemical properties[97].”
BackgroundReview on the Degradation of Poly(lactic acid) during Melt Processing
Velghe, I., Buffel, B., Vandeginste, V., Thielemans, W., & Desplentere, F. (2023) · Polymers · doi:10.3390/polym15092047 · Cited by 146
Nano clays and its composites for food packaging applications
Deshmukh, R. K., Hakim, L., Akhila, K., Ramakanth, D., & Gaikwad, K. K. (2023) · International Nano Letters · doi:10.1007/s40089-022-00388-8 · Cited by 70
Metadata
- Authors
- Araújo, A., Botelho, G., Oliveira, M., & Machado, A. V.
- Venue
- Applied Clay Science
- Publisher
- Elsevier BV
- Published
- 2014-02
- Volume
- 88-89
- Pages
- 144-150
- ISSN
- 0169-1317 (ISSN-L)
- OpenAlex
- W2036297505
- Cited by
- 112
- References
- 12
- FWCI
- 10.35
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.