CoChat

Shrinkage-reducing measures and mechanisms analysis for alkali-activated coal gangue-slag mortar at room temperature

Ma, Hongqiang, Zhu, Hongguang, Chen, Hongyu, Ni, Yadong, Xu, Xiaonan, Huo, Qingjie · 2020 · Construction and Building Materials
Cited by 47

The DOI matches its Crossref record; 2 of the 2 references it cites were found in a registry or an index.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1016/j.conbuildmat.2020.119001

Cites

2 of 2 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Research works printed but not linked: 36

  1. Burciaga-Díaz, 2012, Strength and durability in acid media of alkali silicate-activated metakaolin geopolymers, J. Am. Ceram. Soc., 95, 2307, 10.1111/j.1551-2916.2012.05249.x · DOI
  2. Mobili, 2016, Metakaolin and fly ash alkali-activated mortars compared with cementitious mortars at the same strength class, Cem. Concr. Res., 88, 198, 10.1016/j.cemconres.2016.07.004 · DOI · Paper page
  3. Yang, 2012, Effect of water–binder ratio on the mechanical properties of calcium hydroxide-based alkali-activated slag concrete, Constr. Build. Mater., 29, 504, 10.1016/j.conbuildmat.2011.10.062 · DOI
  4. Lancellotti, 2013, Inorganic polymers from alkali activation of metakaolin: effect of setting and curing on structure, J. Solid State Chem., 200, 341, 10.1016/j.jssc.2013.02.003 · DOI
  5. Lee, 2013, Setting and mechanical properties of alkali-activated fly ash/slag concrete manufactured at room temperature, Constr. Build. Mater., 47, 1201, 10.1016/j.conbuildmat.2013.05.107 · DOI · Paper page
  6. Zhang, 2017, Durability of alkali-activated materials in aggressive environments: A review on recent studies, Constr. Build. Mater., 152, 598, 10.1016/j.conbuildmat.2017.07.027 · DOI · Paper page
  7. Arbi, 2016, A review on the durability of alkali-activated fly ash/slag systems: advances, issues, and perspectives, Ind. Eng. Chem. Res., 55, 5439, 10.1021/acs.iecr.6b00559 · DOI · Paper page
  8. Toniolo, 2017, Boccaccini, Fly ash-based geopolymers containing added silicate waste. A review, Ceram. Int., 43, 14545, 10.1016/j.ceramint.2017.07.221 · DOI
  9. Lura, 2003, Autogenous shrinkage in high-performance cement paste: an evaluation of basic mechanisms, Cem. Concr. Res., 33, 223, 10.1016/S0008-8846(02)00890-6 · doi:10.1016/s0008-8846(02)00890-6
  10. Wehbe, 2017, Combined effect of shrinkage reducing admixtures (sra) and superabsorbent polymers (sap) on the autogenous shrinkage, hydration and properties of cementitious materials, Constr. Build. Mater., 138, 151, 10.1016/j.conbuildmat.2016.12.206 · DOI
  11. Kheradmand, 2017, Shrinkage performance of fly ash alkali-activated cement based binder mortars, KSCE J. Civ. Eng., 22, 1854, 10.1007/s12205-017-1714-3 · DOI
  12. Cartwright, 2015, Shrinkage characteristics of alkali-activated slag cements, J. Mater. Civ. Eng., 27, B4014007, 10.1061/(ASCE)MT.1943-5533.0001058 · DOI · Paper page
  13. Collins, 2000, Effect of pore size distribution on drying shrinking of alkali-activated slag concrete, Cem. Concr. Res., 30, 1401, 10.1016/S0008-8846(00)00327-6 · DOI · Paper page
  14. Fu-Sheng, 2005, Study on modification of the high-strength slag cement material, Cem. Concr. Res., 35, 1344, 10.1016/j.cemconres.2004.10.017 · doi:10.1016/j.cemconres.2004.10.017
  15. Hardjito, 2004, On the development of fly ash-based geopolymer concrete, ACI Mater. J., 101, 467
  16. Fernandez-Jimenez, 2006, Engineering properties of alkali-activated fly ash concrete, ACI Mater. J., 103, 106
  17. Sakulich, 2013, Mitigation of autogenous shrinkage in alkali activated slag mortars by internal curing, Mater. Struct., 46, 1355, 10.1617/s11527-012-9978-z · DOI
  18. Bakharev, 2000, Effect of admixtures on properties of alkali-activated slag concrete, Cem. Concr. Res., 30, 1367, 10.1016/S0008-8846(00)00349-5 · DOI · Paper page
  19. Hailong, 2017, Shrinkage mitigation strategies in alkali-activated slag, Cem. Concr. Res., 101, 131, 10.1016/j.cemconres.2017.08.025 · DOI · Paper page
  20. Yi, 2018, Study on chloride binding capability of coal gangue based cementitious materials, Constr. Build. Mater., 167, 649, 10.1016/j.conbuildmat.2018.02.071 · DOI
  21. Yi, 2018, Preparation and characterization of coal gangue geopolymers, Constr. Build. Mater., 187, 18
  22. Rajabipour, 2008, Interactions between shrinkage reducing admixtures (SRA) and cement paste’s pore solution, Cem. Concr. Res., 38, 606, 10.1016/j.cemconres.2007.12.005 · doi:10.1016/j.cemconres.2007.12.005
  23. Palacios, 2007, Effect of shrinkage-reducing admixtures on the properties of alkali-activated slag mortars and pastes, Cem. Concr. Res., 37, 691, 10.1016/j.cemconres.2006.11.021 · DOI · Paper page
  24. Ma, 2018, Property and cementation mechanism of alkali-activated coal gangue-slag cementitious materials, Chin. J. Mater. Res., 32, 898
  25. Ma, 2019, Study on the drying shrinkage of alkali-activated coal gangue-slag mortar and its mechanisms, Constr. Build. Mater., 225, 204, 10.1016/j.conbuildmat.2019.07.258 · doi:10.1016/j.conbuildmat.2019.07.258
  26. Folliard, 1997, Properties of high performance concrete containing shrinkage reducing admixture, Cem. Concr. Res., 27, 1357, 10.1016/S0008-8846(97)00135-X · doi:10.1016/s0008-8846(97)00135-x
  27. Neto, 2008, Drying and autogenous shrinkage of pastes and mortars with activated slag cement, Cem. Concr. Res., 38, 565, 10.1016/j.cemconres.2007.11.002 · DOI · Paper page
  28. Ye, 2017, Radlińska Aleksandra, Understanding the drying shrinkage performance of alkali-activated slag mortars, Cem. Concr. Compos., 76, 13, 10.1016/j.cemconcomp.2016.11.010 · DOI · Paper page
  29. Mastali, 2018, Drying shrinkage in alkali-activated binders–a critical review, Constr. Build. Mater., 190, 533, 10.1016/j.conbuildmat.2018.09.125 · DOI · Paper page
  30. Ma, 2015, The shrinkage of alkali activated fly ash, Cem. Concr. Res., 68, 75, 10.1016/j.cemconres.2014.10.024 · DOI · Paper page
  31. Thomas, 2006, A colloidal interpretation of chemical aging of the c-s-h gel and its effects on the properties of cement paste, Cem. Concr. Res., 36, 30, 10.1016/j.cemconres.2004.10.022 · DOI
  32. Hou, 2011, Influence of permeability of hcsa expansive agent on high volume fly ash concrete, Key Eng. Mater., 477, 354, 10.4028/www.scientific.net/KEM.477.354 · doi:10.4028/www.scientific.net/kem.477.354
  33. Wei, 2015, Impact on splitting tensile properties of the early age shrinkage-compensating steel fiber reinforced concrete, Bull. Chin. Ceram. Soc., 34, 3004
  34. Ye, 2016, Radlińska Aleksandra, Shrinkage mechanisms of alkali-activated slag, Cem. Concr. Res., 88, 126, 10.1016/j.cemconres.2016.07.001 · DOI · Paper page
  35. Gong, 2018, Influence of shrinkage-reducing agent and polypropylene fiber on shrinkage of ceramsite concrete, Constr. Build. Mater., 159, 155, 10.1016/j.conbuildmat.2017.10.064 · DOI
  36. Izaguirre, 2011, Characterization of aerial lime-based mortars modified by the addition of two different water-retaining agents, Cem. Concr. Comp., 33, 309, 10.1016/j.cemconcomp.2010.09.008 · DOI

Cited by

See all 47

Metadata

Authors
Ma, H., Zhu, H., Chen, H., Ni, Y., Xu, X., & Huo, Q.
Venue
Construction and Building Materials
Publisher
Elsevier BV
Published
2020-08
Volume
252
Pages
119001
ISSN
0950-0618
Cited by
47
References
2
Language
en
Licence
  • www.elsevier.com/tdm/userlicense/1.0/ (tdm)
  • www.elsevier.com/legal/tdmrep-license (tdm)
Funders
  • China Scholarship Council
  • National Natural Science Foundation of China

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.