Degradation mechanisms of high capacity 18650 cells containing Si-graphite anode and nickel-rich NMC cathode

Open access
Li, Xuemin, Colclasure, Andrew M., Finegan, Donal P., Ren, Dongsheng, Shi, Ying, Feng, Xuning, Cao, Lei, Yang, Yuan, Smith, Kandler · 2019 · Electrochimica Acta

Abstract

Abstract Application of advanced anode and cathode materials in commercial lithium-ion batteries is attracting attention due to their high capacity. Silicon (Si)/graphite anodes and nickel (Ni)-rich lithium nickel manganese cobalt oxide with layered structures have been paired in commercial 18650 high energy density cells (∼270 Wh/kg). It is crucial to investigate the cell performance and the aging behavior of this commercial cell. In this study, we present commercial cell degradation mechanisms by comparing fresh and aged electrodes, including changes of crystal structure, morphology, elemental composition, and electrochemical properties. The quantitative analysis was done based on dV/dQ incremental capacity analysis of 18650 cells. To determine the amount of cyclable lithium ions (Li+) and active material loss, the lithiation and delithiation capacity were compared for fresh and aged electrodes in half coin cells. Results showed that even with 5% (by mass) of Si added in the anode, cracks occurred across the anode leading to contact loss and thickening of the solid electrolyte interphase (SEI) layer. Additionally, the average fluorine (F) ratio of the aged anodes was higher compared to that of the fresh anodes. More severely, the F content on the Si aggregations on aged anodes increased to as high as 5 times that of the fresh anode, indicating SEI growth, especially on Si particles. Solid 7Li nuclear magnetic resonance results showed no detectable Li metal deposition on the aged anode. On the cathode side, cracks on the primary particle interfaces contributed to cathode material loss, contact loss, and impedance rise. Therefore, Li+ loss into the thickened SEI layer, particle cracking, and impedance rise are the main reasons behind cell degradation.

Overview

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1016/j.electacta.2018.11.194

Cites

2 of 2 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 2 references

Cited by

See all 170

Metadata

Authors
Li, X., Colclasure, A. M., Finegan, D. P., Ren, D., Shi, Y., Feng, X., Cao, L., Yang, Y., & Smith, K.
Venue
Electrochimica Acta
Publisher
Elsevier BV
Published
2019-02
Volume
297
Pages
1109-1120
ISSN
0013-4686 (ISSN-L)
OpenAlex
W2903030856
Cited by
170
References
2
FWCI
6.96
Type
journal article
Language
en
Open access
bronze

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Degradation mechanisms of high capacity 18650 cells containing Si-graphite anode and nickel-rich NMC cathode. https://app.cochat.ai/papers/10.1016/j.electacta.2018.11.194
The paper
Li, X., Colclasure, A. M., Finegan, D. P., Ren, D., Shi, Y., Feng, X., Cao, L., Yang, Y., & Smith, K. (2019). Degradation mechanisms of high capacity 18650 cells containing Si-graphite anode and nickel-rich NMC cathode. Electrochimica Acta. https://doi.org/10.1016/j.electacta.2018.11.194

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.