Durability of concrete under sulfate attack exposed to freeze–thaw cycles
The DOI matches its Crossref record.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Notably, deterioration severity in 1% Na2SO4 exceeded that observed in both 5% Na2SO4 and pure water environments.”
From Deterioration of Concrete Under the Combined Action of Sulfate Attack and Freeze–Thaw Cycles: A Review (2025) · cites this paper as [18]
In the citing paper
“While mass loss in sulfate solution was consistently reported to be lower than in water throughout testing, damage progression accelerated markedly during later stages.”
From Deterioration of Concrete Under the Combined Action of Sulfate Attack and Freeze–Thaw Cycles: A Review (2025) · cites this paper as [18]
In the citing paper
“Jiang et al. [18,19] reported that in the early stages of the experiment, concrete in 5% Na2SO4 solution exhibited lower compressive strength loss and reduced relative dynamic modulus of elasticity (RDEM) loss compared to water-immersed specimens.”
From Deterioration of Concrete Under the Combined Action of Sulfate Attack and Freeze–Thaw Cycles: A Review (2025) · cites this paper as [18]
In the citing paper
“after 400 freeze–thaw cycles, the compressive strength loss of concrete in 5% Na2SO4 solution was 39.6%, compared to 37.7% in water.”
From Deterioration of Concrete Under the Combined Action of Sulfate Attack and Freeze–Thaw Cycles: A Review (2025) · cites this paper as [18]
In the citing paper
“Moreover, as a consequence of high porosity, the RCA concrete showed more loss in compressive strength compared with ordinary concrete in [41], despite adopting a lower w/b ratio.”
From Performance Evolution of Recycled Aggregate Concrete under the Coupled Effect of Freeze–Thaw Cycles and Sulfate Attack (2022) · cites this paper as [41]
4 more claims about this paper
Create a free account to see every claim other papers make about this one.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
No references could be resolved yet.
Research works printed but not linked: 21
- Al-Amoudi, 1995, Performance of 15 reinforced concrete mixtures in magnesium-sodium sulphate environments, Constr. Build. Mater., 9, 149, 10.1016/0950-0618(95)00007-3 · doi:10.1016/0950-0618(95)00007-3
- Al-Dulaijan, 2003, Sulfate resistance of plain and blended cements exposed to varying concentrations of sodium sulfate, Cem. Concr. Compos., 25, 429, 10.1016/S0958-9465(02)00083-5 · DOI
- Bassuoni, 2009, Durability of self-consolidating concrete to different exposure regimes of sodium sulfate attack, Mater. Struct., 42, 1039, 10.1617/s11527-008-9442-2 · DOI
- Bassuoni, 2009, Durability of self-consolidating concrete to sulfate attack under combined cyclic environments and flexural loading, Cem. Concr. Res., 39, 206, 10.1016/j.cemconres.2008.12.003 · DOI
- Chen, 2012, Underground concrete structure exposure to sulfate and chloride invading environment, J. Cent. S. Univ. Technol., 43, 2803
- Gao, 2013, Concrete deterioration mechanisms under combined sulfate attack and flexural loading, J. Mater. Civ. Eng., 25, 39, 10.1061/(ASCE)MT.1943-5533.0000538 · DOI
- Jin, 2007, Interaction between sulfate and chloride solution attack of concretes with and without fly ash, Cem. Concr. Res., 37, 1223, 10.1016/j.cemconres.2007.02.016 · DOI
- Jin, 2008, Damage of concrete attacked by sulfate and sustained loading, J. Southeast Univ., 24, 69
- Kresten, 1975, The thermal decomposition of thaumasite, Thermochim. Acta, 20, 1
- Liu, 2001, Brief introduction on the study of erosion and prevention of concrete in salt lake and saline soil area of Chaerhan, Chadamu, J. Build. Mater., 4, 395
- Miao, 2001, Effect of sulfate solution on the frost resistance of concrete with and without steel fiber reinforcement, Cem. Concr. Res., 32, 31, 10.1016/S0008-8846(01)00624-X · DOI
- Mu, 2001, Effect of NaCl and Na2SO4 solution on the frost resistance of concrete and its mechanism, J. Chin. Ceram. Soc., 29, 523
- Ramyar, 2007, Sodium sulfate attack on plain and blended cements, Build. Environ., 42, 1368, 10.1016/j.buildenv.2005.11.015 · DOI
- Rasheeduzzafar, 1994, Mechanisms of magnesium-sodium sulfate attack in plain and blended cements, J. Mater. Civ. Eng., 6, 201, 10.1061/(ASCE)0899-1561(1994)6:2(201) · doi:10.1061/(asce)0899-1561(1994)6:2(201
- Shanahan, 2007, Cement composition and sulfate attack part I, Cem. Concr. Res., 37, 618, 10.1016/j.cemconres.2006.12.004 · doi:10.1016/j.cemconres.2006.12.004
- Shi, 2011, A FESEM/EDX investigation into how continuous deicer exposure affects the chemistry of Portland cement concrete, Constr. Build. Mater., 25, 957, 10.1016/j.conbuildmat.2010.06.086 · doi:10.1016/j.conbuildmat.2010.06.086
- Wee, 2000, Sulfate resistance of concrete containing mineral admixtures, J. Mater. Civ. Eng., 97, 536
- Yu, 2005, Effects of flexural loads, chemical attack, carbonation and their combination on freezing–thawing durability of concretes, J. Chin. Ceram. Soc., 33, 492
- Yu, 2008, Durability of concrete subjected to the combined actions of flexural stress, freeze–thaw cycles and bittern solutions, J. Wuhan Univ. Technol. Mater. Sci., 23, 893, 10.1007/s11595-007-6893-1 · doi:10.1007/s11595-007-6893-1
- Zhang, 2011, Frost resistance of concrete under action of magnesium sulfate attack, J. Build. Mater., 14, 698
- Zheng, 2010, Study of deterioration mechanism of concrete in multiaggressive and freeze–thaw environment, J. Build. Struct., 31, 111
Cited by
Li, Y., Wang, R., Li, S., Zhao, Y., & Qin, Y. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.01.084 · Cited by 142
Sulfate attack resistance of recycled aggregate concrete with NaOH-solution-treated crumb rubber
Li, Y., Yang, X., Lou, P., Wang, R., Li, Y., & Si, Z. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123044 · Cited by 81
Wu, H., Lv, C., Xu, Y., Sun, Y., Qu, S., & Zhou, X. (2025) · Materials · doi:10.3390/ma18184309 · Cited by 34
“Jiang et al. [18,19] reported that in the early stages of the experiment, concrete in 5% Na 2 SO 4 solution exhibited lower compressive strength loss and reduced relative dynamic modulus of elasticity (RDEM) loss compared to water-immersed specimens.”
Jia, P., Li, L., Zhou, J., Zhang, D., Guan, Z., Dong, J., & Wang, Q. (2022) · Applied Sciences · doi:10.3390/app12146950 · Cited by 24
Metadata
- Authors
- Jiang, L., Niu, D., Yuan, L., & Fei, Q.
- Venue
- Cold Regions Science and Technology
- Publisher
- Elsevier BV
- Published
- 2015-04
- Volume
- 112
- Pages
- 112-117
- ISSN
- 0165-232X
- Cited by
- 171
- References
- 0
- Language
- en
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Funders
- Durability and Life Forecast of Shotcrete Tunnel Structure Fund (51278403)
- Program for Changjiang Scholars and Innovative Research Team in University (IRT13089)
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Durability of concrete under sulfate attack exposed to freeze–thaw cycles. https://app.cochat.ai/papers/10.1016/j.coldregions.2014.12.006
- The paper
- Jiang, L., Niu, D., Yuan, L., & Fei, Q. (2015). Durability of concrete under sulfate attack exposed to freeze–thaw cycles. Cold Regions Science and Technology. https://doi.org/10.1016/j.coldregions.2014.12.006
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.