The DOI matches its Crossref record; 75 of the 75 references it cites were found in a registry or an index.
The reactant starvation of the proton exchange membrane fuel cells for vehicular applications: A review
Abstract
The short service life of fuel cell is a key problem that restricts the commercialization of fuel cell vehicles. Many scholars have found that gas starvation is one of the most important causes of the proton exchange membrane fuel cell lifetime decay, which leads to a series of severe consequences such as carbon support corrosion, cell reversal and output performance degradation. However, accurate diagnosis and effective mitigation of fuel cell gas starvation are not achieved currently. Gas starvation is a condition that the reaction gas of proton exchange membrane fuel cell working in the sub-stoichiometric state. In this paper, we will study the causes, severe consequences, diagnostic methods and mitigation measures of the gas starvation in proton exchange membrane fuel cells through previous literature review. This research is aim to provide guidance to the diagnose methods, to optimize the system control strategy and structure design and to contribute to the studies which are focus on prolong the proton exchange membrane fuel cell lifetime.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
A Reverse-Current Decay Mechanism for Fuel Cells
Reiser, C. A., Bregoli, L., Patterson, T. W., Yi, J. S., Yang, J. D., Perry, M. L., & Jarvi, T. D. (2005) · Electrochemical and Solid-State Letters · doi:10.1149/1.1896466 · Cited by 976
Aging mechanisms and lifetime of PEFC and DMFC
Knights, S. D., Colbow, K. M., St-Pierre, J., & Wilkinson, D. P. (2004) · Journal of Power Sources · doi:10.1016/j.jpowsour.2003.09.033 · Cited by 753
Pei, P., & Chen, H. (2014) · Applied Energy · doi:10.1016/j.apenergy.2014.03.048 · Cited by 616
Self-citationA review of accelerated stress tests of MEA durability in PEM fuel cells
ZHANG, S., YUAN, X., WANG, H., MERIDA, W., ZHU, H., SHEN, J., WU, S., & ZHANG, J. (2009) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.10.012 · Cited by 525
Analysis of electrocatalyst degradation in PEMFC caused by cell reversal during fuel starvation
Taniguchi, A., Akita, T., Yasuda, K., & Miyazaki, Y. (2004) · Journal of Power Sources · doi:10.1016/j.jpowsour.2003.12.035 · Cited by 525
A quick evaluating method for automotive fuel cell lifetime
PEI, P., CHANG, Q., & TANG, T. (2008) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.04.048 · Cited by 518
Self-citationPEM fuel cell cathode carbon corrosion due to the formation of air/fuel boundary at the anode
Tang, H., Qi, Z., Ramani, M., & Elter, J. F. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.10.059 · Cited by 488
Yousfi-Steiner, N., Moçotéguy, P., Candusso, D., & Hissel, D. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.03.060 · Cited by 431
Ex-situ characterisation of gas diffusion layers for proton exchange membrane fuel cells
El-Kharouf, A., Mason, T. J., Brett, D. J. L., & Pollet, B. G. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.06.099 · Cited by 385
Kıymık, M. K., Güler, İ., Dizibüyük, A., & Akın, M. (2005) · Computers in Biology and Medicine · doi:10.1016/j.compbiomed.2004.05.001 · Cited by 314
Hu, Z., Li, J., Xu, L., Song, Z., Fang, C., Ouyang, M., Dou, G., & Kou, G. (2016) · Energy Conversion and Management · doi:10.1016/j.enconman.2016.09.082 · Cited by 288
In-situ methods for the determination of current distributions in PEM fuel cells
Stumper, J., Campbell, S. A., Wilkinson, D. P., Johnson, M. C., & Davis, M. (1998) · Electrochimica Acta · doi:10.1016/s0013-4686(98)00137-6 · Cited by 252
Analysis of degradation in PEMFC caused by cell reversal during air starvation
TANIGUCHI, A., AKITA, T., YASUDA, K., & MIYAZAKI, Y. (2008) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.02.049 · Cited by 233
Damage to the Cathode Catalyst of a PEM Fuel Cell Caused by Localized Fuel Starvation
Patterson, T. W., & Darling, R. M. (2006) · Electrochemical and Solid-State Letters · doi:10.1149/1.2167930 · Cited by 226
Channel to rib width ratio influence with various flow field designs on performance of PEM fuel cell
Kerkoub, Y., Benzaoui, A., Haddad, F., & Ziari, Y. K. (2018) · Energy Conversion and Management · doi:10.1016/j.enconman.2018.08.041 · Cited by 212
Characterizing the Structural Degradation in a PEMFC Cathode Catalyst Layer: Carbon Corrosion
Young, A. P., Stumper, J., & Gyenge, E. (2009) · Journal of The Electrochemical Society · doi:10.1149/1.3139963 · Cited by 192
Optimization of purge cycle for dead-ended anode fuel cell operation
Chen, J., Siegel, J. B., Stefanopoulou, A. G., & Waldecker, J. R. (2013) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2013.02.022 · Cited by 176
Liang, D., Shen, Q., Hou, M., Shao, Z., & Yi, B. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.06.059 · Cited by 161
Oxygen starvation analysis during air feeding faults in PEMFC
Gérard, M., Poirot-Crouvezier, J.-P., Hissel, D., & Péra, M. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.08.028 · Cited by 154
Systems Strategies to Mitigate Carbon Corrosion in Fuel Cells
Perry, M. L., Patterson, T. W., & Reiser, C. (2006) · ECS Transactions · doi:10.1149/1.2356198 · Cited by 142
Chen, B., Wang, J., Yang, T., Cai, Y., Zhang, C., Chan, S. H., Yu, Y., & Tu, Z. (2016) · Energy · doi:10.1016/j.energy.2016.03.045 · Cited by 135
Study on the processes of start-up and shutdown in proton exchange membrane fuel cells
Shen, Q., Hou, M., Liang, D. S., Zhou, Z., Li, X., Shao, Z., & Yi, B. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.12.075 · Cited by 129
Liu, Z. Y., Brady, B. K., Carter, R. N., Litteer, B. A., Budinski, M. K., Hyun, J. K., & Muller, D. A. (2008) · Journal of The Electrochemical Society · doi:10.1149/1.2956198 · Cited by 128
Carbon Corrosion in PEM Fuel Cell Dead-Ended Anode Operations
Chen, J., Siegel, J. B., Matsuura, T., & Stefanopoulou, A. G. (2011) · Journal of The Electrochemical Society · doi:10.1149/1.3609770 · Cited by 115
30,000 h operation of a 70 kW stationary PEM fuel cell system using hydrogen from a chlorine factory
Verhage, A. J. L., Coolegem, J. F., Mulder, M. J. J., Yildirim, M. H., & de Bruijn, F. A. (2013) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2013.01.152 · Cited by 107
Review of Applications of Impedance and Noise Analysis to Uniform and Localized Corrosion
Gabrielli, C., & Keddam, M. (1992) · CORROSION · doi:10.5006/1.3315878 · Cited by 102
Gerteisen, D., Zamel, N., Sadeler, C., Geiger, F., Ludwig, V., & Hebling, C. (2012) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2012.02.024 · Cited by 98
Cognard, G., Ozouf, G., Beauger, C., Berthomé, G., Riassetto, D., Dubau, L., Chattot, R., Chatenet, M., & Maillard, F. (2017) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2016.08.010 · Cited by 97
Qu, S., Li, X., Hou, M., Shao, Z., & Yi, B. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.080 · Cited by 94
Zhou, F., Andreasen, S. J., Kær, S. K., & Yu, D. (2015) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2014.12.082 · Cited by 92
Pt-Ni Aerogels as Unsupported Electrocatalysts for the Oxygen Reduction Reaction
Henning, S., Kühn, L., Herranz, J., Durst, J., Binninger, T., Nachtegaal, M., Werheid, M., Liu, W., Adam, M., Kaskel, S., et al. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0251609jes · Cited by 87
Henning, S., Ishikawa, H., Kühn, L., Herranz, J., Müller, E., Eychmüller, A., & Schmidt, T. J. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201704253 · Cited by 84
Accelerated test analysis of reversal potential caused by fuel starvation during PEMFCs operation
Kang, J., Jung, D. W., Park, S., Lee, J., Ko, J., & Kim, J. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.01.071 · Cited by 84
Evaluation of self-water-removal in a dead-ended proton exchange membrane fuel cell
Wan, Z., Liu, J., Luo, Z., Tu, Z., Liu, Z., & Liu, W. (2012) · Applied Energy · doi:10.1016/j.apenergy.2012.12.008 · Cited by 84
Membrane electrode assembly degradation by dry/wet gas on a PEM fuel cell
Kang, J., & Kim, J. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.04.077 · Cited by 78
Abbou, S., Dillet, J., Maranzana, G., Didierjean, S., & Lottin, O. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.11.079 · Cited by 78
Mahmoudi, A. H., Ramiar, A., & Esmaili, Q. (2015) · Energy Conversion and Management · doi:10.1016/j.enconman.2015.12.012 · Cited by 77
Modeling hydrogen starvation conditions in proton-exchange membrane fuel cells
Ohs, J. H., Sauter, U., Maass, S., & Stolten, D. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.06.038 · Cited by 76
A comparison of the wavelet and short-time fourier transforms for Doppler spectral analysis
Zhang, Y., Guo, Z., Wang, W., Si-de, H., Lee, T., & Loew, M. H. (2003) · Medical Engineering & Physics · doi:10.1016/s1350-4533(03)00052-3 · Cited by 72
Comprehensive analysis of galvanostatic charge method for fuel cell degradation diagnosis
Hu, Z., Xu, L., Huang, Y., Li, J., Ouyang, M., Du, X., & Jiang, H. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.01.005 · Cited by 71
Siroma, Z., Fujiwara, N., Ioroi, T., Yamazaki, S., Senoh, H., Yasuda, K., & Tanimoto, K. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.062 · Cited by 66
Martinet, S., Durand, R., Ozil, P., Leblanc, P. P., & Blanchard, P. (1999) · Journal of Power Sources · doi:10.1016/s0378-7753(99)00272-4 · Cited by 66
Xu, L., Fang, C., Li, J., Ouyang, M., & Lehnert, W. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.08.099 · Cited by 66
Operation of a planar free-breathing PEMFC in a dead-end mode
Himanen, O., Hottinen, T., & Tuurala, S. (2007) · Electrochemistry Communications · doi:10.1016/j.elecom.2006.12.002 · Cited by 64
Experimental investigation of PEM fuel cell aging under current cycling using segmented fuel cell
Weng, F.-B., Hsu, C.-Y., & Li, C. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.01.065 · Cited by 62
Hu, Z., Yu, Y., Wang, G., Chen, X., Chen, P., Chen, J., & Zhou, S. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.04.023 · Cited by 62
Xiao, Y., Zhan, G., Fu, Z., Pan, Z., Xiao, C., Wu, S., Chen, C., Hu, G., & Wei, Z. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.03.001 · Cited by 61
An investigation into the effect of anode purging on the fuel cell performance
Mokmeli, A., & Asghari, S. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.03.079 · Cited by 61
Jeon, Y., Na, H., Hwang, H., Park, J.-H., Hwang, H. J., & Shul, Y. (2015) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2015.01.010 · Cited by 61
Xu, L., Reimer, U., Li, J., Huang, H., Hu, Z., Jiang, H., Janßen, H., Ouyang, M., & Lehnert, W. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.11.075 · Cited by 61
Cognard, G., Ozouf, G., Beauger, C., Dubau, L., López‐Haro, M., Chatenet, M., & Maillard, F. M. (2017) · Electrochimica Acta · doi:10.1016/j.electacta.2017.05.178 · Cited by 58
An analysis of fluidic voltage statistical correlation for a diagnosis of PEM fuel cell flooding
Giurgea, S., Tirnovan, R. A., Hissel, D., & Outbib, R. (2013) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2013.01.060 · Cited by 57
Roy, S. K., & Orazem, M. E. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.014 · Cited by 56
Zhao, X., Xu, L., Fang, C., Jiang, H., Li, J., & Ouyang, M. (2018) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2018.06.172 · Cited by 53
Self-citationInvestigation of water transport and its effect on performance of high-temperature PEM fuel cells
Zhang, C., Zhang, L., Zhou, W., Wang, Y., & Chan, S. H. (2014) · Electrochimica Acta · doi:10.1016/j.electacta.2014.10.059 · Cited by 52
Air Starvation Induced Degradation in Polymer Electrolyte Fuel Cells
Bodner, M., Schenk, A., Salaberger, D., Rami, M., Hochenauer, C., & Hacker, V. (2017) · Fuel Cells · doi:10.1002/fuce.201600132 · Cited by 52
Jo, Y. Y., Cho, E., Kim, J. H., Lim, T., Oh, I., Kim, S., Kim, H., & Jang, J. H. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.08.035 · Cited by 51
Behavior of a unit proton exchange membrane fuel cell in a stack under fuel starvation
Liang, D., Dou, M., Hou, M., Shen, Q., Shao, Z., & Yi, B. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.02.064 · Cited by 50
Manokaran, A., Pushpavanam, S., Sridhar, P., & Pitchumani, S. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.06.103 · Cited by 48
Yang, X., Ye, Q., & Cheng, P. (2012) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2012.07.011 · Cited by 46
Passive Fault Tolerant Control of PEMFC air feeding system
Lebreton, C., Damour, C., Benne, M., Grondin-Pérez, B., & Chabriat, J.-P. (2016) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2016.06.210 · Cited by 46
A highly stable TiB2-supported Pt catalyst for polymer electrolyte membrane fuel cells
Yin, S., Mu, S. C., Pan, M., & Fu, Z. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.05.033 · Cited by 44
Yu, Y., Wang, G., Tu, Z., Zhan, Z., & Pan, M. (2012) · Electrochimica Acta · doi:10.1016/j.electacta.2012.03.141 · Cited by 43
Electrochemical parameter estimation in operating proton exchange membrane fuel cells
Rubio, M. A., Urquía, A., Kuhn, R., & Dormido, S. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.05.011 · Cited by 42
Fritz, K., Beaucage, P. A., Matsuoka, F., Wiesner, U. B., & Suntivich, J. (2017) · Chemical Communications · doi:10.1039/c7cc03232c · Cited by 37
Lin, R., Cao, C., Ma, J., Gülzow, E. F., & Friedrich, K. A. (2011) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2011.11.046 · Cited by 36
Beauger, C., Testut, L., Berthon‐Fabry, S., Georgi, F., & Guétaz, L. (2016) · Microporous and Mesoporous Materials · doi:10.1016/j.micromeso.2016.06.003 · Cited by 36
Highly Active, Corrosion-Resistant Cathode for Fuel Cells, Based on Platinum and Molybdenum Carbide
Lori, O., Gonen, S., & Elbaz, L. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1161707jes · Cited by 35
Cognard, G., Ozouf, G., Beauger, C., Jiménez‐Morales, I., Cavaliere-Jaricot, S., Jones, D. J., Rozière, J., Chatenet, M., & Maillard, F. M. (2016) · Electrocatalysis · doi:10.1007/s12678-016-0340-z · Cited by 34
Polymer Electrolyte Membrane (PEM) Fuel Cells, Automotive Applications
Kocha, S. S. (2012) · Springer eBooks · doi:10.1007/978-1-4614-5785-5_15 · Cited by 32
Dynamic Response during PEM Fuel Cell Loading-up
Pei, P., Yuan, X. F., Gou, J., & Li, P. (2009) · Materials · doi:10.3390/ma2030734 · Cited by 32
Self-citationElectrochemical Impedance and Acoustic Emission Survey of Water Desorption in Nafion Membranes
Legros, B., Thivel, P., Bultel, Y., Boinet, M., & Nogueira, R. P. (2009) · Electrochemical and Solid-State Letters · doi:10.1149/1.3131728 · Cited by 32
Reversible performance loss induced by sequential failed cold start of PEM fuel cells
Hou, J., Yu, H., Yang, M., Song, W., Shao, Z., & Yi, B. (2011) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2011.06.100 · Cited by 27
Effect of Acid Washing on the Oxygen Reduction Reaction Activity of Pt-Cu Aerogel Catalysts
Henning, S., Kühn, L., Herranz, J. S., Nachtegaal, M., Hübner, R., Werheid, M., Eychmüller, A., & Schmidt, T. J. (2017) · Electrochimica Acta · doi:10.1016/j.electacta.2017.03.019 · Cited by 26
Labbé, F., Disa, E., Ahmad, Y., Guérin, K., Asset, T., Maillard, F. M., Chatenet, M., Metkemeijer, R., & Berthon‐Fabry, S. (2018) · Microporous and Mesoporous Materials · doi:10.1016/j.micromeso.2018.05.019 · Cited by 14
Cited by
Ren, P., Pei, P., Li, Y., Wu, Z., Chen, D., & Huang, S. (2020) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2020.100859 · Cited by 737
Self-citationLü, X., Wu, Y., Lian, J., Zhang, Y., Chen, C., Wang, P., & Meng, L. (2020) · Energy Conversion and Management · doi:10.1016/j.enconman.2020.112474 · Cited by 647
The fuel cell electric vehicles: The highlight review
Pramuanjaroenkij, A., & Kakaç, S. (2023) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2022.11.103 · Cited by 469
Zhao, J., Tu, Z., & Chan, S. H. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.229434 · Cited by 442
Tang, Z., Huang, Q.-A., Wang, Y.-J., Zhang, F., Li, W., Li, A., Zhang, L., & Zhang, J. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.228361 · Cited by 276
Metadata
- Authors
- Chen, H., Zhao, X., Zhang, T., & Pei, P.
- Venue
- Energy Conversion and Management
- Publisher
- Elsevier BV
- Published
- 2019-02
- Volume
- 182
- Pages
- 282-298
- ISSN
- 0196-8904 (ISSN-L)
- OpenAlex
- W2908107822
- Cited by
- 342
- References
- 75
- FWCI
- 14.80
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.