The DOI matches its Crossref record; 59 of the 59 references it cites were found in a registry or an index.
Requirements for the transfer of lead-free piezoceramics into application
Open accessAbstract
The recent review for the Restriction of Hazardous Substances Directive (RoHS) by the expert committee, appointed by the European Union, stated that the replacement of PZT “… may be scientifically and technologically practical to a certain degree …”, although replacement “… is scientifically and technically still impractical in the majority of applications.” Thus, two decades of sustained research and development may be approaching fruition, at first limited to a minority of applications. Therefore, it is of paramount importance to assess the viability of lead-free piezoceramics over a broad range of application-relevant properties. These are identified and discussed in turn: 1. Cost, 2. Reproducibility, 3. Mechanical and Thermal Properties, 4. Electrical Conductivity, and 5. Lifetime. It is suggested that the worldwide efforts into the development of lead-free piezoceramics now require a broader perspective to bring the work to the next stage of development by supporting implementation into real devices. Guidelines about pertinent research requirements into a wide range of secondary properties, measurement techniques, and salient literature are provided.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Saito, Y., Takao, H., Tani, T., Nonoyama, T., Takatori, K., Homma, T., Nagaya, T., & Nakamura, M. (2004) · Nature · doi:10.1038/nature03028 · Cited by 5,475
A manifesto for reproducible science
Munafò, M. R., Nosek, B. A., Bishop, D. V. M., Button, K. S., Chambers, C. D., Percie du Sert, N., Simonsohn, U., Wagenmakers, E.-J., Ware, J. J., & Ioannidis, J. P. A. (2017) · Nature Human Behaviour · doi:10.1038/s41562-016-0021 · Cited by 3,397
Ullmann's Encyclopedia of Industrial Chemistry
(2012) · Choice Reviews Online · doi:10.5860/choice.50-1224 · Cited by 3,049
Large Piezoelectric Effect in Pb-Free Ceramics
Liu, W., & Ren, X. (2009) · Physical Review Letters · doi:10.1103/physrevlett.103.257602 · Cited by 2,764
MERZ, W. J. (1972) · Nature · doi:10.1038/236245a0 · Cited by 2,440
Wu, J., Xiao, D., & Zhu, J. (2015) · Chemical Reviews · doi:10.1021/cr5006809 · Cited by 1,608
Ceramic Processing and Sintering
(2003) · Routledge eBooks · doi:10.4324/9780203912263 · Cited by 1,464
BaTiO3-Based Piezoelectrics: Fundamentals, Current Status, and Perspectives
Acosta, M., Novak, N., Rojas, V., Patel, S., Vaish, R., Koruza, J., Rossetti, G. A., & Rödel, J. (2017) · Applied Physics Reviews · doi:10.1063/1.4990046 · Cited by 1,451 · cited 9×
“Only a few coercive stress values are currently available for leadfree piezoceramics: NBT-xBT [19,98], BCTZ [99], BF-BKT [100], and KNN [101,102].”
BackgroundInfluentialSelf-citationReview: liquid phase sintering
German, R. M., Suri, P., & Park, S. J. (2009) · Journal of Materials Science · doi:10.1007/s10853-008-3008-0 · Cited by 1,444
Colloidal Processing of Ceramics
Lewis, J. A. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01560.x · Cited by 1,371
Transferring lead-free piezoelectric ceramics into application
Rödel, J., Webber, K. G., Dittmer, R., Jo, W., Kimura, M., & Damjanovic, D. (2015) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2014.12.013 · Cited by 1,323
Self-citationNational Power and the Structure of Foreign Trade
Oliver, H., & Hirschman, A. (1946) · Southern Economic Journal · doi:10.2307/1052282 · Cited by 1,221
Base-Metal Electrode-Multilayer Ceramic Capacitors: Past, Present and Future Perspectives
Kishi, H., Mizuno, Y., & Chazono, H. (2003) · Japanese Journal of Applied Physics · doi:10.1143/jjap.42.1 · Cited by 1,171
Li, J., Wang, K., Zhu, F., Cheng, L., & Yao, F. (2013) · Journal of the American Ceramic Society · doi:10.1111/jace.12715 · Cited by 878
Self-citationNational Power and the Structure of Foreign Trade, by Albert O. Hirschman
Florinsky, M. T. (1946) · Political Science Quarterly · doi:10.2307/2144611 · Cited by 732
Wiley encyclopedia of electrical and electronics engineering
(1999) · Choice Reviews Online · doi:10.5860/choice.37-1289 · Cited by 696
dc Electrical Degradation of Perovskite‐Type Titanates: I, Ceramics
Waser, R., Baiatu, T., & Härdtl, K. (1990) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1990.tb09809.x · Cited by 680
Scott, J. F. (2008) · Journal of Physics: Condensed Matter · doi:10.1088/0953-8984/20/02/021001 · Cited by 637
Ceramics: Mechanical properties, failure behaviour, materials selection
(2000) · Annales de Chimie Science des Mat�riaux · doi:10.1016/s0151-9107(00)88627-4 · Cited by 595
High‐Performance Lead‐Free Piezoceramics with High Curie Temperatures
Lee, M. H., Kim, D. J., Park, J. S., Kim, S. W., Song, T. K., Kim, M., Kim, W., Do, D., & Jeong, I. (2015) · Advanced Materials · doi:10.1002/adma.201502424 · Cited by 577
Temperature‐Insensitive (K,Na)NbO3‐Based Lead‐Free Piezoactuator Ceramics
Wang, K., Yao, F., Jo, W., Gobeljic, D., Shvartsman, V. V., Lupascu, D. C., Li, J., & Rödel, J. (2013) · Advanced Functional Materials · doi:10.1002/adfm.201203754 · Cited by 574
Self-citationData-Driven Review of Thermoelectric Materials: Performance and Resource Considerations
Gaultois, M. W., Sparks, T. D., Borg, C. K. H., Seshadri, R., Bonificio, W. D., & Clarke, D. R. (2013) · Chemistry of Materials · doi:10.1021/cm400893e · Cited by 500
BiFeO 3 Ceramics: Processing, Electrical, and Electromechanical Properties
Rojac, T., Bencan, A., Malic, B., Tutuncu, G., Jones, J. L., Daniels, J. E., & Damjanovic, D. (2014) · Journal of the American Ceramic Society · doi:10.1111/jace.12982 · Cited by 482
Zhang, R., Jiang, B., & Cao, W. (2001) · Journal of Applied Physics · doi:10.1063/1.1390494 · Cited by 450
The effect of uniaxial stress on the electro-mechanical response of 8/65/35 PLZT
Lynch, C. S. (1996) · Acta Materialia · doi:10.1016/s1359-6454(96)00062-6 · Cited by 435
Mechanisms of aging and fatigue in ferroelectrics
Genenko, Y. A., Glaum, J., Hoffmann, M. J., & Albe, K. (2015) · Materials Science and Engineering: B · doi:10.1016/j.mseb.2014.10.003 · Cited by 400
(1950) · Medical Entomology and Zoology · Cited by 396
Davis, M., Damjanovic, D., & Setter, N. (2006) · Physical Review B · doi:10.1103/physrevb.73.014115 · Cited by 302
Sintering of Lead-Free Piezoelectric Sodium Potassium Niobate Ceramics
Malič, B., Koruza, J., Hreščak, J., Bernard, J., Wang, K., Fisher, J., & Benčan, A. (2015) · Materials · doi:10.3390/ma8125449 · Cited by 279
Self-citationHigh Strain Piezoelectric Multilayer Actuators?A Material Science and Engineering Challenge
Randall, C. A., Kelnberger, A., Yang, G. Y., Eitel, R. E., & Shrout, T. R. (2005) · Journal of Electroceramics · doi:10.1007/s10832-005-0956-5 · Cited by 251
Ihlefeld, J. F., Harris, D. T., Keech, R., Jones, J. L., Maria, J., & Trolier‐McKinstry, S. (2016) · Journal of the American Ceramic Society · doi:10.1111/jace.14387 · Cited by 250
Advanced piezoelectric materials
Uchino, K. (2010) · Woodhead Publishing Limited eBooks · doi:10.1533/9781845699758 · Cited by 236
Defect control for low leakage current in K0.5Na0.5NbO3 single crystals
Kizaki, Y., Noguchi, Y., & Miyayama, M. (2006) · Applied Physics Letters · doi:10.1063/1.2357859 · Cited by 223
Bobnar, V., Kutnjak, Z., Pirc, R., & Levstik, A. (1999) · Physical Review B · doi:10.1103/physrevb.60.6420 · Cited by 184
Ibn-Mohammed, T., Koh, S. C. L., Reaney, I. M., Acquaye, A., Wang, D., Taylor, S., & Genovese, A. (2016) · Energy & Environmental Science · doi:10.1039/c6ee02429g · Cited by 180
Sommer, R., Yushin, N. K., & van der Klink, J. J. (1993) · Physical Review B · doi:10.1103/physrevb.48.13230 · Cited by 173
Damjanovic, D., Biancoli, A., Batooli, L., Vahabzadeh, A., & Trodahl, J. (2012) · Applied Physics Letters · doi:10.1063/1.4714703 · Cited by 171
Gao, J., Hu, X., Zhang, L., Li, F., Zhang, L., Wang, Y., Hao, Y., Zhong, L., & Ren, X. (2014) · Applied Physics Letters · doi:10.1063/1.4885675 · Cited by 155
Influence of Electric Field and Mechanical Stresses on the Fracture of Ferroelectrics
Schneider, G. A. (2007) · Annual Review of Materials Research · doi:10.1146/annurev.matsci.37.052506.084213 · Cited by 155
Thermal conductivity of perovskite ferroelectrics
Tachibana, M., Kolodiazhnyi, T. V., & Takayama‐Muromachi, E. (2008) · Applied Physics Letters · doi:10.1063/1.2978072 · Cited by 131
(Ba,Ca)(Zr,Ti)O3 lead-free piezoelectric ceramics—The critical role of processing on properties
Bai, Y., Matoušek, A., Tofel, P., Bijalwan, V., Nan, B., Hughes, H., & Button, T. W. (2015) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2015.05.010 · Cited by 120
Webber, K. G., Vögler, M., Khansur, N. H., Kaeswurm, B., Daniels, J. E., & Schader, F. H. (2017) · Smart Materials and Structures · doi:10.1088/1361-665x/aa590c · Cited by 106
Self-citationKobayashi, K., Doshida, Y., Mizuno, Y., & Randall, C. A. (2012) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2012.05266.x · Cited by 100
Carpenter, M. A. (2015) · Journal of Physics Condensed Matter · doi:10.1088/0953-8984/27/26/263201 · Cited by 99
Constraint-induced crack initiation at electrode edges in piezoelectric ceramics
Lucato, S. L. D. S. E., Lupascu, D. C., Kamlah, M., Rödel, J., & Lynch, C. S. (2001) · Acta Materialia · doi:10.1016/s1359-6454(01)00169-0 · Cited by 99
Self-citationGuo, H., Voas, B. K., Zhang, S. J., Zhou, C., Ren, X., Beckman, S. P., & Tan, X. (2014) · Physical Review B · doi:10.1103/physrevb.90.014103 · Cited by 82
Multifunctional Polycrystalline Ferroelectric Materials: Processing and Properties
Pardo, L., & Ricote, J. (2011) · Springer series in materials science · doi:10.1007/978-90-481-2875-4 · Cited by 80
Vapour pressure and mixing thermodynamic properties of the KNbO 3 –NaNbO 3 system
Popović, A., Bencze, L., Koruza, J., et al. (2015) · RSC Advances · doi:10.1039/c5ra11874c · Cited by 74
Self-citationSolid state synthesis and sintering of solid solutions of BNT–xBKT
Kainz, T., Naderer, M., Schütz, D., Fruhwirth, O., Mautner, F. A., & Reichmann, K. (2014) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2014.04.040 · Cited by 58
Iamsasri, T., Tutuncu, G., Uthaisar, C., Wongsaenmai, S., Pojprapai, S., & Jones, J. L. (2015) · Journal of Applied Physics · doi:10.1063/1.4905613 · Cited by 55
Brandt, D. R. J., Acosta, M., Koruza, J., & Webber, K. G. (2014) · Journal of Applied Physics · doi:10.1063/1.4879395 · Cited by 49
Self-citationKNN–NTK composite lead-free piezoelectric ceramic
Matsuoka, T., Kozuka, H., Kitamura, K., Yamada, H., Kurahashi, T., Yamazaki, M., & Ohbayashi, K. (2014) · Journal of Applied Physics · doi:10.1063/1.4898586 · Cited by 43
Mechanical stability of piezoelectric properties in ferroelectric perovskites
Schader, F. H., Morozov, M. I., Wefring, E. T., Grande, T., & Webber, K. G. (2015) · Journal of Applied Physics · doi:10.1063/1.4919815 · Cited by 38
Self-citationHigh Bipolar Fatigue Resistance of BCTZ Lead‐Free Piezoelectric Ceramics
Zhang, Y., Glaum, J., Ehmke, M. C., Blendell, J. E., Bowman, K. J., & Hoffman, M. (2015) · Journal of the American Ceramic Society · doi:10.1111/jace.13927 · Cited by 37
Determination of the True Operational Range of a Piezoelectric Actuator
Webber, K. G., Franzbach, D. J., & Koruza, J. (2014) · Journal of the American Ceramic Society · doi:10.1111/jace.13024 · Cited by 30
Self-citationBismuth, Bismuth Alloys, and Bismuth Compounds
Krüger, J., Winkler, P., Lüderitz, E., et al. (2003) · Ullmann's Encyclopedia of Industrial Chemistry · doi:10.1002/14356007.a04_171 · Cited by 26
Crack‐Growth‐Velocity‐Dependent R ‐Curve Behavior in Lead Zirconate Titanate
Lucato, S. L. D. S. E. (2003) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2003.tb03417.x · Cited by 25
Kaushal, A., Olhero, S. M., & Ferreira, J. M. F. (2013) · Journal of Materials Chemistry C · doi:10.1039/c3tc30741g · Cited by 24
Rojas, V., Koruza, J., Patterson, E. A., Acosta, M., Jiang, X., Liu, N., Dietz, C., & Rödel, J. (2017) · Journal of the American Ceramic Society · doi:10.1111/jace.15013 · Cited by 24
Self-citation
Cited by
Schileo, G., & Grancini, G. (2021) · Journal of Materials Chemistry C · doi:10.1039/d0tc04552g · Cited by 472
Emerging new phase boundary in potassium sodium-niobate based ceramics
Lv, X., Zhu, J., Xiao, D., Zhang, X.-X., & Wu, J. (2020) · Chemical Society Reviews · doi:10.1039/c9cs00432g · Cited by 393
Nano-domains in lead-free piezoceramics: a review
Lv, X., Zhang, X.-X., & Wu, J. (2020) · Journal of Materials Chemistry A · doi:10.1039/d0ta03201h · Cited by 283
Metadata
- Authors
- Koruza, J., Bell, A. J., Frömling, T., Webber, K. G., Wang, K., & Rödel, J.
- Venue
- Journal of Materiomics
- Publisher
- Elsevier BV
- Published
- 2018-03
- Volume
- 4
- Issue
- 1
- Pages
- 13-26
- ISSN
- 2352-8478 (ISSN-L)
- OpenAlex
- W2785317191
- Cited by
- 286
- References
- 59
- FWCI
- 12.47
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.